Experimental study on fatigue behavior of innovative hollow composite bridge slabs

  • Yang Chen;Zhaowei Jiang;Qing Xu;Chong Ren
    • Steel and Composite Structures
    • /
    • v.46 no.6
    • /
    • pp.745-757
    • /
    • 2023
  • In order to study the fatigue performance of the flat steel plate-lightweight aggregate concrete hollow composite bridge slab subjected to fatigue load, both static test on two specimens and fatigue test on six specimens were conducted. The effects of the arrangement of the steel pipes, the amplitude of the fatigue load and the upper limit as well as lower limit of fatigue load on failure performance were investigated. Besides, for specimens in fatigue test, strains of the concrete, residual deflection, bending stiffness, residual bearing capacity and dynamic response were analyzed. Test results showed that the specimens failed in the fracture of the bottom flat steel plate regardless of the arrangement of the steel pipes. Moreover, the fatigue loading cycles of composite slab were mainly controlled by the amplitude of the fatigue load, but the influences of upper limit and lower limit of fatigue load on fatigue life was slight. The fatigue life of the composite bridge slabs can be determined by the fatigue strength of bottom flat steel plate, which can be calculated by the method of allowable stress amplitude in steel structure design code.

Residual Stress and Elastic Modulus of Y2O3 Coating Deposited by EB-PVD and its Effects on Surface Crack Formation

  • Kim, Dae-Min;Han, Yoon-Soo;Kim, Seongwon;Oh, Yoon-Suk;Lim, Dae-Soon;Kim, Hyung-Tae;Lee, Sung-Min
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.6
    • /
    • pp.410-416
    • /
    • 2015
  • Recently, a new $Y_2O_3$ coating deposited using the EB-PVD method has been developed for erosion resistant applications in fluorocarbon plasma environments. In this study, surface crack formation in the $Y_2O_3$ coating has been analyzed in terms of residual stress and elastic modulus. The coating, deposited on silicon substrate at temperatures higher than $600^{\circ}C$, showed itself to be sound, without surface cracks. When the residual stress of the coating was measured using the Stoney formula, it was found to be considerably lower than the value calculated using the elastic modulus and thermal expansion coefficient of bulk $Y_2O_3$. In addition, amorphous $SiO_2$ and crystalline $Al_2O_3$ coatings were similarly prepared and their residual stresses were compared to the calculated values. From nano-indentation measurement, the elastic modulus of the $Y_2O_3$ coating in the direction parallel to the coating surface was found to be lower than that in the normal direction. The lower modulus in the parallel direction was confirmed independently using the load-deflection curves of a micro-cantilever made of $Y_2O_3$ coating and from the average residual stress-temperature curve of the coated sample. The elastic modulus in these experiments was around 33 ~ 35 GPa, which is much lower than that of a sintered bulk sample. Thus, this low elastic modulus, which may come from the columnar feather-like structure of the coating, contributed to decreasing the average residual tensile stress. Finally, in terms of toughness and thermal cycling stability, the implications of the lowered elastic modulus are discussed.

Estimation Method of Residual Performance for Hollow Slab at Elevated Temperature (고온에 노출된 중공슬래브의 잔존성능 추정방법)

  • Choi, Hyun-Ki;Chung, Joo-Hong;Choi, Chang-Sik
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.5
    • /
    • pp.643-650
    • /
    • 2014
  • Generally, the reinforced concrete slab has great fire resistance performance because concrete has excellent thermal material properties under fire. But, in the case of hollow slab, it will be expected that hollow slabs have different temperature distribution and fire endurance performance compare to reinforced concrete slab. Because hollow slab has internal void space that occurs decreasing regenerative effect of concrete and formation of internal air layer. Evaluation method for fire resistance performance of hollow slabs was proposed using $wickstr{\ddot{o}}m^{\prime}s$ method. For the casual use of evaluation, simplified method was proposed which was limited to solid slab and donut type hollow slab which was developed by authors of this research paper. Also, verification on proposed method was performed by comparing results of fire experiment for hollow slab and evaluation results. Proposed method of the results of this study was possible to predict the residual strength and temperature distribution of slabs under fire.

Evaluation of Post-Buckling Residual Strength of H-Section Steel Column for Both Ends are Fixed Condition (양단고정 단부구속에 따른 H 형 강재기둥의 좌굴 후 잔존내력 평가)

  • Abebe, Daniel Yeshewawork;Choi, Jae Hyouk;Kim, Jin Hyang
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.1
    • /
    • pp.83-88
    • /
    • 2013
  • Progressive collapse is a chain reaction of failures propagating throughout a portion of a structure that is disproportionate to the original local failure. When column members are subjected to unexpected load (compression load), they will buckle if the applied load is greater than the critical load that induces buckling. The post-buckling strength of the columns will decrease rapidly, but if there is enough residual strength, the members will absorb the potential energy generated by the impact load to prevent progressive collapse. Thus, it is necessary to identify the relationship of the load-deformation of a column member in the progressive collapse of a structure up to final collapse. In this study, we carried out nonlinear FEM analysis and based on deflection theory, we investigated the load-deformation relationship of H-section steel columns when both ends were fixed.

Study on Crashworthiness of Icebreaker Steel: Part II Ship Side Structural Behavior Due to Impact Bending (쇄빙선의 내충격 특성에 관한 실험적 연구: 제2부 선체 구조의 충격 굽힘 특성)

  • Noh, Myung-Hyun;Lee, Jae-Yik;Han, Donghwa;Choung, Joonmo
    • Journal of Ocean Engineering and Technology
    • /
    • v.30 no.4
    • /
    • pp.277-286
    • /
    • 2016
  • The first part of this study found the tendencies of the mechanical properties of two arctic structural steels (EH32 and FH32). In the second part, the crashworthiness of stiffened panels scaled down from the side frame structure of a Korean research icebreaker was determined. A procedure for designing the shapes and sizes of the stiffened panels, mass and shape of a drop striker, and a large temperature chamber, and then manufacturing these, is introduced in detail. From impact bending tests for the stiffened panels, the residual permanent deformations and deformation histories over time were captured using manual measurement and video image analyses. Numerical simulations of the impact bending tests were carried out for three different finite element models, which were mainly composed of shell elements, solid elements, and solid elements, with welding beads. It was proven from a comparison of the test results and numerical simulation results that the solid element model with the welding bead consideration approached the test results in terms of the residual deformations as long as the strain rate effect was taken into account.

Nanoscale Longitudinal Normal Strain Behavior of ${Si_3}{N_4}$-to-ANSI 304L Brazed Joints under Pure Bending Condition

  • Seo, D.W.;Lim, J.K.
    • International Journal of Korean Welding Society
    • /
    • v.4 no.1
    • /
    • pp.46-52
    • /
    • 2004
  • To combine the mechanical advantages of ceramics with those of metals, one often uses both materials within one composite component. But, as known, they have different material properties and fracture behaviors. In this study, a four-point bending test is carried out on $Si_3N_4$ joined to ANSI 304L stainless steel with a Ti-Ag-Cu filler and a Cu interlayer at room temperature to evaluate their longitudinal strain behaviors. And, to detect localized strain, a couple of strain gages are pasted near the joint interfaces of the ceramic and metal sides. The normal strain rates are varied from $3.33{\times}10^5$ to $3.33{\times}10^{-1}s^{-1}$ Within this range, the experimental results showed that the four-point bending strength and the deflection of the interlayer increased with increasing the strain rate.

  • PDF

Investigation of Pyrolyzed Polyimide Thin Film as MEMS Material

  • Naka, Keisuke;Nagae, Hideki;Ichiyanagi, Masao;Jeong, Ok-Chan;Konishi, Satoshi
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • v.5 no.1
    • /
    • pp.38-44
    • /
    • 2005
  • Pyrolyzed polyimide is explored in terms of MEMS material. This paper describes chemical, electrical, mechanical properties of pyrolyzed polyimide (PIX-1400) thin film as MEMS material. When polyimide thin film was pyrolyzed at $800^{\circ}C$ for 60 minutes in $N_{2}$ ambient, the residual ratio of pyrolyzed film thickness measured with a surface profiler is about 49 %, and the resistivity is about $2.17{\times}10^{-2}\;{Omega}cm$. From the result of the load-deflection test, the estimated Young's modulus and initial average stress of pyrolyzed polyimide are 67 GPa and 30 MPa, respectively. As one demonstration of MEMS structures of pyrolyzed polyimide, the fabrication method of the microbridge structure is proposed for a micro heater and a resonator.

Effect of The Bending Strain of FRP Tube for Composite Bushing with Winding Tension (와인딩 장력이 composite 부싱용 FRP tube의 굽힘변형에 미치는 영향)

  • Cho, Han-Goo;Yoo, Dae-Hoon;Kang, Hyung-Kyung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.380-381
    • /
    • 2009
  • This paper describes effect of the bending strain of FRP tube for composite bushing with winding tension. The composite bushing can be formed, by adding silicone rubber sheds to a tube of composite materials. The FRP tube is internal insulating part of a composite bushing and is designed to ensure the mechanical characteristics. Generally the properties of FRP tube can be influenced by the winding angle, wall thickness and winding tension. As winding tension is increased glass contents was increased in the range of 70.4~76.6%. In the bending test, winding tension is increased residual displacement was decreased in the range of 14.0~12.2 mm.

  • PDF

Impact behavior of including the boundary between A356/SiCw and Al alloy (Al alloy와의 경계면을 포함한 A356/SiCw의 충격거동)

  • 조종인;남현욱;한경섭
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.05a
    • /
    • pp.97-100
    • /
    • 2002
  • In this research, the impact behavior of the boundary between MMC-reinforced SiC whisker and Al alloy were studied. It is known that the resultant of the interfacial reaction between SiC whisker and Al alloy has brittle and low toughness property. In this paper, impact behavior of graded MMC & Al alloy shows the interfacial opening at the boundary. Generally this phenomenon is generated by thermal residual stress, brittle interfacial reaction resultant and difference of the deflection. So, these results may be interpreted as a macroscopic method of measuring the interfacial strength between matrix and reinforcement

  • PDF

Warping Analysis of Unsymmetric Laminated Composites (비대칭 복합적층판 의 Warping 해석)

  • 전완주;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.7 no.4
    • /
    • pp.404-409
    • /
    • 1983
  • The warping of unsymmetric laminated composites is induced by residual curing stress at the room temperature. Classical lamination theory (C.L.T.) predicts the room temperature shapes of all unsymmetric laminates to be a saddle. Experimental observations, however, indicate some unsymmetric laminated composites have cylindrical room temperature shapes. This anomalous behavior is explained by the extention of C.L.T. which involves Von Karman's large deflection theory. It is shown that, depending on the thickness, width, length, curing temperature and room temperature of the laminate, critical boundaries of the shape change are determined. Theoretical predictions are compared with experimental results of Toray Graphite/Epoxy {O$_{n}$/90$_{n}$}$_{T}$./....