• 제목/요약/키워드: Spinel structure

검색결과 289건 처리시간 0.033초

카올리나이트의 상전이반응 과정 연구 (An Investigation of the Transformation Sequence from Kaolinite to Mullite)

  • 이수정;김윤중;문희수
    • 한국광물학회지
    • /
    • 제11권1호
    • /
    • pp.32-44
    • /
    • 1998
  • The transformation sequence of kaolinite to mullite is examined with new electron diffraction data obtained mainly by an energy filtering transmission electron microscope. Kaolinite is transformed finally into mullite and cristobalite through several steps of continuous reactions by heating, which result in metakaolinite, microcrystalline spinel-type phase and amorphous silica. Metakaolinite maintains a short-range order in its structure ven at $920^{\circ}C$. Spinel phase results from a topotactictransformation of metakaolinite apart from the breakdown of metakaolinite structure. the first strong exothermic peak on DTA curve is mainly due to the extraction of amorphous silica from metakaolinite and the gradual nucleation of mullite. Metakaolinite decomposes around$ 940^{\circ}C$ to mullite that doesn't show a clear crystallographic relationship to the parent metakaolinite structure. However, spinel phase produced previously is maintained. The initially formed spinel and mullite phases are suggested to be Al-rich, but progressively gain Si in their structures at higher temperatures. Spinel phase decomposes completely through a second weak exothermic reaction promoting the growth of mullite, and crystallization of amorphous silica to cristobalite.

  • PDF

스피넬계 Mn-Zn 페라이트의 망간이온이 미치는 영향 (Behavior of Mn Ions in Spinel-type Mn-Zn-Fe Oxide System)

  • 권오흥
    • 자원리싸이클링
    • /
    • 제9권5호
    • /
    • pp.11-15
    • /
    • 2000
  • The sample made of $Mn_3O_4$ indicated an excellent frequency dependency for intial permeability and core loss. Moreover the homogeneity of cation configuration in he spinel structure was confirmed by X-ray diffraction analysis. The result of homogeneity of the spinel structural coincided with the analytical results of temperature dependence of magnetization. Furthermore, the influence of manganese oxide as starting material, on homogeneity of spinel structure was examined by using thermogravimetry-differential thermal analysis. It may be concluded that the reaction between $Mn_3O_4$ and Fe-Zn oxide mixture proceeds at fist in all combination of manganese oxide and oxie mixture, and then Mn-Zn-Fe spinel was formed.

  • PDF

Structural, Magnetic, and Optical Studies on Normal to Inverse Spinel Phase Transition in FexCo3-xO4 Thin Films

  • Kim, Kwang-Joo;Kim, Hee-Kyung;Park, Young-Ran;Ahn, Geun-Young;Kim, Chul-Sung;Park, Jae-Yun
    • 한국자기학회지
    • /
    • 제15권2호
    • /
    • pp.96-99
    • /
    • 2005
  • Phase transition from normal- to inverse-spinel structure has been observed for $Fe_xCo_{3-x}O_4$ thin films as the Fe composition (x) increases from 0 to 2. The samples were fabricated as thin films by sol-gel method on Si(100) substrates. X-ray diffraction measurements revealed a coexistence of two phases, normal and inverse spinel, for $0.76{\le}x{\le}0.93$. The normal-spinel phase is dominant for $x{\le}0.55$ while the inverse-spinel phase for $x{\ge}l.22$. The cubic lattice constant of the inverse-spinel phase is larger than that of the normal-spinel phase. For both phases the lattice constant increases with increasing x. X-ray photoelectron spectroscopy measurements revealed that both $Fe^{2+}$ and $Fe^{3+}$ ions exist with similar strength in the x=0.93 sample. Conversion electron $M\ddot{o}ssbauer$ spectra measured on the same sample showed that $Fe^{2+}$ ions prefer the octahedral $Co^{3+}$ sites, indicating the formation of the inverse-spinel phase. Analysis on the measured optical absorption spectra for the samples by spectroscopic ellipsometry indicates the dominance of the normal spinel phase for low x in which $Fe^{3+}$ ions tend to substitute the octahedral sites.

NiO-ZnO-$Fe_2O_3$-$TiO_2$-$SnO_2$ 계 Spinel 고용체의 생성과 발색에 관한 연구 (Formation and Color of the Spinel Solid Solution in NiO-ZnO-$Fe_2O_3$-$TiO_2$-$SnO_2$ System)

  • 이응상;이진성
    • 한국세라믹학회지
    • /
    • 제28권4호
    • /
    • pp.305-314
    • /
    • 1991
  • This study was conducted to research the formation and the color development of NiO-ZnO-Fe2O3-TiO2-SnO2 system for the purpose of synthesizing the spinel pigments which are stable at high temperature. After preparing ZnO-Fe2O3 as a basic composition, {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.Fe2O3 system, {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.TiO2 system, and {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.SnO2 system were prepared with {{{{ chi }}=0, 0.2, 0.5, 0.7, 1 mole ratio respectively. The manufacturing was carried out at 128$0^{\circ}C$ for 30 minutes. The reflectance measurement and the X-ray analysis of these specimens were carried out and the results were summarized as follows. 1. In the specimens which included NiO, it was difficult for the spinel structure to be formed. 2. As increasing the contents of NiO and Fe2O3, all the groups which were yellow or green colored changed to brown. 3. NiO-ZnO-Fe2O3 system and NiO-ZnO-TiO2 system formed the spinel structure and the illmenite structure appeared in NiO-TiO2 system.

  • PDF

An Overview of Chemically/Surface Modified Cubic Spinel LiMn2O4 Electrode for Rechargeable Lithium Batteries

  • Jung, Kyu-Nam;Pyun, Su-Il
    • 전기화학회지
    • /
    • 제9권4호
    • /
    • pp.158-169
    • /
    • 2006
  • The present article is concerned with the overview of the chemically/surface modified cubic spinel $LiMn_2O_4$ as a cathode electrode far lithium ion secondary batteries. Firstly, this article presented a comprehensive survey of the cubic spinel structure and its correlated electrochemical behaviour of $LiMn_2O_4$. Subsequently, the various kinds of the chemically/surface modified $LiMn_2O_4$ and their electrochemical characteristics were discussed in detail. Finally, this article reviewed our recent research works published on the mechanism of lithium transport through the chemically/surface modified $Li_{1-\delta}Mn_2O_4$ electrode from the kinetic view point by the analyses of the experimental potentiostatic current transients and ac-impedance spectra.

바리스터의 전기적 특성 (The Electrical Characteristics of Varistor.)

  • 홍경진;장동환;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 센서 박막재료
    • /
    • pp.52-56
    • /
    • 2001
  • The Breakdown electric field of ZnO semiconductor devices in voltage-current characteristics was increased by increasing of additive materials. The specimen that has not additive materials was not formed spinel structure. The critical voltage that has not spinel structure was 235[V]. When the additive materials has 0.5 and 2[mol%], the Breakdown electric field was 840 and 758[V] in each additive materials. The Breakdown electric field of varistors as a factor of voltage and current was increased by addition of oxide antimony. The varistors that has oxide antimony was linearly increased in low electric field.

  • PDF

ZnO 소자의 비직선 특성 (The Non-Linear Characteristics of ZnO Devices.)

  • 홍경진;전경남;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 센서 박막재료
    • /
    • pp.43-46
    • /
    • 2001
  • The ZnO devices using semiconductor properties, to include $MnO_2$, $Y_2O_3$ and other material, was fabricated by $Sb_2O_3$ mol ratio from 1 to 4 [mol%]. The non-linearity factor was calculated by setting current to be $1[mA/cm^2]$ and $10[mA/cm^2]$. The spinel structure was fonned by $Sb_2O_3$ addition and it was depressed the ZnO grain formation. The grain growing was controlled by spinel structure that has improved the non-linearity factors. The breakdown voltage characteristics of semiconductor devices to increase with $Sb_2O_3$ was increased in voltage-current. The non-linearity value of ZnO semiconductor devices was 45 over.

  • PDF

Li-Mn계 산화물의 치환 및 첨가에 따른 물성 변화 (Properties Changing depends on Substituents or Dopants of Li-Mn oxide material)

  • 이대진;지미정;최병현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.289-289
    • /
    • 2007
  • Spinel structured $LiMn_2O_4$ is more economic and environmental friendly to be used as commercial active material for secondary battery compared to Co-oxide material active material, but spinel structure of $LiMn_2O_4$ is unstable and its capacitance decreases with increase of cycle. Therefore, the purpose of our sturdy is to improve the stability of $LiMn_2O_4$ spinel structure and increase its capacitance by using substituents or dopants. $LiMn_2O_4$ powder was synthesized by charging substituents or dopants mole fractions, and temperatures. Crystal state, structure and specific surface area of the synthesized powder were measured and also characteried electrochemically by measuring its impedance, charge-discharge capacitance and etc.

  • PDF

$ZnO-Fe_2O_3-TiO_2-SnO_2$계 Spinel 안료 고용체의 생성과 발색 (Formation and Color of the Spinel Solid-Solution in $ZnO-Fe_2O_3-TiO_2-SnO_2$ System)

  • 박철원;이진성;이웅재
    • 한국세라믹학회지
    • /
    • 제31권2호
    • /
    • pp.213-219
    • /
    • 1994
  • The formations of spinel and colors of ZnO-Fe2O3-TiO2-SnO2 system have been researched on the basis of ZnO-Fe2O3 system. Specimens were prepared by substituting Fe3+, with Ti4+ or Sn4+ when mole ratios between Fe3+ and Ti4+ or between Fe3+ and Sn4+ were 0.2 mole. The reflectance measurement and X-ray diffraction analysis of the formation of spinel and the colors of there specimens were carried out. ZnO-Fe2O3 system in which Fe2O3 was substituted with SnO2 and TiO2 was formed the spinel structure of 2ZnO.TiO2, 2ZnO.SnO2, ZnO.Fe2O3. The stable stains which were colored with yellow and brown could be manufactured.

  • PDF

스피넬상 마그네타이트의 수소환원에 의한 활성화 (Activation of Spinel Phase Magnetite by Hydrogen Reduction)

  • 류대선;이동석;이풍헌;김순태
    • 한국세라믹학회지
    • /
    • 제37권6호
    • /
    • pp.559-563
    • /
    • 2000
  • To decompose carbon dioxide, magnetite was synthesized with 0.2M-FeSO4$.$7H2O and 0.5 M-NaOH by coprecipitation. The deoxidized magnetite was prepared from the magnetite by hydrogen reduction for 1, 1.5, 2 hr. The degree of hydrogen reduction and the decomposition rate of carbon dioxide were investigated with hydrogen reduction time. The crystal structure of the magnetite was identified spinel structute by the X-ray powder diffractions. After magnetite was reduced by hydrogen, magnetite reduced by hydrogen become new phae(${\alpha}$-Fe2O3, ${\alpha}$-Fe) and spinel type simultaneously. After decomposing of carbon dioxide at 350$^{\circ}C$, new phse(${\alpha}$-Fe2O3, ${\alpha}$-Fe) were removed and the spinel type only existed. The specific surface area of the synthesized magnetite was 46.69㎡/g. With the increase of the hydrogen reduction time, the grain size, the hydrogen reduction degree and the decomposition rate of carbon dioxide was increased.

  • PDF