• Title/Summary/Keyword: Silk-II

검색결과 117건 처리시간 0.026초

Silk I형 결정을 얻기 위한 투석의 pH조건 (Dialytic pH Condition for Obtaining Silk I Type Structure)

  • 김동건
    • 한국잠사곤충학회지
    • /
    • 제39권1호
    • /
    • pp.67-72
    • /
    • 1997
  • As a condition for obtaining the silk I type crystal that has stability and high reproducibility, after dissolving silk fibroin crystalline part (Fcp), the changes of recrystallized crystal structure according to dialytic pH were examined by x-ray diffraction and differential thermal analysis. The Fcp was obtained from the aqueous solution of silk fibroin enzymatic proteolyzed by chymotrypsin. The crystal structure of Fcp showed silk II type. When the Fcp was dissolved by 10M LiBr aqueous solution, the Fcp1 showed the silk II type at pH 9. However, besides the silk II type, the silk I type structure begins to appear at pH 8 and only the silk I type structure was found below pH 6. On the other hand, the Fcp2 that calcium chloride was used in the dissolution found only the silk I type crystal structure below pH8.

  • PDF

Silk Fibroin 막에 관한 연구(I) -Silk Fibroin막의 구조특성- (Studies on Silk Fibroin Membranes(I) -Structure of Silk Fibroin Membranes and Their properties-)

  • 최해욱;박수민;김경환
    • 한국염색가공학회지
    • /
    • 제6권1호
    • /
    • pp.62-70
    • /
    • 1994
  • Silk fibroin was dissolved in 9.3 M LiBr aqueous solution at 4$0^{\circ}C$ for 1 hour. The dissolved silk fibroin was regenerated by casting the dialyzed solution into the membrane. The freshly prepared silk fibroin membrane was soluble in water and was. mainly consisted of random coil conformation. By the treatments in saturated water vapor at 3$0^{\circ}C$ and in 75% ethanolic aqueous solution (V/V), the insoluble membranes were obtained and the structure and morphology of those were investigated for the structure by means of X-ray diffraction analysis, infrared spectroscopy, thermal analysis. Rheovibron and scanning electron micrograph. Silk II type crystals were obtained by treating amorphous silk fibroin membrane in the random coil conformtion with 75% ethanol solution(V/V). Crystallization to silk II type crystals occured even after a few minutes, and a large number of silk II type crystals were formed after 30 mins. On the other and, the membrane treated in saturated water vapor was composed of the mixtures of silk I and silk II type crystals. A large number of silk I and silk II type crystals were formed after 24 hours. The micro brownian motion in the amorphous regions of silk fibroin membrane started at about 175~185$^{\circ}C$. $\alpha$ dispersion appeared at about 20$0^{\circ}C$ in the amorphous membrane, and at about 22$0^{\circ}C$ in the crystalline membrane. The crystallization of random coil conformation to silkII type crystals occured at about 215$^{\circ}C$. The surface, bottom and cross-section of the membranes were observed by scanning electrom microscope. Fine forms alike spherulites appeared at the surface of crystalline membrane.

  • PDF

효소반응에 의한 견피브로인의 전이 (Transition of Silk Fibroin by Enzymatic Reaction)

  • 김동건;최진협;소서효
    • 한국잠사곤충학회지
    • /
    • 제39권1호
    • /
    • pp.73-78
    • /
    • 1997
  • 분자량 약 7000의 Fcp는 효소분해역반응을 이용하는 것에 의해 분자량 약 17000과 약 24000까지 고분자량화된 PIFcp가 얻어졌다. 또, 효소분해의 역반응에 의해 고분자량화되는 것은 일부의 Fcp이며 Silk II형결정으로부터 Silk I형결정으로 전이하는 것은 대부분의 Fcp에서 나타났다. 이 PIFcp는 X선회절과 시차열분석(DTA)의 결과로부터 어느정도 안정한 Silk I형의 결정구조를 가지는 것이 확인되었다.

  • PDF

동물성 섬유에 대한 Lac추출물의 염색성(II) -매염방법과 매염제 종류의 효과- (Dyeabilites of Lac extract onto the silk and wool fabrics(II) -Effects of mordanting methods and various mordants-)

  • 김호정;박문영;이문철
    • 한국의류학회지
    • /
    • 제27권9_10호
    • /
    • pp.1134-1143
    • /
    • 2003
  • The purpose of this study is to investigate surface color change and effects of mordants on the K/S values of silk and wool fabrics dyed with Lac extract, according to the mordanting methods and conditions such as temperature, concentration and time of the mordanting bath. The results were as follow; 1 K/S values of the silk and wool fabrics according to the temperature of the mordanting bath were shown a slight decline beyond 40$^{\circ}C$. 2. Surface color of the silk changed from red to reddish purple and that of the wool showed red tone when mordanted with Aluminum postassium sulfate, Copper acetate and Copper (II) sulfate regardless of the mordanting conditions. 3. The light and dry cleaning fastness of silk and wool fabrics dyed with Lac extract according to the mordanting methods were very good.

천연염료에 관한 연구(II) -자근색소에 의한 견섬유염색 - (Studies on the Natural dyes(II) - Dyeing of silk fibers by Gromwell color matter -)

  • 조경래
    • 한국의류학회지
    • /
    • 제13권4호
    • /
    • pp.370-379
    • /
    • 1989
  • In previous paper, the optical behavior of coloring matter of Cromwell under several conditions were investigated. In this paper, the fading behavior of color solution extracted from Growell by methanol, dyeing properties of this color on the silk fibers in water and methanol, the three property of color of dyed silk fabrics, and fading behavior of dyed silk fabrics with Cromwell color under light and washing were discussed.

  • PDF

Silk Fibroin 막에 관한 연구 (II) -Silk Fibroin 막에 대한 산성염료의 흡착- (Studies on Silk Fibroin Membranes(II) -Adsorption of Acid Dyes in Silk Fibroin Memberane-)

  • 최해욱;박수민;김경환
    • 한국염색가공학회지
    • /
    • 제6권3호
    • /
    • pp.60-66
    • /
    • 1994
  • With the view of studying on the dual adsorption mechanism of acid dyes in connection with the structural difference of silk fibroin, silk fiber and silk fibroin memberane were used for equilibrium dyeing at $60^{\circ}C$, $70^{\circ}C$, $80^{\circ}C$ and pH 3.2, pH 5.0. The dyes used were C.I.Acid Orange 7 and C.I.Acid Red 88 introduced aromatic hydrocabon into Acid Orange 7. From the adsorption isotherm experiment, the total uptake of dyes can be described by Langmuir sorption and Nernst partition. Nernst partition. Nernst partition coefficient $K_1$ decrease of crystalline regions and orientation. The saturation value S of Acid Red 88 were large than total amino group contents and it was attributed it hydrophobic bond. On the other hand, the standard afficity and enthalpy were increased with the in crease of hydrophobic part of dyes. Both $k_1$ and $K_2$ were decreased with the increase of pH, but $k_2$ were more effected than $K_1$.

  • PDF

봉선화 추출액의 견직물 염색(II) (A Study on the Dyeing Properties of Silk Fabrics Dyed with Impatiens balsamina extract(II))

  • 김애순
    • 한국염색가공학회지
    • /
    • 제16권3호
    • /
    • pp.1-7
    • /
    • 2004
  • To study the dyeability(K/S value) and surface color of silk fabrics dyed with Impatiens balsamina extract, its flower, leaf and stem, was extracted by water. This paper investigated some experiments with Impatiens balsamina extract under the various dyeing conditions such as dyeing temperature, dyeing time, repetition of dyeing, dyeing pH with silk fabrics. The results obtained were as follows. 1. It was found that it $\lambdamax$. of silk fabrics dyed with Impatiens balsamina extract was 260nm and its flower, leaf, stem and flowers(white, pink, violet) had same it $\lambdamax$ at 260nm. 2. K/S value was increased when dyeing temperature, repetition of dyeing and time was higher, value of munsell of silk fabrics dyed with Impatiens balsamina extract was yellow-red. dyeing temperature, repetition of dyeing and time was higher, shifted to longer wavelength side. 3. pH added acetic acid was colored reddish yellow-red, but pH added alum was colored yellowish yellow-red in silk fabrics dyed with Impatiens balsamina extract and repetition of dyeing was increased the dye-uptake.

생사검사에 있어서 현행방법과 전자식 방법에 대한 비교분석 II. Uster Tester 3의 세리프렌 검사 정확도와 검사효율 (Comparison of the Electronic Methods of Raw Silk Testing and Grading with Those of the Current Methods II. The Effectiveness and Convenience of Raw Silk Inspection Process by Uster Tester III)

  • 최병희;김한수
    • 한국잠사곤충학회지
    • /
    • 제34권1호
    • /
    • pp.72-80
    • /
    • 1992
  • These studies were brought about to know how much the elctronic methods of raw silk testing is correct, effective and convenient in the testing process. These effectiveness and convenience for the testing process under the emergency of the automatic system in raw silk inspecting process, the convenience of inspection in crease in it's capability decreasing the necessary working members, but as certain defect, the corresponding time span needs more than the former case in kind. Judging from the above mentioned carefully, it is necessary or even immidiate for participants to deeply study and search in earnest as well, before adopting the so called International Method of Raw Silk Test and Classification which was proposed by S.S.C in 1990.

  • PDF

옻나무 추출액에 의한 견직물, 나일론 직물의 염색성과 자외선 차단성 (Dyeing Properties and Ultraviolet-cut Ability of Silk and Nylon Fabrics Dyed with Rhus verniciflua Extracts)

  • 최인려
    • 복식문화연구
    • /
    • 제16권1호
    • /
    • pp.158-165
    • /
    • 2008
  • The purpose of this study was to investigate the dyeing property and ultraviolet-cut ability on silk 100% and nylon 100% fabrics dyed with Rhus verniciflua extracts. This study was investigated K/S values, surface color, washing fastness, dry cleaning fastness and ultraviolet-cut ability of the silk and nylon fabrics dyed with Rhus verniciflua extracts under the various dyeing conditions. As mordanting were used Tin(II) Chloride dihydrate $(SnCl_2{\cdot}2H_2O)$, Copper(II) sulfate pentahydrate$(CuSO_5{\cdot}5H_2O)$, Iron(II)Chloride$(FeC_2{\cdot}4H_2O)$. pH was adjusted by sodium carbonate$(Na_2CO_3)$ and formic acid(HCOOH). The optimum dyeing temperature, dyeing time, and pH of the silk fabrics dyed with Rhus verniciflua extracts were $90^{\circ}C$, 100min, and in the nylon fabrics were $90^{\circ}C$, 45min. It were colored(munsell value) 6.4Y 7.5/4.1 in the silk fabrics and colored 4.3Y 6.6/5.9 in the nylon fabrics dyed with Rhus verniciflua extracts. Washing fastness and dry-cleaning fastness in the silk and nylon fabrics dyed with mordanting agent improved in $4{\sim}5$ grade. UV-A test showed that nylon fabrics a high rate of 92% with Rhus verniciflua extracts.

  • PDF

견의 결정성에 관한 연구(II) -견 피브로인의 산 처리에 의한 결정화와 황변억제효과에 대하여- (A Study on the Crystallinity in Silk Fibers(II) -Crystallization in Silk Fibroin by Acid Treatment and Its Photoyellowing Reduction Effect-)

  • 장정대;최석철
    • 한국염색가공학회지
    • /
    • 제6권2호
    • /
    • pp.24-29
    • /
    • 1994
  • In order to investigate the crystallization in silk fibroin induced by acid treatment and its photo-yellowing reduction effect. silk fibroin were immersed in PH 3.5~4.0 sulfuric acid and 0.01N hydro-chloric acid at 2$0^{\circ}C$, and the changes of crystallinity were measured by infrared spectroscopy, X-ray diffraction. Yellowness index caused by UV irradiation were also observed. The results are as follows : 1. ${\beta}$-form transition occurs when the silk fibroin are immersed at 2$0^{\circ}C$ in pH 3.5~4.0 sulfuric acid and 0.01N hydro-chloric acid. Formation of new hydrogenbond in molecules on the amorphous region induced ${\beta}$-form structure, and increased crystallinity. 2. Crystallization owing to $\beta$-form transition reduced the initial yellowness index by ultraviolet irradiation.

  • PDF