The effects of different polishing techniques on the staining resistance of CAD/CAM resin-ceramics

  • Sagsoz, Omer;Demirci, Tevfik;Demirci, Gamze;Sagsoz, Nurdan Polat;Yildiz, Mehmet
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권6호
    • /
    • pp.417-422
    • /
    • 2016
  • PURPOSE. The purposes of this study were to evaluate the staining resistance of CAD/CAM resin-ceramics polished with different techniques and to determine the effectiveness of the polishing techniques on resin-ceramics, comparing it with that of a glazed glass-ceramic. MATERIALS AND METHODS. Four different CAD/CAM ceramics (feldspathic ceramic: C-CEREC Blocs, (SIRONA) and three resin-ceramics: L-Lava Ultimate, (3M ESPE), E-Enamic, (VITA) and CS-CeraSmart, (GC)) and one light cure composite resin: ME-Clearfil Majesty Esthetic (Kuraray) were used. Only C samples were glazed (gl). Other restorations were divided into four groups according to the polishing technique: nonpolished control group (c), a group polished with light cure liquid polish (Biscover LV BISCO) (bb), a group polished with ceramic polishing kit (Diapol, EVE) (cd), and a group polished with composite polishing kit (Clearfil Twist Dia, Kuraray) (kc). Glazed C samples and the polished samples were further divided into four subgroups and immersed into different solutions: distilled water, tea, coffee, and fermented black carrot juice. Eight samples ($8{\times}8{\times}1mm$) were prepared for each subgroup. According to CIELab system, four color measurements were made: before immersion, immersion after 1 day, after 1 week, and after 1 month. Data were analyzed with repeated measures of ANOVA (${\alpha}=.05$). RESULTS. The highest staining resistance was found in gl samples. There was no difference among gl, kc and cd (P>.05). Staining resistance of gl was significantly higher than that of bb (P<.05). Staining resistances of E and CS were significantly higher than those of L and ME (P<.05). CONCLUSION. Ceramic and composite polishing kits can be used for resin ceramics as a counterpart of glazing procedure used for full ceramic materials. Liquid polish has limited indications for resin ceramics.

레진과 치과용 도재의 접착 (BONDING BETWEEN RESIN AND CERAMICS)

  • 김선재;이근우;한종현
    • 대한치과보철학회지
    • /
    • 제45권2호
    • /
    • pp.159-168
    • /
    • 2007
  • Statement of problem: Literature showed different results on the durability of bonded ceramic restoration. Purpose: The purpose of this article is to review the effect of surface treatment of ceramics in resin-ceramic bond to get predictable results. Material and method: PubMed data base was utilized to search the articles which were written in English and published in 1986 and 2006. Some electronic published articles which are forthcoming to publish in paper were also included for this review. This review article focused on the effect of acid etching and silane application on the silica based ceramics. The durability of resin-ceramic bonding, the methodology for bond strength test and resin bonding to alumina or zirconia based ceramics were compared in brief at the end of the review. Results and Conclusion: the effect of silane application can be influenced by the contaminations of saliva or solutions. Micromechanical retention by acid etching as well as silane application plays an important role in initial and durable bond strength between resin and ceramic. The use of phosphate modified resin cement following tribochemical silica coating and silane application produced best bond strength for alumina or zirconia based ceramics.

Mechanical Properties and Density Profile of Ceramics Manufactured from a Board Mixed with Sawdust and Mandarin Peels

  • Jung-Woo HWANG;Seung-Won OH
    • Journal of the Korean Wood Science and Technology
    • /
    • 제51권2호
    • /
    • pp.98-108
    • /
    • 2023
  • In this study, the boards were manufactured according to the mandarin peels addition rate using sawdust and mandarin orange peel. After that, the mechanical properties and density profile of ceramics prepared by conditions through resin impregnation process and carbonization process were investigated. The bending and compression strengths of ceramics tended to increase as the resin impregnation rate increased. When the resin impregnation rate was 70%, the highest values were 8.58 MPa and 14.77 MPa, respectively. Also, the mechanical properties of ceramics according to carbonization temperature showed the highest values at 1,200℃ for bending strength of 11.09 MPa and compression strength of 17.20 MPa. The bending strength and compression strength according to the mandarin peels addition rate showed the highest values at 8.62 MPa and 14.16 MPa, respectively, when the mandarin orange peel addition rate was 5%. The mechanical properties tended to decrease when the addition rate of mandarin orange was increased. The density profile of ceramics showed a similar tendency to the mechanical properties. It can be seen that the density distribution from the surface layer to the center layer is more uniform as the resin impregnation rate and carbonization temperature increase and the mandarin peels addition rate decreases.

톱밥과 왕겨 혼합보드로 제조된 세라믹의 표면 온도 변화 - 수지함침율 및 탄화온도의 영향 - (A Change in Surface Temperature of Ceramics Made from Board Mixed with Sawdust and Rice Husk - Effect of Resin Impregnation Rate and Carbonization Temperature -)

  • 오승원;박희준
    • Journal of the Korean Wood Science and Technology
    • /
    • 제38권1호
    • /
    • pp.43-48
    • /
    • 2010
  • 톱밥과 왕겨로 제조된 혼합보드로 세라믹을 제조한 후 수지함침율 및 소성온도에 따른 세라믹의 표면온도를 조사하였다. 경과시간 초기에 표면온도가 급상승 하였으며 수지함침율 60~70%와 소성온도 $1200^{\circ}C$로 제조된 세라믹의 표면온도가 가장 높았다. 히터의 표면온도보다 혼합세라믹의 표면온도 하강속도가 느려 혼합세라믹의 열 보존력이 높음을 알 수 있었다.

Repair bond strength of resin composite to bilayer dental ceramics

  • Ataol, Ayse Seda;Ergun, Gulfem
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권2호
    • /
    • pp.101-112
    • /
    • 2018
  • PURPOSE. The purpose of this study was to investigate the effect of various surface treatments (ST) on the shear bond strength of resin composite to three bilayer dental ceramics made by CAD/CAM and two veneering ceramics. MATERIALS AND METHODS. Three different bilayer dental ceramics and two different veneering ceramics were used (Group A: IPS e.max CAD+IPS e.max Ceram; Group B: IPS e.max ZirCAD+IPS e.max Ceram, Group C: Vita Suprinity+Vita VM11; Group D: IPS e.max Ceram; Group E: Vita VM11). All groups were divided into eight subgroups according to the ST. Then, all test specimens were repaired with a nano hybrid resin composite. Half of the test specimens were subjected to thermocycling procedure and the other half was stored in distilled water at $37^{\circ}C$. Shear bond strength tests for all test specimens were carried out with a universal testing machine. RESULTS. There were statistically significant differences among the tested surface treatments within the all tested fracture types (P<.005). HF etching showed higher bond strength values in Groups A, C, D, and E than the other tested ST. However, bonding durability of all the surface-treated groups were similar after thermocycling (P>.00125). CONCLUSION. This study revealed that HF etching for glass ceramics and sandblasting for zirconia ceramics were adequate for repair of all ceramic restorations. The effect of ceramic type exposed on the fracture area was not significant on the repair bond strength of resin composites to different ceramic types.

CERAMIC INLAY RESTORATIONS OF POSTERIOR TEETH

  • Jin, Myung-Uk;Park, Jeong-Won;Kim, Sung-Kyo
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2001년도 춘계학술대회
    • /
    • pp.235-237
    • /
    • 2001
  • ;Dentistry has benefited from tremendous advances in technology with the introduction of new techniques and materials, and patients are aware that esthetic approaches in dentistry can change one's appearance. Increasingly. tooth-colored restorative materials have been used for restoration of posterior teeth. Tooth-colored restoration for posterior teeth can be divided into three categories: 1) the direct techniques that can be made in a single appointment and are an intraoral procedure utilizing composites: 2) the semidirect techniques that require both an intraoral and an extraoral procedure and are luted chairside utilizing composites: and 3) the indirect techniques that require several appointments and the expertise of a dental technician working with either composites or ceramics. But, resin restoration has inherent drawbacks of microleakage. polymerization shrinkage, thermal cycling problems. and wear in stress-bearing areas. On the other hand, Ceramic restorations have many advantages over resin restorations. Ceramic inlays are reported to have less leakage than resin restoration and to fit better. although marginal fidelity depends on technique and is laboratory dependent. Adhesion of luting resin is more reliable and durable to etched ceramic material than to treated resin composite. In view of color matching, periodontal health. resistance to abrasion, ceramic restoration is superior to resin restorationl. Materials which have been used for the fabrication of ceramic restorations are various. Conventional powder slurry ceramics are also available. Castable ceramics are produced by centrifugal casting of heat-treated glass ceramics. and machinable ceramics are feldspathic porcelains or cast glass ceramics which are milled using a CAD/CAM apparatus to produce inlays (for example, Cered. They may also be copy milled using the Celay apparatus. Pressable ceramics are produced from feldspathic porcelain which is supplied in ingot form and heated and moulded under pressure to produce a restoration. Infiltrated ceramics are another class of material which are available for use as ceramic inlays. An example is $In-Ceram^{\circledR}$(Vident. California, USA) which consists of a porous aluminum oxide or spinell core infiltrated with glass and subsequently veneered with feldspathic porcelain. In the 1980s. the development of compatible refractory materials made fabrication easier. and the development of adhesive resin cements greatly improved clinical success rates. This case report presents esthetic ceramic inlays for posterior teeth.teeth.

  • PDF

Light transmittance of CAD/CAM ceramics with different shades and thicknesses and microhardness of the underlying light-cured resin cement

  • Jafari, Zahra;Alaghehmand, Homayoon;Samani, Yasaman;Mahdian, Mina;Khafri, Soraya
    • Restorative Dentistry and Endodontics
    • /
    • 제43권3호
    • /
    • pp.27.1-27.9
    • /
    • 2018
  • Objectives: The aim of this in vitro study was to evaluate the effects of the thickness and shade of 3 types of computer-aided design/computer-aided manufacturing (CAD/CAM) materials. Materials and Methods: A total of 120 specimens of 2 shades (A1 and A3) and 2 thicknesses (1 and 2 mm) were fabricated using VITA Mark II (VM; VITA Zahnfabrik), IPS e.max CAD (IE; IvoclarVivadent), and VITA Suprinity (VS; VITA Zahnfabrik) (n = 10 per subgroup). The amount of light transmission through the ceramic specimens was measured by a radiometer (Optilux, Kerr). Light-cured resin cement samples (Choice 2, Bisco) were fabricated in a Teflon mold and activated through the various ceramics with different shades and thicknesses using an LED unit (Bluephase, IvoclarVivadent). In the control group, the resin cement sample was directly light-cured without any ceramic. Vickers microhardness indentations were made on the resin surfaces (KoopaPazhoohesh) after 24 hours of dark storage in a $37^{\circ}C$ incubator. Data were analyzed using analysis of variance followed by the Tukey post hoc test (${\alpha}=0.05$). Results: Ceramic thickness and shade had significant effects on light transmission and the microhardness of all specimens (p < 0.05). The mean values of light transmittance and microhardness of the resin cement in the VM group were significantly higher than those observed in the IE and VS groups. The lowest microhardness was observed in the VS group, due to the lowest level of light transmission (p < 0.05). Conclusion: Greater thickness and darker shades of the 3 types of CAD/CAM ceramics significantly decreased the microhardness of the underlying resin cement.

훼손 도자기 결실부 복원을 위한 3D 세라믹 프린팅 기술의 기초 적용성 연구 (A Study on the Applicability of 3D Ceramic Printing Technology for Restoration of the Missing Part of Damaged Ceramics)

  • 오승준;위광철
    • 한국융합학회논문지
    • /
    • 제11권11호
    • /
    • pp.165-173
    • /
    • 2020
  • 훼손 도자기의 결실부 복원은 ABS, PLA 등이 적용되고 있으나 도자기 재질과는 유사하지 않아 세라믹 수지에 대한 물성 및 적용성 연구를 진행해보고자 하였다. 기존 복원 방법인 거푸집과 ABS 수지 복원, 세라믹 수지의 실제 복원 및 물성 실험을 진행하였다. 연구 결과 세라믹 수지의 복원부 제작은 기존 재료에 비해 정밀도가 높아 미세한 형상의 출력이 가능하고, 표면 질감, 광택이 L30과 ABS 수지보다 우수하였다. 물성 측정 결과 수축, 변형이 없고 압축강도가 높아 기존 재료에 비해 내구성이 우수하나 비중과 경도 값은 복원부 제작 후 가공성이 저하될 수 있는 요소로 작용될 수도 있을 것으로 사료된다. 본 연구에서 적용된 세라믹 수지의 장기적인 모니터링과 신뢰성 및 안정성 평가, 너무 얇거나 긴 형태의 복원부 출력 시 원형복원성 등에 대한 추가적인 연구가 이루어져야 할 것으로 판단된다.

Curing Behavior of Phenolic Resin with Humid Atmosphere on The Porous $ZrO_2$ ceramics

  • 윤상현;김장훈;김주영;이준태;이희수
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.57.1-57.1
    • /
    • 2011
  • The effects of relative humidity on the properties of the porous $ZrO_2$ ceramics were investigated in terms of the curing behavior of phenolic resin as a binder. The $ZrO_2$ powders containing 5wt% of phenolic resin were conditioned in a consistent chamber condition at a temperature of $50^{\circ}C$ and different humidity levels (25, 50, 75, and 95%) for 1 h. The exposure of humid atmosphere caused changes of density and microstructure in the green bodies. The higher level the powders were exposed to the humid atmosphere, the lower green density was obtained and the more irregular microstructure was observed due to aggregation by the curing of phenolic resin. After firing, the porosity of specimens has risen from 35.7% to 38.1% and Young's modulus has declined in response to the variation of green density. These results could be explained by the degree of resin cure which was associated with the area under the exothermic peak enclosed by a baseline of DSC thermogram curve. Also, the curing behavior of phenolic resin according to relative humidity has been confirmed by decrease of ether groups which have interacted with the phenolic-OH group and the hexamine as a curing agent. Consequently, it could be demonstrated that increase the relative humidity during fabrication of porous $ZrO_2$ diminished the compaction and properties of specimens after firing owing to curing of phenolic resin.

  • PDF

Bond strength of resin cement to $CO_2$ and Er:YAG laser-treated zirconia ceramic

  • Kasraei, Shahin;Rezaei-Soufi, Loghman;Heidari, Bijan;Vafaee, Fariborz
    • Restorative Dentistry and Endodontics
    • /
    • 제39권4호
    • /
    • pp.296-302
    • /
    • 2014
  • Objectives: It is difficult to achieve adhesion between resin cement and zirconia ceramics using routine surface preparation methods. The aim of this study was to evaluate the effects of $CO_2$ and Er:YAG laser treatment on the bond strength of resin cement to zirconia ceramics. Materials and Methods: In this in-vitro study 45 zirconia disks (6 mm in diameter and 2 mm in thickness) were assigned to 3 groups (n = 15). In control group (CNT) no laser treatment was used. In groups COL and EYL, $CO_2$ and Er:YAG lasers were used for pretreatment of zirconia surface, respectively. Composite resin disks were cemented on zirconia disk using dual-curing resin cement. Shear bond strength tests were performed at a crosshead speed of 0.5 mm/min after 24 hr distilled water storage. Data were analyzed by one-way ANOVA and post hoc Tukey's HSD tests. Results: The means and standard deviations of shear bond strength values in the EYL, COL and CNT groups were $8.65{\pm}1.75$, $12.12{\pm}3.02$, and $5.97{\pm}1.14MPa$, respectively. Data showed that application of $CO_2$ and Er:YAG lasers resulted in a significant higher shear bond strength of resin cement to zirconia ceramics (p < 0.0001). The highest bond strength was recorded in the COL group (p < 0.0001). In the CNT group all the failures were adhesive. However, in the laser groups, 80% of the failures were of the adhesive type. Conclusions: Pretreatment of zirconia ceramic via $CO_2$ and Er:YAG laser improves the bond strength of resin cement to zirconia ceramic, with higher bond strength values in the $CO_2$ laser treated samples.