Mechanical properties and immersion characteristics of sensitinized STS310S, STS316L and STS347H in the range of 480~720℃

480~720℃에서 예민화한 STS310S, STS316L 및 STS347H의 기계적 성질 및 침지 특성

  • Kim, Young-Soo (Graduate School, Pukyong National University) ;
  • Lee, So-Young (Graduate School, Pukyong National University) ;
  • Do, Jae-Yoon (Busan campus, Korea Polytechnics VII) ;
  • Ahn, Seok-Hwan (Department of Mechatronics, Jungwon University) ;
  • Nam, Ki-Woo (Department of Materials Science and Engineering, Pukyong National University)
  • 김영수 (부경대학교 대학원) ;
  • 이소영 (부경대학교 대학원) ;
  • 도재윤 (한국폴리텍 7대학 부산캠퍼스) ;
  • 안석환 (중원대학교 메카트로닉스공학과) ;
  • 남기우 (부경대학교 재료공학과)
  • Received : 2016.03.22
  • Accepted : 2016.05.30
  • Published : 2016.06.30

Abstract

The current study was carried to understand the immersion characteristics and mechanical properties of heat treated stainless steels. Stainless steels (STS310S, STS316L and STS347H) were thermally treated at temperature ranges from 480 to $720^{\circ}C$. Nominal stress was determined to be slightly different depending on the heat treatment temperature. The Cr concentration in STS310S was increased at the temperatures of 600 and $660^{\circ}C$, whereas the Cr concentration in STS316L and STS347H were almost constant regardless of heat treatment temperatures. Vickers hardness was found larger as a thermal treatment temperature was increased. Immersion tests of the stainless steels were also carried out in acidic solution and alkaline solution for 240 hours. Among three different stainless steels, the pitting was detected in the acidic solution, not in the alkaline solution. The pitting of STS347H was occurred more than STS310S and STS316L.

Keywords

References

  1. R. Beneke and R. F. Sandenbergh, 1989, "The Influence of Nitrogen and Molybdenum on the Sensitization Properties of Low-Carbon Austenitic Stainless Steels", Corrosion Science, Vol. 29, pp. 543-555. https://doi.org/10.1016/0010-938X(89)90006-1
  2. M. G. Fontana and N. D. Green, 1978, "Corrosion Engineering 2nd ed.", McGraw-Hill, New York, U.S.A.
  3. Y. J. Rhee, Y. S. Kim and Y. S. Park, 1992, "Effects of Grain Size and Phase on Corrosion Resistance and Mechanical Properties of AISI 304 and AISI 430 Alloys", Journal of the Corrosion Science Society of Korea, Vol. 21, pp. 95-110.
  4. E. A. Trillo, R. Beltran, J. G. Maldonado, R. J. Romero, L. E. Murr, W. W. Fisher and A. H. Advani, 1995, "Combined Effects of Deformation (Strain and Strain State), Grain Size, and Carbon Content on Carbide Precipitation and Corrosion Sensitization in 304 Stainless Steel", Materials Characterization, 35, 99-112. https://doi.org/10.1016/1044-5803(95)00072-0
  5. P. Atanda, A. Fatudimu and O. Oluwole, 2010, "Sensitiszation Study of Normalized 316L Stainless Steel", Journal of Minerals & Materials Characterization & Engineering, Vol. 9, pp. 13-23. https://doi.org/10.4236/jmmce.2010.91002
  6. E. C. Bain, R. H. Abora and J. T. B. Rutherford, 1933, "The Nature and Prevention of Intergranular Corrosion in Austenitic Stainless Steels", Transactions of the American Society for Steel Treating, Vol. 21, pp. 481-509.
  7. C. Stawstrom and M. Hillert, 1969, "An Improved Depleted-Zone Theory of Intergranular Corrosion of 18-8 Stainless Steel", Journal of Iron and Steel Institute, Vol. 207, pp. 77-85.
  8. T. M. Devine, 1979, "Mechanism of Intergranular Corrosion and Pitting Corrosion of Austenitic and Duplex 308 Stainless Steel", Journal of The Electrochemical Society, Vol. 126, pp. 374-385. https://doi.org/10.1149/1.2129046
  9. C. S. Tedman, D. A. Jr. Vermilyea and J. H. Rosolowski, 1971, "Intergranular Corrosion of Austenitic Stainless Steel", Journal of The Electrochemical Society, Vol. 118, pp. 192-202. https://doi.org/10.1149/1.2407966
  10. S. C. Tjong, J. Kepner and Z. Eliezer, 1983, "An Electrochemical Evaluation of Sensitization in Homopolar Welds", Journal of American Welding Society, Welding Research (Supplement), Vol. 62, pp. 19-20.
  11. B. T. Kim and K. K. Baek, 1988, "A Study on Evaluation of Degree of Sensitization in AISI 304 Stainless Steel and Its Welding Heat Affected Zone by An Electrochemical Method", Journal of The Corrosion Science Society of Korea, Vol. 17, pp. 99-109.
  12. J. H. Shin and J. B. Lee, 2006, "Critical Pitting Temperature of 2205 Duplex Stainless Steels Using Immersion and Electrochemical Polarization Test Methods", Journal of the Korean Institute Surface Engineering, Vol. 39, pp. 18-24.
  13. M. I. Kim, 1991, "Hardness of Heat Treated Components", Journal of the Korean Society for Heat Treatment, Vol. 4, pp. 61-64.
  14. K. W. Nam, S. S. Park and S. H. Ahn, 2003, "Ultrasonic Characteristics of Base and Welded Metal of STS316L", Korean Journal of Metals and Materials, Vol. 41, pp. 186-195.
  15. Y. T. Jeong, 2015, "Effect of Stabilization Heat treatment on the Precipitation Behavior of Super 304H, 347H Stainless Steels Weld HAZ during Aging", Master Thesis of Hanyang university.

Cited by

  1. Corrosion Resistance of EH36 Steel for Ship by Salt Spray vol.22, pp.3, 2018, https://doi.org/10.9726/kspse.2018.22.3.044
  2. Tribological Characteristics and Corrosion Resistance of SM45C for Mechanical Structural Steel vol.23, pp.1, 2016, https://doi.org/10.9726/kspse.2019.23.1.027