Evaluation of Optimum Mixing Rate and Durability of Concrete Using Water Granulated Slag Fine Aggregate (수쇄 페로니켈슬래그 잔골재를 이용한 콘크리트의 최적 혼합률 및 내구 특성 평가)

  • Choi, Yun-Wang;Park, Man-Seok;Lee, Kwang-Myong;Bae, Su-Ho;Kim, Jee-Sang
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.1
    • /
    • pp.120-127
    • /
    • 2011
  • Recently, there are problems due to the exhaustion of natural aggregate resources, and strict restrictions. In this study, the possibility of using Water Granulated Ferro-Nickel slag as a substitutive material of fine aggregate is determined from the properties of mechanical and durability for the concrete that is made with Water Granulated Ferro-Nickel slag. According to the test results, when the mixing rate of Water Granulated Ferro-Nickel Slag aggregates concrete is adjusted, up to 50% of its aggregates by mixing rate can be mixed with general aggregates. The optimum mix ratio is considered to be 40%. The freezing and thawing resistance of Water Granulated Ferro-Nickel Slag aggregates concrete is identical to that of general aggregates concrete, while the carbonation resistance is found to be same as or lower than that of general aggregates concretes.

  • PDF

A Fundamental Study on Manufacturing Condition the High Quality Recycled Fine Aggregate by Low Speed Wet Rotary Mill (저속습식마쇄기를 이용한 고품질 순환잔골재 제조에 관한 기초적 연구)

  • Kim, Ha-Seog;Lee, Gyung-Hyun;Ra, Jeong-Min;Park, Hyo-Jin;Lim, Dae-Bin;Kim, Jin-Man
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2009.11a
    • /
    • pp.65-68
    • /
    • 2009
  • Recycled aggregate by the recycling construction waste has a lot of advantage such as the developing the alternative resource and protecting of environment. However, recycled aggregate is used as the low quality grade, because the technic to remove old mortar from aggregate is low level. To use the recycled aggregate as high quality grade, it is important to develop the technic to produce the high quality recycled aggregate. To manufacture the high quality recycled aggregate, old mortar attached on the aggregates should remove efficiently. Therefore, in this study, we suggested the optimum condition to remove old mortar effectively using sulfuric acid and low speed wet rotary mill for high quality recycled fine aggregate. The results shows that the recycled aggregate satisfy on the standards of KS F 2573 in density, absorption and solid volume when, adequate condition of sulfuric mole ratio and aggregate ratio are make.

  • PDF

Effect of Recycled Aggregate Substitution to Zero-cement Concrete which uses Blast Furnace Slag Power (고로슬래그 미분말 사용 무 시멘트 콘크리트의 품질에 미치는 순환골재 치환율의 영향)

  • Feng, Hai-Dong;Cho, Man-Gi;Son, Ho-Jung;Han, Min-Cheol;Yang, Seong-Hwan;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2012.05a
    • /
    • pp.287-288
    • /
    • 2012
  • In this study, Analyzed the effect of the change in RFA and RCA substitution rate on the concrete containing BS bonding materials but no cement. The findings are as follows. First, the fresh concrete has less slump value and air contents as more RFA and RCA is used. In case of hardened concrete, as more RFA and RCA are used, the higher the compressive strength of concrete becomes. Especially, the compressive strength of concrete which used recycled aggregates only is found to be 2.2 times as high as that of concrete using natural fine and coarse aggregates only. But if the concrete is to be used as the structural concrete having the compressive strength of 13.8 MPa, the alkaline materials and some cement are required to be added.

  • PDF

The Improvement of Properties of Recycled aggregates using Concrete Waste by Pre-heating Method. (예비가열법에 의한 폐콘크리트 재생골재의 물성개선)

  • 최현수;김효열;최봉철;강병희
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.05a
    • /
    • pp.73.2-79
    • /
    • 2003
  • The purpose of this study is to provide the basic data on the optimum method for interfacial separation for an effective recycle of concrete waste by using the thermal properties of concrete. Therefore, this study is proceeded by dividing the interface of concrete into cement paste and fine aggregates or mortar and coarse aggregate, considering the aspect of recycled cement and aggregate as the recycling use of concrete waste. As results of the experiment, in case of recycle cement, the interfacial separation is easily appeared, but it is shown that the mixed amount of powder included in fine aggregate doesn't greatly decrease. But, in case of recycle coarse aggregate, the effect of interfacial separation by preliminary heating is predominant. Especially, the bonding rate of mortar is the lowest when it is heated 5 times for 120 minutes at $300^{\circ}C$. Hence, it is considered that it will be an excellent effect of quality control when the results of this study is applied to a manufacturing system of recycle coarse aggregate which is about to put into practical use.

  • PDF

Effect of Recycled Aggregates Powder on the Properties of Zero Cement Mortar Using the Recycled Fine Aggregates and Fly-Ash (순환잔골재와 플라이애시를 사용하는 무 시멘트 모르타르의 특성에 미치는 순환골재 미분말의 영향)

  • Park, Kyung-Taek;Son, Seok-Heon;Han, Cheon-Goo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.12 no.2
    • /
    • pp.161-168
    • /
    • 2012
  • The purpose of this study was to investigate the influence of recycled aggregates powder (RP) contents on recycled aggregates (RA) using fly-ash (FA) mortar in a condition of zero cement targeting earth filling materials, and the results can be summarized as follows. First, there was a tendency that as RP contents increased, W/B and air contents increased also. In the case of compressive strength, the strength was hardly developed at the early age, which was prior to 14 days; however, with the starting point of 14 days of age, strength of around 1.5~2.0 MPa was developed when it arrived at 28 days. At a curing temperature of $20^{\circ}C$, the more RP contents increased, the more the compressive strength increased in comparison with FA 100% at all levels except RP 100 %, showing the highest compressive strength at RP 25 %. At a curing temperature of $35^{\circ}C$, the temperature-dependence appeared to be large, as the RP contents were decreased compared to the curing temperature of $20^{\circ}C$. In addition, based on SEM analysis, this study was able to confirm that a pozzolanic reaction formed by an alkali stimulus of RA with the lapse of certain days even in 100 percent FA, causing the densification of tissues, and with RP 25%, hydrate was created the most densely by the hydration of unhydrated cement particles and pozzolanic reaction of FA.

Effect of Fine Particle Cement and Recycled Aggregates as Alkali Activator on the Engineering Properties and Micro-Structure of High Volume Blast Furnace Slag Concrete (알칼리 자극제로서 미분시멘트와 순환골재가 고로슬래그 다량치환 콘크리트의 공학적 특성 및 미세구조에 미치는 영향)

  • Han, Min-Cheol;Lee, Hyang-Jae;Han, Cheon-Goo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.13 no.6
    • /
    • pp.602-608
    • /
    • 2013
  • The aim of this study is to investigate experimentally the effect of the combination of fine particle cement with high Blaine fineness (FC) and recycled aggregates on the engineering properties and micro structure of high volume blast furnace slag (BS) concrete with 75% BS and 21 MPa. FC manufactured by particle classification at the plant with Blaine fineness of more than $7000cm^2/g$ was used as additional alkali activator for high volume blast furnace slag concrete made with recycled fine and coarse aggregates. FC was replaced by 15, 20 and 25% OPC. Test results showed that the incorporation of FC resulted in an increase in the compressive strength compared to BS concrete without FC by as much as 30% due to accelerated hydration and associated latent hydraulic reaction. It was found that the use of FC and recycled aggregates played an important role in activating BS for high volume BS concrete by offering sufficient alkali.

A Fundamental Study on Supply Status and Use Plan of Fine Aggregates (잔골재의 수급현황 및 활용방안에 관한 기초적 연구)

  • Yu Myoung Youl;Lee Sea-Hyun;Lee Hyun-Soo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.101-104
    • /
    • 2005
  • It analyzed the supply status of fine aggregate and find the point of issue related alternative fine aggregate through researches and interviews. The conclusions of the study are as follows. 1. Ready mixed concrete manufacture used crushed fine aggregate (15.5$\%$) and recycled fine aggregate (1.5$\%$) for alternatives aggregate than 1.3$\%$ in 1991. It is not allowed to use a recycled fine aggregate in ready mixed concrete, but they used it. 2. All alternative aggregate are satisfied the Korean Standard, But they showed low properties of mortar compared to when it replaced with natural fine aggregate. So, it is needed to make another special Korean Standard to use alternative aggregate in normal concrete by mixing method to recover the workability and compressive strength.

  • PDF

Compressive Strength Evaluation of Concrete with Mixed Plastic Waste Aggregates Filled with Blast Furnace Slag Fine Powder (무기충진재를 혼입한 복합 폐플라스틱 골재를 활용한 콘크리트 압축강도 특성)

  • Lee, Jun;Kim, Kyung-Min;Cho, Young-Keun;Kim, Ho-Kyu;Kim, Young-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.253-259
    • /
    • 2021
  • Plastic wastes generated from household waste are separated by mixed discharge with foreign substances, and recycling is relatively low. In this study, the effect of the ratio and content of mixed plastic waste coarse aggregate(MPWCA)s and mixed plastic waste fine aggregate(MPWFA)s filled with blast furnace slag fine powder on the slump and compressive strength of concrete was evaluated experimentally. The MPWCAs were found to have a similar fineness modulus, but have a single particle size distribution with a smaller particle size compared to coarse aggregates. However, the MPWFAs were found to have a single particle size distribution with a larger fineness modulus and particle size compared to fine aggregates. Meanwhile, the effect of improving the density and filling pores by the blast furnace slag fine power was found to be greater in the MPWFA compared to the MPWCA. As the amount of the mixed plastic waste aggregate(MPWA)s increased, the slump and compressive strength of concrete decreased. In particular, the lower the slump and compressive strength of concrete was found to decrease the greater the amount of MPWFA than MPWCA when the amount of MPWA was the same. This is because of the entrapped air and voids formed under the angular- and ROD-shaped aggregates among the MPWFAs. On the other hand, the addition of the admixture and the increase in the unit amount of cement were found to be effective in improving the compressive strength of the concrete with MPWAs.

Quality of High Volume Blast Furnace Slag Mortar Depending on Desulfurization Gypsum Treating Methods and Fine Aggregate Type (탈황석고의 가공법 및 잔골재종류 변화에 따른 고로슬래그 미분말 다량 치환 모르타르의 품질 특성)

  • Han, Cheon-Goo;Lee, Dong-Yun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.2
    • /
    • pp.157-164
    • /
    • 2016
  • In this research, based on the condition of using desulfurization gypsum(FGD) as a stimulator for high-volume blast furnace slag cement mortar, sieving and heating process methods of removing activated carbon in FGD were compared with the non-processed FGD and recycled and natural fine aggregates were compared for suitable aggregate to be used. According to the result of experiment, sieving with 0.3mm was more efficient than $500^{\circ}C$ heating for processing the FGD, and recycled fine aggregate showed more favorable result than natural fine aggregate at the FGD content was 5 to 10%. On the other hand, the mortar mixture including recycled fine aggregate had a high drying shrinkage, and absorption ratio, and thus specific limitations on applying recycled fine aggregate should be required.