• 제목/요약/키워드: Solution immersion treatment

검색결과 118건 처리시간 0.026초

Effect of Zincate Treatment Time on Dissolution Behavior and Deposition of Copper on AZ31 Mg alloy in Pyrophosphate Bath

  • Van Phuong, Nguyen;Moon, Sungmo
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.194.1-194.1
    • /
    • 2016
  • The present study investigated the effect of zincate treatment time on the dissolution behavior and the deposition of copper by immersion process and electroplating process on AZ31 Mg alloy substrate in a copper pyrophosphate bath. Without zincate pretreatment, the AZ31 Mg substrate quickly dissolved in the copper pyrophosphate solution although an external cathodic current was applied. The copper layers deposited on non-zincate treated AZ31 Mg alloy substrate by both immersion and electroplating processes showed very porous structure and very poor adhesion. With increasing zincate treatment time up to 2 min, the dissolution of AZ31 substrate in pyrophosphate solution rapidly decreased and the deposited copper layer was less porous and exhibited stronger adhesion. The immersion of AZ31 Mg sample in zincate solution for 5 min was found as a critical time for producing a non-porous and adherent electrodeposited copper layer on AZ31 Mg alloy. The optimum zincating time can be determined by observing the open circuit potential (OCP) of AZ31 Mg alloy samples in a copper pyrophosphate electroplating bath. The OCP reached a stable value of about -0.10 V (vs. SCE) after 5 min of immersion in the copper pyrophosphate electroplating solution.

  • PDF

이중(二重) 확산처리법(擴散處理法)에 의(依)한 간벌(間伐) 소경재(小經材)의 방부처리(防腐處理) (Preservative Treatment of Thinned Small-diameter Logs by Double-diffusion Processes)

  • 김규혁;김재진;지우근
    • Journal of the Korean Wood Science and Technology
    • /
    • 제19권4호
    • /
    • pp.7-17
    • /
    • 1991
  • The feasibility of treating three softwood(Japanese larch pitch pine, and Korean pine) thinned logs by double-diffusion treatment processes was investigated. Some posts were incised before immersion, and others were imersed in hot copper sulfate solution. Comparison among species indicated that. in general, pitch pine was most treatable and Japanese larch least treatable. For all three species, almost all treatment schedules gave consistently good penetration and high net retention, but very steep gradient of preservative distribution. As expected, the treatability was increased by the extension of immersion time, increased concentration of treating solution, incising. and heating of the first solution. Of the variables tested, it appears that heating of the first solution is the most important. From the data in this paper, it may be concluded that, if the first solution is not heated, the best schedule is #3. If the first solution is healed. it appears the best schedules are #10 or #11. Since heating of the first solution improves the treatability. schedules # 10 or :#11 are recommended if the cost of heating might be justified. The data presented in this paper indicate that double-diffusion treatment processes seem to offer a promise as a comparatively effective and easy-operating method of treating thinned logs for the small-scale production of treated stock.

  • PDF

480~720℃에서 예민화한 STS310S, STS316L 및 STS347H의 기계적 성질 및 침지 특성 (Mechanical properties and immersion characteristics of sensitinized STS310S, STS316L and STS347H in the range of 480~720℃)

  • 김영수;이소영;도재윤;안석환;남기우
    • 동력기계공학회지
    • /
    • 제20권3호
    • /
    • pp.43-50
    • /
    • 2016
  • The current study was carried to understand the immersion characteristics and mechanical properties of heat treated stainless steels. Stainless steels (STS310S, STS316L and STS347H) were thermally treated at temperature ranges from 480 to $720^{\circ}C$. Nominal stress was determined to be slightly different depending on the heat treatment temperature. The Cr concentration in STS310S was increased at the temperatures of 600 and $660^{\circ}C$, whereas the Cr concentration in STS316L and STS347H were almost constant regardless of heat treatment temperatures. Vickers hardness was found larger as a thermal treatment temperature was increased. Immersion tests of the stainless steels were also carried out in acidic solution and alkaline solution for 240 hours. Among three different stainless steels, the pitting was detected in the acidic solution, not in the alkaline solution. The pitting of STS347H was occurred more than STS310S and STS316L.

Facile Modulation of Electrical Properties on Al doped ZnO by Hydrogen Peroxide Immersion Process at Room Temperature

  • Park, Hyun-Woo;Chung, Kwun-Bum
    • Applied Science and Convergence Technology
    • /
    • 제26권3호
    • /
    • pp.43-46
    • /
    • 2017
  • Aluminum-doped ZnO (AZO) thin films were deposited by atomic layer deposition (ALD) with respect to the Al doping concentrations. In order to explain the chemical stability and electrical properties of the AZO thin films after hydrogen peroxide ($H_2O_2$) solution immersion treatment at room temperature, we investigated correlations between the electrical resistivity and the electronic structure, such as chemical bonding state, conduction band, band edge state below conduction band, and band alignment. Al-doped at ~ 10 at % showed not only a dramatic improvement of the electrical resistivity but also excellent chemical stability, both of which are strongly associated with changes of chemical bonding states and band edge states below the conduction band.

PEO 처리시 Ca-GP첨가에 따른 AZ31합금의 내식성 및 표면특성에 관한 연구 (A study on corrosion resistance and surface properties of AZ31 alloy according to Ca-GP addition during PEO treatment)

  • 이준수;박제신;박일송
    • 한국표면공학회지
    • /
    • 제54권5호
    • /
    • pp.238-247
    • /
    • 2021
  • PEO (plasma electrolytic oxidation) was applied to modify the surface of AZ31 magnesium alloy in this study. The mixed solution of sodium hydroxide (NaOH) and sodium silicate (Na2SiO3) was used as the electrolyte, and 0 - 0.05 g/L of Ca-GP (Glycerol Phosphate Calcium salt) was added in the electrolyte as an additive. PEO treatment was conducted at a current density of 30mA/cm2 for 5 minutes using a DC power supply. The surface properties were identified by SEM, XRD and surface roughness analyses, and the corrosion resistance was evaluated by potentiodynamic polarization and immersion tests. In addition, the biocompatibility was evaluated by immersion test in SBF solution. As the concentration of Ca-GP was increased, the surface morphology was denser and more uniform, and the amount of Ca and the thickness of oxide layer increased. Only Mg peak was observed in XRD analysis due to very thin oxide layer. The corrosion resistance of PEO-treated samples increased with the concentration of Ca-GP in comparision with the untreated sample. In particular, the highest corrosion resistance was identified at the group of 0.04g Ca-GP through potentiodynamic polarization and immersion tests in saline solution (0.9 wt.%NaCl). During the immersion in saline solution, pH rapidly increased at the beginning of immersion period due to rapid corrosion, and then increase rate of pH decreased. However, the pH value in the SBF temporarily increased from 7.4 to 8.5 during the day, then decreased due to the inhibition of corrosion with HA(hydroxyapatite) formation.

AZ91 마그네슘 합금의 PEO 피막 형성거동에 미치는 HF전처리의 영향 (Effect of pre-treatment of AZ91 Mg alloy in HF solution on PEO film formation behavior)

  • 권두영;송풍근;문성모
    • 한국표면공학회지
    • /
    • 제54권4호
    • /
    • pp.184-193
    • /
    • 2021
  • This study demonstrates formation behavior and morphological changes of PEO (Plasma Electrolytic Oxidation) films on AZ91 Mg alloy as a function of pre-treatment time in 1 M HF solution at 25 ± 1 ℃. The electrochemical behavior and morphological changes of AZ91 Mg alloy in the pre-treatment solution were also investigated with pre-treatment time. The PEO films were formed on the pre-treated AZ91 Mg alloy specimen by the application of anodic current 100 mA/cm2 of 300 Hz AC in 0.1 M NaOH + 0.4 M Na2SiO3 solution. Vigorous generation of hydrogen bubbles were observed upon immersion in the pre-treatment solution and its generation rate decreased with immersion time. It was also found that 𝛽-Mg17Al12 in AZ91 Mg alloy was dissolved and a protective thin film of MgF2 was formed on the AZ91 Mg alloy surface during the pre-treatment process in the 1 M HF solution. PEO film did not grow on the AZ91 Mg alloy specimen when the surface was not pre-treated and irregular PEO films with nodular defects were formed for the specimens pre-treated up to 1 min. Uniform PEO films were formed when the AZ91 Mg alloy specimen was pre-treated more than 3 min. The growth rate of PEO films on AZ91 Mg alloy increased significantly with increasing pre-treatment time.

Corrosion of Zinc Coated Steel in Magnetically Treated 3% Sodium Chloride Solution

  • Chiba, A.;Ohki, T.;Wu, Wen-Chang
    • Corrosion Science and Technology
    • /
    • 제5권2호
    • /
    • pp.39-44
    • /
    • 2006
  • The dissolution amount of Zn plate was $0.058mg/cm^2$ in the non-magnetically treated solution, and was $0.059mg/cm^2$ in the magnetically treated solution after 24 hours of immersion. The magnetic treatment had no effect to corrosion of Zn plate as pH on surface was not recognized the difference. The addition of Zn(II) ion in the solution was prepared to the effects of corrosion and dissolution of Fe. The regularity was not obtained the effect of the magnetic treatment on the dissolution of Fe plate.

용체화처리된 주조용 Mg-8%Al-X%Zn 합금의 부식 거동 (Corrosion Behavior of Solution-Treated Mg-8%Al-X%Zn Casting Alloys)

  • 전중환;황인제
    • 열처리공학회지
    • /
    • 제28권3호
    • /
    • pp.126-133
    • /
    • 2015
  • The aim of this study is to investigate the effect of solution treatment on the corrosion behavior of Mg-8%Al-(0-1)%Zn casting alloys in 1M NaCl aqueous solution. After the solution treatment, all alloys showed single ${\alpha}$-(Mg) phase microstructure by dissolution of ${\beta}(Mg_{17}Al_{12})$ phase into the ${\alpha}$-(Mg) matrix. The $H_2$ evolution volume decreased with an increase in Zn content, which indicates that the addition of Zn plays a beneficial role in decreasing corrosion rate of the Mg-Al-Zn alloy in solution-treated state. The microstructural evaluations on the corrosion products and corroded surfaces after the immersion test in 1 M NaCl solution revealed that the incorporation of more $Al_2O_3$ and ZnO into the corrosion product, by which the penetration of $Cl^-$ ions is impeded, are thought to be responsible for the better corrosion resistance in relation with the Zn addition.

Localized Corrosion Resistance and Microstructural Changes in UNS N07718 Alloy After Solution Heat Treatment

  • Yoon-Hwa Lee;Jun-Seob Lee;Soon il Kwon;Jungho Shin;Je-Hyun Lee
    • Corrosion Science and Technology
    • /
    • 제23권2호
    • /
    • pp.166-178
    • /
    • 2024
  • The localized corrosion resistance of UNS N07718 alloy was investigated after solution heat treatment. When the alloy was heat-treated at 1050 ℃ for 2.5 hours, it experienced an increase in average grain diameter, a reduction in grain boundary area, and the dissolution of delta phases along grain boundaries. Additionally, primary metallic nitrides (MN) and metallic carbides (MC), enriched with either Ti or Nb, were identified and exhibited a random distribution within the microstructures. Despite the solution heat treatment, the composition, diameter, and abundance of MNs and MCs remained relatively consistent. The critical pitting temperature (CPT), as determined by the ASTM G48-C immersion test, revealed similar values of 45 ℃ for both treated and untreated alloys. However, a decrease in maximum pit depth and corrosion rate was observed after the solution heat treatment. The microstructural changes that occurred during the heat treatment and their potential implications were discussed to understand the influence of the solution heat treatment.

무전해 니켈 도금액 pH 변화에 따른 ENIG/Sn-Ag-Cu솔더 접합부의 취성파괴 특성 (Brittle Fracture Behavior of ENIG/Sn-Ag-Cu Solder Joint with pH of Ni-P Electroless Plating Solution)

  • 서원일;이태익;김영호;유세훈
    • 마이크로전자및패키징학회지
    • /
    • 제27권3호
    • /
    • pp.29-34
    • /
    • 2020
  • 본 연구에서는 무전해 니켈 도금액 pH 변화에 따른 electroless nickel immersion gold (ENIG)/Sn-3.0wt.%Ag-0.5wt.%Cu(SAC305) 솔더 접합부 취성 파괴 거동에 대하여 평가하였다. ENIG 표면처리를 위한 무전해 니켈 도금액의 pH는 4.0에서 5.5로 변화 시켰다. 무전해 니켈 도금 후 Ni-P 표면 관찰 결과, 도금액의 pH가 낮아질수록 Ni-P 층 nodule 표면에 핀홀이 증가하였다. 솔더링 후 접합부 계면에서는 (Cu,Ni)6Sn5 금속간화합물이 형성되었으며, 무전해 니켈 도금액의 pH가 증가할수록 솔더접합부의 계면 금속간화합물의 두께는 증가하였다. 고속전단 시험을 통하여 ENIG/SAC305 솔더 접합부의 취성파괴 거동을 확인하였으며, 무전해 니켈 도금액의 pH가 증가할수록 솔더접합부의 전단강도는 감소하는 경향을 보였다. 또한, 솔더 접합부의 취성 파괴율은 pH가 5일 때 가장 높은 값을 보였다.