• 제목/요약/키워드: Shear adhesion strength

검색결과 232건 처리시간 0.024초

Kevlar-29 섬유강화 복합재료의 기계적 계면 특성 연구 (Studies on Mechanical Interfacial Properties of Kevlar-29 Fibers Reinforced Composites)

  • Park, Soo-Jin;Seo, Min-Kang;Ma, Tae-Jun;Lee, Jae-Rock
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2001년도 추계학술발표대회 논문집
    • /
    • pp.158-162
    • /
    • 2001
  • The effects of chemical treatment on Kevlar-29 fibers have been studied in a composite system. The surface characteristics of the Kevlar-29 fibers were characterized by pH, acid-base value and X-ray photoelectron spectroscopy (XPS). The mechanical interfacial properties of final composites were studied by interlaminar shear strength (ILSS) and critical stress intensity factor ($K_{IC}$). Also, the impact properties of the composites were investigated in the differentiating studies between initiation and propagation energies, and ductile index (DI) along with maximum farce and total energy. It was found that the chemical treatment with phosphoric acid ($H_3PO_4$) solution significantly affected the degree of adhesion at interfaces between fibers and resin matrix, resulting in improving the mechanical interfacial strength of the composites. This was probably due to the presence of chemical polar groups on Kevlar surfaces, leading to an increment of interfacial binding force in a composite system.

  • PDF

A STUDY ON THE ADHESION OF A SOFT LINER CONTAINING 4-META TO THE BASE METAL ALLOY AND ITS VISCOELASTIC PROPERTY

  • Park Hyun-Joo;Kim Chang-Whe;Kim Yung-Soo
    • 대한치과보철학회지
    • /
    • 제41권6호
    • /
    • pp.732-746
    • /
    • 2003
  • Statement of problem. Soft lining materials, also referred to as tissue conditioning materials, tissue heating materials, relining materials, soft liners or tissue conditioners, were first introduced to dentistry by a plastic manufacturer in 1959. Since the introduction of the materials to the dental field, their material properties have been continually improved through the effort of many researchers. Soft lining materials have become widely accepted, particularly by prosthodontists, because of their numerous clinical advantages and ease of manipulation. Unfortunately, few reports have been issued upon the topic of increasing the bond strength between the base metal alloy used in cast denture bases and PMMA soft liner modified with 4-META, nor upon the pattern of debonding and material change in wet environment like a intra oral situation. Purpose. The purposes of this study were comparing the bond strength between base metal alloy used for the cast denture bases and PMMA soft liner modified with 4-META, and describing the pattern of debonding and material property change in wet environment like the intraoral situation. Material and Methods. This study consisted of four experiments: 1. The in vitro measurement of shear bond strength of the adhesive soft liner. 2. The in vitro measurement of shear bond strength of the adhesive soft liner after 2 weeks of aging. 3. A comparison of debonding patterns. 4. An evaluation the Relation time of modified soft liner. The soft liner used in this study was commercially available as Coe-soft (GC America.IL.,USA), which is provided in forms of powder and liquid. This is a PMMA soft liner commonly used in dental clinics. The metal primer used in this study was 4-META containing primer packed in Meta fast denture base resin (Sun Medical Co., Osaka, Japan). The specimens were formed in a single lap joint desist which is useful for evaluating the apparent shear bond strength of adhesively bonded metal plate by tensile loading. Using the $20{\times}20mm$ transparent grid, percent area of adhesive soft liner remaining on the shear area was calculated to classify the debonding patterns. To evaluate the change of the initial flow of the modified adhesive soft liner, the gelation time was measured with an oscillating rheometer (Haake RS150W/ TC50, Haake Co., Germany). It was a stress control and parallel plate type with the diameter of 35mm. Conclusion. Within the conditions and limitations of this study, the following conclusions were drawn as follows. 1. There was significant increase of bond strength in the 5% 4-META, 10% 4-META containing groups and in the primer coated groups versus the control group(P<0.05). 2. After 2 weeks of aging, no significant increase in bond strength was found except for the group containing 10% 4-META (P<0.05). 3. The gelation times of the modified soft liner were 9.3 minutes for the 5% 4-META containing liner and 11.5 minutes for the 10% 4-META liner. 4. The debonding patterns of the 4-META containing group after 2 weeks of aging were similar to those of immediaely after preparation, but the debonding pattern of the primer group showed more adhesive failure after 2 weeks of aging.

Analytic adherend deformation correction in the new ISO 11003-2 standard: Should it really be applied?

  • Ochsner, A.;Gegner, J.;Gracio, J.
    • 접착 및 계면
    • /
    • 제5권2호
    • /
    • pp.14-26
    • /
    • 2004
  • For reliable determination of mechanical characteristics of adhesively bonded joints used e.g. as input data for computer-aided design of complex components, the thick-adherend tensile-shear test according to ISO 11003-2 is the most important material testing method. Although the total displacement of the joint is measured across the polymer layer directly in the overlap zone in order to minimize the influence of the stepped adherends, the substrate deformation must be taken into account within the framework of the evaluation of the shear modulus and the maximum shear strain, at least when high-strength adhesives are applied. In the standard ISO 11003-2 version of 1993, it was prescribed to perform the substrate deformation correction by means of testing a one-piece reference specimen. The authors, however, pointed to the excessive demands on the measuring accuracy of the extensometers connected with this technique in industrial practice and alternatively proposed a numerical deformation analysis of a dummy specimen. This idea of a mathematical correction was included in the revised ISO 11003-2 version of 2001 but in the simplified form of an analytical method based on Hooke's law of elasticity for small strains. In the present work, it is shown that both calculation techniques yield considerably discordant results. As experimental assessment would require high-precision distance determination (e.g. laser extensometer), finite element analyses of the deformation behavior of the bonded joint are performed in order to estimate the accuracy of the obtained substrate deformation corrections. These simulations reveal that the numerical correction technique based on the finite element deformation modeling of the reference specimen leads to considerably more realistic results.

  • PDF

매입형 합성보의 전단합성거동에 대한 비교분석 (Analysis of the Load Carrying Behavior of Shear Connection at the Interface of Encased Composite Beams)

  • 신현섭;허병욱;배규웅;김긍환
    • 한국강구조학회 논문집
    • /
    • 제20권1호
    • /
    • pp.67-79
    • /
    • 2008
  • 본 연구에서는 매입형 합성보에서 전체 보의 휨거동 및 합성면에서의 상대변위(Slip) 등을 분석함으로써 화학적 부착, 부착파괴 후 기계적 맞물림 및 마찰작용, 전단 스터드가 합성보 전체의 강도 및 강성과 합성단면에서의 전단합성거동에 기여하는 정도를 해석해 보고자 한다. 이를 위해 U자형 성형강판을 이용한 합성보 및 CT형강 용접방식 강판성형 합성보에 대해 구조성능 실험과 유한요소해석을 수행하였다. 실험 및 해석결과에 의하면, 전단 스터드의 설치 유무에 따라 매입형 합성보의 극한 모멘트성능 차이는 약 10% 미만을 나타내었다. 이것은 강재 보의 단면형상으로 인한 화학적 및 기계적 부착력이 크기 때문에 이에 의한 합성작용으로도 일정 이상의 모멘트성능 발휘가 가능하여 완전합성상태에 해당하는 소성 모멘트내력과의 차이가 비교적 크지 않으며, 합성율이 증가하는 것에 비해 휨모멘트 내력은 완만하게 증가하기 때문으로 나타났다.

고막 패각의 콘크리트 잔골재로 재활용 방안에 관한 연구 (A Study Properties of concrete Recycling Cockle Shells as Fine Aggregate)

  • 김정섭;김광섭;김판선
    • 한국건축시공학회지
    • /
    • 제4권1호
    • /
    • pp.141-146
    • /
    • 2004
  • 1) As a result of compressive strength experiment, rupture compressive strength showed more increases in specimens of 15% and 20% of Cockle shells in those of non-mixture. Comparing compressive strength between no-mixed Specimens and Specimens of containing Cockle shells, Specimens containing Cockle shells showed higher strength in 60 days and 90 days of age, and as ark Cockle is contained and age is elapsed, compressive strength is also increased In addition, estimation of compressive strength by reactive hardness in concrete using Cockle shells as aggregate shows low reliability. 2) As a result of experimenting compressive strength after heating, Specimens containing Cockle shells and non-mixed Specimens showed similar strength at $200^{\circ}C$, but compressive strength was lowered as content of Cockle shells increased at over $400^{\circ}C$ and heating temperature was higher. It is because Cockle shells was fired by heat and then its adhesion and bonding capacity were lost. 3) To sum up the above experimental results, it is found that using splitted Cockle shells as aggregate for concrete by 10%~20% showed the same or higher compressive strength and shear strength as concretes using general aggregate and it can be used as substitute aggregate of concrete. It is considered that for future use of splitted Cockle shells as substitute concrete aggregate, continuous researches of its durability, applicability and economy are needed.

Preparation of Solventless UV Curable Thermally Conductive Pressure Sensitive Adhesives and Their Adhesion Performance

  • Baek, Seung-Suk;Park, Jinhwan;Jang, Su-Hee;Hong, Seheum;Hwang, Seok-Ho
    • Elastomers and Composites
    • /
    • 제52권2호
    • /
    • pp.136-142
    • /
    • 2017
  • Using various compositions of thermally conductive inorganic fillers with boron nitride (BN) and aluminum oxide ($Al_2O_3$), solventless UV-curable thermally conductive acrylic pressure sensitive adhesives (PSAs) were prepared. The base of the PSAs consists of 2-ethylhexyl acrylate, 2-hydroxyethyl acrylate, and isobornyl acrylate.The compositions of the thermally conductive inorganic fillers were 10, 15, 20, and 25 phr in case of BN, and 20:0, 15:5, 10:10, 5:15, and 0:20 phr in case of $BN/Al_2O_3$. The adhesion properties like peel strength, shear strength, and probe tack, and the thermal conductivity of the prepared PSAs were investigated with different thermally conductive inorganic filler contents. There were no significant changes in photo-polymerization behavior with increasing BN or $BN/Al_2O_3$ content. Meanwhile, the conversion rate and transmittance of the PSAs decreased and their thermal stabilities increased with increasing BN content. Their adhesion properties were also independent of the BN or $BN/Al_2O_3$ content. The dispersibility of BN in the acrylic PSAs was better than that of $Al_2O_3$ and it ranked the thermal conductivity in the following order: BN > $BN/Al_2O_3$ > $Al_2O_3$.

실란커플링제 처리가 폴리케톤섬유/에폭시 복합재료의 계면접착성 및 물성에 미치는 영향 (Effect of Silane Coupling Agent on the Interfacial Adhesion and Mechanical Properties of Polyketone Fiber Reinforced Epoxy Composites)

  • 조하니;양지우;임현수;오우진;이승구
    • 한국염색가공학회지
    • /
    • 제29권2호
    • /
    • pp.77-85
    • /
    • 2017
  • The interfacial adhesion between fiber and matrix affects the physical properties of fiber reinforced composites. In this study, 3-(Methacryloyloxy)propyltrimethoxy silane(MPS) coupling agent was used to increase the interfacial adhesion between polyketone fiber and epoxy resin. The change of surface chemical composition of polyketone fiber treated with MPS was analyzed using a FTIR-ATR. The interfacial bonding between fiber and resin increased with silane coupling agent largely. Consequently, interfacial shear strength(IFSS) was enhanced with increasing concentration of MPS coupling agent and thus, the physical properties of the composites such as flexural properties and dynamic mechanical properties were changed. Flexural strength and modulus increased when the MPS concentration was higher than 0.5wt%. The dynamic storage modulus of Polyketone/Epoxy composites treated with MPS was higher than that of the untreated one. When the MPS concentration of 3wt%, the highest storage modulus was obtained.

Retention of Endothelial Cells adhered on Polyurethane Surface under Flow Condition

  • Chang, Jun-Keun;Chang, Hyun-A;Kim, Jin-Hee;Kim, Jong-Won;Han, Dong-Chul;Min, Byoung-Goo
    • 대한의용생체공학회:의공학회지
    • /
    • 제17권3호
    • /
    • pp.355-364
    • /
    • 1996
  • Construction of the stable monolayer of endothelial cells onto physicochemically modified polymeric surFace is one of the appropriate method to develop the small caliber vascular graft with the long-term patency. In this study, we constructed the monolayer of endothelial cells on the fibronectin rind the extracellular matrix-coated polyurethane surface derived from human fibroblast cells. To elucidate the adhesion strength of endothelial cells on the extracellular matrix-coated polyurethane, a laminar flow chamber apparatus was developed to exposure the shear stress on the apical membrane of ondothelial cells. Endothelial cells show the strongest adhesion after two days of seeding onto the fibronectin-coated polyurethane surface, whereas endothelial cells on the extracellular matrix derived from the human flbroblast cells show the minimal doubling time of cellular growth.

  • PDF

Effects of different primers on indirect orthodontic bonding: Shear bond strength, color change, and enamel roughness

  • Tavares, Mirella Lemos Queiroz;Elias, Carlos Nelson;Nojima, Lincoln Issamu
    • 대한치과교정학회지
    • /
    • 제48권4호
    • /
    • pp.245-252
    • /
    • 2018
  • Objective: We aimed to perform in-vitro evaluation to compare 1) shear bond strength (SBS), adhesive remnant index (ARI), and color change between self-etched and acid-etched primers; 2) the SBS, ARI and color change between direct and indirect bonding; and 3) the enamel roughness (ER) between 12-blade bur and aluminum oxide polisher debonding methods. Methods: Seventy bovine incisors were distributed in seven groups: control (no bonding), direct (DTBX), and 5 indirect bonding (ITBX, IZ350, ISONDHI, ISEP, and ITBXp). Transbond XT Primer was used in the DTBX, ITBX, and ITBXp groups, flow resin Z350 in the IZ350 group, Sondhi in the ISONDHI group, and SEP primer in the ISEP group. SBS, ARI, and ER were evaluated. The adhesive remnant was removed using a low-speed tungsten bur in all groups except the ITBXp, in which an aluminum oxide polisher was used. After coffee staining, color evaluations were performed using a spectrophotometer immediately after staining and prior to bonding. Results: ISONDHI and ISEP showed significantly lower SBS (p < 0.01). DTBX had a greater number of teeth with all the adhesive on the enamel (70%), compared with the indirect bonding groups (0-30%). The ER in the ITBX and ITBXp groups was found to be greater because of both clean-up techniques used. Conclusions: Direct and indirect bonding have similar results and all the primers used show satisfactory adhesion strength. Use of burs and polishers increases the ER, but polishers ensure greater integrity of the initial roughness. Resin tags do not change the color of the teeth.

포푸라와 일본잎갈나무의 집성재 제조에 관한 연구 (A Study on the Fabrication of the Laminated Wood Composed of Poplar and Larch)

  • 조재명;강선구;김기현;정병재
    • Journal of the Korean Wood Science and Technology
    • /
    • 제2권2호
    • /
    • pp.25-31
    • /
    • 1974
  • 포푸라와 일본잎갈나무는 속성조림 수종으로 적극 장려되고 있으나 구조용재로서 저재질인 까닭에 그 이용도가 제한되고 있다. 따라서 이들의 이용도 증진과 수요의 안정화를 위하여 대량으로 소비되는 일반 건축용재로 이용할 수 있는 형질의 개량과 강도 증진을 목적으로 임업시험장에서 1967년부터 포푸라와 일본잎갈나무의 집성재 제조조건을 구명하기 위하여 본 시험연구를 시작하여 현재까지 포푸라와 일본잎갈나무의 접착, scarf 접착성능과 실대형통직, 만곡 집성재의 제조조건 및 이 수종 구성집성재 제조에 의한 포푸라재의 집성강도 증진과 lamina 형질이 집성 강도에 마치는 영향을 구명한 결과 다음과 같은 결론을 얻었다. 1. 접착제 Resorcinol Plyophen #6000에 의한 미류(Populus deltoides)와 일본잎갈나무(Larix leptolepis)의 단일 수종, 이수종 접착성능, 방부처리, 미류의 접착성능과 미류와 일본잎갈나무의 scarf 접속 정착성능 및 방부처리, 마류의 scarf 접착성능을 구명한 결과 1.1 Block 전단 및 안장선단 시험에 의한 접착성능은 평균 목파율이 65%로 우수하였고, 미류는 촉단면이 경단면보다, 일본잎갈나무는 경단면이 촉단면 보다 접착성이 양호하였다(표 1, 2참조). 1. 2 방부제 Na-PCP는 resorcinol 수지 접착제의 접착력에 영향 하였으나 집성재 제조에 요구되는 접착력에는 영향하지 않았다(표 3, 4참조). 1. 3 Plane scarf joint 접착에 있어서 안전한 scarf비는 일본잎갈나무 1/12이상, 미류는 1/6이상이 요구되고 방부처리 미류의 plane scarf joint 접착의 안전 scarf 비도 무처리재와 같이 1/6 이상이 요구되었다(표 5, 6, 7 및 8참조). 2. 접착제 Resorcinol Plyophen #6000에 의한 미류와 일본잎갈나무의 단일 수종 및 이수종구성 집성재의 상대 접착력과 삶음반복 접착력 및 접착층의 박리시험에 의한 접착성능을 구명한 결과 2.1 실대형 통직, 만곡 집성재의 block 전단 상태 접착강도는 허용 최소상태 접착강도의 3배 이상이였으며 삶음반복 접착 강도는 상태접착 강도의 1/2로 감소 되었으나, 허용 최소 기준 삶음반복 접착강도의 2배 이상으로 실대형 내수 집성재 제조의 안전성이 확인되였다(표 9 및 10참조). 2.2 실대형 통직, 만곡집성재의 박리율은 미류, 이수종(일본잎갈나무+미류), 일본잎갈나무의 순으로 높았으나 최대치는 일본잎갈나무의 통직집성재(3.5%)로서 허용 최대 기준율보다 적었다.(표 11 참조) 3. urea 수지 접착제에 의한 이태리포푸라(Populus euramericana)와 일본잎갈나무의 단수종, 이수종 및 lamina 형질에 따른 5 ply 구성 통직 접성재의 휨강도 시험, 압축강도 시험에 의한 집성강도와 접착성능을 구명한 결과 3.1 집성강도가 요구되는 건축 구조용재를 목적으로 이태리포푸라와 일본잎갈나무의 이수종 구성 집성재를 제조할 때에는 수종 구성을 L(일본잎갈나무)+P(이태리포푸라)+L+P+L로 하는 것이 양호하였다.(표 12참조) 3.2 수심과 옹이를 가지는 lamina로 구성된 집성재의 경성 강도는 무결점 lamina로 구성된 집성재 강도보다 현저히 강도가 감소되므로 강도가 요구되는 구조용재로서의 집성재 제조에는 이들 결점 부재의 분산 집성이 필요하였다.(표 13참조) 3.3 실대형 통직 집성재의 FPL 전단 상태 접착강도는 허용 최소기준 상태 접착강도의 2배 이상으로 urea 수지접착제로서 이을 수종의 내장주조용 집성재 제조가 가능하였다.

  • PDF