• 제목/요약/키워드: R-D diagram

검색결과 126건 처리시간 0.027초

THE C-M DIAGRAM OF THE GLOBULAR CLUSTER, NGC 6752

  • Lee, See-Woo;Cannon, R.D.
    • 천문학회지
    • /
    • 제13권1호
    • /
    • pp.15-26
    • /
    • 1980
  • The BV-photographic photometry was made for 1714 stars (V<19.5) in NGC 6752. The C-M diagram of this cluster shows an unusually extended blue horizontal branch $(V=13.5{\sim}17.8)$ with a wide gap $(V=16{\sim}16.7)$ and the well defined giant branch with gaps at V=13.85 and 16.2. The turnoff point is defined at $V=17.25{\pm}0.15$ and (B-V) = $0.46{\pm}0.02$. If we take $V_{HB}=13.85$ for NGC 6752, then ${\Delta}V=2.80,\;(B-V)_{0,g}=0.76\;and\;{\Delta}V_{TO}=3.40$ and the chemical abundance is estimated to be [Fe/H]=-1.67 or $Z=4.3{\times}10^{-4}\;and\;Y=0.26$. Some other physical parameters of this cluster are derived and compared with those for the well observed clusters M 3, M 13, M 15 and M 92.

  • PDF

CDM을 이용한 Ball-Beam 위치제어 (A Position control of Ball-Beam using CDM)

  • 정지연;추연규;임영도
    • 한국지능시스템학회:학술대회논문집
    • /
    • 한국퍼지및지능시스템학회 2002년도 추계학술대회 및 정기총회
    • /
    • pp.139-142
    • /
    • 2002
  • 제어 시스템에서 제어기를 설계하는 방법에는 기존 PID 설계 기법인 Ziegler-Nichols와 Jung, R. C. Dorf 방법들이 있다. 본 논문은 Shunji Manabe의 계수도법(CDM Coefficient Diagram Method)을 이용하여 Ball-Beam 시스템을 제어하기 위한 PID 제어기를 설계한다. PID 제어기의 각 파라메터인 P, I, D 계수는 시스템의 속도와 안정성에 기인하는 표준 안정도 지수$(\gamma)$와 등가시정수$(\tau)$ 로부터 얻 어진다. 등가시정수$(\tau)$와 안정도 지수$(\gamma)$는 제어기 파라메터의 대수적 형태와 절대적인 관계가 있다. 그러므로 설계된 제어기로부터 빠른 상승시간과 안정된 정상상태 응답을 얻을 수 있다. Ball-Beam 시스템에 CDM 제어기를 적용한 결과 시스템의 안정도, 정확성 그리고 강인성에 있어서 퍼지 제어기나 PID 제어기에 비해 뛰어난 응답 특성을 확인하였다

변형률속도 효과를 고려한 AZ31B 판재의 온간 성형한계도 예측 - II (Prediction of the Forming Limit Diagram for AZ31B Sheet at Elevated Temperatures Considering the Strain-rate Effect - II)

  • 최선철;김헌영;김형종
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.285-288
    • /
    • 2009
  • The purpose of this study is to predict the forming limit diagram (FLD) of strain-rate sensitive materials on the basis of the Marciniak and Kuczynski (M-K) theory. The strain-rate effect is taken into consideration in such a way that the stress-strain curves for various strain-rates are inputted into the formulation as point data, not as curve-fitted models such as power function. Tensile tests and R-value tests were carried out at several levels of temperature and strain-rate from $25^{\circ}C$ to $300^{\circ}C$ and 0.16 to 0.00016/s, respectively to obtain the mechanical properties of AZ31B magnesium alloy sheet. The FLD of this material was experimentally obtained by limit dome height tests with the punch velocity of 0.1 and 1.0 mm/s at $250^{\circ}C$. The M-K theory-based FLD predicted using Yld2000-2d yield criterion was compared with the experimental results.

  • PDF

마찰교반용접(FSW) 된 알루미늄 합금(AA6111-T4, AA5083-H18) 및 DP강 판재의 인장 실험시 파단 현상 해석 (Analysis of Failure Phenomena in Uni-axial Tension Tests of Friction Stir Welded AA6111-T4, AA5083-H18 and DP-Steel)

  • 박상준;엄기문;마닝;안강환;정경환;;;;정관수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.258-261
    • /
    • 2007
  • Failure phenomena in uni-axial tension test were experimentally and numerically investigated for AA6111-T4, AA5083-H18 and DP-Steel, which were friction-stir welded with the same and different thicknesses. Forming limit diagram(FLD) was measured using hemispherical dome stretching tests for base materials and also predicted by Hill's bifurcation and M-K theories for welded areas. Finite element simulations well predicted hardening behaviors, failure locations as well as failure patterns for the uni-axial tension tests especially utilizing very fine meshes and FLD along with stress softening.

  • PDF

마찰교반용접(FSW) 된 알루미늄 합금(AA6111-T4, AA5083-H18) 및 DP강 판재의 인장 실험시 파단 현상 해석 (Analysis of Failure Phenomena in Uni-axial Tension Tests of Friction Stir Welded AA6111-T4, AA5083-H18 and DP-Steel)

  • 박상준;엄기문;마닝;안강환;정경환;;;;정관수
    • 소성∙가공
    • /
    • 제16권4호
    • /
    • pp.304-308
    • /
    • 2007
  • Failure phenomena in uni-axial tension test were experimentally and numerically investigated for AA6111-T4, AA5083-H18 and DP-Steel, which were friction-stir welded with the same and different thicknesses. Forming limit diagram(FLD) was measured using hemispherical dome stretching tests for base materials and also predicted by Hill's bifurcation and M-K theories for welded areas. Finite element simulations well predicted hardening behaviors, failure locations as well as failure patterns for the uni-axial tension tests especially utilizing very fine meshes and FLD along with stress softening.

NO OPEN CLUSTER IN THE RUPRECHT 93 REGION

  • Cheon, So-Ra;Sung, Hwan-Kyung;Bessell, M.S.
    • 천문학회지
    • /
    • 제43권4호
    • /
    • pp.115-121
    • /
    • 2010
  • UBVI CCD photometry is obtained for the Ruprecht 93 (Ru 93)region. We are unable to confirm the existence of an intermediate-age open cluster in Ru 93 from the spatial distribution of blue stars. On the other hand, we find two young star groups in the observed field: the nearer one (Ru 93 group) comprises the field young stars in the Sgr-Car arm at $d{\approx}2.1$ kpc, while the farther one (WR 37 group) is the young stars around WR 37 at $d{\approx}4.8$ kpc. We derive an abnormal extinction law ($R_V$ = 3.5) in the Ruprecht 93 region.

ON THE 2-BRIDGE KNOTS OF DUNWOODY (1, 1)-KNOTS

  • Kim, Soo-Hwan;Kim, Yang-Kok
    • 대한수학회보
    • /
    • 제48권1호
    • /
    • pp.197-211
    • /
    • 2011
  • Every (1, 1)-knot is represented by a 4-tuple of integers (a, b, c, r), where a > 0, b $\geq$ 0, c $\geq$ 0, d = 2a+b+c, $r\;{\in}\;\mathbb{Z}_d$, and it is well known that all 2-bridge knots and torus knots are (1, 1)-knots. In this paper, we describe some conditions for 4-tuples which determine 2-bridge knots and determine all 4-tuples representing any given 2-bridge knot.

3차원 적분법을 이용한 변류기의 누설 인덕턴스에 대한 연구 (A Study on the Leakage Inductance in Current Transformers by 3D Integral Methods)

  • 이희갑;박용필;이성일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.116-118
    • /
    • 2002
  • This paper presents leakage magnetic field and leakage inductance calculations in current transformer by means of 3-D Integral methods. From the distribution diagram of leakage magnetic flux to be analyzed using program called TRACAL 3, it confirms a parallel to the winding axis direction of the leakage flux lines in the air gap between the windings. The leakage inductances $L_{r1}\;and\;L_{r2}$ of the primary and secondary windings were calculated, their values are 4.23 mH and 0.49 mH, respectively. They are also similar to the measured values of the leakage inductances for the experimental verification, 4.06 mH and 0.47 mH.

  • PDF

식쌍성 T LMi의 궤도요소와 공전주기 변화에 관한 연구 (Orbital Elements and Period Variation of the Eclipsing Binary T LMi)

  • 오규동
    • Journal of Astronomy and Space Sciences
    • /
    • 제4권2호
    • /
    • pp.69-80
    • /
    • 1987
  • Okazaki(1997)의 2색(V와B)의 광전측광에 의한 광도곡선을 Wilson and Devinney모델을 이용하여 T LMi의 광전궤도요소를 구하였으며 지금까지 발표된 이 별의 극심시각을 문헌으로 수집하여 궤도공전주기변화를 분석하였다.T LMi의 공전주기 변화는 simusoidal한 주기변화를 나타내며 그 진폭은 $0.^{d}0425$ 이고 장주기변화는 $62.^{y}01$ 로 나타났다. 한편, 이번 연구에서 얻어진 T LKi의 물리적 성질에 따르면 이 별은 "R CMa" 형으로 분류한다는 것은 재검토가 있어야 하겠다.검토가 있어야 하겠다.

  • PDF

Behaviour of nitrided layer formed on S45C carbon steel during gaseous nitriding

  • 손석원;유광춘;이원범
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.171.1-171.1
    • /
    • 2016
  • 재료의 표면 강화 방법 중의 하나인 질화공정을 이용하여 탄소강 S45C 소재의 질화 거동에 대하여 연구하였다. $520^{\circ}C$ 온도에서 질화 공정을 진행하여 공정시간에 따른 Kn값을 수소 센서로 측정하여 공정시간에 따른 N-potential의 변화와 그에 따른 화합물층 성장 및 화합물층의 상변화에 대해 관찰하였다. 화합물 층의 미세구조 변화는 광학현미경 및 주사전자현미경을 통해 관찰하였다. 가스 질화 처리 후 표면경도는 약 600Hv의 경도값이 측정되었고, 공정 시간이 늘어남에 따라 화합물층 및 경화깊이가 증가되고 표면 화합물이 성장하여 porous가 감소하는 것을 확인 할 수 있다. 경화깊이는 1440분 일 때 약 0.5mm 경화 깊이를 얻었고, 화합물층의 성장은 ${\varepsilon}$상(Fe2-3N)과 ${\gamma}$'상(Fe4N)으로 두 개의 상으로 형성되는 것을 관찰할 수 있었다. 시험 결과를 바탕으로 S45C 소재의 탄소 함량에 따른 lehrer diagram을 열역학 적으로 계산하고 화합물층의 형성 기구에 대해 비교 분석하였다.