• 제목/요약/키워드: Ram Speed

검색결과 194건 처리시간 0.023초

반응고 A356 합금의 재가열 특성 및 반용융 압출 (Thixo Extrusion and Reheating Characteristics of Semi Solid A356 Alloy)

  • 김대환;정현주;심성용;임수근;이상용
    • 한국주조공학회지
    • /
    • 제34권4호
    • /
    • pp.123-129
    • /
    • 2014
  • This work presents the results of a thixo-extrusion process applied to aluminum alloy and and reheating characteristics of semi-solid A356 Alloy using have been discussed. The reheating experiment was performed using an electric resistance furnace and multi-stage heating for uniform reheating. The thixo-extrusion was performed at the optimal reheating conditions of the semi-solid A356 alloy, the the extrusion conditions were an extrusion ratio of 33 and ram speed of 6 mm/sec. The results showed that the thixo-extrusion of semi-solid A356 alloy fabricated by the cooling slope reduced the extrusion pressure by 180% in comparison with hot extrusion, and that a sound extrusion could be obtained in spite of the same extrusion ratio and strain rate.

SM45C강의 온도변화에 따른 Nd:YAG 레이저 표면경화 특성 (Characteristics of Surface Hardening of Nd:YAG Laser According to Temperature Changes of SM45C)

  • 이가람;양윤석;황찬연;유영태
    • 한국생산제조학회지
    • /
    • 제21권6호
    • /
    • pp.988-997
    • /
    • 2012
  • Laser surface hardening is one of core technologies to enhance various characteristics such as the strength, hardness, toughness, abrasion resistance, and fatigue resistance for the mold material. This paper focuses on testing characteristics of the laser heat treatment according to the preheating parameters in case of the SM45C medium carbon steel. In this paper, we assume that the power and travel speed of the laser are 1,800W and 0.5m/min, respectively, and the range of the preheating temperature is $50^{\circ}C{\sim}300^{\circ}C$. From the result of the test, we observed that the hardness width and depth are enhanced as the temperature is increased. Also, the best average hardness was 751.7Hv for the temperature of $100^{\circ}C$.

반용융 압출에 의한 A7075 합금의 등방성 제어 (Isotropy Control of 7075 Al Wrought Alloy by Thixoextrusion)

  • 윤영옥;김세광
    • 한국주조공학회지
    • /
    • 제30권6호
    • /
    • pp.210-216
    • /
    • 2010
  • The aim of this study is to characterize a thixoextruded 7075 Al wrought alloy bar in terms of its isotropic behavior through the optical microscope, mechanical test and electron back scattered diffraction. It is also discussed of the extrudability improvement for 7075 Al wrought alloy by thixoextrusion, with emphasis on controlling thixoextrusion parameters. Hot extrusion shows that the maximum extrusion pressure depends on their characteristics in terms of flow stress and hot workability. In the contrary, thixoextrusion demonstrates that the maximum extrusion pressure is almost uniform regardless of the experimental parameters, such as initial ram speed, die bearing length and thixoextrusion temperature. The hot extruded microstructures become elongated to extrusion direction, while the thixoextruded microstructures are isotropic and homogeneously distributed due to the existence of liquid phase between solid grains during the process. The grain refinement due to dynamic recrystallization during thixoextrusion has been also occurred. Subsequent recrystallization would lead to the strengthening of mechanical properties, as observed in the study. The important point is that the values of tensile, yield strength and elongation of the thixoextruded bar without plastic deformation are similar to those of the hot extruded bar with severe plastic deformation.

분말압출법으로 제조된 $SiC_p$/2024Al 복합재료에 있어서 압출온도와 다이각이 기계적 성질에 미치는 영향 (The Effect of Extrusion Temperature and Die Angle on Mechanical Properties of $SiC_p$/2024Al Composites Fabricated by Powder Extrusion Method)

  • 성병진
    • 한국분말재료학회지
    • /
    • 제2권1호
    • /
    • pp.44-52
    • /
    • 1995
  • Effects of the extrusion temperature and die angle on the tensile properties of SiCIyAl composites in powder extrusion have been investigated. SiCP/Al composites were extruded at various extrusion temperatures (450, 500, $550^{\circ}C$) under the extrusion ratio of 25 : 1. The ram speed was maintained at 13 cm/min for all the extrusion conditions. The surface of the extruded rod appeared to be smooth without tearing at 450 and 50$0^{\circ}C$, whereas it was very rough due to tearing at $550^{\circ}C$. It was found that the tensile strength and elongation of the composites extruded at $500^{\circ}C$ are greater than those of composites extruded at $450^{\circ}C$ This is due to the easier plastic deformation of composite extruded at $500^{\circ}C$, compared with the composites extruded at $450^{\circ}C$. The effect of die angle was examined under 20=60, 120, $180^{\circ}$die angles at extrusion temperature of $500^{\circ}C$ under 25:1 extrusion ratio. The tensile strength of the composites extruded with 20=$60^{\circ}$approved to be higher than that of the composties extruded with 28 : 120 and $180^{\circ}$This is attributable to the higher extrusion pressure, which mixed composite powders could be densely consolidated at elevated temperatures, resulting from high friction force between billet and sliding surface of conical die.

  • PDF

전압 표준용 RSFQ counter회로의 설계 (Circuit design of an RSFQ counter for voltage standard applications)

  • 남두우;김규태;김진영;강준희
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 추계학술대회 논문집
    • /
    • pp.127-130
    • /
    • 2003
  • An RSFQ (Rapid Single Flux Quantum) counter can be used as a frequency divider that was an essential part of a programmable voltage standard chip. The voltage standard chip is composed of two circuit parts, a counter and an antenna Analog signal of tens to hundreds ㎓ may be applied to a finline antenna part. This analog signal can be converted to the stream of SFQ voltage pulses by a DC/SFQ circuit. The number of voltage pulses can be reduced by 2n times when they pass through a counter that is composed of n T Flip-Flops (Toggle Flip-Flop). Such a counter can be used not only as a frequency divider, but also to build a programmable voltage standard chip. So, its application range can be telecommunication, high speed RAM, microprocessor, etc. In this work, we have used Xic, WRspice, and L-meter to design an RSFQ counter. After circuit optimization, we could obtain the bias current margins of the T Flip-Flop circuit to be above 31% Our RSFQ counter circuit designs were based on the 1 ㎄/$\textrm{cm}^2$ niobium trilayer technology.

  • PDF

도시형자기부상열차 열차제어시스템 RAMS 분석에 관한 연구 (A Study on the RAMS Analysis of Urban Maglev Train Control System)

  • 윤학선;이기서;류승균;양동인
    • 한국철도학회논문집
    • /
    • 제14권6호
    • /
    • pp.515-525
    • /
    • 2011
  • 도시형 자기부상열차 실용화사업에 적용된 유도무선루프방식 열차제어시스템에 대하여 최상위 레벨에서 전체 시스템에 대한 시스템 분류, 기능 분석을 시행하고 차상신호설비, 지상신호설비로 나누어 신뢰도, 가용도, 유지보수도 및 안전도를 수식을 통하여 분석한 결과를 제시하였다. RAM 분석은 신뢰도 블록도(RBD)를 각 장치별로 적용하여 시스템 서비스 가용도를 산출하였고, 안전도 분석은 PHA(예비위험원 분석), FMEA (고장모드영향분석), HAZOP을 통한 각각의 정상사상(Top Event)의 FTA(고장트리분석)을 시행하고 그 결과를 제시하여 RAMS 목표 값에 도달함을 수식을 통하여 증명하였다.

Development of a Controller for Polishing Robot Attached to Machining Center and Its Performance Evaluation

  • Go, Seok-Jo;Lee, Min-Cheol
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 1998년도 제13차 학술회의논문집
    • /
    • pp.346-351
    • /
    • 1998
  • Cutting process has been automated due to progress of CNC and CAD/CAM, but polishing process has been only depended on experiential knowledge of expert. Polishing work for a curved surface die demands simple and repetitive operations but requires much time for its high precision. Therefore it is operated in the handiwork by skilled worker. However the workers intend to avoid gradually polishing work because of the poor environments such as dust and noise. In order to reduce the polishing time and solve the problem of shortage of skilled workers, it has been done some research for an automation of polishing. To automate the polishing process, a 2 axes polishing robot which is attached to a 3 axes machining center has been developed by our previous research. This automatic polishing robot is able to keep the polishing tool normal on the curved surface of die. Therefore its performance of polishing is improved because of always keeping the tool normal on the surface. In this paper, the smaller sized polishing robot is developed to improve polishing performance. And the controller for 2 axes polishing robot is developed. The controller is composed of TMS320C31 with high speed which is 40-ns instruction cycle time, RAM memory with 64K words, digital input with 64 bits, digital output with 32 bits, and D/A converter with 4 channels, which is 12 bits resolution. To evaluate polishing performance of this developed robot, polishing experiment for shadow mask was carried out.

  • PDF

Bulk-Si와 PD-SOI에 형성된 SiGe p-MOSFET의 전기적 특성의 비교 (Comparison of Electrical Characteristics of SiGe pMOSFETs Formed on Bulk-Si and PD-SOI)

  • 최상식;최아람;김재연;양전욱;한태현;조덕호;황용우;심규환
    • 한국전기전자재료학회논문지
    • /
    • 제20권6호
    • /
    • pp.491-495
    • /
    • 2007
  • This paper has demonstrated the electrical properties of SiGe pMOSFETs fabricated on both bulk-Si and PD SOI substrates. Two principal merits, the mobility increase in strained-SiGe channel and the parasitic capacitance reduction of SOI isolation, resulted in improvements in device performance. It was observed that the SiGe PD SOI could alleviate the floating body effect, and consequently DIBL was as low as 10 mV/V. The cut-off frequency of device fabricated on PD SOI substrate was roughly doubled in comparison with SiGe bulk: from 6.7 GHz to 11.3 GHz. These experimental result suggests that the SiGe PD SOI pMOSFET is a promising option to drive CMOS to enhance performance with its increased operation frequency for high speed and low noise applications.

냉각판으로 제조한 반응고 AM100A 마그네슘 합금의 미세조직 및 열간 압출성 (The Microstructures and Hot Extrudability of Semi-solid AM100A Magnesium Alloy Fabricated by Cooling Plate)

  • 김대환;성영록;심성용;이상용;김광삼;임수근
    • 한국주조공학회지
    • /
    • 제29권3호
    • /
    • pp.144-149
    • /
    • 2009
  • In this study, we investigated optimum condition of cooling plate method to obtain semi-solid AM100A Mg alloy with fine and globular morphology. AM100A Mg alloy were hot extruded at $380^{\circ}C$ extrusion temperature under extrusion ratio of 25 : 1 and ram speed of 2.4 mm/sec. Vickers hardness test, optical microscopy, scanning electron microscopy, and image analyzer were performed to identify the optimum conditions of cooling plate method. Optimum conditions of cooling plate method to fabricate semi-solid AM100A Mg alloy with fine and globular microstructures were achieved at a pouring temperature of $602^{\circ}C$ and the angle of cooling plate of 60 degree.

슬림형 광 디스크 드라이브의 방진설계 (An Anti-vibration Design of Slim-type Optical Disk Drive)

  • 김남웅;김국원;홍구;정문채;김외열
    • 소음진동
    • /
    • 제9권2호
    • /
    • pp.324-330
    • /
    • 1999
  • With the increase of track density, high rotational speed and the compatibility for various media such as CD-ROM, CD-R/RW, DVD-ROM/RAM/RW etc. in optical disk drive, the effective anti-vibration design is so crucial for robust operaton. Especailly when the drive is self-excited by unbalanced disk, internal sled base vibration and its external transmission to the case bring about so severe problem. Generally these two consideration points the practical anti-vibration design process to control thses two conflictive properties using finite element analysis. As an example of the design process, Duro 25 and 40 visco-elastic rubber mount was selected and analyzed. The stiffness obtained from FEM rubber model was well matched with the experiments. Also it was confirmed that the internal and external vibration induced from unbalanced disk have good agreement with experimental results. The proposed design process is adopted to the slim-type optical disk drive.

  • PDF