재생굵은골재를 사용한 콘크리트의 유동특성에 관한 실험적 연구 (The Experience Study on the Floating Properties of Concrete with Recycled Coarse Aggregate)

  • 백철우;김호수;최성우;반성수;류득현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.94-97
    • /
    • 2003
  • Recently, owing to the deterioration of reconstruction and the construction, much of the construction waste is discharged in our construction field, and the amount of construction waste are rapidly increased. These waste are raised to financial and environmental problems, so the method of reusing waste concretes has been studied and carried out many direction. Especially being want of resources, if waste concrete could be recycled as aggregate for concrete, it will contribute to solve the exhaustion of natural aggregate, in terms of saving resources and protecting environment. This study is that the floating properties of concrete with recycled coarse aggregate were investigated for the substitution of recycled coarse aggregate. The result of this study, in case of water reducing, the property of harden concrete for the substitution ratio of recycled coarse aggregate was increased. The Quality of recycled coarse aggregate concrete was improved by water reducing.

  • PDF

순환잔골재 모르타르의 염해저항성 평가 (Evaluation on Chloride Attack Resistance of Recycled Fine Aggregate Mortar)

  • 장현식;김규용;윤민호;최경철;김홍섭;이보경
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.52-53
    • /
    • 2016
  • Mechanical properties and durability of recycled aggregate concrete was known to decrease due to the adhesive mortar of recycled aggregate. But in this study, As the result of chloride diffusion resistance of recycled fine aggregate mortar, the mechanical properties are reduced according to the increase of the substitute ratio of recycled fine aggregate. But the chloride diffusion coefficient was almost same with natural fine aggregate mortar.

  • PDF

순환잔골재를 사용한 모르타르의 염화물확산계수 평가 (Evaluation on Chloride Diffusion Coefficient of Mortar with Recycled Fine Aggregate)

  • 윤민호;김규용;최경철;황의철;서원우;이상윤
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 춘계 학술논문 발표대회
    • /
    • pp.209-210
    • /
    • 2016
  • Mechanical properties and durability of recycled aggregate concrete was known to decrease due to the adhesive mortar of recycled aggregate. But in this study, As the result of chloride diffusion resistance of recycled fine aggregate mortar, the mechanical properties are reduced according to the increase of the substitute ratio of recycled fine aggregate. But the chloride diffusion coefficient was almost same with natural fine aggregate mortar.

  • PDF

순환골재를 이용한 플라이애시 콘크리트의 역학적 특성 (Mechanical Properties of Recycled Aggregate Concrete Containing Fly Ash)

  • 양인환;전병관
    • 한국건설순환자원학회논문집
    • /
    • 제5권2호
    • /
    • pp.144-151
    • /
    • 2017
  • 이 연구에서는 순환굵은골재와 플라이애시를 사용한 콘크리트의 압축강도 및 탄성계수의 역학적 특성을 연구하였다. 실험변수로써 굵은순환골재의 치환율과 플라이애시 치환율을 고려하였다. 실험에서 고려된 순환굵은골재의 치환율은 0, 30, 50 및 70%이고, 플라이애시 치환율은 0, 15 및 30%이다. 실험변수에 따른 순환골재 콘크리트의 7일, 28일 및 91일 재령의 압축강도와 탄성계수 특성을 분석하였다. 플라이애시를 혼입하지 않은 콘크리트의 압축강도와 탄성계수에 비해 플라이애시 치환율이 30%인 배합의 각 재령별 압축강도와 탄성계수 감소효과는 뚜렷하게 나타난다. 따라서 순환골재콘크리트에서 30%이하 수준의 플라이애시의 혼입이 역학적 특성 측면에서 적정하다고 판단된다.

PET와 재생골재를 이용한 폴리머콘크리트의 역학적 특성 (Mechanical Characteristics of Recycled PET Polymer Concrete with Demolished Concrete Aggregates)

  • 조병완;이두화;박승국
    • 콘크리트학회논문집
    • /
    • 제17권3호
    • /
    • pp.335-342
    • /
    • 2005
  • 천연 건설자원이 고갈되어감에 따라, 심각한 환경오염을 일으키고 있는 각종 산업폐기물의 재활용을 통해 새로운 건설소재를 개발하기 위하여, 폐플라스틱과 폐 콘크리트를 재활용한 폴리머콘크리트의 역학적 특성을 분석하였다. 본 연구에서는 폐 PET를 재생한 불포화 폴리에스테르 수지를 재생골재와 결합시켜, 재생골재 및 수지변화량에 따른 역학적 특성과 내화학성 실험을 실시하였으며 실험결과, 재생수지 및 골재를 사용한 폴리머콘크리트(RPC)의 강도는 수지의 함량이 증가함에 따라 차츰 증가하는 추세를 보였다. 하지만 어느 수지량의 한계점 (대략 $13{\~}17\%$)에선 더 이상의 강도증가는 나타내지 않고 있음을 확인할 수 있었다 또한 재생골재 함량이 증가할수록 강도와 탄성계수는 감소하였으나 수지량 $17\%$에서는 이러한 현상이 나타나지 않았다. 선형대수회귀 분석을 통해 수지량 $9\%$일 때의 압축강도와 휨, 할렬 인장강도의 상관관계를 확인한 결과 높은 신뢰도를 보임을 알 수 있었다. 하지만 수지량이 증가함에 따라 뚜렷한 상관관계가 나타나지 않는 경향을 나타내었다. 재생골재를 사용한 폴리머콘크리트의 내화학성에 따른 중량변화와 강도실험은 비교적 산과 염에 강한 특성을 나타내었다. 그리고 염산 $30\%$의 수용액에선 알칼리수용액 $40\%$ 보다는 강한 저항성을 나타내었음을 압축강도 및 중량변화를 통해 확인할 수 있었다.

코어 및 비파괴 시험에 의한 재생골재 콘크리트의 압축강도 평가에 대한 실험적 연구 (An Experimental Study on the Evaluation of Compressive Strength of Recycled Aggregate Concrete by the Core and the Non-Destructive Testing)

  • 양근혁;김용석;정헌수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.133-136
    • /
    • 2005
  • Compressive strength of recycled aggregate concrete was tested by the core and by the non-destructive testing. A prediction model of compressive strength considering the replacement level of recycled aggregate was suggested by multi-regression analysis and was compared with test results. Also, Test results showed that the ratio of compressive strength by core and non-destructive testing to actual was somewhat affected by the replacement level of recycled aggregate.

  • PDF

미분 제거방식이 다른 2종의 재생 잔골재가 콘크리트외 특성에 미치는 영향 (A Study on the Properties of Recycled Concrete Using Recycled Fine Aggregates with different Removal formulas of Powder In Aggregate)

  • 이문환;이세현;심종우
    • 콘크리트학회논문집
    • /
    • 제17권1호
    • /
    • pp.95-104
    • /
    • 2005
  • 습식 및 건식 생산방식에 의해 생산된 양질의 재생 잔골재를 사용한 콘크리트의 특성을 분석하여 콘크리트용 재생 잔골재로서의 활용가능성에 대해 연구 분석한 결과는 다음과 같다. 재생 잔골재 콘크리트의 공기량은 재생 잔골재의 생산시 포함된 모르타르로 인해 치환률 증가에 따라 공기량이 상승되는 것으로 나타났다. 하지만 건식 생산된 잔골재를 사용한 콘크리트의 경우, 공기량의 증가율이 상대적으로 낮았다. 슬럼프는 습식 및 건식 생산공정과는 관계없이 재생 잔골재의 치환율이 증가됨에 따라 전체적으로 감소되는 경향을 보였다. 이는 재생 잔골재에 있는 모르타르 입자가 콘크리트의 잉여수를 흡착하여 유동성을 저하시켰기 때문인 것으로 판단된다. 압축강도는 재생 잔골재 치환율이 증가함에 따라 전반적으로 감소되는 것으로 나타났으나, 배합에 따라 재생 잔골재 치환율 25, 50%에서 물시멘트비 감소효과에 의한 부분적 증가 현상도 나타났다. 이러한 현상은 조기재령에서도 동일하게 나타나 재생골재콘크리트의 현장적용시에도 응결지연 등에 대한 우려는 없을 것으로 판단된다. 인장강도 결과 역시, 습식 및 건식 재생 잔골재 혼입률 25% 수준에서 가장 우수한 인장강도를 보였다 이를 종합하면, 재생 잔골재의 종류 및 물리적 성질에 따라 다소 차이는 예상되나, 콘크리트용 골재로서 건식 및 습식 생산된 재생 잔골재를 콘크리트용 골재로서 대체 사용하는 경우, 물시멘트비 등에 따라 다소 차이는 있었으나 전반적으로 치환율 25%이하에서는 물리적 역학적 성질에 심각한 저하 현상 없이 콘크리트의 제성질 발현이 가능한 것으로 판단된다.

순환잔골재의 다량 사용에 따른 모르타르의 특성 (Characteristic of Cementitious Mortar Using High Volume of Recycled Fine Aggregate)

  • 김상철;박도국;육근창
    • 한국건설순환자원학회논문집
    • /
    • 제4권3호
    • /
    • pp.235-242
    • /
    • 2016
  • 본 연구에서는 순환골재의 다량활용 일환으로 품질이 천연골재에 비해 매우 열악하고 관리가 어려운 것으로 알려져 있는 순환잔골재 만을 사용하여 그 치환률에 따른 모르타르의 성상변화에 대해 검토하였다. 실험결과, 골재 자체의 입도는 표준입도분포 범위를 벗어났고 조립률이 다소 높게 나타났다. 또한 모르타르로 제작한 경우, 완전히 제거되지 않은 시멘트페이스트의 다공성과 흡수성으로 인해 유동성 및 공기량 저하, 건조수축량 증가 등 불리한 조건들이 나타났지만, 강도 측면에서는 천연잔골재를 사용한 모르타르의 강도를 상회하는 결과가 나타나 물-시멘트비 조정과 화학혼화제의 적절한 사용을 통해 목표로 하는 일반강도 이상의 강도확보가 가능하며, 프리캐스트 콘크리트 제품에는 순환잔골재의 다량 사용이 가능한 것으로 나타났다.

건축기준 완화를 위한 순환골재 콘크리트 적용 시의 품질 특성 연구 (A Study on the Quality Properties When Applying Recycled Aggregate Concrete for the Construction Standard Mitigation)

  • 우경섭;김정호;이세현;오중근
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제24권3호
    • /
    • pp.63-69
    • /
    • 2020
  • 우리나라는 전체 폐기물 발생량 중 건설폐기물 발생량은 약 47.3%로 가장 많은 비중을 차지하고 있고 그 중 폐콘크리트가 약 62.8%로 재활용이 시급한 상황이다. 이에 정부는 건설폐기물의 재활용을 촉진하기 위해 순환골재의 다양하고 폭넓은 활용을 권장하고 있다. 또한 건축물에 콘크리트용 순환골재를 사용할 경우 용적률, 건축높이 등 건축기준을 완화해주고 있다. 그 기준은 콘크리트용 순환골재 최대 25% 사용 시 용적률을 최대 15% 완화해 주는 조건이다. 이에 본 연구는 순환골재의 콘크리트용으로의 사용을 적극 권장하고자 콘크리트용 순환골재 사용 시 건축기준의 완화 내용을 검토하였고 순환골재 중 순환굵은골재을 사용하여 치환율에 따른 배치플랜트에서의 적정 혼합시간을 도출하였다. 또한 건조수축 개선을 위해 순환골재용 혼화제를 사용하여 순환굵은골재 치환율별 콘크리트의 물리, 역학적 특성에 대해 비교 분석하여 건조수축 개선 효과를 나타내어 향후 현장에 안정적으로 적용이 가능할 것으로 판단된다.

순환 슬러지 및 순환 유리골재를 사용한 순환 상온아스팔트 혼합물의 기초특성 (Fundamental Properties of Recycled Cold Asphalt Mixtures with Recycled Sludge and Recycled Glass Aggregate)

  • 이후석;강석표;강혜주;이민희
    • 한국건설순환자원학회논문집
    • /
    • 제8권3호
    • /
    • pp.302-309
    • /
    • 2020
  • 건설폐기물 중간처리시설에서 발생하고 있는 폐슬러지를 건조 분쇄한 순환 슬러지와 재활용되지 못하는 폐유리병을 가공처리한 순환 유리골재를 순환 상온아스팔트에 적용하기 위한 기초연구로서 순환 슬러지 및 순환 유리골재의 사용에 따른 순환 상온아스팔트의 특성을 비교·검토하였다. 그 결과 순환 슬러지를 채움재로서 사용량을 증가할수록 순환 상온아스팔트 혼합물의 마샬 안정도, 간접인강강도, 인장강도비는 감소하고 흐름값, 공극률은 증가하는 것으로 나타났다. 또한 순환 유리골재를 사용함으로서 순환 상온아스팔트 혼합물의 마샬 안정도, 간접인강강도, 인장강도비는 감소하고 흐름값, 공극률은 증가하는 것으로 나타났다.