흑연과 지르콘의 상대적 함량에 따른 마찰재의 고온 마찰 및 마모특성 (High temperature Friction and Wear of Friction Material; The Effect of the Relative Amount of Graphite and Zirconium Silicate (ZrSiO$_4$))

  • 김성진;장호
    • Tribology and Lubricants
    • /
    • 제16권5호
    • /
    • pp.365-372
    • /
    • 2000
  • Tribological behavior of novolac resin-based friction materials with three different relative amounts of graphite and zirconium silicate was investigated by using a pad-on-disk type friction tester. The goal of this paper is to examine the effects of the relative amount of a lubricant and an abrasive in the automotive friction material on friction and wear characteristics at elevated temperature. Friction and wear of friction materials were affected by the existence of transfer film(3$\^$rd/ body layer) at friction interface and the composition of friction material, especially lubricant amount. The friction material with higher content of graphite indicated homogenized and durable transfer film, and resulted in stable friction coefficient regardless of the increase in friction heat. The experimental result also showed that the higher concentration of ZrSiO$_4$ in friction material aggravated friction stability and wear resistance due to the higher friction heat generated at fiction interface during high temperature friction test.

수중환경에서 Fe계 벌크 비정질 합금의 트라이볼로지적 거동 (Tribological Behavior of Fe-based Bulk Amorphous Alloy in a Distilled Water Environment)

  • 장범택;이승훈
    • Tribology and Lubricants
    • /
    • 제30권5호
    • /
    • pp.295-302
    • /
    • 2014
  • The tribological behavior of an Fe-based bulk amorphous alloy while sliding against a AISI 304 disc is investigated using a unidirectional pin-on-disc type tribometer in dry and distilled water environments. The rod-shaped bulk pins are fabricated by suction casting. The crystallinities of the bulk amorphous alloys before and after the friction tests are determined by X-ray diffraction. The friction coefficient and specific wear rate of the amorphous pin in the water environment are found to be twice and thrice as much as in the dry environment at a low applied pressure, respectively. However, at a higher pressure, the friction coefficient and specific wear rate are 0.4 and 1.02 mg/(Nm/s), respectively, in the water environment. A microstructure analysis shows that the worn surface of the alloy is characterized by delamination from the smooth friction surface, and thus delamination is the main wear mechanism during the friction test in dry sliding environment. In contrast, brittle fracture morphologies are apparent on the friction surface formed in distilled water environment. For the sample tested at a lower sliding speed, the XPS data from the oxide layer are similar to those of the pure element with weak suboxide peaks. For higher sliding speeds, all the main sharp peaks representing the core level binding energies are shifted to the oxide region.

탄소 섬유 복합재의 마찰 및 마모 특성에 미치는 속도 효과 (Effect of sliding velocity on the wear and friction characteristics of a carbon fiber composites)

  • 고성위;양병춘
    • 수산해양기술연구
    • /
    • 제40권4호
    • /
    • pp.337-343
    • /
    • 2004
  • 탄소 섬유강화 에폭시기지 복합재의 경면 가공한 스테인레스 강 상대재와 마찰과 마모에 바탕을 둔 연구에서 다음과 같은 결론을 얻었다. (1) 일방향 탄소섬유 강화 복합재의 마모 거동에 미치는 미끄럼 방향의 효과는 다르며 작용하는 마모 메커니즘의 형태에 의존한다. (2) 상온에서 경면 가공한 스테인리스 스틸에 대하여 미끄럼이 일어나면 AP 방향에서 높은 마모 저항과 낮은 마찰계수가 관찰되었다. (3) 복합재의 비마모율은 미끄럼 속도가 증가하면 N방향과 P방향에서는 감소하는 경향을 보이며, AP 방향에서는 증가하다가 감소한다. 이것은 마모 메카니즘의 영향으로 속도가 증가하면 마모 이착막의 생성이 빨라져 이착막 속의 탄소섬유가 윤활제의 역할을 하기 때문이다. (4) 복합재의 마찰계수는 미끄럼 속도가 증가하면 3방향 모두 증가하다가 일정한 값에 수렴하면 N방향이 가장 크며, P방향과 AP방향 순이다. 이는 N방향에서 마찰초반에 발생한 섬유의 쟁기질에 의한 상대재 표면의 손상과 돌기변형에 따른 것이며, AP방향의 마찰계수가 가장 낮다.

플라즈마 전해산화법에 의해 형성된 알루미늄 합금의 양극산화피막 내마모 특성에 관한 연구 (A Study on the Wear Resistance Characteristics of Anodic Oxide Films Formed on Aluminium alloy using a Plasma Electrolytic Oxidation)

  • 정우철;진연호;최진주;양재교
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.381-386
    • /
    • 2018
  • In this study, plasma electrolytic oxidation (PEO) method was used to from anodic oxide films on Al alloy and their resistance and morphological characteristics were investigated as a function of film formation voltage and treatment time. Cross-sectional morphology and composition of the PEO films were analyzed by SEM (Scanning Electron Microscopy) and EDS (Energy Dispersive Spectroscopy). The PEO films showed increased surface roughness and thickness with of film formation voltage and treatment time. The wear resistance was found to be the best for the PEO film formed for 5 min at 500V which is attributed to be denser structure relatively and lower surface roughness.

점토 결합 SiC 소결체의 마찰 마모 특성 (Tribological Properties of Clay Bonded SiC)

  • 한상준;이경희;이재한;김홍기
    • 한국세라믹학회지
    • /
    • 제32권9호
    • /
    • pp.1027-1032
    • /
    • 1995
  • SiC had been widely applied for mechanical sealing as a sealing material. SiC sintering is commonly made of reaction sintering, presureless sintering, and hot isostatic pressing (HIP) sintering. In this investigation, however, clay bonded sintering was used to avoide any complications of the special sintering methods as mentioned above. In order to prevent harmful SiC oxidation in the clay bonded sintering, clay and frit were used to form the SiC oxidation protecting layer and graphite was added to provide high solid lubricity. As a result, the material with 6% clay (clay 5.4% and frit 0.6%) and 2~4% graphite (45 mesh) sintered at 140$0^{\circ}C$ for 3 hours, showed the following physical properties; porosity 6%, static friction coefficient 0.15, kinematic coefficient 0.1,. and specific wear rate 4.8$\times$10-8 $\textrm{mm}^2$kgf-1. On the other hand, the flexural strength was 900kgf/$\textrm{cm}^2$. This tribological characteristic properties were similar to those of the reaction sintered SiC except the flexural strength.

  • PDF

Tribological Properties of Ti(C,N)-based Cermet after Hot Isostatic Pressing at High Nitrogen Pressure

  • Xiong, Wei-hao;Zheng, Li-yun;Yan, Xian-mei
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.663-664
    • /
    • 2006
  • Sintered Ti(C,N)-based cermets were treated with hot isostatic pressing (HIP) at different nitrogen pressures. The tribological properties of the treated cermets have been evaluated. The results show that a hard near-surface area rich in TiN formed after HIP treatment. The cermets treated at higher pressure had a relatively lower friction coefficient and specific wear rate. In all cases the microhardness of treated cermets is higher than that without HIP natridation. The wear mechanisms of cermets were hard particle flaking-off and ploughing. It was also found that the HIP natridation is well-suited for improving the tribological properties of cermets.

  • PDF

Tribology of Clay Bonded Silicon Carbide

  • Lee, Kyunghee;Kim, Honggi
    • The Korean Journal of Ceramics
    • /
    • 제2권4호
    • /
    • pp.226-230
    • /
    • 1996
  • A small amount of fine particle graphite was added to $\alpha$-SiC and $\beta$-SiC having certain particle distributions, and they were mixed clay and frit. After forming, they were sintered at 140$0^{\circ}C$ for 3 hours. Tribological properties of sintered $\alpha$-SiC-$\beta$-SiC-graphite-clay (frit) system showed that kinetic friction coefficient was 0.108, specific wear rate was 1.3${\times}10^-8\;mm^2$.$kgf^1$, and torque was 0.01kgf.cm at the wrench torque of 100 kgf.cm.

  • PDF

THINNED PIPE MANAGEMENT PROGRAM OF KOREAN NUCLEAR POWER PLANTS

  • Lee, S.H.;Lee, Y.S.;Park, S.K.;Lee, J.G.
    • Corrosion Science and Technology
    • /
    • 제14권1호
    • /
    • pp.1-11
    • /
    • 2015
  • Local wall thinning and integrity degradation caused by several mechanisms, such as flow accelerated corrosion (FAC), cavitation, flashing and/or liquid drop impingements, are a main concern in carbon steel piping systems of nuclear power plant in terms of safety and operability. Thinned pipe management program (TPMP) had been developed and optimized to reduce the possibility of unplanned shutdown and/or power reduction due to pipe failure caused by wall thinning in the secondary side piping system. This program also consists of several technical elements such as prediction of wear rate for each component, prioritization of components for inspection, thickness measurement, calculation of actual wear and wear rate for each component. Decision making is associated with replacement or continuous service for thinned pipe components. Establishment of long-term strategy based on diagnosis of plant condition regarding overall wall thinning is also essential part of the program. Prediction models of wall thinning caused by FAC had been established for 24 operating nuclear plants. Long term strategies to manage the thinned pipe component were prepared and applied to each unit, which was reflecting plant specific design, operation, and inspection history, so that the structural integrity of piping system can be maintained. An alternative integrity assessment criterion and a computer program for thinned piping items were developed for the first time in the world, which was directly applicable to the secondary piping system of nuclear power plant. The thinned pipe management program is applied to all domestic nuclear power plants as a standard procedure form so that it contributes to preventing an accident caused by FAC.

HIPS 복합재의 전기적 및 마모 특성에 미치는 다중벽 탄소나노튜브의 영향 (Effects of Multi-walled Carbon Nanotubes on Electrical and Wear Characteristics of High Impact Polystyrene Composites)

  • 정연우;김경식;이현우;정만우;이재혁;김재현;이학주;김광섭
    • Tribology and Lubricants
    • /
    • 제31권3호
    • /
    • pp.95-101
    • /
    • 2015
  • Carbon nanotubes (CNTs) are widely used in polymer composites as filler materials to enhance various characteristics of the composites because of their remarkable mechanical, electrical, and thermal properties. In this study, we investigate the effects of MWCNTs on the electrical and wear characteristics of high-impact polystyrene (HIPS) composites, and compare the results with the effects of carbon black (CB). The HIPS composites are classified as Bare-HIPS, MWCNT-HIPS composites containing 2, 3, 4, and 5 wt% MWCNTs, and CB-HIPS containing 17 wt% CB. Electrical characteristics are evaluated by measuring the surface resistance using a 4-point probe. Wear characteristics are evaluated using the reciprocating wear test, and a chrome steel ball with a curvature of 6.3 mm is used as the counterpart. The results show that the addition of MWCNTs or CB can improve the electrical and wear characteristics of HIPS composites. In the case of MWCNT-HIPS composites, surface resistance, friction coefficient, and specific wear rate decrease as the concentrations of MWCNTs increase. Moreover, the addition of MWCNTs is more effective in improving the electrical and wear characteristics of HIPS composites compared to the addition of CB. To fabricate the HIPS composite with appropriate electrical and wear characteristics, more than 4 wt% MWCNTs is added to HIPS.

의복의 거잡감이 대인지각에 미치는 영향 (The Effect of Feeling Distance on Clothes in the Person Perception)

  • 박성순;이경희
    • 한국의류학회지
    • /
    • 제18권1호
    • /
    • pp.31-42
    • /
    • 1994
  • The purpose of this study was to investigate the effect of feeling distance of clothes in the person perception. The specific objectives were: 1) to investigate whether the compositions of clothes affect the rate of detouring, ; 2 ) to investigate whether the gender compositions of dyads affect the rate of detouring, ; 3) to investigate whether the distance between members of dyads affect the rate of detouring. ; 3) to investigate whether the distance between members of dyads affect the rate of detouring. ; 4) to investigate the .effect of the interaction among the compsitions of clothes, the gender compositions, and the distance between members of dyads in the person perception. For this study, two male and two female undergraduates were selected and wore business suit or casual wear as given by the researcher. The distance between members of dyads ranged from 100cm to 170cm with an increment unit of loom. The data from our observation were analysed by x2-test, ANOVA, and MCA. The major findings were ; 1) In male/male dyad, distance perception from clothes were affected by the compositions of clothes at all distance. In maleffemale dyad, when the distance between members of dyad is short, distance perception from clothes were affected by the compositions of clothes modes, 2) When two members of dyad wear business suit, distance perception from clothes were affected by the gender composions of dyads. 3) Distance perception from clothes were affected by distance factors at all the gender compositions of dyads. 4) In the person perception, the most imprtant clue was the distance between members of dyads. The pllysical distance, which was formed by clothes, was between 130cm and 140cm.

  • PDF