오스테나이트계 스테인리스강 용접부의 금속학적 현상에 관한 연구(2) - STS 304 용접부 조직특성 및 고온균열 감수성에 미치는 질소의 영향 - (A Study of Weld Fusion Zone Phenomena in Austenitic Stainless Steels(2) - Effects of Nitrogen on Microstructural Evolution and Hot Cracking Susceptibility GTA Welds in STS 304 -)

  • 이종섭;김숙환
    • Journal of Welding and Joining
    • /
    • 제18권1호
    • /
    • pp.59-69
    • /
    • 2000
  • The purpose of the present study was to investigate weld metallurgical phenomena such as primary solidification mode, microstructural evolution and hot cracking susceptibility in nitrogen-bearing austenitic stainless steel GTA welds. Eight experimental heats varying nitrogen content from 0.007 to 0.23 wt.% were used in this study. Autogenous GTA welding was performed on weld coupons and the primary solidification mode and their microstructural characteristics were investigated from the fusion welds. Varestraint test was employed to evaluate the solidification cracking susceptibility of the heats and TCL(Total Crack Length) was used as cracking susceptibility index. The solidification mode shifted from primary ferrite to primary austenite with an increase in nitrogen content. Retained delta ferrite exhibited a variety of morphology as nitrogen content varied. The weld fusion zone exhibited duplex structure(austenite+ferrite) at nitrogen contents less than 0.10 wt.% but fully austenitic structure at nitrogen contents more than 0.20 wt.%. The weld fusion zone in alloys with about 0.15 wt.% nitrogen experienced primary austenite + primary ferrite solidification (mode AF) and contained delta ferrite less than 1% at room temperature. Regarding to solidification cracking susceptibility, the welds with fully austenitic structure exhibited high cracking susceptibility while those with duplex structure low susceptibility. The cracking susceptibility increased slowly with an increase in nitrogen content up to 0.20 wt.% but sharply as nitrogen content exceeded 0.20 wt.%, which was attributed to solidification mode shift fro primary ferrite to primary austenite single phase solidification.

  • PDF

Ni-Al 합금의 일방향 응고 거동에 미치는 Re 및 응고속도의 영향 (The Effect of Re addition and Solidification Rate on the Directional Solidification Behavior of Ni-Al Alloy)

  • 이만길;유영수;조창용;이재현
    • 한국주조공학회지
    • /
    • 제27권6호
    • /
    • pp.243-249
    • /
    • 2007
  • The effect of Re addition and solidification rate on the directional solidification behavior of Ni-Al model alloy has been investigated. Directional solidification (DS) were carried out using the modified Bridgman furnace with various solidification rates. The solid/liquid interface during directional solidification was preserved by quenching the specimen after the desired volume fraction of original liquid was solidified. The equilibrium partition coefficients of Al and Re Were estimated by measuring the compositions at the quenched solid/liquid interface. Then, the effect of Re addition on the elemental segregation behavior was carefully analyzed. The differential scanning calorimetry results showed that the Re addition results in increased ${\gamma}'$ solvus and freezing range of the alloy. It was also shown that the primary dendrite arm spacing gradually decreases with increasing the Re content, while the secondary dendrite arm spacing appears to be independent on the Re content. The compositional analyses clearly revealed that the segregation of Al increased with increasing the Re content and solidification rate, while that of Re was found to be independent on the solidification rate in the range of $10{\sim}100{\mu}m/s$ due to its sluggish diffusion rate in the Ni solid solution.

Influences of boron and silicon in insert alloys on microstructure and isothermal solidification during TLP bonding of a duplex stainless steel using MBF-35 and MBF-30

  • 원신건;김명복;강정윤
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.59-59
    • /
    • 2009
  • The influences of B and Si in the filler metals on microstructure and isothermal solidification during transient liquid-phase (TLP) bonding of a nitrogen-containing duplex stainless steel with MBF-30 (Ni-4.5wt.%Si-3.2wt.%B) and MBF-35 (Ni-7.3wt.%Si-2.2wt.%B), were studied at the temperature range of $1030-1090^{\circ}C$ with various times from 60 s to 3600 s under a vacuum of approximately $10^{-5}$ Torr. In case of the former, BN, $Ni_3B$ and $Ni_3Si$ precipitates were formed in the bonding region. BN and $Ni_3Si$ secondary phases were present in the joint for the latter case. The formation of $Ni_3B$ within the joint centerline is dependent on B content. The morphology of $Ni_3Si$ is dominated by Si concentration. A difference between the times for complete isothermal solidification obtained by the experiments and the conventional TLP bonding diffusion model was observed when using MBF-35. According to the simulated results, the isothermal solidification completion time for MBF-35 case was smaller than that in MBF-30. However, this experimental value obtained using MBF-35 was notably larger than that obtained using MBF-30. Isothermal solidification of liquid MBF-30 is controlled by the first isothermal solidification regime dependent on B diffusion model, whereas that of liquid MBF-35 experiences two isothermal solidification regimes and is mainly controlled by the second isothermal solidification dependent on Si diffusion model. In addition, only if Si content exceeds a critical value, the slower 2nd solidification regime will commence.

  • PDF

다결정 실리콘 웨이퍼 직접제조에 대한 공정변수 영향 (Effect of Processing Parameters on Direct Fabrication of Polycrystalline Silicon Wafer)

  • 위성민;이진석;장보윤;김준수;안영수;윤우영
    • 한국주조공학회지
    • /
    • 제33권4호
    • /
    • pp.157-161
    • /
    • 2013
  • A ribbon-type polycrystalline silicon wafer was directly fabricated from liquid silicon via a novel technique for both a fast growth rate and large grain size by exploiting gas pressure. Effects of processing parameters such as moving speed of a dummy bar and the length of the solidification zone on continuous casting of the silicon wafer were investigated. Silicon melt extruded from the growth region in the case of a solidification zone with a length of 1cm due to incomplete solidification. In case of a solidification zone wieh a length of 2 cm, on the other hand, continuous casting of the wafer was impossible due to the volume expansion of silicon derived from the liquid-solid transformation in solidification zone. Consequently, the optimal length of the solidification zone was 1.5 cm for maintaining the position of the solid-liquid interface in the solidification zone. The silicon wafer could be continuously casted when the moving speed of the dummy bar was 6 cm/min, but liquid silicon extruded from the growth region without solidification when the moving speed of the dummy bar was ${\geq}$ 9 cm/min. This was due to a shift of the position of the solid-liquid interface from the solidification zone to the moving area. The present study reports experimental findings on a new direct growth system for obtaining silicon wafers with both high quality and productivity, as a candidate for an alternate route for the fabrication of ribbon-type silicon wafers.

PFC법에 있어서의 Al-Cu 다결정리본의 응고특성 (Solidification Characteristics of Al-Cu Polycrystalline Ribbons in Planar Flow Casting)

  • 이경구;이상목;홍준표
    • 한국주조공학회지
    • /
    • 제15권4호
    • /
    • pp.408-415
    • /
    • 1995
  • Polycrystalline Al-Cu ribbons were produced by planar flow casting(PFC). Solidification behavior and microstructual changes of the ribbons have been investigated as a function of ribbon thickness and processing parameters. The solidification front velocity, V varies within the ribbon, decreasing with increasing the distance, S from the wheel-contact surface, as $V=17.6S^{-1}$. In Al-4.5wt%Cu alloy, rapid decrease in solidification velocity toward the free surface causes a change in solidification morphology from planar to cellular, and finally, to dendritic. The length and inclination of columnar grains solidified with planar front were related to the wheel velocity. The transition from particulate degenerate eutectic structure to regular lamellar eutectic structure was observed to be caused by a difference of the relative growth velocites of ${\alpha}-Al$ and ${\theta}$ during solidification in the Al-Cu eutectic alloy.

  • PDF

분무성형 공정에서 분무액적의 열이력 해석 및 고상분율 예측 (Thermal History Analysis and Solid Fraction Prediction of Gas-Atomized Alloy Droplets during Spray Forming)

  • 이언식
    • 한국분말재료학회지
    • /
    • 제1권1호
    • /
    • pp.85-94
    • /
    • 1994
  • In order to predict droplet velocity and temperature profiles and fractional solidification with flight distance during spray forming, the Newtonian heat transfer formulation has been coupled with the classical heterogeneous nucleation and the specific solidification process. It has been demonstrated that the thermal profile of the droplet in flight is significantly affected by process parameters such as droplet size, initial gas velocity, undercooling. As the droplet size and/or the initial gas velocity increase, the onset and completion of solidification are shifted to greater flight distances and the solidification process also extends over a wider range of flight distances. The amounts of solid fractions formed during recoalescence, segregated solidification and eutectic solidification are insensitive to droplet size and initial gas velocity whereas those are strongly affected by the degree of undercooling. There are good linear relations between the undercooling and the corresponding solid fractions generated during recoalesced, segregated and eutectic stages.

  • PDF

정수슬러지로부터 중금속 용출 억제를 위한 최적 고화조건 (Optimal Solidification Conditions for Suppression of Heavy Metal Elution from Water Treatment Sludge)

  • 이병대;김영찬;이진식
    • 한국응용과학기술학회지
    • /
    • 제22권4호
    • /
    • pp.379-384
    • /
    • 2005
  • In general, water treatment sludge (WTS) had high concentration of heavy metal, thus it made the reuse or recycling of WTS difficult. The optimal solidification conditions for maximum suppression of heavy metal elution from WTS were decided in this study. Under the optimal solidification conditions (i.e., temperature, $320^{\circ}C;$ ratio of WTS and MgO, 9:1; solidification time, 1hr), all of heavy metal including aluminum were not detected. Therefore there are no problems for reuse or recycling of WTS which was solidified under the optimal solidification conditions found in the study.

액상확산접합한 Ni기 초내열합금의 등온응고거동에 미치는 모재결정입계의 영향 (The Effect of Base Metal Grain Boundary on Isothermal Solidification Phenomena during TLP Bonding of Ni Base Superalloys)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권3호
    • /
    • pp.325-333
    • /
    • 2001
  • The effect of base metal grain size on isothermal solidification behavior of Ni-base superalloy, CMSX-2 during transient liquid phase (TLP) bonding was investigated employing MBF-80 insert metal. TLP-bonding of single crystal. coarse-grained and fine-grained CMSX-2 was carried out at 1373∼1548k for various holding time in vacuum. The eutectic width diminished linearly with the square root of holding time during isothermal solidification process for single crystal, coarse-grained and fine-grained base metals. The completion time for isothermal solidification decreased in the order ; single crystal, coarse-grained and fine-grained base metals. The difference of isothermal solidification rates produced when bonding the different base metals could be explained quantitatively by the effect of base metal grain boundaries on the apparent average diffusion coefficient of boron in CMSX-2.

  • PDF

일방향 응고법을 이용한 Mar M-247LC 초내열합금의 액상 물성 측정 (Estimation of Liquid Physical Properties of Mar-M247LC Superalloy by Directional Solidification)

  • 김현철;이재현;서성문;김두현;조창용
    • 한국재료학회지
    • /
    • 제11권9호
    • /
    • pp.721-726
    • /
    • 2001
  • Directional solidification experiments have been carried out at the solidification rates from 0.5 to 50$\mu\textrm{m}$/s in Mar M-247LC superalloy in which several important liquid properties were estimated by analyzing the interface stability and temperature gradient at the solid/liquid interface. The diffusion coefficient in the liquid was estimated by employing the constitutional supercooling criterion. The temperature gradients changed with solidification rates and latent heat of solidification. The thermal conductivities of solid and liquid could be estimated by heat flux balance at the solid liquid interface.

  • PDF

연약점토의 함수비 변화가 고화처리토의 강도에 미치는 영향 (Effect of Water Content Change of Soft Clay on Strength of Solidification Agent Treated Soil)

  • 김광빈;이용안;이광준;김유성
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.553-560
    • /
    • 2002
  • The improvement effect of soft ground is estimated by unconfined strength mainly. The unconfined strength of solidification agent treated soil is likely to vary with ununiformed mixing ratio and water content change of in-situ ground place by place. So, it is unreasonable to apply a solidification agent mixing ratio obtained from laboratory test results on all over the soft ground. In this study, it was analysed how the unconfined strength would be effected by the water content of soft ground. For this study, a series of unconfined compressive tests are peformed on various water content soil samples. The test results showed that the strength was fallen to 30∼80% by two times increase of water content approximately, This means that strength of solidification agent treated soil is influenced greatly by water content of raw soft ground and mixing ratio of solidification agent. It was suggested that the method how to decide the mixing ratio with soft ground water content.

  • PDF