자외선 가속열화에 따른 옥외용 폴리머 절연재료의 표면열화 분석 (Analysis of Surface Degradation on Accelerated UV-treated Polymeric Housing Materials for Outdoor Insulator)

  • 연복희;이상용;허창수;심대섭;조한구
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제50권10호
    • /
    • pp.479-488
    • /
    • 2001
  • The effects of accelerated Ultraviolet (UV) radiation on High temperature vulcanized (HTV), Room temperature vulcanized (RTV) silicone rubber and two types of ethylene propylene diene terpolymer (EPDM) used for composite insulator were inverstigated by hydrophobicity class (HC), surface voltage decay after corona charging, SEM-EDS, FTIR and XPS. The contact angle in two kinds of silicone rubber was scarcely change, but EPDM occurred to the loss of hydrophobicity followed by surface cracking and chalking. The surface voltage decay on UV-treated silicone rubber and EPDM showed a different decay trend with UV treatment. EDS and XPS analysis indicated that the oxygen content increased with UV treatment time in all samples. For silicone rubber, the oxidized groups of inorganic silica-like structure increased with UV treatment time. The oxidized carbon of C=0, O=C-O in EPDM increased. These oxidized surface for each material had different electrostatic characteristics, so deposited charges were expected to have different impacts on their surface hydrophobicity. The degradation mechanism based on our results was discussed.

  • PDF

Rubber gaskets for fuel cells-Life time prediction through acid ageing

  • Kim, Mi-Suk;Kim, Jin-Kuk
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2007년도 추계학술대회 논문집
    • /
    • pp.47-51
    • /
    • 2007
  • The present paper reports the life time prediction of Acrylonitrile-Butadiene rubber (NBR) fuel cell gasket materials as a function of operational variables like acid concentration, ageing time and temperature. Both material and accelerated acid-heat aging tests were carried out to predict the useful life of the NBR rubber gasket for use as a fuel cell stack. The acid ageing of the gasket compounds has been investigated at 120, 140 and $160^{\circ}C$, with aging times from 3 to 600 h and increasing acid ($H_2SO_4$) concentrations of 5, 6, 7 and 10 vol%. Material characteristics the gas compound such as cross-link density, tensile strength and elongation at break were studied. The hardness of the NBR rubber was found to decrease with decreasing acid concentration at both 120 and $140^{\circ}C$, but at $160^{\circ}C$ interestingly the hardness of the NBR rubber increased abruptly in a very short time at different acid concentrations. The tensile strength and elongation at break were found to decrease with increase in both the acid concentrate ion & temperature. The life time of the compounds were evaluated using the Arrhenius equation.

  • PDF

고무 패드 벤딩 공정설계에 관한 실험적 연구 (Experimental Study on Process Design of Rubber Pad Bending)

  • 권혁철;임용택;지동철;이명호
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.407-412
    • /
    • 2000
  • In this study, a research for process design in bending of structural frame of AA6061-T6 with rubber pad was conducted. In this process, the conventional lower die made of metal is replaced with a polyurethane pad, resulting in high flexibility during bending. Vulcanized polyurethane rubber with shore A hardness of 60 was used for the pad. Experiments on a newly developed bending machine were carried out by controlling the stroke of the roller and horizontal movement of roller pad lower die. From this, the relation between roller path and geometry of the materials bent was obtained for the process design of producing roof rail part of a passenger car and the experimental result was compared with the target profile. For more accurate process design, it is required to control the roller path interactively. Based on the experience in developing the prototype bending machine, it is construed that a fully automated bending system with rubber pad to produce various light-weight components for automotive body frames can be successfully developed.

  • PDF

비등온 TGA를 이용한 ACM 고무복합재료의 열분해 거동 연구 (Non-isothermal TGA Study on Thermal Degradation Kinetics of ACM Rubber Composites)

  • 안원술;이형석
    • Elastomers and Composites
    • /
    • 제48권2호
    • /
    • pp.161-166
    • /
    • 2013
  • 비등온 TGA 실험방법을 이용하여 가교 사이트가 서로 다른 chlorine cure-site ACM 고무와 carboxylic cure-site ACM 고무 두 종류에 대하여 열분해 거동을 연구하였다. 분해 반응이 최대인 점의 온도는 모든 승온 속도에서 carboxylic cure-site ACM 고무의 열분해 특성이 상대적으로 더 안정함을 보여 주었다. Kissinger의 해석 방법에 의한 활성화에너지는 chlorine cure-site ACM 및 carboxylic cure-site ACM 고무에 대하여 각각 118.6 및 105.5 kJ/mol로 나타났으며, Flynn-Wall-Ozawa의 해석방법에서의 전환율 0.1~0.2 범위의 평균과 유사한 값을 나타내었다. 반응차수 해석으로부터 두 시험편 모두 일반적인 고무와 유사한 다중 복합반응에 의하여 열분해 반응이 진행됨을 알 수 있었다.

자동차 그로멧의 유한요소해석 및 노화시험에 대한 연구 (A Study on Finite Element Analysis and Aging Test for Automotive Grommet)

  • 이성범;염상훈;한창용;우창수
    • Elastomers and Composites
    • /
    • 제47권3호
    • /
    • pp.201-209
    • /
    • 2012
  • 그로멧은 자동차의 고무부품들 중의 하나로 에틸렌 프로필렌 고무로 구성되어 있으며, 고무의 비선형 초탄성 성질은 고무제품의 거동을 예측하는데 중요하다. 본 논문에서는, 일축인장시험과 이축인장시험을 통하여 안정된 응력-변형률 관계를 구하고 그로멧에 대한 유한요소해석을 수행하였고, 수명예측을 위한 노화시험을 소개하였다.

Synthesis and Properties of High Voltage Silicone Rubber by Platinum-based Flame Retardant

  • Jung, Se-Young;Kim, Byung-Kyu
    • Transactions on Electrical and Electronic Materials
    • /
    • 제7권6호
    • /
    • pp.283-292
    • /
    • 2006
  • So that high-strength and electrical properties apply by excellent high voltage insulator electricity material, ATH content and platinum-based flame retardant that influence in flame retardant and tracking characteristic among composite of silicone rubber studied mechanical strength and influence getting to electrical properties. Composition of ${\alpha}$, ${\omega}-vinyl$ poly (dimethyl-methylphenyl) siloxane(VPMPS) of a polymer quantity made doing mole of D4, $D3^{Me,Ph}$ and VMS by 1000:15:0.2 mole ratio and uses basic catalyst tetramethylammonium silanolate(TMAS) and do opening equilibrium polymerization to be used to main polymer for high voltage insulation insulator. Control ATH content and content of platinum-based flame retardant and made high voltage insulation silicone rubber. Measured mechanical strength of making silicone rubber using UTM, and tracking characteristic according to standard of IEC 60587, flame retardant test studied effect that flame retardant characteristic gets in tracking characteristic, measuring according to UL94V method of test.

고차단성 자동차 부품용 고무소재 (Elastomeric High Barrier Materials for Vehicle)

  • 김진국
    • Elastomers and Composites
    • /
    • 제46권1호
    • /
    • pp.2-9
    • /
    • 2011
  • 가스와 증기에 대한 투과성(Permeability to gases and Vapors)은 고무 제품을 타이어 튜브나 다이아후램(diaphragm)과 같은 제품으로 사용하고자 할 때 아주 중요한 특성이다. 모든 고무는 가스와 증기에 대하여 투과성이 있다. 그러나 그 투과 속도는 고무 재질에 따라 아주 다르다. 일반적으로 실리콘 고무의 투과성이 제일 크고, 그 다음으로 NR, EPDM, SBR, CR, NBR, FPM, ECO, IIR 순이다. 이러한 투과성은 같은 원료고무를 사용해도 사용 배합약품의 종류에 따라 크게 다를 수도 있다. 고무와 기체와의 메커니즘은 발포고무에 매우 중요하게 되어 이에 대한 연구$^{1-7}$는 많이 이루어졌으나 고무의 차단성에 대한 연구는 그리 많지 않다. 고무소재의 투과성 또는 차단성 기능을 주기위하여 나노복합탄성체$^8$의 기술 동향 및 코팅에 의한 기능성 향상$^{9-13}$을 하거나 열가소성탄성체 본문에서 적용하는 기술이 있는데 자동차에 사용되는 액체 및 기체 차단용 고무부품에 대하여 몇가지 소개하여 본다.

침적 소독이 고무 인상재의 크기 안정성에 미치는 영향 (THE EFFECT OF IMMERSION DISINFECTION ON THE DIMENSIONAL STABILITY OF RUBBER IMPRESSION MATERIALS)

  • 민권남;방몽숙
    • 대한치과보철학회지
    • /
    • 제36권3호
    • /
    • pp.496-505
    • /
    • 1998
  • The purpose of this study was to evalute the effect of immersion disinfection on the dimensional stability of rubber impression materials. The metallic master model was made in order to simulate the intraoral arch form. Impressions were made from four impression materials (Exaflex, Extrude, Reprosil, Impregum-F) and immersed in three disinfectant solutions (Wydex, Vi-Pon, Potadine). Casts from the impressions were measured according to the interpreparation distance. The A-B and The B-D abutment distance were compared with the control group and disinfected groups. The results were as follows; 1. The measurements of the stone cast increased relative to the master model and there was a significant difference (P<0.05). 2. The relative dimensional change of the stone cast as compared with master model ranged from 0.10% to 0.56% in the A-B distance and ranged from 0.04% to 0.27% in the B-D distance. 3. The dimensional change of the disinfected groups as compared with the control group was significantly different in the three impression materials except for Impregum-F (P<0.05). 4. The relative dimensional change of the disinfected groups compared with the control group ranged from 0% to 0.20% in the A-B distance and ranged from -0.09% to 0.11% in the B-D distance. These results suggest that immersion disinfection of rubber impression materials by chemical disinfectants causes very small dimensional change and the change is clinically acceptable for prothesis fabrication

  • PDF

폐타이어 고무분말 재활용을 위한 화학적 탈황과 기계적 물성 평가 (Chemical Devulcanization for the Recycling of Rubber Powder of Waste Tires and Mechanical Properties)

  • 안주영;박종문;방대석;김봉석;오명훈
    • 자원리싸이클링
    • /
    • 제24권3호
    • /
    • pp.59-65
    • /
    • 2015
  • 세계적으로 폐타이어를 포함한 가황고무제품의 재활용 문제가 심각하게 대두되고 있다. 특히 자동차 수요량이 증대됨에 따라 발생하는 폐타이어는 매립이나 소각 시 가교결합 된 황 성분에 의해 2차 환경오염을 일으킨다. 또한 재생고무로 이용 시 가교 결합된 황에 의해 원료 고무와의 결합을 방해하여 적절한 물성을 가지지 못한다. 따라서 폐타이어 고무분말 재활용을 위해서 탈황 처리와 관련된 기술개발이 활발하게 이루어져 왔다. 탈황 처리 공정을 거쳐 재생된 폐타이어는 원료 고무와 혼합된 후 가황공정을 통하여 용도에 맞는 제품으로 제조 할 수 있다. 본 연구에서는 화학적 탈황법을 이용해 폐타이어를 탈황하여 탈황 정도를 분석하였다. 2-butanol 용액을 이용하여 온도, 탈황처리시간 등의 변수에 따른 탈황 효과를 살펴보았다. 고무시료를 유기용매에 팽윤한 후 100, 150, $200^{\circ}C$에서 1~5hr 동안 탈황처리 하였다. 그 후 평행팽윤법을 이용해서 수평균분자량과 가교밀도를 계산하여 정량적으로 탈황도를 분석하였다. 또한 Hot press를 이용하여 인장시편을 제조한 후 기계적 물성도 평가하였다.

광기능성시트 보호용 천연고무계 점착제의 점착 물성 (Adhesion Performance of Natural Rubber-based Pressure-Sensitive Adhesives for Protecting of Opto-functionalized Sheet)

  • 박영준;임동혁;김현중;송현석;권혁진
    • 접착 및 계면
    • /
    • 제8권2호
    • /
    • pp.15-21
    • /
    • 2007
  • 광기능성시트 보호용 점착제를 제조하기 위하여 천연고무와 DCPD계 점착부여수지, 세 종류의 지방족 점착부여수지를 이용하여 천연고무계 점착제를 제조하였다. 또한, 천연고무의 낮은 응집력을 대체하기 위하여 점착부여수지의 함량이 고정된 상태에서 SIS 블록공중합체를 함량비에 따라 첨가하여 점착제를 제조하였다. 제조한 점착제의 점착물성을 초기점착력과 박리강도로써 평가하였다. 천연고무/점착부여수지의 초기점착력은 점착부여수지의 함량이 증가함에 따라 증가하다 최대값을 보이고 감소하였다. 또한, 지방족계 점착부여수지의 연화점이 증가함에 따라 초기점착력이 다소 증가하였다. 점착부여수지의 함량이 50 wt%까지는 박리강도가 증가하였으나 그 이상의 함량에서는 혼합파괴 현상을 보였다. SIS가 블랜드된 점착제의 초기점착력은 지방족계 점착부여수지의 함량이 20~40 wt%에서 최대값을 보였으나 20 wt%에서 fibrillation 현상을 나타내었고 박리강도는 40 wt%에서 최대값을 나타내었다.

  • PDF