석조문화재 오염물 제거 방안의 표준화 수립 및 가치정립 I -설문조사의 통계를 중심으로- (Formation of Standardization and Valuation of Decontamination for Stone Culture Heritage I -Based on the Questionnaire-)

  • 김진형;정용재;김사덕
    • 보존과학연구
    • /
    • 통권28호
    • /
    • pp.169-182
    • /
    • 2007
  • It is very difficult to attain stable and satisfactory result satisfaction from newly developed materials and methodologies for conservation of cultural properties. In order for an effective conservation method, it is necessary that the manual for application of the proper materials and its methodology should be set up. However, stone conservation value must be established in advance of the manual, because the philosophical concepts and the technical methodology are not standardized. In this study, therefore, the conservators' opinion about the conservation for stone artifacts was collected. The opinions were based on the questionnaire about cleaning of surface contamination on masonry, and hereafter those will be referred to the conservation method about stone artifacts.

  • PDF

논산 관촉사 석등의 훼손도 진단 및 기원암의 성인적 해석 (Deterioration Diagnosis and Petrogenesis for Rock Properties of the Stone Lantern in the Gwanchoksa Temple, Nonsan, Korea)

  • 이명성;이정은;표수희;송치영;이찬희
    • 보존과학회지
    • /
    • 제17권
    • /
    • pp.5-18
    • /
    • 2005
  • 논산 관촉사 석등은 암회색을 띠는 화강섬록암으로 구성되어 있다 이 석등은 전체적으로 S자형으로 뒤틀려 있으며 상대석과 1층 옥개석 하부에는 표면박리가 발생하여 석재의 표면이 심하게 부서지고 있다. 이차적 오염도 심각하여 . 부재사이에 삽입된 철편의 산화에 의한 변색과 강수의 유동흔적을 따라 나타나는 회백색 및 암흑색의 침전물이 산재한다. 석등의 표면에는 지의류와 선태류가 피복되어 있어 다양한 형태의 생물학적 훼손을 저감하기 위한 보존처리가 요구된다 또한 석등의 구조적 안정과 표면마모 및 기계적 풍화를 저지하기 위해 환경변화에 대한 장기적인 모니터 링과 함께 풍화요소를 저감할 수 있는 보존방법을 강구해야 할 것이다. 이 석등의 부재는 산출상태와 암석학적 및 지구화학적 특성이 주변의 기반암과 동일한 성인을 갖는 것으로 보아 주변의 석재를 이용하여 석등을 제작하였을 가능성이 높다.

  • PDF

석조문화재 디지털복원 및 구조안정성 평가를 위한 3차원 영상분석: 마곡사오층석탑 (3D Image Analysis for Digital Restoration and Structural Stability Evaluation of Stone Cultural Heritage: Five-storied Magoksa Temple Stone Pagoda)

  • 조영훈;이찬희
    • 보존과학회지
    • /
    • 제25권2호
    • /
    • pp.115-130
    • /
    • 2009
  • 이 연구에서는 공주 마곡사오층석탑을 대상으로 3차원 스캐닝 시스템을 적용하여 디지털 복원 및 구조안정성평가를 수행하였다. 이를 위해 16방향에서 측정한 레이저 스캐닝 데이터를 7단계의 데이터처리 프로그램 과정에 활용하여 석탑의 디지털복원을 완성했다. 디지털복원 결과, 전반적으로 층별 부재의 높이와 폭은 방위에 따라 약간의 차이가 있었고, 각 층별 옥개석의 폭은 매우 큰 차이를 나타냈다. 탑신의 층별 폭은 1층에서 5층으로 갈수록 줄어들지만 체감비율은 일정하지 않았다. 구조해석을 위한 3차원 영상분석 결과, 1층 탑신이 남동쪽으로 기울어진 것을 제외하고는 2층 탑신부터 상륜부까지 모두 북서쪽으로 변위가 발생하였다. 이와 같은 3차원 영상분석이 석조문화재에 지속적으로 사용되기 위해서는 측정방법의 정량화가 필요하며, 훼손도 정량평가와 같은 다양한 분야에도 적용되어야 할 것이다.

  • PDF

석조문화재의 보존처리 후 표면상태 모니터링 기술 연구 (Monitoring Technology on the Surface Condition after Conservation Treatment of Stone Cultural Heritage)

  • 박성미;전유근;이명성
    • 보존과학연구
    • /
    • 통권34호
    • /
    • pp.32-48
    • /
    • 2013
  • 이 연구는 석조문화재의 보존관리매뉴얼 구축을 위해 과거 보존처리가 이루어진 문화재를 대상으로 표면상태 및 물성변화를 객관적이고 효율적으로 모니터링 하는 기법을 개발하여 적용성을 평가한 것이다. 사진 촬영과 그리드를 이용한 훼손지도 작성과 테이프 접착 테스트는 석조문화재의 표면상태 변화와 훼손 위치를 파악하고 입상분해 정도를 정성적으로 평가하는데 매우 유용한 기법으로 확인되었다. 또한 디지털 휴대용 현미경 관찰과 초음파탐사는 광물입자의 풍화 및 결합상태, 균열 간격 등을 모니터링하고 보존처리 전과 후의 표면물성 변화를 평가하는데 매우 효과적인 평가기법으로 판단된다. 이 방법들은 간단한 메뉴얼화와 기술교육을 통해 문화재 관리 실무자들이 현장에서 간편하게 이용할 수 있으며, 보존처리 후 표면 변화가 관찰되는 3년마다 정기적으로 모니터링을 실시함으로써 석조문화재의 장기적이고 체계적인 보존관리기법으로 활용될 수 있을 것이다.

  • PDF

서울 원각사지 십층석탑의 표면오염물 형성과정 (Forming Process of Surface Contaminants on Ten-story Stone Pagoda of Wongaksa Temple, Seoul)

  • 전유근;이명성;김유리;이선명;임보아
    • 보존과학회지
    • /
    • 제32권3호
    • /
    • pp.365-375
    • /
    • 2016
  • 이 논문에서는 원각사지 십층석탑 표면에 발생한 오염물의 형성과정을 연구하였다. 연구결과, 흑색오염물은 석탑의 화학적인 풍화로 인해 석고가 일차적으로 형성되고 공기 중의 탄소화합물이 석탑표면에 고착되면서 생성된 흑연에 의해 발생한 것으로 판단되며, 발생시기는 1933년 이전으로 확인되었다. 백색오염물은 보호각 상부 마감재의 노후화 및 구조물의 훼손으로 발생한 방해석이 석탑표면에 재결정화 되면서 형성되었으며, 발생시기는 보호각이 설치된 1998년에서 2013년 사이에 발생한 것으로 판단된다. 원각사지 십층석탑의 장기적인 보존을 위해서는 보호각 상부에 형성된 오염물의 제거, 구조물의 방청처리 및 지속적인 모니터링이 요구된다.

Morphological Characteristics of Endocarp in Relation to Seed Dormancy of 18 Rubus Species in Korea

  • Choi, Go Eun;Jeong, Mi jin;Lee, Hayan;Ko, Chang Duck;Park, Jae In;Ghimire, Balkrishna
    • 농업생명과학연구
    • /
    • 제51권6호
    • /
    • pp.15-22
    • /
    • 2017
  • The microstructure observation of seed surface structure is needed for protocols of breaking dormancy of seeds with physical dormancy. The seeds of Rubus species are surrounded by a thick, hard endocarp; together, the seed and endocarp make up the stone. We evaluate stone characteristics of 18 species of Rubus through optical microscopic observation, and correlate different stone characteristics with endocarp thickness. As a result of stone size comparison, Rubus species were classified as big stones group including R. parvifolius and R. idaeus, small stones group including R. longisepalus var. longisepalus, R. corchorifolius and R. hirsutus, and middle stones group including rest of the species. The result of this study revealed that stone size and the endocarp thickness in Rubus species was various characteristics in each species. Furthermore stone size and stone weight were also well correlated endocarp thickness and result indicated that heavy stones had harder endocarp than lighter one. Thus from the result of this study it can be presumed that only one stone characteristic approach may be sufficient to estimate other characteristics in Rubus.

석조문화재 보존처리제의 현황 조사 - '접착충전제와 발수·강화제'를 중심으로- (Research on present statue of conservation materials in the stone cultural heritage - Focus on adhesive, filler, repellent, consolidant materials -)

  • 송치영;한민수;이장존;전병규
    • 보존과학연구
    • /
    • 통권29호
    • /
    • pp.163-182
    • /
    • 2008
  • Precise scientific-diagnosis for preserving stone cultural properties has been well-advanced, but research on proper methods for conservation, restoration and repair is still in early stage. Accordingly it is quite difficult to establish conservation treatment methods compatible to unique characteristics and environments of each cultural property. We tried to select most compatible conservation materials through thorough assessment of conservation materials in current use. This research is focused on conservation and restoration materials except cleaner, which are used as adhesive, filler, repellent and consolidant. Conservation treatments for stone cultural properties were first tested in 1960's and have been carried out by various methods under relevant organizations and conservation treatment companies since. We investigated present status of conservation materials being used for cultural properties. Based on these data, we will look through types and properties of the conservation materials to figure out existing problems. Among many kinds of resins, the ratio of conservation materials used in cultural properties is very low. Therefore, new conservation materials equipped with proved long-term stability should be developed as soon as possible.

  • PDF

부여 무량사오층석탑의 종합 풍화훼손도 평가 (Synthetic deterioration assessment of the five storied stone pagoda in the Mooryangsa temple, Buyeo, Korea)

  • 송치영;이미혜;조영훈;이찬희
    • 보존과학연구
    • /
    • 통권27호
    • /
    • pp.103-128
    • /
    • 2006
  • Rock properties of the five storied stone pagoda in the Mooryangsa temple are consist mainly in medium grained biotite granite with partly pegmatite veinlet. A part of the foundation stone is substituted in identical rock properties of the pagoda. The upper part of the pagoda is used purples and stone, gray shale and granodiorite. The most serious problem of the pagoda is structual instability from centered subsidence of the ground in northwestern direction remarkably. In southern view, the upper part of the pagoda also is slanted a little in right, it will need reinforcement by engineering method for structual stability of the stone pagoda. Weathering states of the stone pagoda are affected results of natural and artifical factors due to the surface-exfoliation, fine-fissure, crack, falling offs. On the rock surface of the pagoda, ferro-manganese hydroxide compounds are coated along the rainpathway. Also, bryophyte range concentration spreads raindrops face of roof rock properties, which areadd biological weathering effects. For the synthetic evaluation of the deterioration state, we make detailed surface weathering maps, it will be contribute to investigation for future conservation schemes.

  • PDF

감은사지(感恩寺址) 서탑출토(西塔出土) 보단측면석(步段側面石)의 보존처리(保存處理) (Conservation Treatment of Stairway-side Stone Panels Taken Out from West Pagoda of Gameunsa-site)

  • 김종우;정태화;정수연
    • 박물관보존과학
    • /
    • 제9권
    • /
    • pp.59-66
    • /
    • 2008
  • 국립경주박물관 옥외전시장에 전시되고 있었던 보단측면석은 과거 접합·복원부분의 풍화로 인하여 박리 및 박락이 진행되었다. 따라서 풍화된 암석에 대한 편광현미경 관찰 및 분석을 통한 암석 내의 팽윤성광물의 확인, Schmidt Hammer 반발경도 측정 및 Karsten Tube를 사용하여 모세관물흡수율을 조사하였다.

석조문화재 균열부 보존처리 충전제의 현황과 임상실험 고찰 - 활석을 혼합 한 충전제의 표면변화를 중심으로 - (A Study of Stone Cultural Heritage on Filler Status and Clinical Trials of Conservation Treatment in Cracks - Focusing on the Change in Surface of the Filler by Mixing the Talc -)

  • 이태종;오정현;김사덕;이장존
    • 보존과학회지
    • /
    • 제30권4호
    • /
    • pp.383-393
    • /
    • 2014
  • 석조문화재 균열부분과 표면 마무리를 위한 보존처리는 현재까지 에폭시수지에 다양한 충전제를 혼합하여 사용하게 된다. 장기적 보존을 위해 이와 같은 보존처리는 필요하다. 하지만 보존처리 된 54건에 대한 현장조사와 임상실험 결과 충전제 중 활석이 포함된 경우 표면변색과 균열 등 재 손상이 확인되었다. 현장조사는 수리보고서와 처리 담당자 인터뷰, 현미경조사, 현장에서 수습한 처리 시편의 ICP 분석을 병행하여 활석 사용여부를 확인하였다. 임상실험은 현장조사에서 확인된 활석에 의한 영향평가를 위해 촉진내후성시험 후 색차와 초음파측정을 실시하였으며 그 결과 활석이 포함된 시편에서의 물성저하가 두드러졌다. 따라서 향후 균열부분 보존처리는 활석의 사용은 자제하고 동질 석분만을 충전제로 선택하여 처리할 것을 제안한다.