The Microstructure of the Reaction -Bonded $Si_3N_4$ Formed in the Various Atmosphere (질화분위기에 따른 반응결합 질화규소의 미세구조변화)

  • 박지연;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.5
    • /
    • pp.61-66
    • /
    • 1986
  • The gas mixtures ($H_2$/$N_2$, He/$N_2$) having a high thermal conductivity allow the heat generated by the nitriding exotherm to be dissipated from the compact in to the nitriding atmosphere permitting a more accurate control of temperature and produces a more uniform microstructure. In order to observe the effect of the mixed gas atmosphere on the microsturcture of RBSN. the specimen was nitrided in the mixed gas atmosphere which was containe up to 50vol% $H_2$ or He for 0-12 hrs at 135$0^{\circ}C$. The addition of hydrogen to nitrogen gas resulted in the growth of a-needle at the early stage of nitrding increase of the reaction rate and a finer and more uniform microstructure. in case of the addition of helium the behaviour of reaction was similar to the one with pure nitrogen. As the amount of helium was increased a coarse microstructure was formed.

  • PDF

Fabrication of Porous RBSN Ceramics with Aligned Channels by an Ice-Templating Method

  • Kim, Dong-Seok;Go, Jae-Ung;Kim, Do-Gyeong
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2012.05a
    • /
    • pp.97.1-97.1
    • /
    • 2012
  • Porous ceramics are widely used for applications such as catalysis supports, gas distributors and filters such as DPF. For these purpose, it is important to have proper porosity controlling pore structure while maintaining mechanical and thermal properties. In this work, we have prepared the porous ceramic structures made of reaction bonded silicon nitride with hierarchical pore structures. Uni-directionally aligned pore channels, which are mostly filled with ${\beta}$-Si3N4 whiskers, were achieved by an ice-templating method. The structures of the pore channels and the walls are controllable by the processing conditions, such as solid concentration, freezing rate of the slurry, and additives. We have investigated and characterized the influences of the conditions on the microstructures and the properties, such as porosity, pore size distribution, lamellar thickness, wavelength, and orientations. The compressive strength test and flow test was performed to determine the structural integrity and air permeability.

  • PDF

Rigid-Body-Spring Networks를이용한 철근콘크리트의 Lap Splice 설계 모델 시뮬레이션

  • Yun, Seung-Hyeon;Park, Ji-Un
    • Proceeding of EDISON Challenge
    • /
    • 2017.03a
    • /
    • pp.180-186
    • /
    • 2017
  • 거의 모든 철근콘크리트 구조물의 보강 강재는 분할된 두개 이상의 철근으로 제작되며, 이러한 철근의 분할 부위를 평행한 두개의 철근으로 겹쳐 설치하는 것을 겹이음(Lap splice)이라고 부른다. 일반적으로 겹이음 설계는 무리없이 설계 강도를 만족시킬 뿐만 아니라 충분히 긴 수명을 가진다. 그러나 550MPa 이상의 항복 강도를 갖는 철근이나 인장 부재의 설계, 초고성능 섬유보강 콘크리트의 보강재 설계와 같은 경우, 현행 철근 겹이음 설계만으로는 그 한계가 발생한다. 따라서 현 겹이음 설계는 관련 기준의 추가와 구조적인 측면에서의 개선이 필요할 것으로 보여지며, 이를 위해 적절한 실험과 데이터 분석, 그리고 컴퓨터를 이용한 새로운 설계 모델의 개발 등의 과정이 필요할 것으로 여겨진다. 본 연구는 균질하지 않은 물성의 파괴를 다루는 RBSN(Rigid-Body-Spring Networks)을 통한 컴퓨터 시뮬레이션으로 더 효과적이고 정확한 겹이음 설계가 가능할 것으로 판단하고, 실제 모델링으로 그 가능성을 검증하였다.

  • PDF

Characterization of Pore Structures for Porous Sintered Reaction-Bonded Silicon Nitrides with Varied Pore-Former Content

  • Park, Young-Jo;Song, In-Hyuck;Kim, Hai-Doo
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.11
    • /
    • pp.675-680
    • /
    • 2008
  • The effect of pore former content on both porosity and pore structure was investigated for porous sintered reaction-bonded silicon nitrides (SRBSNs). A spherical PMMA with $d_{50}=8{\mu}m$ was employed as a pore-former. Its amount ranged from 0 to 30 part. Porous SRBSNs were fabricated by post-sintering at various temperatures where the porosity was controlled at $12{\sim}52%$. The strong tendency of increasing porosity with PMMA content and decreasing porosity with sintering temperature was observed. Measured pore-channel diameter increased $(0.3{\rightarrow}1.1{\mu}m)$ with both PMMA content and sintering temperature.

The behavior of Si During Sintering of Reaction Bonded Silicon Nitride (반응결합 질화수소의 소결시 규소의 거동에 관한 연구)

  • 김재룡;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.5
    • /
    • pp.67-74
    • /
    • 1986
  • To investigate the effects of unreacted silicon on the $\alpha$/$\beta$transfornation variation of morphology and mechanical strength of Sintered Reaction Bonded Silicon Nitride the mixtures of $\alpha$-$Si_3N_4$ and Si powder and Reaction Bonded Silicon Nitride were heat treated. The heat-treatments were performed in Ar atmosphere in order to inhibit the nitridation of silicon. In the mixtures heat-trated at 1$700^{\circ}C$ the amount of $\beta$-TEX>$Si_3N_4$transformed from $\alpha$-TEX>$Si_3N_4$was sigmoidally increased and the equiaxed $\alpha$-TEX>$Si_3N_4$grains elongated with the amount of silicon and heat treating time. And large $\beta$-TEX>$Si_3N_4$grains grown into silicon were observed. On the other hand there was no change in the heat-treatment of pure $\alpha$-TEX>$Si_3N_4$In case of the heat-treatment of RBSN the same phenomena due to the silicon appearing from the decomposition of $\alpha$-Smatte and needle were observed. From the three point bending test the strength of the sintered specimens with the and without 5wt% silicon addition had 53Kg/$mm^2$ and 73Kg/$mm^2$ respectively.

  • PDF

Fabrication of β-SiAlONs by a Reaction-Bonding Process Followed by Post-Sintering

  • Park, Young-Jo;Noh, Eun-Ah;Ko, Jae-Woong;Kim, Hai-Doo
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.5
    • /
    • pp.452-455
    • /
    • 2009
  • A cost-effective route to synthesize $\beta$-SiAlONs from Si mixtures by reaction bonding followed by post-sintering was investigated. Three different z values, 0.45, 0.92 and 1.87, in $Si_{6-z}Al_zO_zN_{8-z}$ without excess liquid phase were selected to elucidate the mechanism of SiAlON formation and densification. For RBSN (reaction-bonded silicon nitride) specimens prior to post-sintering, nitridation rates of more than 90% were achieved by multistep heating to $1400^{\circ}C$ in flowing 5%$H_2$/95%$N_2$; residual Si was not detected by XRD analysis. An increase in density was acquired with increasing z values in post-sintered specimens, and this tendency was explained by the presence of higher amounts of transient liquid phase at larger z values. Measured z values from the synthesized $\beta$-SiAlONs were similar to the values calculated for the starting compositions. Slight deviations in z values between measurements and calculations were rationalized by a reasonable application of the characteristics of the nitriding and post-sintering processes.

A Study of Thermo-Mechanical Behavior and Its Simulation of Silicon Nitride Substrate on EV (Electronic Vehicle)'s Power Module (전기자동차 파워모듈용 질화규소 기판의 열기계적 특성 및 열응력 해석에 대한 연구)

  • Seo, Won;Jung, Cheong-Ha;Ko, Jae-Woong;Kim, Gu-Sung
    • Journal of the Semiconductor & Display Technology
    • /
    • v.18 no.4
    • /
    • pp.149-153
    • /
    • 2019
  • The technology of electronic packaging among semiconductor technologies is evolving as an axis of the market in its own field beyond the simple assembly process of the past. In the field of electronic packaging technology, the packaging of power modules plays an important role for green electric vehicles. In this power module packaging, the thermal reliability is an important factor, and silicon nitride plays an important part of package substrates, Silicon nitride is a compound that is not found in nature and is made by chemical reaction between silicon and nitrogen. In this study, this core material, silicon nitride, was fabricated by reaction bonded silicon nitride. The fabricated silicon nitride was studied for thermo-mechanical properties, and through this, the structure of power module packaging was made using reaction bonded silicon nitride. And the characteristics of stress were evaluated using finite element analysis conditions. Through this, it was confirmed that reaction bonded silicon nitride could replace the silicon nitride as a package substrate.

The Effect of Si3N4 Addition on Nitriding and Post-Sintering Behavior of Silicon Powder Mixtures

  • Park, Young-Jo;Ko, Jae-Woong;Lee, Jae-Wook;Kim, Hai-Doo
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.4
    • /
    • pp.363-368
    • /
    • 2012
  • Nitriding and post-sintering behavior of powder mixture compacts were investigated. As mixture compacts are different from simple Si compacts, the fabrication of a sintered body with a mixture composition has engineering implications. In this research, in specimens without a pore former, the extent of nitridation increased with $Si_3N_4$ content, while the highest extent of nitridation was measured in $Si_3N_4$-free composition when a pore former was added. Large pores made from the thermal decomposition of the pore former collapsed, and they were filled with a reaction product, reaction-bonded silicon nitride (RBSN) in the $Si_3N_4$-free specimen. On the other hand, pores from the decomposed pore former were retained in the $Si_3N_4$-added specimen. Introduction of small $Si_3N_4$ particles ($d_{50}=0.3{\mu}m$) into a powder compact consisting of large silicon particles ($d_{50}=7{\mu}m$) promoted close packing in the green body compact, and resulted in a stable strut structure after decomposition of the pore former. The local packing density of the strut structure depends on silicon to $Si_3N_4$ size ratio and affected both nitriding reaction kinetics and microstructure in the post-sintered body.

Sintered-reaction Bonded Silicon Nitride Densified by a Gas Pressure Sintering Process - Effects of Rare Earth Oxide Sintering Additives

  • Lee, Sea-Hoon;Ko, Jae-Woong;Park, Young-Jo;Kim, Hai-Doo;Lin, Hua-Tay;Becher, Paul
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.4
    • /
    • pp.318-324
    • /
    • 2012
  • Reaction-bonded silicon nitrides containing rare-earth oxide sintering additives were densified by gas pressure sintering. The sintering behavior, microstructure and mechanical properties of the resultant specimens were analyzed. For that purpose, $Lu_2O_3-SiO_2$ (US), $La_2O_3$-MgO (AM) and $Y_2O_3-Al_2O_3$ (YA) additive systems were selected. Among the tested compositions, densification of silicon nitride occurred at the lowest temperature when using the $La_2O_3$-MgO system. Since the $Lu_2O_3-SiO_2$ system has the highest melting temperature, full densification could not be achieved after sintering at $1950^{\circ}C$. However, the system had a reasonably high bending strength of 527 MPa at $1200^{\circ}C$ in air and a high fracture toughness of 9.2 $MPa{\cdot}m^{1/2}$. The $Y_2O_3-Al_2O_3$ system had the highest room temperature bending strength of 1.2 GPa.

Densification Behavior of Reaction-Bonded Silicon Nitride Prepared by Using Coarse Si Powders (조대 Si입자분말을 사용한 질화반응 Si3N4의 치밀화 거동)

  • 이주신;문지훈;한병동;박동수;김해두
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.1
    • /
    • pp.45-50
    • /
    • 2002
  • Effect of sintering additives on the densification behavior of reaction-bonded silicon nitride prepared by using coarse Si powders is discussed. Sintering additives such as 6 wt% $Y_2O_3$+1wt% $A1_2O_3$ (6YlA) did not give rise to full densification, while full densification was obtained by using the sintering additives such as 6wt% $Y_2O_3$+3 wt% $A1_2O_3$+ 2wt% $SiO_2$ (6Y3A2S) and 9wt% $Y_2O_3$+ 1.5wt% $A1_2O_3$+ 3wt% $SiO_2$ (9Yl.5A3S). In the case of 6Y3A2S addition, high fracture strength of 960 MPa and the fracture toughness of $6.5 MPa.m^{1/2}$ were obtained.