S-RCAT (Spherical Recess Cell Allay Transistor) 구조에 따른 FN Stress 특성 열화에 관한 연구 (The Research of FN Stress Property Degradation According to S-RCAT Structure)

  • 이동인;이성영;노용한
    • 전기학회논문지
    • /
    • 제56권9호
    • /
    • pp.1614-1618
    • /
    • 2007
  • We have demonstrated the experimental results to obtain the immunity of FN (Fowler Nordheim) stress for S-RCAT (Spherical-Recess Cell Array Transistor) which has been employed to meet the requirements of data retention time and propagation delay time for sub-100-nm mobile DRAM (Dynamic Random Access Memory). Despite of the same S-RCAT structure, the immunity of FN stress of S-RCAT depends on the process condition of gate oxidation. The S-RCAT using DPN (decoupled plasma nitridation) process showed the different degradation of device properties after FN stress. This paper gives the mechanism of FN-stress degradation of S-RCAT and introduces the improved process to suppress the FN-stress degradation of mobile DRAM.

Effect of Extraction Time on the Rheological Properties of Sericin Solutions and Gels

  • Yoo, Young Jin;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제27권1호
    • /
    • pp.180-184
    • /
    • 2013
  • Recently, silk sericin has attracted the attention of researchers owing to its useful properties as a biomaterial including 1) good wound healing and cell activities, 2) fast gelation character, and 3) high water retention property. In the present study, silk sericin was prepared using different extraction times in hot water and the effect of extraction time on the rheological properties of sericin solutions and gels was examined. It was found that the production yield of sericin increased with extraction time. The shear viscosity of sericin solutions and gels decreased with increasing extraction time due to a decrease in sericin molecular weight. When the sericin solution transformed to a gel, the viscosity increased and the shear thinning behavior was more evident. In addition, the shear stress measurements indicated that the slip between the sericin samples and the measuring plate of the rheometer was increased by the gelation of sericin. The compression strength of sericin gel could be increased remarkably (by more than 100 fold) by preparation using the freezing and thawing method.

Supercapacitive Properties of Composite Electrode Consisting of Activated Carbon and Di(1-aminopyrene)quinone

  • Kim, Kwang Man;Lee, Young-Gi;Park, Jeong Ho;Ko, Jang Myoun
    • ETRI Journal
    • /
    • 제38권2호
    • /
    • pp.252-259
    • /
    • 2016
  • Di(1-aminopyrene)quinone (DAQ) as a quinone-containing conducting additive is synthesized from a solution reaction of 1-aminopyrene and hydroquinone. To utilize the conductive property of DAQ and its compatibility with activated carbon, a composite electrode for a supercapacitor is also prepared by blending activated carbon and DAQ (3:1 w/w), and its supercapacitive properties are characterized based on the cyclic voltammetry and galvanostatic charge/discharge. As a result, the composite electrode adopting DAQ exhibits superior electrochemical properties, such as a higher specific capacitance of up to $160F{\cdot}g^{-1}$ at $100mV{\cdot}s^{-1}$, an excellent high-rate capability of up to $1,000mV{\cdot}s^{-1}$, and a higher cycling stability with a capacitance retention ratio of 82% for the 1,000th cycle.

효소처리에 의한 제지적성 개선

  • 김형진;조병묵
    • 한국펄프종이공학회:학술대회논문집
    • /
    • 한국펄프종이공학회 2000년도 춘계학술발표논문집
    • /
    • pp.39-46
    • /
    • 2000
  • In pulp and papermaking process, enzymatic treatment of pulp fibres has been a topic of increasing interest in last decade. Lots of patents, papers and research reports were published on the application of enzymes in the fields of enzymatic bleaching, deinking, slime control, pitch control, waste water treatment and fibre modification. Cellulase and hemicellulase are the principal enzymes used for the modification of fibre property. This study was carried out for determinating the behaviors of enzyme to pulp fibres. A commercial enzyme, Denimax BT which is consisted with cellulase and hemicellulase, was treated to the kraft pulp produced from domestic hardwood mixtures. Results were mainly concentrated on the behaviors of freeness, drainability and fines content of fibres, and physical properties of paper with enzyme treatment. The freeness levels and dewatering ability were developed, and the fines contents were decreased. The creation of fines were controlled by the method of pre-enzyme treatment prior to fibre beating. The mechanical strength of paper, like tensile, burst, tear strength and folding endurance, were remarkably improved by the pre-enzyme treatment.

  • PDF

첨가제를 병용한 섬유의 물리적 전처리의 효과 (Effect of Papermaking Additives on Fiber Mechanical Pretreatment)

  • 서영범;이민구;하인호;조욱연
    • 펄프종이기술
    • /
    • 제35권4호
    • /
    • pp.1-7
    • /
    • 2003
  • In this study, fiber mechanical pretreatment before refining was executed with the addition of papermaking addiditives to find synergistic effects on fiber property improvement. Three fiber furnishes (SwBKP, KOCC, and BCTMP), and five different additives (CMC, CPAM, PEO, NaOH, $Na_2O_2$) were used. It was confirmed again that fiber mechanical pretreatment using Hobart mixer was a special way to modify fiber properties, where fiber WRV (water retention value) increases without losing fiber length. For SwBKP, addition of small amount of CMC (0.2% OD basis), and for KOCC, PEO (0.2% OD basis) caused additional significant improvement of the fiber furnish properties, respectively. Other additives did not cause adverse effects on the mechanical pretreatment, or better. For BCTMP, NaOH addition followed by mechanical pretreatment caused more than 20% improvement in tensile and tear strength simultaneously, compared to the control. The yellowing caused by the treatment of NaOH on BCTMP could be minimized by using $Na_2O_2$ without losing the positive effect of NaOH.

Al-Fe-Cr-Ti 나노결정 합금분말의 자기펄스 성형 및 마모 특성 (Magnetic Pulsed Compaction of nanostructured Al-Fe-Cr-Ti Powder and wear properties)

  • 김준호;홍순직
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.528-530
    • /
    • 2008
  • The effect of consolidation temperature on the microstructure, density and mechanical properties (especially, wear property) of $Al_{92.5}-Fe_{2.5}-Cr_{2.5}-Ti_{2.5}$ alloy fabricated by gas atomization and magnetic pulsed compaction was investigated. All consolidated alloys consisted of homogeneously distributed fine-grained fcc-Al matrix and intermetallic compounds. Relative higher mechanical properties in the MPCed specimen were attributed to the retention of the nanostructure in consolidated bulk without cracks. The as consolidated bulk by magnetic pulsed compaction showed the enhanced wear properties than that of a general consolidation process. In addition, the wear mechanism and fracture mode of MPCed bulk was discussed.

  • PDF

Variation of the Transport Property in Lap-Jointed YBCO Coated Conductor Tapes with Tension and Bending Deformation

  • Dizon, John Ryan C.;Bonifacio, Rolly;Park, Sung-Taek;Shin, Hyung-Seop
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제9권4호
    • /
    • pp.11-15
    • /
    • 2007
  • In practical applications of HTS tapes for electric devices such as coils and power cables, the jointing of HTS tapes is inevitable even though long length tapes have recently been achieved. The critical current, $I_c$, degradation behaviors with tensile and bending deformations were investigated in commercially available YBCO coated conductor tapes. When the V-I relationship was measured at the jointed section of the lap-jointed YBCO CC tapes, the resistance at the joint decreased with increasing joint length. The critical load for 95% $I_c$ retention were determined for the IBAD and RABiTS YBCO tapes and they were 175 and 355N, respectively. Fracture occurred at the unjointed part which represents strong copper lamination and solder jointing. The electro-mechanical properties of lap-jointed CC tapes depended on the properties of single tapes. The V-I behavior under bending strain was similar with the tensile case.

A/W사로 편성한 1×1 리브편의 물성 평가 (Physical Properties of 1×1 Rib Knitted Fabrics Using A/W)

  • 예수정;김인영
    • 한국의류산업학회지
    • /
    • 제14권4호
    • /
    • pp.629-634
    • /
    • 2012
  • Knitted fabric using acrylic/wool blended yarn (A/W) is increasingly used in the knit industry; subsequently, research on knitted fabric using A/W has increased. This study presents an scientific database from evaluating physical properties of $1{\times}1$ rib stitch using A/W. In this study,$1{\times}1$ rib stitch using A/W were made at various knitting tensions (dial no. 2-6) and the number (4-6) of ply yarn. The physical properties of $1{\times}1$ rib stitch using A/W were measured and analyzed. The density was in the range 5.5-6.4 wales/cm and 4.0-5.6 courses/cm, respectively. The density increased when less plying yarns and more knitting tension were added during knitting. The thickness was in the range of 1.592-2.362 mm and the tensile strength was in the range 32.75-53.63 Kgf/mm. The burst strength was in the range 107.8-139.2 $N/cm^2$. Thickness, tensile strength, and burst strength increased as the number of ply yarn and the knitting tension increased. The elongation and the recovery extension rate were in the range 102.29-112.13% and 96.4-97.7%, respectively. The heat retention rate was in the range 59.3-65.1%. There was no difference of the elongation and the recovery extension rate and the heat retention rate by the knitting tension and the number of the ply yarn. The permeability was in the range 170.5-396.3 $cm^3/cm^2/sec$. Air permeability decreased as the number of ply yarn and the knitting tension increased. The pilling properties were excellent for all $1{\times}1$ rib stitches.

제올라이트 주입이 활성슬러지 플럭에 미치는 영향 (The effect of zeolite addition on floc in activated sludge process)

  • 이형술;박세진;윤태일
    • 청정기술
    • /
    • 제7권1호
    • /
    • pp.35-42
    • /
    • 2001
  • 본 연구에서는 zeolite를 활성슬러지 공정에 주입할 경우 zeolite가 biofloc에 미치는 영향에 대해 알아보기 위해 수행되었다. 두 반응기를 동일 조건으로 운전하였으며 하나는 표준 활성슬러지 공정 (CU)으로, 다른 하나는 zeolite를 폭기조내 4,000 mg/l로 유지 (ZU)하며 비교하였다. 슬러지 플럭 입경을 측정한 결과, 두 반응기 모두 SRT (Solid Retention Time)가 증가함에 따라 플럭 크기도 비례하여 증가하였으나 ZU가 모든 조건에서 CU보다 작은 평균 입경을 나타내었다. 한편, 두 반응기에 대해 슬러지 침전성을 비교한 결과, ZU는 SRT변화에 관계없이 3.4~11m/h의 침전속도를 나타내며 SVI(Sludge Volume Index)도 50~108 ml/g으로 양호한 침전상태를 보였다. 그러나 CU는 SRT 증가에 따라 슬러지 침전성이 큰 영향을 받았고 SRT 40일에서 Sphaerotilus가 우점종을 나타내었으며 이 결과, 슬러지가 전혀 침전하지 않았다.

  • PDF

Metal Biosorption by Surface-Layer Proteins from Bacillus Species

  • Allievi, Mariana Claudia;Florencia, Sabbione;Mariano, Prado-Acosta;Mercedes, Palomino Maria;Ruzal, Sandra M.;Carmen, Sanchez-Rivas
    • Journal of Microbiology and Biotechnology
    • /
    • 제21권2호
    • /
    • pp.147-153
    • /
    • 2011
  • Bacillus species have been involved in metal association as biosorbents, but there is not a clear understanding of this chelating property. In order to evaluate this metal chelating capacity, cultures and spores from Grampositive bacteria of species either able or unable to produce surface layer proteins (S-layers) were analyzed for their capacity of copper biosorption. Only those endowed of S-layers, like Bacillus sphaericus and B. thuringiensis, showed a significant biosorption capacity. This capacity (nearly 50%) was retained after heating of cultures, thus supporting that structural elements of the envelopes are responsible for such activity. Purified S-layers from two Bacillus sphaericus strains had the ability to biosorb copper. Copper biosorption parameters were determined for strain B. sphaericus 2362, and after analyses by means of the Langmuir model, the affinity and capacity were shown to be comparable to other bacterial biosorbents. A competitive effect of $Ca^{2+}$ and $Zn^{2+}$, but not of $Cd^{2+}$, was also observed, thus indicating that other cations may be biosorbed by this protein. Spores that have been shown to be proficient for copper biosorption were further analyzed for the presence of S-layer content. The retention of S-layers by these spores was clearly observed, and after extensive treatment to eliminate the S-layers, the biosorption capacity of these spores was significantly reduced. For the first time, a direct correlation between S-layer protein content and metal biosorption capacity is shown. This capacity is linked to the retention of S-layer proteins attached to Bacillus spores and cells.