저탄소 그린콘크리트의 내구 특성 (Durability Properties of Low Carbon Green Concrete)

  • 조일호;성찬용
    • 한국농공학회논문집
    • /
    • 제55권6호
    • /
    • pp.11-17
    • /
    • 2013
  • This study was performed to evaluate the chlorine ion penetration resistance, chemical resistance and freezing and thawing resistance used ordinary portland cement, crushed coarse aggregate, crushed sand, river sand, fly ash, limestone powder, blast furance slag powder and superplasticizer to find optimum mix design of low carbon green concrete for structures. The performance of low carbon green concrete used fly ash, limestone powder and blast furnace slag powder were remarkably improved. This fact is expected to have economical effects in the manufacture of low carbon green concrete for offshore structures. Accordingly, the fly ash, limestone powder and blast furnace slag powder can be used for offshore structure materials.

수재사 모릍의 Flow특성에 관한 연구 (An Experimental Study on the Flow Characteristics of Mortar use Quenched Blast-Furnace Slag)

  • 양범석;임남기;이영도;이종균;정란;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.215-222
    • /
    • 1997
  • Flow experimental on not to be solid mortar which use Quenched Blast-furnace Slag as a fine aggregate was carried out for basic research data about fundamental study of application possibility of Quenched Blast-furnace Slag as a fine aggregate. It gives following result. The substitution rate is inversely proportional to Flow and C/S-rate same that. The relation with W/C-rate augment appear proportional : in case of C/S-rate, 1:3 increasing degree is a half of sand mortar that. Consequencely, Quenched Blast-furnace Slag motar is a counteraction to Flow in as same water content per unit. But suitable substitution rate and C/S-rate influence a little to the mortar consistency. And that reason, if C/S-rate and substitution rate will be regulated when we mix the mortar with quenched Blast-furnace Slag. that will be economic mixture.

  • PDF

페로니켈 슬래그 골재를 활용한 비소성 시멘트 모르타르의 강도 특성 (Strength of Non-Sintered Cement Mortar Using Ferro-nickel Slag Aggregate)

  • 윤민식;나형원;형원길
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 봄 학술논문 발표대회
    • /
    • pp.17-18
    • /
    • 2022
  • Carbon dioxide emissions in the construction sector account for 38% of all industries, and environmental destruction is occurring due to indiscriminate use of natural resources. The purpose of this study is to develop by-product aggregate Non-Sintered Cement(NSC) that can replace sand used as natural aggregate and Portland cement. Therefore, Ground Granulated Blast Furnace Slag, Type C Fly Ash and Type F Fly Ash are used to replace cement, and water granulated ferro-nickel slag(FNS) is used to replace aggregate. The flow, compressive strength and flexural strength of the formulation using sand as an aggregate and the formulation replacing 100% FNS were compared. As a result of the experiment, the formulation using FNS had higher overall strength than the formulation using sand, and as the substitution rate of Type C fly ash increased, the strength was the best. Formulation using FNS is more fluid than using sand. Through this study, we show the possibility of 100% substitution of FNS and its applicability to secondary concrete products of by-product aggregate NSC.

  • PDF

트라우즐 연주시험과 수치해석에 의한 전색 매질별 발파효과 영향에 관한 연구 (Study on Blast Effects of Stemming Materials by Trauzl Lead Block Test and Numerical Analysis)

  • 고영훈;김승준;;양형식
    • 화약ㆍ발파
    • /
    • 제35권4호
    • /
    • pp.19-26
    • /
    • 2017
  • 트라우즐 연주시험은 폭발물의 영향을 측정하기 위한 방법 중 하나이다. 일정크기 연주기둥 중앙의 발파공 내부에서 폭발에 의한 용적 확대량을 측정하여 폭발력을 측정하는데 이용된다. 본 연구에서는 발파공 내부 폭약주변의 채움재에 따른 폭발영향을 비교분석하기 위하여 트라우즐 연주시험 및 AUTODYN 수치해석을 하였다. 사용폭약은 일반 에멀젼 폭약을 적용하였고, 디커플링 조건과 모래, 물, 젤라틴의 충전재를 선정하였다. 시험 및 수치해석 결과 연주블록 발파공의 확대 정도는 물과 젤라틴이 유사하였고, 모래, 디커플링 조건 순으로 확대치를 나타냈다. 또한 연주기둥 외곽에서 측정한 동적 변형률 및 수치해석 전달압력의 경우 시험결과와 상응하였고, 같은 양상을 확인할 수 있었다.

고로슬래그와 극한미생물을 이용한 모래의 고결화 연구 (A Study on Cementation of Sand Using Blast Furnace Slag and Extreme Microorganism)

  • 박성식;최선규;남인현
    • 한국지반공학회논문집
    • /
    • 제30권1호
    • /
    • pp.93-101
    • /
    • 2014
  • 본 논문에서는 자원 재활용을 위해 시멘트를 전혀 사용하지 않고 잠재 수경성을 지닌 고로슬래그와 알칼리 활성화제를 이용하여 모래를 고결시키는 연구를 수행하였다. 기존 수산화칼슘이나 수산화나트륨과 같은 화학적 알칼리 활성화제뿐 아니라 pH 10 이상에서 생존하는 극한미생물을 화학적 알칼리 활성화제에 혼합한 미생물 알칼리 활성화제를 개발하여 흙의 고결 가능성을 평가하였다. 낙동강모래에 고로슬래그의 함유량을 네 종류(4, 8, 12, 16%)로 달리하면서 화학적 또는 미생물 알칼리 활성화제를 혼합하여 공시체를 제작한 다음 7일 동안 대기중 양생시킨 후 일축압축시험을 실시하였다. 알칼리 활성화제의 종류에 관계없이 고로슬래그의 함유량이 4%에서 16%로 증가함에 따라 건조밀도가 증가하면서 일축압축강도는 평균 178kPa에서 2,435kPa까지 증가하였다. 화학적 알칼리 활성화제를 사용한 경우, 수산화칼슘이 포함된 공시체의 일축압축강도가 수산화나트륨을 사용한 경우보다 5-54% 정도 높게 나타났다. 한편 본 연구에서 개발한 미생물 알칼리 활성화제를 사용한 경우, 수산화칼슘 성분이 포함된 공시체의 경우에는 화학적 알칼리 활성화제보다 일축압축강도가 11-60% 감소하였으나, 수산화나트륨이 포함된 경우에는 일축압축강도가 19-121% 증가하였다. 고결된 공시체에서 C-S-H 화합물이 생성되었으며, SEM분석에서 고로슬래그 함유량이 증가할수록 수화물의 양도 증가하였다.

순환잔골재 치환율 변화에 따른 3성분계 무기결합재 모르타르의 유동 및 강도특성 (Flowing and Strength Properties of Ternary System Inorganic Composite Mortar according to the Change of Replacement Ratio of Recycled Sand)

  • 배상우;박종필;김규용;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 춘계 학술논문 발표대회
    • /
    • pp.99-100
    • /
    • 2012
  • This study tried to present the appropriate replacement ratio of the recycled sand through the properties of the ternary system inorganic composite mortar according to replacement ratio change of the recycled sand about the natural sand through test verification. The flowing and compressive strength was degraded as the replacement ratio of the experimental result recycled sand increased. The appropriate replacement ratio of the recycled sand according to it was shown up less than 15%.

  • PDF

고로수쇄 슬래그 잔골재의 품질에 대한 고찰 (A Study on the Quality of the Water Coold Blast Furnace Slag Fine Aggregate)

  • 문한영;최연왕;김기형
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1990년도 봄 학술발표회 논문집
    • /
    • pp.24-28
    • /
    • 1990
  • The purpose of this study is to examine through the experimental study whether the water cooled unprocessed blast furnace slag produced in the country is useful for the fine aggregate of concrete or not. The results of this study show that the quality of the water cooled blast furnace slag is inferior to that of natural river sand and that the concrete made by substituting the water cooled blast furnace slag for fine aggregate have a tendency to decrease to some extent in strength. But if the water cooled blast furnace slag is transformed into more hardened state material, to use it as the fine aggregate of concrete will be possible.

  • PDF

고로슬래그와 알칼리 활성화제를 이용한 모래 고결 및 조기강도에 관한 연구 (A Study on Sand Cementation and its Early-Strength Using Blast Furnace Slag and Alkaline Activators)

  • 박성식;최선규
    • 한국지반공학회논문집
    • /
    • 제29권4호
    • /
    • pp.45-56
    • /
    • 2013
  • 본 연구에서는 자원 재활용을 위해 시멘트를 전혀 사용하지 않고 잠재 수경성을 지닌 고로슬래그를 이용하여 사질토를 고결시키고자 하였다. 알칼리 활성화제에 의해 경화되는 고로슬래그의 함유량과 알칼리 활성화제의 종류를 달리 하여 이들이 사질토의 조기강도에 미치는 영향에 대하여 연구하였다. 고로슬래그의 함유량을 사질토의 4, 8, 12, 16%로 하고 여섯 종류(두 종류의 천연재료, 네 종류의 화학약품)의 알칼리 활성화제를 사용하여 공시체를 제작하였다. 제작한 공시체는 3일 또는 7일 동안 대기중 양생한 다음 일축압축강도시험을 실시하였다. 알칼리 활성화제 종류에 따른 일축압축강도는 탄산칼륨, 수산화칼슘, 수산화나트륨, 수산화칼륨 순으로 높게 측정되었으며, 동일한 성분을 가진 천연재료보다 화학약품을 사용한 공시체의 일축압축강도가 높게 나타났다. 3일 양생한 공시체 중 최대 일축압축 강도가 발현된 것은 16%의 고로슬래그에 수산화칼륨을 사용한 경우로 3MPa 정도의 강도가 측정되었으며, 이는 초속 경시멘트 16%를 사용한 공시체 강도의 37%에 해당된다. 알칼리 활성화제 종류에 관계없이 고로슬래그 함유량이 증가함에 따라 건조밀도가 증가하면서 일축압축강도도 증가하였으며, 양생기간이 3일에서 7일로 증가함에 따라 최대 97%의 강도 증가가 발생하였다. 고결된 모래의 XRD 분석 결과 C-S-H 화합물이 생성되었으며, SEM 분석 결과에서는 고로슬래그 함유량이 증가할수록 생성되는 수화물도 증가하여 모래 입자를 에워싸는 형태를 보였다.

고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구 (A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

Experimental study on rheology, strength and durability properties of high strength self-compacting concrete

  • Bauchkar, Sunil D.;Chore, H.S.
    • Computers and Concrete
    • /
    • 제22권2호
    • /
    • pp.183-196
    • /
    • 2018
  • The rheological behaviour of high strength self compacting concrete (HS-SCC) studied through an experimental investigation is presented in this paper. The effect of variation in supplementary cementitious materials (SCM) $vis-{\grave{a}}-vis$ four different types of processed crushed sand as fine aggregates is studied. Apart from the ordinary Portland cement (OPC), the SCMs such as fly ash (FA), ground granulated blast furnace slag (GGBS) ultrafine slag (UFS) and micro-silica (MS) are used in different percentages keeping the mix -paste volume and flow of concrete, constant. The combinations of rheology, strength and durability are equally important for selection of mixes in respect of high-rise building constructions. These combinations are referred to as the rheo-strength and rheo-durability which is scientifically linked to performance based rating. The findings show that the fineness of the sands and types of SCM affects the rheo-strength and rheo-durability performance of HS-SCC. The high amount of fines often seen in fine aggregates contributes to the higher yield stress. Further, the mixes with processed sand is found to offer better rheology as compared to that of mixes made using unwashed crushed sand, washed plaster sand, washed fine natural sand. The micro silica and ultra-fine slag conjunction with washed crushed sand can be a good solution for high rise construction in terms of rheo-strength and rheo-durability performance.