Impact Fracture and Shear Strength Characteristics on Interfacial Reaction Layer of Nb/MoSi2 Laminate Composite

  • Lee, Sang-Pill;Yoon, Han-Ki;Park, Won-Jo
    • International Journal of Ocean Engineering and Technology Speciallssue:Selected Papers
    • /
    • 제3권1호
    • /
    • pp.35-39
    • /
    • 2000
  • The present study dealt with the relationships among the interfacial shear strength, the thickness of interfacial reaction layer and the impact value of $Nb/MoSi_2$ laminate composites. In addition, the tensile test was conducted to evaluate the fracture strain of $Nb/MoSi_2$ laminate composites. To change the thickness of the reaction layer, $Nb/MoSi_2$ laminate composites alternating sintered MoSi2 layers and Nb foils were fabricated as the parameter of hot press temperature. It has been found that the growth of the reaction layer increases the interfacial shear strength and decreases the impact value by localizing a plastic deformation of Nb foil. There also exist appropriate shear strength and the thickness of the reaction layer, which are capable of maximizing the fracture energy of $Nb/MoSi_2$.

  • PDF

Ni-P/Au UBM을 갖는 Pb-free 솔더 접합부의 전단강도 평가에 관한 연구 (A Study on Evaluation of Shear Strength for Pb-free Solder Joint with Ni-P/Au UBM)

  • 조성근;양성모;유효선
    • 한국생산제조학회지
    • /
    • 제20권2호
    • /
    • pp.187-192
    • /
    • 2011
  • UBM(Under Bump Metallurgy) is very important for successful realization of Flip-Chip technology. In this study, it is investigated the interfacial reactions between various Sn-Ag solder alloys and Ni-P/Au UBM and Cu plate finish. It is also evaluated the shear strength by using the micro shear-punch test method for Sn-37Pb alloy, binary and ternary alloys of environment-friendly Pb-free solder alloys which are applied in the electronic packages. In terms of interfacial microstructure, the Pb-free solder joints have thicker IMCs than the Sn-Pb solder joints. The thickness of IMC is related to Reflow time. The IMC has been observed to grow with the increase in Reflow time. As a result of the shear test, in case of Max. shear strength, Pb-free solder showed the highest strength value and Sn-37Pb showed the lowest strength value 10 be generally condition of Reflow time.

상아질 표면 처리 방법에 따른 Compomer의 전단 결합 강도 (SHEAR BOND STRENGTH OF COMPOMER ACCORDING TO DENTIN SURFACE TREATMENT)

  • 오영학;홍찬의
    • Restorative Dentistry and Endodontics
    • /
    • 제26권2호
    • /
    • pp.171-179
    • /
    • 2001
  • The purpose of this study was to evaluate the shear bond strength of compomers according to dentin surface treatment. Two materials of compomer were devided into six groups. The compomer used in this study were Dyract AP(D) and F2000(F), Group 1 (DN) and 4(FN) were treated according to manufacturers instructions as control groups. Group 2(DE) and 5(FE) were treated with 37% phosphoric acid and group 3(DA) and 6(FA) were treated with air abrasion unit (80 psi, 50 m aluminum oxide particles) respectively as experimental groups. After dentin surface treatment, compomers were bonded. Completed samples were stored in 100% humidity. 37C during 7 days, and then, the shear bond strength of specimens were evaluated. The results were as follows: 1. In the case of Dyract AP, the shear bond strength was showed the highest value of 9.10 MPa in dentin surface treatment with air abrasion unit. but there were no significant differences to the other groups. 2. In the case of F2000. the shear bond strength was showed the highest value of 13.51MPa and there were significant differences to the other groups(p<0.05). 3. The shear bond strength of F2000 was higher than Dyract AP in each dentin surface treatment. and in the case of etching and air abrasion. there were significant differences(p<0.05). 4. As a result of observation of SEM. the most of fracture pattern was adhesive failure in group 1(DN), 2(DE) and 4(FN), and cohesive failure in group 3(DA), S(FE) and 6(FA).

  • PDF

고밀도 폴리에틸렌으로 접착한 합판의 접착성질과 해부학적 관찰 (Adhesion Characteristics and Anatomic Scanning of Plywood Bonded by High Density Polyethylene)

  • 한기선;이화형
    • Journal of the Korean Wood Science and Technology
    • /
    • 제25권3호
    • /
    • pp.16-23
    • /
    • 1997
  • This study was carried out to discuss feasibility of high density polyethylene(HDPE) as a new substitute for the conventional adhesives in plywood manufacture. Plywood was composed of radiata pine(Pinus radiata) and Malas(Homallium feotidium) veneers and bonded by HDPE. Adhesion characteristics and anatomical scanning has been examined through tensile-shear strength test and scanning electron microscopy(SEM). The results are as follows; 1. Optimum loading quantity was 15g/$(30.3{\times}30.3)cm^2$, and tensile-shear strength increased with the increase of loading quantity. 2. Even at the hot pressing time of 1 minute, tensile-shear strength met the value of KS(over the 7.5kgf/$cm^2$), and tensile-shear strength increased with the increase of hot pressing time. 3. Plywood composed of veneer at moisture content of 19.6% showed similar tensile-shear strength to that at air conditioned moisture content of 11.4%. 4. Under the same condition of hot pressing time, tensile-shear strength of plywood bonded by HDPE met the KS value of boil and wet test and proved the same group as phenol formaldehyde adhesive. 5. HDPE films showed mechanical adhesion through penetration into the lathe check and ray of veneer.

  • PDF

그루브 압축에 의한 알루미늄의 집합조직 (Texture Development by Groove Pressing in Aluminum)

  • 박종진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 춘계학술대회논문집
    • /
    • pp.206-209
    • /
    • 2000
  • Groove pressing which is analogous to groove rolling in the aspect of deformation mode was designed and influence of the uncommon shear deformation on the development of texture and R value was investigated. Texture developed by the groove pressing were measured as well as predicted. It was found out that the main component in the developed texture was {40。, 45。, 0。} in ODF which was regarded as a rotated Bs component and rarely observed in a plain rolling. The maximum R value was predicted to be 3.8 in 45。 direction which might be attributed to the new component.

  • PDF

LES를 이용한 복단면 개수로의 바닥전단응력 분포특성 분석 (Analysis of Bed Shear Stress Distributions in Compound Open Channels Using Large Eddy Simulation.)

  • 이두한
    • Ecology and Resilient Infrastructure
    • /
    • 제5권4호
    • /
    • pp.199-209
    • /
    • 2018
  • 하천설계에서 제방과 홍수터의 안정성 확보를 위해서는 바닥전단응력을 고려하는 것이 필수적이다. 본 연구에서는 다양한 하폭과 수심에 따른 복단면의 바닥전단응력을 모의하여 분포 특성을 분석하였다. 바닥전단응력 분포에 지배적인 영향을 주는 이차류를 모의하기 위하여 OpenFOAM의 large eddy simulation (LES)를 적용하였으며 하폭과 수심을 고려하여 12개의 케이스를 모의하였다. 모의 결과를 이용하여 시간 평균 유속 분포, 이차류 분포, 바닥전단응력 분포 등의 특성에 대하여 분석하였다. 홍수터 바닥전단응력 분포는 전체적으로 홍수터 좌안에서 높은 값이 나타나고 우안 방향으로 감소하는 경향을 확인하였으나 이차류에 의해 상당한 국부적인 변화가 나타남을 확인하였다. 홍수터의 수심이 얕은 경우에는 홍수터의 바닥전단응력이 평균전단응력의 0.8배 이하로 낮은 값이 나타나고 있으나 홍수터의 수심이 깊은 경우에는 평균전단응력의 1.2-1.4배의 높은 값이 나타남을 확인하였다. 홍수터의 폭이 좁은 경우에는 홍수터 우안 측벽의 영향으로 국부적으로 높은 값이 나타나는 것도 확인할 수 있었다.

One-bottle 상아질 접착제의 전단결합강도와 접착성에 관한 부식시간의 효과 (THE EFFECT OF ETCHING TIME ON SHEAR BOND STRENGTH AND ADAPTIBILITY OF ONE-BOTTLE DENTIN ADHESIVE)

  • 박광수;박일윤;조영곤
    • Restorative Dentistry and Endodontics
    • /
    • 제24권1호
    • /
    • pp.240-250
    • /
    • 1999
  • The purpose of this study was to evaluate the effect of different etching time on the shear bond strength and adaptibility of composite to enamel and dentin when used one-bottle adhesive Prime & Bond$^{TM}$ 2.0. The proximal and occlusal surfaces of 88 extracted human molars were ground to expose enamel(n=44) and dentin (=44) using diamond wheel saw. Teeth were randomly assigned to four test groups(n=11) and received the following treatments : Control group were conditioned with 36% phosphoric acid for 20 sec. according to the manufacturer's directions. Experimental 10 sec. group, 30 sec. group and 60 sec. group were conditioned with 36% phosphoric acid for 10 sec., 30 sec. and 60 sec., respectively. Teeth were rinsed and dried for 2 sec. Prime & Bond$^{TM}$ 2.0 were applied according to the manufacturer's directions and Spectrum$^{TM}$ TPH composite resins were bonded to enamel and dentin surfaces. All specimens were stored in distilled water for 24 hours. Eighty specimens were sheared in a Universal Testing Machine with a crosshead speed of 5mm/minute. One way ANOVA and LSD test were used for statistical analysis of the data. Failure modes of all specimens after shear bond strength test were examined and listed. Also, representive postfracture modes and eight specimens were examined under scanning electron microscope. The results of this study were as follows: 1. The shear bond strength to enamel was the highest value in 30 sec. group (20.68${\pm}$8.54MPa) and the lowest value in 10 sec. group (14.92${\pm}$6.07MPa), so there was significant difference of shear bond strength between two groups (p<0.05). But there was no significant difference among other groups (p>0.05). With longer etching time to enamel from 10 sec. to 30 sec., higher the shear bond strength was obtained, but the shear bond strength was decreased at 60 sec. etching time. 2. The shear bond strength to dentin was the highest value in control group (13.08${\pm}$6.25MPa) and the lowest value in 60 sec. group (9.47${\pm}$3.35MPa), but there was no significant difference among the all groups (p>0.05). The eching time over 20 sec. decreased the shear bond strength to dentin. 3. In SEM observation, the enamel and resin interfaces were showed close adaptation with no relation to etching time of enamel. And the dentin and resin interfaces were showed close adaptation at 20 sec. and 30 sec. etching time, but showed some gaps at 10 sec. and 60 sec. etching time. Accordingly, these results indicated that a appropriate etching time in Prime & Bond$^{TM}$ 2.0 was required to be 30 sec. in enamel and 20 sec. in dentin for the high shear bond strength and good adaptation between the composite resin and tooth substance.

  • PDF

Shear Flow 속에 있는 Circular Cylinder 표면의 압력분포 및 경계층 연구 (A study for the pressure distribution and the boundary layer around a circular cylinder in a shear flow)

  • 이상섭
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제27권6호
    • /
    • pp.753-758
    • /
    • 2003
  • In this study. an experiment has been performed to investigate distributions of static pressure around a circular cylinder in a uniform shear flow which is made by a specially designed wind tunnel. From the computation program(BLAYER), various boundary layer value are obtained depending on the shear flow rate. It is basical design data that boundary layer flow phenomenon of nuclear power plant heat exchanger tube surroundings. airfoil. and others flow fields.

Shear-induced microstructure and rheology of cetylpyridinium chloride/sodium salicylate micellar solutions

  • Park, Dae-Geun;Kim, Won-Jong;Yang, Seung-Man
    • Korea-Australia Rheology Journal
    • /
    • 제12권3_4호
    • /
    • pp.143-149
    • /
    • 2000
  • In this article, we considered shear-induced microstructure and rheological behavior of micellar solutions of cationic surfactant, cetylpyridinium chloride (CPC) in the presence of a structure-forming additive, sodium salicylate (NaSal). Shear viscosity, shear moduli and flow birefringence were measured as functions of the surfactant and additive concentrations. In the presence of NaSal, the micellar solution exhibited the non-linear rheological behavior due to the formation of supramolecular structures when the molar ratio of NaSal to CPC exceeded a certain threshold value. Flow birefringence probed the change in micelle alignment under shear flow. At low shear rates, the flow birefringence increased as the shear rate increased. On the other hand, fluctuation of flow birefringence appeared from the shear rate near the onset of shear thickening, which was caused by shear-induced coagulation or aggregation. These results were confirmed by the SEM images of in situ gelified micelle structure through sol-gel route.

  • PDF

A SHEAR BOND STRENGTH OF RESIN CEMENTS BONDED TO PRESSABLE PORCELAIN WITH VARIOUS SURFACE TREATMENTS

  • Lee Jong-Yeop;Im Eui-Bin
    • 대한치과보철학회지
    • /
    • 제41권3호
    • /
    • pp.379-386
    • /
    • 2003
  • Statement of problem. Resin cements are widely used in adhesive dentistry specially on all ceramic restorations. It is needed to find out adequate bonding strength between different porcelain surface treatments, commercially available porcelains, and different resin cement systems. Purpose. The purpose of this study was to evaluate shear bond strength of resin cements bonded to porcelains in three different modalities; 5 different porcelain surface treatments, 3 different resin cement systems and 3 different commercially available pressable porcelains. Material and Method. This study consisted of 3 parts. Part I examined the effect of five different surface treatments on the pressable porcelain. Fifty discs (5 mm in diameter and 3 mm in height) of Authentic porcelain were randomly divided into 5 groups (n = 10). The specimens were sanded with 320 grit SiC paper followed by 600 grit SiC paper. The specimens were treated as follow: Group 1-Sandblasting (aluminum oxide) only, Group 2 - sandblasting/ silane, Group 3 - sandblasting/ acid etching/ silane, Group 4 - acid etching only, Group 5 - acid etching/ silane. Part II examined the shear bond strength of 3 different resin cement systems (Duolink, Variolink II, Rely X ARC) on acid etching/ silane treated Authentic pressable porcelain. Part 3 examined the shear bond strength of Duolink resin cement on 3 different pressable porcelains (Authentic, Empress I, Finesse). All cemented specimens were stored in distilled water for 2 hours and tested with Ultradent shear bond strength test jig under Universal Instron machine until fracture. An analysis of variance(ANOVA) test was used to evaluate differences in shear bond strength. Result. The shear bond strength test resulted in the following: (1) Acid etched porcelains recorded greater shear bond strength values to the sandblasted porcelains. (2) Silane treated porcelains recorded greater shear bond strength values to non-silane treated porcelains. (3) There was no significant difference between sandblasting/ acid etching/ silane treated and acid etching/ silane treated porcelains. However those values were much higher than other three groups. (4) The shear bond strength with Variolink II was lower than the value of Duolink or Rely X ARC. (5) The shear bond strength of Finesse was lower than the value of Authentic or Empress I.