Forming Process of Surface Contaminants on Ten-story Stone Pagoda of Wongaksa Temple, Seoul  

Chun, Yu Gun (Conservation Science Division, National Research Institute of Cultural Heritage)
Lee, Myeong Seong (Conservation Science Division, National Research Institute of Cultural Heritage)
Kim, Yuri (Conservation Science Division, National Research Institute of Cultural Heritage)
Lee, Sun Myung (Conservation Science Division, National Research Institute of Cultural Heritage)
Lim, Bo A (Conservation Science Division, National Research Institute of Cultural Heritage)
Publication Information
Journal of Conservation Science / v.32, no.3, 2016 , pp. 365-375 More about this Journal
Abstract
This study was interpreted the forming process of surface contaminants on ten-story stone pagoda of Wongaksa temple, Seoul. Results of research, we estimated that black contaminants were formed by graphite stuck carbon in air pollution substance after that gypsum was generated by chemical weathering on stone pagoda. White contaminants were built by recrystallization of calcite that were made by decomposition of finishing materials and structure on the stone surface. To preserve a long-term of stone pagoda in Wongaksa temple, there were required that continuous monitoring, anticorrosion treatment and contaminants cleaning of protective facilities.
Keywords
Wongaksa temple; Stone pagoda; Surface contaminants; Protective facilities; Monitoring;
Citations & Related Records
Times Cited By KSCI : 7  (Citation Analysis)
연도 인용수 순위
1 Chosun Historical Remains Illustration, 1933, Photographs of ten-story stone pagoda of Wongaksa temple.
2 Chun, Y.G., Lee, C.H., Jo, S.N., Jo, Y.H., Park, G.J. and Yang, P.S., 2008, Measurement of crack depth and weathering degree using ultrasonic velocity and deterioration evaluation of the Unhyungung stone water container. Journal of Conservation Science, 24(1), 1-11. (in Korean with English abstract)
3 Chun, Y.G., Lee, J.M., Lee, M.H., Park, S.M., Lee, S.M. and Lee, M.S., 2014, Long term monitoring of deterioration condition for the rock-carved Buddha triad in Seosan, Korea. Journal of Conservation Science, 30(4), 439-446. (in Korean with English abstract)   DOI
4 Chun, Y.G., Lee, M.S., Lee, J.M. and Lee, J.J., 2013, Conservation treatment and deterioration evaluation of the Namwon Singyeri Maaeyeoraejwasang (Rock-carved seated Buddha statue), Korea. Journal of Conservation Science, 29(4), 321-332. (in Korean with English abstract)   DOI
5 Cultural Heritage Administration, 2016, Detail description of ten-story stone pagoda of Wongaksa temple. http://www.cha.go.kr/
6 Davidge, R.W., 1981, Cracking at grain boundaries in polycrystalline brittle materials. Acta Metal., 29, 1696-1702.
7 Jo, Y.H. and Lee, C.H., 2011, Making method of deterioration map and evaluation techniques of surface and threedimensional deterioration rate for stone cultural heritage. Journal of Conservation Science, 27(3), 251-260. (in Korean with English abstract)
8 Do, J.Y. and Kim, J.H., 2006, The studies of surface contaminants and cleaning method 10th-storied stone pagoda in Gyeongcheonsa temple. National Research Institute of Cultural Heritage, 217-242. (in Korean)
9 Everett, D.H., 1961, The thermodynamics of frost damage to porous solids. Transactions of the Faraday Society, 57, 1541-1551.   DOI
10 Gang, S.H., 1994, Amazing sculpture of Tapgol pagoda! : History of Wongaksa temple. National Palace Museum of Korea, 131-132. (in Korean)
11 Johnson, B., Gangi, A. and Handin, J., 1978, Thermal cracking of rock subjected to slow uniform temperature changes. 19th US Symp. on Rock Mech., 259-267.
12 Lee, C.H., Jo, Y.H. and Chun, Y.G., 2009, Establishment of ultrasonic measurement and correlations of direct-indirect method for weathering evaluation of stone cultural heritage. Journal of Conservation Science, 25(3), 233-244. (in Korean with English abstract)
13 Lee, C.H., Yi, J.E., Shin, E.J. and Kim, S.D., 2008, Deterioration degree and petrological characteristics of the 10th-storied stone pagoda in Gyeongcheonsa temple, Korea. Journal of the Geological Society of Korea, 44, 765-779. (in Korean with English abstract)
14 Lee, S.W., 1994, Amazing sculpture of Tapgol pagoda! : Geological study about weathering of 10th-storied stone pagoda in Wongaksa temple. National Palace Museum of Korea, 125-128. (in Korean)
15 Yoo, J.H., Lee, C.H. and Chun, Y.G., 2014, Material characteristics, deterioration evaluation and crack depth estimation for Mulgyeseowon stele in Changnyeong, Korea. Journal of Conservation Science, 30(4), 427-438. (in Korean with English abstract)   DOI
16 Lee, S.M., Lee, M.S., Chun, Y.G., Lee, J.M. and Morii, M., 2012, Weathering characteristics according to seawater immersion of the Magai Wareiishi Jizo (Buddhist statue carved on rock surface) in Hiroshima, Japan. Journal of Conservation Science, 28(4), 329-341. (in Korean with English abstract)   DOI
17 Schulson, E.M., 1998, Ice damage to concrete. CRREL, Special report, 98-106.
18 Sim, D.S., 1994, Amazing sculpture of Tapgol pagoda! : A survey of 10th-storied stone pagoda in Wongaksa temple. National Palace Museum of Korea, 80-94. (in Korean)
19 Tharp, T.M., 1987, Conditions for crack propagation by frost wedging. Geological Society of America Bulletin, 99, 94-102.   DOI