Effects of Two-Step Annealing Process on the Pulsed Laser Ablated Lead Zirconate Titanate Thin Films

  • Rhie, Dong-Hee
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • v.3C no.2
    • /
    • pp.43-47
    • /
    • 2003
  • Lead zirconate titanate (PZT) thin films were fabricated by the pulsed laser ablation deposition (PLAD) method onto Pt/Ti/SiO$_2$/Si substrates. Crystalline phases as well as preferred orientations in PZT films were investigated by X-ray diffraction analysis (XRD). The well-crystallized perovskite phase and the (101) preferred orientation were obtained by two-step annealing at the conditions of $650^{\circ}C$, 1 hour. It was found that the temperature for the pulsed laser ablated PZT films annealed via a two-step annealing process can be reduced 20$0^{\circ}C$ compared to that of the conventional three-step annealing temperature profile for enhancing the transformation of the perovskite phase. The remanent polarization and the coercive field of this film were about 20 $\mu$C/$\textrm{cm}^2$ and 46 kV/cm, while the dielectric constant and loss values measured at 1 KHz were approximately 860 and 0.04, respectively. The interesting phenomena of this film, such as vertical shift in hysteresis curve, are also discussed.

Fabrication and Properties of ZnSnO3 Piezoelectric Films Deposited by a Pulsed Laser Deposition (Pulsed Laser Deposition 방법으로 증착된 ZnSnO3 압전 박막의 성장과 특성 평가)

  • Park, Byeong-Ju;Yoon, Soon-Gil
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.1
    • /
    • pp.18-21
    • /
    • 2014
  • Because the Pb-based piezoelectric materials showed problems such as an environmental pollution. lead-free $O_3$ materials were studied in the present study. The $O_3$ thin films were deposited at $640^{\circ}C$ on $Pt/Ti/SiO_2$ substrate by pulsed laser deposition (PLD) and were annealed for 5 min at $750^{\circ}C$ using rapid thermal annealing (RTA) in nitrogen atmosphere. Samples annealed at $750^{\circ}C$ showed a smooth morphology and an improvement of the dielectric and leakage properties, as compared with as-grown samples. However, electrical properties of the $O_3$ thin films obtained in the present study should be improved for piezoelectric applications.

Visible light emission from $C_60$ and Si nanoparticle film by laser process (C60 및 Si 초미립자 박막의 Laser 반응에 의한 가시광선발광)

  • ;Hideomi Koinuma
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.598-601
    • /
    • 2000
  • We investigated the fabrication of Si nanoparticle and $C_{60}$ thin films by pulsed laser ablation. As a result, we observed visible green photoluminescence spectra in the Si/C$_{60}$ multilayer films after laser annealing. It is considered that this green photoluminescence is occurred from SiC particles, which is produced reaction of Si nanoparticles with $C_{60}$ via laser annealing.ing.

  • PDF

Analytic Study on Pulsed-Laser Polishing on Surface of NAK80 Die Steel (펄스레이저에 의한 NAK80 금형강 표면연마의 해석적 연구)

  • Kim, Kwan-Woo;Kim, Seung-Hwan;Cho, Hae-Yong
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.14 no.6
    • /
    • pp.136-141
    • /
    • 2015
  • Laser surface polishing is a polishing method for improving surface roughness using an integrated laser beam. Using a laser for surface polishing can improve the surface condition without physical contact or chemical action. Laser polishing has mainly been used to polish the surface of diamond or optical articles, such as lenses and glasses. Recently, diverse studies on laser polishing for metals have been conducted. The analytic study of laser surface polishing has been conducted with experimental trials for comparison, so that the proper conditions for laser polishing can be recommended. In this study, laser surface polishing was simulated in order to predict the heat-affected zone on the die steel depending on the power of the pulsed laser. The simulated results were verified by comparing them to those of the experimental trials. Through this study, therefore, the application of FEM to the selection of appropriate laser conditions could be possible.

Characteristics of Output Energy and Optical Parameters in Welding of Braun Tubes by Pulsed Nd:YAG Laser (펄스 Nd:YAG 레이저에 의한 브라운관 부품의 용접시 빔의 출력특성과 광학변수)

  • Kim Jong-Do;Ha Seung-Hyup
    • Laser Solutions
    • /
    • v.8 no.1
    • /
    • pp.27-37
    • /
    • 2005
  • During laser spot welding of the braun tube electron gun, phenomena such as serious spattering and oxidative reaction, etc. were occurred. The spatter occurred from weld pool affects the braun tube, namely it blocks up a very small hole on the shadow mask and causes short circuit between two poles of the electron gun. We guessed that high power density and oxidative reaction are main sources of these problems. So, we studied to prevent and to reduce spatter occurring in spot welding of the braun tube electron gun using pulsed Nd:YAG laser. The characteristics of laser output power was estimated, and the loss of laser energy by optical parameter and spatter was measured by powermeter. The effects of welding parameters, laser defocused distance and incident angle, were investigated on the shape and penetration depth of the laser welded bead in flare and flange joints. From these results, the laser peak power was a major factor to control penetration depth and to occur spatter. It was found that the losses of laser energy by optic parameter and sticked spatter affect seriously laser weldability of thin sheets.