Casting Conditions and Solidification Characteristics of Sn-Zn Alloys (Sn-Zn합금의 주조조건과 응고특성)

  • Song, Tae-Seok;Kim, Myung-Han;Jo, Hyung-Ho;Ji, Tae-Gu
    • Journal of Korea Foundry Society
    • /
    • v.18 no.6
    • /
    • pp.570-577
    • /
    • 1998
  • An investigation has been conducted to describe solidification characteristics in Sn-Zn binary system and Sn-Zn-Ag ternary system added by Ag produced by the continuous casting process using heated mold as a basic study for developing Pb-free solder materials. To obtain the continuous casting rods with mirror surface and near net shape at higher casting speed, water flow rates must be increased and mold temperature must be lowered. However, surface tearing in the casting rods occured at lower continuous casting speed while break out occured at higher continuous casting speed even if optimum conditions such as water flow rate and heated mold temperature are determined. Primary ${\alpha}Sn$ and eutectic structure in unidirectioally solidified Sn-Zn alloys were finer with increased casting speed. But, directionality may not be expected for primary Zn in hypereutectic Sn-Zn alloy. It was found that the addition of $0.2{\sim}0.8%$ Ag promoted the growth of primary ${\alpha}Sn$ dendrites. The changes of tensile strength and elongation in Sn-Zn binary alloys were not observed while the increase of tensile strength and the decrease of elongation in Sn-Zn-Ag ternary alloys were observed with increased casting speed.

  • PDF

Oxidation characteristics of solder alloys for the photovoltaic module (태양전지 묘듈용 솔드 합금의 산화 특성)

  • Kim, Hyo Jae;Lee, Young Eun;Lee, Gu;Kang, Gi Hwan;Choi, Byung Ho
    • Journal of the Korean Solar Energy Society
    • /
    • v.34 no.1
    • /
    • pp.98-104
    • /
    • 2014
  • Photovoltaic (PV) cell is considered as one of the finest ways to utilize the solar power. A study of improving solar cell's efficiency is important because the lifetime of solar cell is determined by photovoltaic module technology. Therefore, oxidation (and/or corrosion) of solder materials will be one of the primary yield and long-term reliability risk factor. Recently, the development of lead-free solder alloy has been done actively about lead-free solder alloys of the thermodynamic and mechanical properties. However, the oxidation behavior have rarely been investigated In this study, the oxidations of 60 wt% Sn-40 wt% Pb, 62 wt% Sn-36 wt% Pb -2 wt% Ag, 50wt% Sn-48 wt% Bi-2 wt% Ag alloys for the interconnect ribbon after exposure in atmosphere at $100^{\circ}C$ for several times were investigated. The wettability of 62 wt% Sn-36 wt% Pb-2 wt% Ag and 50 wt% Sn-48 wt% Bi-2 wt% Ag solders was also studied to compare with that of 60 wt% Sn-40 wt% Pb alloy. The results howed that the zero cross time and the wetting time of 50 wt% Sn-48 wt% Bi-2 wt% Ag solder were better than other two samples. The surface of tested samples was analyzed by XPS. The XPS result showed that in all samples, SnO grew first and then the mixture of SnO and $SnO_2$ was detected. $SnO_2$ grew predominantly for the long time aging. Moreover XPS depth profile analysis has found surface enrichment of tin oxide.

Bending Impact Properties Evaluation of Sn-xAg-Cu Lead Free Solder Composition and aging treatment (시효처리한 Sn-xAg-Cu계 무연솔더 조성에 따른 굽힘충격 특성평가)

  • Jang, Im-Nam;Park, Jai-Hyun;Ahn, Yong-Sik
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.18 no.2
    • /
    • pp.49-55
    • /
    • 2011
  • The failure of electronic instruments is mostly caused by heat and shock. This shock causes the crack initiation at the solder joint interface of PCB component which is closely related with the formation of intermetallic compound(IMC). The Ag content in Pb-free Sn-xAg-0.5Cu solder alloy used in this study was 1.0, 1.2 and 3.0 wt.%, respectively. After soldering with PCB component, isothermal aging was performed to 1000 hrs. The growth of IMC layer was observed during isothermal aging. The drop impact property of solder joint was evaluated by impact bending test method. The solder joint made with the solder containing lower Ag content showed better impact bending property compared with that with higher Ag content. On the contrary to this result, the solder joint made with solder containing higher Ag content showed better impact bending property after aging. It should be caused by the formation of fine $Ag_3Sn$, which relieved the impact. It showed consequently the different effect of fine $Ag_3Sn$ and coarse $Cu_6Sn_5$ particles formed in the IMC layer on the impact bending property.

A Study on the Phase Identification of Dental Amalgams (의과용 아말감의 합금상 판별에 관한 연구)

  • 이규환;신명철
    • Journal of Biomedical Engineering Research
    • /
    • v.2 no.1
    • /
    • pp.39-46
    • /
    • 1981
  • Microstructural phases of the dental amalgams have been studied by optical microscope, scanning electron microprobe and X-ray diffractometer. r1 ($Ag_2Hg_3$) phase and r2 ($Sn_{7-8}Hg$) phase are found on conventional compositioned alloys. On high copper single compositioned alloy, rl ($Ag_2Hg_3$) phase and V ($Cu_6Sn_5$) phase are found but brittle r2 ($Sn_(7-8)Hg$) phase.

  • PDF

Creep Deformation Behaviors of Tin Pest Resistant Solder Alloys (Tin Pest 방지 솔더합금의 크리프 특성)

  • Kim S. B.;Yu Jin;Sohn Y. C.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.1 s.34
    • /
    • pp.47-52
    • /
    • 2005
  • Worldwide movement for prohibition of Pb usage drives imminent implementation of Pb-free solders in microelectronic packaging industry. Reliability information of Pb-free solders has not been completely constructed yet. One of the potential reliability concerns of Pb-free solders is allotropic transformation of Sn known as tin pest. Volume increase during the formation of tin pest could deteriorate the reliability of solder joints. It was also reported that the addition of soluble elements (i.e. Pb, Bi, and Sb) into Sn can effectively suppress the tin pest. However, the mechanical properties of the tin pest resistant alloys have not been studied in detail. In this study, lap shear creep test was conducted with Sn and Sn-0.7Cu based solder alloys doped with minor amount of Bi or Sb. Shear strain rates of the alloy were generally higher than those of Sn-3.5Ag based alloys. Rupture strains and corresponding Monkman- Grant products were largest for Sn-0.5Bi alloy and smallest for Sn-0.7Cu-0.5Sb alloy. Rupture surface Sn-0.5Bi alloy showed highly elongated $\beta$-Sn globules necked to rupture by shear stresses, while elongation of $\beta$-Sn globules of Sn-0.7Cu-0.5Sb alloy was relatively smaller.

  • PDF

Study on the Prediction of Fatigue Life of BGA Typed Solder Joints (BGA 형태 솔더 접합부의 피로 수명 예측에 관한 연구)

  • Kim, Seong-Keol;Kim, Joo-Young
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.17 no.1
    • /
    • pp.137-143
    • /
    • 2008
  • Thermal fatigue life prediction for solder joints becomes the most critical issue in present microelectronic packaging industry. And lead-free solder is quickly becoming a reality in electronic manufacturing fields. This trend requires life prediction models for new solder alloy systems. This paper describes the life prediction models for SnAgCu and SnPb solder joints, based upon non-linear finite element analysis (FEA). In case of analyses of the SnAgCu solder joints, two kinds of shapes are used. As a result, it is found that the SnAgCu solder has longer fatigue life than the SnPb solder in temperature cycling analyses.

Enhancing Die and Wire Bonding Process Reliability: Microstructure Evolution and Shear Strength Analysis of Sn-Sb Backside Metal (다이 및 와이어 본딩 공정을 위한 Sn-Sb Backside Metal의 계면 구조 및 전단 강도 분석)

  • Yeo Jin Choi;Seung Mun Baek;Yu Na Lee;Sung Jin An
    • Korean Journal of Materials Research
    • /
    • v.34 no.3
    • /
    • pp.170-174
    • /
    • 2024
  • In this study, we report the microstructural evolution and shear strength of an Sn-Sb alloy, used for die attach process as a solder layer of backside metal (BSM). The Sb content in the binary system was less than 1 at%. A chip with the Sn-Sb BSM was attached to a Ag plated Cu lead frame. The microstructure evolution was investigated after die bonding at 330 ℃, die bonding and isothermal heat treatment at 330 ℃ for 5 min and wire bonding at 260 ℃, respectively. At the interface between the chip and lead frame, Ni3Sn4 and Ag3Sn intermetallic compounds (IMCs) layers and pure Sn regions were confirmed after die bonding. When the isothermal heat treatment is conducted, pure Sn regions disappear at the interface because the Sn is consumed to form Ni3Sn4 and Ag3Sn IMCs. After the wire bonding process, the interface is composed of Ni3Sn4, Ag3Sn and (Ag,Cu)3Sn IMCs. The Sn-Sb BSM had a high maximum shear strength of 78.2 MPa, which is higher than the required specification of 6.2 MPa. In addition, it showed good wetting flow.

A Study on Wetting, Interfacial Reaction and Mechanical Properties between Sn-Bi-Ag System Solders and Cu Substrate (Sn-Bi-Ag계 땜납과 Cu기판과의 젖음성, 계면 반응 및 기계적 성질에 관한 연구)

  • Seo, Youn-Jong;Lee, Kyung-Ku;Lee, Doh-Jae
    • Journal of Korea Foundry Society
    • /
    • v.17 no.3
    • /
    • pp.245-251
    • /
    • 1997
  • Solderability, interfacial reaction and mechanical properties of joint between Sn-Bi-Ag base solder and Cu-substrate were studied. Solders were subjected to aging treatments to see the change of mechanical properties for up to 30 days at $100^{\circ}C$, and then also examined the changes of microstructure and morphology of interfacial compound. Sn-Bi-Ag base solder showed about double tensile strength comparing to Pb-Sn eutectic solder. Addition of 0.7wt%Al in the Sn-Bi-Ag alloy increase spread area on Cu substrate under R-flux and helps to reduce the growth of intermetallic compound during heat-treatment. According to the aging experiments of Cu/solder joint, interfacial intermetallic compound layer was exhibited a parabolic growth to aging time. The result of EDS, it is supposed that the soldered interfacial zone was composed of $Cu_6Sn_5$.

  • PDF