Kim, Min-Gyun;Kam, Sang-Kyu;Jeon, Yong-Han;Kim, Nam-Jin
Journal of the Korea Safety Management & Science
/
v.21
no.4
/
pp.45-49
/
2019
The basalt fiber is expected to become a trend for industrial fibers as they have better properties of heat-resistant, non-combustion, absorbent, soundproof, moistureproof, lightweight, corrosion resistant, and high strength properties. Also, the fiber is found to be non-toxic and harmless to the human body. Therefore, in this study, we analyzed the chemical and mineral compositions of powdered sludge of basalt produced at seven sites on Jeju Island for the development of fire resistance insulating material for a building. The results showed that the basalt stone sludge is made from only sodium calcium aluminum silicate and ferridioside components unlike the basalt rock.
Proceedings of the Korea Concrete Institute Conference
/
1997.10a
/
pp.777-784
/
1997
This paper is fundamental study to develop ceiling materials, using the properties of Zeolite, stone dust and sludge for the purpose of prevention of environmental pollution and reuse of industrial wastes. According to latin square method, We estimated to the significant level ad optimum level for a significant factor, and investigated to the significant degree to extend each factor for required capacity. Thus, we investigated for required capacity in ceiling material such as, compressive and bending strength, absorptivity and thermal conductivity.
The amounts of waste stone and stone powder sludge that occurred in the quarry and processing plant of s stone plates, have been increased with the development of stone industry. The manufactunng process of 따tificial s stone was studied to reduce the outlet of these wastes and utilIze them as raw materials for architecture, interior decoration and art work. In order to compare the properties of artiflcial stone with those of natural building-stone, the physi$\alpha$II properties of artificial stone such as specific gravity, absorption ratio, elastic wave velocity, compressive s strength, tensile strength, shore hardness, elasticity and Poission's ratio were measured. From the mesaured d data of physical properties, it was found that physical propertIes of artificial stone were controlled by homogeneous m mixing ratio of constituents, molding pressure, and amount of binder. Also, from the thermo-gravimetric analysis, it was found that artIfIcial stone manufactured had a good thermal stability up to $300^{\circ}C$. It was concluded that t the optimum conditions for manufacturing process of artificial stone were $200kg/\textrm{cm}^2$ of molding pressure, 12-15 w weight % of binder amounts.
This paper is concerned chiefly with the method of porous foam manufacture using basalt stone powder sludge. The hydrogen peroxide($H_2O_2$) of bloating agent has lots of problems to manufacture porous lightweight aggregate due to fast reaction rate with cement or calcium hydroxide($Ca(OH)_2$). The $H_2O_2$ injecting method using nozzle for manufacturing porous lightweight aggregate is proposed, in this study. This method is to inject $H_2O_2$ at the pressure of 10 MPa on upper side of slurry mixing materials such as stone powder sludge and quick-lime(CaO) by injector. The specimen was dried in furnace at $100^{\circ}C$ for 1 hour and cured at ambient temperature for 30 days. We analyzed the characteristics including specific gravity and water absorption. The experiments were found that the porous foam has low specific gravity, high water absorption and uniform distribution of porous more than manufactured foam by general bloating methods.
Proceedings of the Korea Concrete Institute Conference
/
1997.10a
/
pp.785-790
/
1997
In domestic, it is not a little results to use natural mineral, stone and sludge as a construction materials. Accordingly, it is required to study for higher application from of resources these materials in its economic and environmental aspects. So, the purpose of this study is to develop the excellent construction materials, a as compare with existing floor materials in material capacity and economic aspects, using natural zeolite, stone dust and sludge. In this viewpoint, this paper investigated to the required capacity such as, compressive strength, bending strength and absorption according to experiment.
Proceedings of the Korea Concrete Institute Conference
/
2001.05a
/
pp.269-274
/
2001
The purpose of this study is to evaluate basic properties of artificial aggregate using concrete sludge according to mixing ratio. Cement, waste phosphogypsum and Powder of blast furnace slag are used with binder of artificial aggregate. Specific gravity, absorption are tested for basic property, and impacting, abrasion and crushing tests are done for characteristics of strength on the aggregate, including comparison with crushed stone. Bry specific gravity was ranged about 1.16 to 1.30 the test result of the aggregates and shape is round In the result of tests, it is concluded that qualities of the aggregates using concrete sludge are slightly lower than crushed stone but it is similiar with sintering artificial lightweight aggregate in high temperature.
Jeong Ji Yong;Choi Sun Mi;Sun Joung, Soo;Choi Se Jin;Lee Seong Yeon;Kim Jin Man
Proceedings of the Korea Concrete Institute Conference
/
2005.11a
/
pp.765-768
/
2005
This study is investigated the strength properties of ALC(Autocalved Lightweight Concrete) using SPS(Stone Powder Sludge), to develop recycling technique of SPS. At a given replacement percent of SPS and addition percent of foam, the results show that its the strength properties are equal or higher than the quartz used in a raw material of ALC, and it is also found that the addition percent of the foam and the strength properties have a certain relation of linear.
This study was carried out to remove the iron and impurities usmg hydrocyclone and HGMS for recycling of sludge from the granite stone cutting and polishing industrγ in the basic of chemi떠1 analysis and minerallogical investigation. This sludge consist of 70.9% $SiO_2$ 13.6% $Al_2O_3$ and It also contained 2.52% of $Fe_2O_7$ and 0.29% of $TiO_2$, as a main impurities to decrease the whiteness. As the result of hydrocyclone experiment, It was very good condition that are 100~150 g/l of sludge amount, 2.0~ 2.5 mm of underflow nozzle size, and 1.2~1.6 kg/$\textrm{cm}^2$ of pressure for 85% sludge product with the $-37{\mu}\textrm{m}$ size. $Fe_2O_3$ and $TiO_2$, contents by treatment of HGMS were decreased with 0.65% and 0.07% each at 10,000 gauss of magnetic field strength, and addih$\upsilon$n of Sodium tripolyphosphate as a dispersant was effected to get low grade F Fe,Ol and TiO, concentrate. PhYSIcal properties of this stone sludge product were showed 58.5% of whiteness, 1 13.4% of firing shrinkage and 3.0812 $\textrm{m}^2$/g of specific surface area.
Kim, Chan-Kee;Bak, Gueon-Jun;Cho, Won-Beom;Lee, Jong-Cheon
Journal of the Korean Geosynthetics Society
/
v.12
no.3
/
pp.55-64
/
2013
In this study, a series of the isotropic compression-expansion tests and the Undrained triaxial tests were performed on low-plastic silt of Pocheon stone sludge. Using the tests results the characteristic of the parameters of Lade's single hardening constitutive model were investigated. We also observed that predicted values from the Lade's single hardening constitutive model were well consistent with the observed data. In experimental results the deviator stress showed the work hardening behaviour after reaching its yield stress. Therefore practically useful failure criterion for low-plastic silt were required. The stress-strain behavior predicted by 11 soil parameters are compared with the results obtained 9 parameters by correlation between h and ${\eta}_1$ and constant ${\alpha}$. They are poor matched each other.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.