• Title/Summary/Keyword: Proton Exchange Membrane

Search Result 528, Processing Time 0.03 seconds

Computational fluid dynamics analysis on the effect of inlet humidity for the performance of PEMFC with serpentine flow-fields (입구 가습량이 고분자 전해질 연료전지의 성능에 미치는 영향에 대한 CFD 해석연구)

  • Oh, Gyu-Hwan;Lee, Kyu-Jin;Nam, Jin-Hyun;Kim, Charn-Jung
    • Proceedings of the KSME Conference
    • /
    • 2008.11b
    • /
    • pp.2828-2833
    • /
    • 2008
  • Water management is one of many operating parameters, which influences the performance and stability of a proton exchange membrane fuel cell (PEMFC). Local humidity condition including liquid water saturation has profound impacts on the distributions of overpotentials, current density, and membrane water content. Computational fluid dynamics simulations were conducted to investigate the effect of the inlet humidity variation on the performance of a PEMFC of $9\;cm^2$ active cell area with serpentine flow fields. The results showed that the performance of the simulated PEMFC remained at an almost same level when the cathode inlet humidity was changed from 100% to 60%, while reaching its maximum at air humidity of 80%. However, further decrease in the cathode inlet humidity below 40% started to significantly deteriorate the performance of the PEMFC. The variations of overpotentials, membrane water content, etc. due to the change in the cathode inlet humidity were also discussed.

  • PDF

Performance of Fuel Cell with PEMFC Fabricated under Different Pressure (고분자 전해질 연료전지 성능에 미치는 MEA 가압제조 공정 조건의 영향)

  • Lee, Ki-Seong;Sim, Sooman;Kim, Dongmin
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.24 no.1
    • /
    • pp.70-75
    • /
    • 2013
  • It has fabricated membrane electrode assemblies (MEA) for proton exchange membrane fuel cell by hot-pressing method. The hot-pressing was used for the fabrication of MEA which is composed of commercial platinum electrode on carbon paper. The performance of MEA was studied with different fabrication conditions of temperature, pressure and torque. As the temperature increased, the performance of MEA was increased. and started to decrease l after arrived at the maximum performance of MEA. This is related with good contact between electrode and polymer electrolyte membrane at high temperature and microstructural change at much higher temperature. Similarly, as the pressure increased, the performance of the MEA increased up to highest values and start to decrease. According to the our results, the maximal performance of the MEA was at the temperature of $140^{\circ}C$ and the pressure of $1.5{\times}10^3$ kPa. The optimal torque to assemble the single stack was 3.2 N m.

Modeling of Water Transportation in Dynamic Load Proton Exchange Membrane (PEM) Fuel Cell Power Generator (동적부하 PEM 연료전지 발전기에 있어서의 수분전달 모델링)

  • Agung, Bakhtiar;Choi, Kwang-Hwan;Kim, Young-Bok
    • Journal of the Korean Solar Energy Society
    • /
    • v.31 no.2
    • /
    • pp.1-7
    • /
    • 2011
  • PEM 연료전지에 있어서 수분의 균형이 연료전지의 시스템 성능에 현저한 영향을 미친다. 그래서 수분 균형은 가장 중요한 요소 중의 일부가 되었으며, 이에 관한 연구가 광범위하게 이루어지고 있다. 적절한 수분 균형을 유지하기 위해서는 적당한 멤브레인 수화작용(membrane hydration)이 필요하며, 반대로 촉매층(catalyst layer)에서의 익수(water flooding)현상이 없어져야 한다. 따라서 이와 같은 동적 상태에서 PEM 연료전지 내의 수분 균형을 유지하기 위해서는, 고도의 동적 수분 조정 기술이 확보되어야 한다. 현재의 연구는 이러한 특성을 고려하여 PEM 연료전지에서 동적부하 상태에서의 수분 이동에 관한 일차원 해석 모델에 관한 것이다. 금번 모델링의 결과, 양극촉매층(CCL, cathode catalystlayer)에서의 수분 상태는 거의 포화 단계에 이르고 있음을 보여주고 있으며, 이 모델링은 연료전지가 작동되는 동안의 CCL에 나타나는 수분의 양상을 예측하는데 활용될 수 있다. 본 논문에서는 수분 이동 모델이 국제규격에 따라 다양한 수송기관이 가동될 때, 동적부하 상태에서 서로 다른 차이점을 발견하기 위한 시뮬레이션 결과에 초점이 맞추어져 있다. 이 모델링을 적용한 결과, 수분 포화도가 상태에 따라 상이하게 나타남을 알 수 있었고, 또한 정적 수분 조절 요소에 따라 최적 상태가 모든 동적 분포에 따라 달라짐을 알 수 있었다.

Purification of Biohydrogen Produced From Palm Oil Mill Effluent Fermentation for Fuel Cell Application

  • Rohani, Rosiah;Chung, Ying Tao;Mohamad, Izzati Nadia
    • Korean Chemical Engineering Research
    • /
    • v.57 no.4
    • /
    • pp.469-474
    • /
    • 2019
  • Fermentation of palm oil mill effluent (POME) produces biohydrogen in a mixture at a specific set condition. This research was conducted to purify the produced mixed biohydrogen via absorption and membrane techniques. Three different solvents, methyl ethanolamine (MEA), ammonia ($NH_3$) and potassium hydroxide (KOH) solutions, were used in absorption technique. The highest $H_2$ purity was found using 1M MEA solution with 5.0 ml/s feed mixed gas flow rate at 60 minutes absorption time. Meanwhile, the purified biohydrogen using a polysulfone membrane had the highest $H_2$ purity at 2~3 bar operating pressure. Upon testing with proton exchange membrane fuel cell (PEMFC), the highest current and power produced at 100% $H_2$ were 1.66 A and 8.1 W, while the lowest were produced at 50/50 vol% $H_2/CO_2$ (0.32 A and 0.49 W). These results proved that both purification techniques have significant potential for $H_2$ purification efficiency.

Numerical Simulation of the Oscillating Flow Effect in the Channel of Polymer Electrolyte Membrane Fuel Cell (왕복 유동을 통한 확산증대 효과가 연료전지 성능에 미치는 영향에 대한 수치해석)

  • Kim, Jongmin;Kang, Kyung-Sik
    • Journal of the Korea Safety Management & Science
    • /
    • v.20 no.4
    • /
    • pp.7-13
    • /
    • 2018
  • This study investigates the enhancement of the oxygen diffusion rate in the cathode channel of a proton exchange membrane fuel cell (PEMFC) by pure oscillating flow, which is the same as the mechanism of human breathe. Three-dimensional numerical simulation, which has the full model of the fuel cell including electrochemical reaction, ion and electronic conduction, mass transfer and thermal variation and so on, is performed to show the phenomena in the channel at the case of a steady state. This model could analysis the oscillating flow as a moving mesh calculation coupled with electrochemical reaction on the catalyst layer, however, it needs a lot of calculation time for each case. The two dimensional numerical simulation has carried on for the study of oscillating flow effect in the cathode channel of PEMFC in order to reduce the calculation time. This study shows the diffusion rate of the oxygen increased and the emission rate of the water vapor increased in the channel by oscillating flow without any forced flow.

Effect of Annealing Temperature on the Durability of PEMFC Polymer Membrane (PEMFC 고분자막의 어닐링 온도가 내구성에 미치는 영향)

  • Lee, Mihwa;Oh, Sohyeong;Park, Yujun;Yoo, Donggeun;Park, Kwonpil
    • Korean Chemical Engineering Research
    • /
    • v.60 no.1
    • /
    • pp.7-11
    • /
    • 2022
  • In the membrane forming process of a proton exchange membrane fuel cell (PEMFC), drying and annealing heat treatment processes are required for performance and durability. In this study, the optimal annealing temperature for improving the durability of the polymer membrane was studied. It was annealed in the temperature range of 125~175 ℃, and thermal stability and hydrogen permeability were measured as basic data of durability at each annealing temperature. The electrochemical durability was analyzed by Fenton reaction and open circuit voltage (OCV) holding. The annealing temperature of 165 ℃ was the optimal temperature in terms of thermal stability and hydrogen permeability. In the Fenton reaction, the fluorine emission rate of the membrane annealed at 165 ℃ was the lowest, and the lifespan of the membrane annealed at 165 ℃ was the longest in the OCV holding experiment, confirming that 165 ℃ was the optimal temperature for the durability of the polymer membrane.

Research of Characterization of Covalently Cross-linked SPEEK/Cs-Substituted MoPA/Ceria 1wt% Composite Membrane for Water Electrolysis (Cs 치환에 따른 수전해용 공유가교 SPEEK/Cs(n)-MoPA/Ceria 1%(n = 1~3) 복합막의 특성 연구)

  • Park, Daeyoung;Hwang, Sungha;Oh, Seunghee;Yoon, Daejin;Kang, Ansoo;Moon, Sangbong;Chung, Janghoon
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.25 no.1
    • /
    • pp.1-10
    • /
    • 2014
  • Ceria ($CeO_2$) was used to scavenge free radicals which attack the membrane in the polymer electrolyte membrane water electrolysis (PEMWE) circumstance and to increase the duration of the membrane. In order to improve the electrochemical, mechanical and electrocatalytic characteristics, engineering plastic of the sulfonated polyether ether ketone (SPEEK) as polymer matrix was prepared in the sulfonation reaction of polyether ether ketone (PEEK) and the organic-inorganic blended composite membranes were prepared by sol-gel casting method with loading the highly dispersed ceria and cesium-substituted phophomolybdic acid(Cs-MoPA) with cross-linking agent contents of 0.01mL. In conclusion, CL-SPEEK/$Cs_{(2.5)}$-MoPA/ceria(1%) membrane showed the optimum results such as 0.1095S/cm of proton conductivity at $80^{\circ}C$, 2.906meq./g-dry-membrane of ion exchange capacity and mechanical characteristics, and 49.73MPa of tensile strength which were better than Nafion 117 membrane.

Moisture Absorption Characteristics of Pt/Nafion Membrane for PEMFC Prepared by a Drying Process (건식법에 의해 제조한 PEMFC용 Pt/나피온 막의 흡습 특성)

  • Lee, Jae-Young;Lee, Hong-Ki
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.23 no.4
    • /
    • pp.310-315
    • /
    • 2012
  • A simple drying process was developed for the preparation of a Pt/Nafion self-humidifying membrane to be used for a proton-exchange membrane fuel cell (PEMFC). Platinum (II) bis (acetylacetonate), $Pt(acac)_2$ was sublimed, penetrated into the surface of a Nafion film and then reduced to Pt nanoparticles simultaneously without any support of a reducing agent in a glass reactor at $180^{\circ}C$ for 15 min. The process was carried out in $N_2$ atmosphere to prevent the oxidation of Pt nanoparticles at high temperature. The morphology and distribution of the Pt nanoparticles were observed by transmission electron microscopy (TEM) and energy dispersive spectroscopy (EDS), and we found that the average Pt particle size was ca. 3.7 nm, the penetration depth was ca. $17{\mu}m$. Almost all Pt nanoparticles were formed just beneath the surface and the number density decreased rapidly as the penetration depth increased. To estimate water absorption characteristics of the Nafion membranes, water uptake at an isothermal condition was measured by dynamic vapor sorption (DVS), and it was found that water uptake of the Pt/Nafion membrane was higher than that of the neat Nafion membrane.

Characterization of Polyester Cloth as an Alternative Separator to Nafion Membrane in Microbial Fuel Cells for Bioelectricity Generation Using Swine Wastewater

  • Kim, Taeyoung;Kang, Sukwon;Sung, Je Hoon;Kang, Youn Koo;Kim, Young Hwa;Jang, Jae Kyung
    • Journal of Microbiology and Biotechnology
    • /
    • v.26 no.12
    • /
    • pp.2171-2178
    • /
    • 2016
  • Polyester cloth (PC) was selected as a prospective inexpensive substitute separator material for microbial fuel cells (MFCs). PC was compared with a traditional Nafion proton exchange membrane (PEM) as an MFC separator by analyzing its physical and electrochemical properties. A single layer of PC showed higher mass transfer (e.g., for $O_2/H^+/ions$) than the Nafion PEM; in the case of oxygen mass transfer coefficient ($k_o$), a rate of $50.0{\times}10^{-5} cm{\cdot}s^{-1}$ was observed compared with a rate of $20.8{\times}10^{-5}cm/s$ in the Nafion PEM. Increased numbers of PC layers were found to reduce the oxygen mass transfer coefficient. In addition, the diffusion coefficient of oxygen ($D_O$) for PC ($2.0-3.3{\times}10^{-6}cm^2/s$) was lower than that of the Nafion PEM ($3.8{\times}10^{-6}cm^2/s$). The PC was found to have a low ohmic resistance ($0.29-0.38{\Omega}$) in the MFC, which was similar to that of Nafion PEM ($0.31{\Omega}$); this resulted in comparable maximum power density and maximum current density in MFCs with PC and those with Nafion PEMs. Moreover, a higher average current generation was observed in MFCs with PC ($104.3{\pm}15.3A/m^3$) compared with MFCs with Nafion PEM ($100.4{\pm}17.7A/m^3$), as well as showing insignificant degradation of the PC surface, during 177 days of use in swine wastewater. These results suggest that PC separators could serve as a low-cost alternative to Nafion PEMs for construction of cost-effective MFCs.

The Preparation and Characteristics of Covalently Cross-Linked SPEEK/Cs-TPA/Ceria Composite Membranes for Water Electrolysis (수전해용 공유가교 SPEEK/Cs-TPA/Ceria 복합막의 제조 및 특성 연구)

  • Song, Minah;Ha, Sungin;Park, Deayong;Ryu, Cheolhwi;Moon, Sangbong;Kang, Ansoo;Chung, Janghoon
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.23 no.5
    • /
    • pp.437-447
    • /
    • 2012
  • Ceria ($CeO_2$) was used to scavenge free radicals which attack the membrane in the polymer electrolyte membrane water electrolysis (PEMWE) circumstance and to increase the duration of the membrane. In order to improve the electrochemical, mechanical and electrocatalytic characteristics, engineering plastic of the sulfonated polyether ether ketone (SPEEK) as polymer matrix was prepared in the sulfonation reaction of polyether ether ketone (PEEK) and the organic-inorganic blended composite membranes were prepared by sol-gel casting method with loading the highly dispersed ceria and cesium-substituted tungstophosphoric acid (Cs-TPA) with cross-linking agent contents of 0.01 mL. In conclusion, CL-SPEEK/Cs-TPA/ceria (1%) membrane showed the optimum results such as 0.130 S/cm of proton conductivity at $80^{\circ}C$, 2.324 meq./g-dry-membrane of ion exchange capacity and mechanical characteristics, and 65.03 MPa of tensile strength which were better than Nafion 117 membrane.