• 제목/요약/키워드: Pulsed Laser deposition

검색결과 639건 처리시간 0.022초

펄스 레이져 증착법으로 성장한 ZnO 박막의 마이크로 PL 특성 분석 (Investigation on the Micro-photoluminescence of ZnO Thin Films Grown by Pulsed Laser Deposition)

  • 이득희;임재현;김상식;이상렬
    • 한국전기전자재료학회논문지
    • /
    • 제22권9호
    • /
    • pp.756-759
    • /
    • 2009
  • We described the growth of undoped ZnO thin films and their optical properties changing with a various growth temperature. The undoped ZnO thin films were grown on $c-Al_2O_3$ substrates using pulsed laser deposition (PLD) at room temperature, 200, 400, and $600^{\circ}C$, respectively. Field emission microscopy (FE-SEM) measurements showed that the grain size of undoped ZnO thin films are increasing as a increase of growth temperature. In addition, we were investigated that the structural and optical properties of undoped ZnO thin films by x-ray diffraction (XRD) and photoluminescence (PL) studied. Also, we could confirmed that the exciton luminescence was strongly related to charge trap by grain boundary of the samples using micro-PL measurement.

Luminescence Characteristics of Red Light Emitting (YVO4:Eu Thin-Film Phosphors Deposited on Si Substrate Using Pulsed Laser Deposition

  • Kim, Dong-Kuk;Kang, Wee-Kyung
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권12호
    • /
    • pp.1859-1862
    • /
    • 2004
  • Europium doped yttrium vanadate ($YVO_4$:Eu) phosphor thin films were grown using a pulsed laser deposition (PLD) technique on silicon substrate. The structural characterization carried out on a series of ($YVO_4$:Eu films at post annealing temperature in the range of 550 $^{\circ}C$-1150 $^{\circ}C$ indicating that films were preferentially (200) oriented at post annealing temperature above 950 $^{\circ}C.$ Photoluminescence of thin film increased with the increase of post annealing temperature and ambient oxygen pressure though the thin film has the powder-like surface morphology at oxygen pressure above 200 mTorr. Photoluminescence decay from $^5D_1$ level of $Eu^{3+}$ show the great concentration dependency, which can be used as a good parameter to control the composition of ($YVO_4$:Eu thin film.

레이저 어블레이션에 의한 $(Pb,La)TiO_3$ 박막의 제작 (Fabrication of $(Pb,La)TiO_3$ Thin Films by Pulsed Laser Ablation)

  • 박정흠;김준한;이상렬;박종우;박창엽
    • 한국전기전자재료학회논문지
    • /
    • 제11권2호
    • /
    • pp.133-137
    • /
    • 1998
  • $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3(PLT(28))$ thin films were fabricated by pulsed laser deposition. PLT films deposited on $Pt/Ti/SiO_2/Si$ at $600^{\circ}C$ had a preferred orientation in (111) plane and at $550^{\circ}C$ had a (100) preferred orientation. We found that (111) preferred oriented films had well grown normal to substrate surface. This PLT(28) thin films of $1{\mu}m$ thickness had dielectric properties of ${\varepsilon}_r$=1300, dielectric $loss{\fallingdotseq}0.03 $. and had charge storage density of 10 [${\mu}C/cm^2$] and leakage current density of less than $10^{-6}[A/cm^2]$ at 100[kV/cm]. These results indicated that the PLT(28) thin films fabricated by pulsed laser deposition are suitable for DRAM capacitor application.

  • PDF

펄스 레이저 증착법에 의한 DLC 박막의 내마모성 특성변화 (Characterization of tribologic DLC thin films fabricated by pulsed laser deposition)

  • 심경석;이상렬
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.851-853
    • /
    • 1999
  • DLC thin films have been fabricated by pulsed laser deposition with various deposition parameters. The characterization of fabricated thin films was performed depending on the deposition parameters. As the kinetic energies provided by deposition temperature and the laser energy density were increased, the film showed graphite properties. Structural properties of the films were investigated by Raman spectroscopy. The growth energy should be optimized to fabricate high quality DLC thin films. DLC films showed high hardness and their friction coefficient was measured to be about 0.2 regardless of the load of the ball pin.

  • PDF

펄스레이저 증착법으로 성장된 ZnO 박막의 어닐링 온도변화에 따른 구조적, 광학적 특성에 관한 연구 (Annealing Effect on the structural and optical properties of ZnO thin films prepared by Pulsed Laser Deposition)

  • 김재홍;이천
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.54-57
    • /
    • 2004
  • ZnO thin films on (001) sapphire substrates have been deposited by pulsed laser deposition(PLD) technique using an Nd:YAG laser with a wavelength of 266 m. During deposition, the experiment of the deposition of ZnO thin films has been performed for substrate temperatures in the range of $400^{\circ}C$ and flow rate of 350 sccm, films have been annealed at various substrate temperatures after deposition. After post-annealing treatment in the oxygen ambient, the structural properties of ZnO thin films were characterized by diffraction (XRD), SEM and the optical of the ZnO were characterized by photoluminescence (PL).

  • PDF

PLD에 의해 제조된 PZT 박막의 미세구조가 강유전 특성에 미치는 영향 (Effects of microstructures on ferroelectric properties of PZT thin films prepared by PLD)

  • 백동수;김민철;신현용;박용웅;윤석진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.224-227
    • /
    • 1999
  • Ferroelectric Pb(Zr$\sub$0.52/Ti$\sub$0.48/)O$_3$ thin films were fabricated by pulsed laser deposition, mainly varying process conditions such as substrate temperature, oxygen pressure, and laser energy, PZT films annealed at more than 600$^{\circ}C$ were crystallized into pure perovskite phases regardless of deposition temperatures. Lower deposition temperature of 400$^{\circ}C$ accompanied with post-annealing at 650$^{\circ}C$ resulted in denser microstructures with extremely small grains compated to those of thin films annealed at higher deposition temperatures. Hysteresis curves of thin film with small grains exhibitied good squareness and low leakage characteristics.

  • PDF

PLD 기술로 제작된 ZnO 박막의 특성 (Characterization of ZnO Thin Films prepared by Pulsed Laser Deposition Technique)

  • 노임준;신백균;이능헌;김용혁;지승한;이상희;한상옥
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1404-1405
    • /
    • 2006
  • Transparent ZnO thin films were deposited on quartz substrates by a KrF pulsed laser deposition (PLD) technique with different process conditions such as substrate temperature ($T_s$) and oxygen ambient pressure ($pO_2$). Surface morphology, crystal structure, and electrical properties of the ZnO films were investigated in order to characterize their thin film properties. The pulsed laser deposited ZnO films showed highly c-oriented crystalline structures depending on the process conditions: the highest FWHM (Full Width Half Maximum) value of (002) peak was observed for the ZnO film prepared at $T_{s}=550^{\circ}C$, $pO_2$=5mTorr and laser fluence of $2J/cm^2$.

  • PDF

펄스 레이저 증착법에 의해 제작된 Laser pulse repetition rate의 변화에 따른 $Pb(Zr_{0.48}Ti_{0.52})O_3$ (PZT) 박막의 전기적 특성 (Effect of Laser Pulse Repetition Rate on the Electrical Properties of $Pb(Zr_{0.48}Ti_{0.52})O_3$ (PZT) Thin Films grown by Pulsed Laser Deposition)

  • 이동화;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.11-12
    • /
    • 2005
  • [ $Pb(Zr_{0.48}Ti_{0.52})O_3$ ] (PZT) thin films were deposited on Pt(111)/Ti/$SiO_2$/Si substrates by pulsed laser deposition. In order to study the effect of different laser pulse repetition rate on the dielectric and ferroelectric properties of PZT thin films,2 Hz and 5 Hz of laser pulse repetition rate were selected. We compared the results of XRD pattern, dielectric constant and hysteresis characteristics. From the experimental data, we found that the electrical properties of PZT thin films which grown ar 2 Hz of laser pulse repetition rate were better than those which grown at 5 Hz of laser pulse repetition rate.

  • PDF

PLD를 이용한 ZnO 박막의 후열처리에 관한 연구 (Effects of post-annealing treatment of ZnO Thin Films by Pulsed Laser Deposition)

  • 김재홍;이천
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 하계학술대회 논문집 C
    • /
    • pp.1627-1630
    • /
    • 2004
  • ZnO thin films on (001) sapphire substrates have been deposited by pulsed laser deposition(PLD) technique using an Nd:YAG laser with a wavelength of 266nm. Before post-annealing treatment in the oxygen ambient, the experiment of the deposition of ZnO thin films has been performed for substrate temperatures in the range of $300{\sim}450^{\circ}C$ and flow rate of 100${\sim}$700 seem. In order to investigate the effect of post-annealing treatment of ZnO thin films, films have been annealed at various temperatures after deposition. After post-annealing treatment in the oxygen ambient, the structural properties of ZnO thin films were characterized by X-ray diffraction(XRD) and the optical properties of the ZnO were characterized by photoluminescence(PL).

  • PDF