• 제목/요약/키워드: Process tape

검색결과 319건 처리시간 0.022초

Algorithm of solving the problem of small elastoplastic deformation of fiber composites by FEM

  • Polatov, Askhad M.;Khaldjigitov, Abduvali A.;Ikramov, Akhmat M.
    • Advances in Computational Design
    • /
    • 제5권3호
    • /
    • pp.305-321
    • /
    • 2020
  • In this paper is presented the solution method for three-dimensional problem of transversely isotropic body's elastoplastic deformation by the finite element method (FEM). The process of problem solution consists of: determining the effective parameters of a transversely isotropic medium; construction of the finite element mesh of the body configuration, including the determination of the local minimum value of the tape width of non-zero coefficients of equation systems by using of front method; constructing of the stiffness matrix coefficients and load vector node components of the equation for an individual finite element's state according to the theory of small elastoplastic deformations for a transversely isotropic medium; the formation of a resolving symmetric-tape system of equations by summing of all state equations coefficients summing of all finite elements; solution of the system of symmetric-tape equations systems by means of the square root method; calculation of the body's elastoplastic stress-strain state by performing the iterative process of the initial stress method. For each problem solution stage, effective computational algorithms have been developed that reduce computational operations number by modifying existing solution methods and taking into account the matrix coefficients structure. As an example it is given, the problem solution of fibrous composite straining in the form of a rectangle with a system of circular holes.

의료용 폴리우레탄 Pre-polymer의 중합공정 최적화 (Process Optimization of Polyurethane Pre-polymer for Medical Application)

  • 허광태;구양;하만경;곽재섭
    • 한국금형공학회:학술대회논문집
    • /
    • 한국금형공학회 2008년도 하계 학술대회
    • /
    • pp.203-208
    • /
    • 2008
  • Recently, the modern society in development and industrial growth is investing a lot of time and much effort to improvement and environment of life quality. Thus, the casting tape which uses environmentally friendly and human body friendly water hardening process Polymer is rapidly substituted for the gypsum cast product which has been plentifully used in medical treatment. Until currently, prior researches have a tendency to focusing the analysis about chemical creation expense and reaction quality rather than the issue about optimization of the process for this polymerization. In the polymerization process which has been accomplished with actual same chemical creation expense, there has been a problem which is the possibility of getting a different result. This is because the optimization of respectively control factors is not accomplished which affect at polymerization process. Therefore, this research sees the chemical qualities of casting tape Polymer, consequently selects the polymerization process which is suitable. And, by using a experimental design, this research will evaluate the affects which the respective factors have on remaining NCO and viscosity. futhermore, this research will carry out the process optimization which can get the above results.

  • PDF

수계 테이프 케스팅 법에 의한 봉상 γ-LiAlO2 입자 강화 MCFC 매트릭스 제조 공정의 최적화 (Optimization of Rod-shaped γ-LiAlO2 Particle Reinforced MCFC Matrices by Aqueous Tape Casting)

  • 최현종;신미영;현상훈;임희천
    • 한국세라믹학회지
    • /
    • 제46권3호
    • /
    • pp.282-287
    • /
    • 2009
  • Rod-shaped particle reinforced $LiAlO_2$ matrices for MCFC were fabricated by an aqueous tape-casting technique. The hydrolysis reaction and agglomeration of $\gamma-LiAlO_2$ particles in aqueous slurries were inhibited by additions of $LiOH{\cdot}H_2O$ and glycerin to the aqueous $\gamma-LiAlO_2$ slurry. The tape-casting, performed using the aqueous slurry containing protein albumin, was fast and led to an effective drying at casting temperature range of $60{\sim}65^{\circ}C$. The strength of the particle reinforced matrix was improved about 4 times compared to that of matrix without reinforcement. Pore size distribution ($0.1{\sim}0.4{\mu}m$) and porosity ($50{\sim}60%$) of the reinforced matrices were determined to be appropriate for the MCFC matrix. The aqueous tape casting process is not only environmental-friendly but also efficient for fabricating MCFC matrices compared to non-aqueous tape casting.

$Nb_3Sn$ 복합초전도 테이프의 미시적 변형거동 특성평가를 위한 음향방출기법 적용에 관한 연구 (A Study on Microscopic Deformation Behaviors of $Nb_3Sn$ Superconducting Composite Tape using Acoustic Emission Technique)

  • 이민래;이준현
    • Composites Research
    • /
    • 제12권6호
    • /
    • pp.22-30
    • /
    • 1999
  • $Nb_3Sn$ 복합초전도 테이프는 금속간 화합물로서 다른 초전도 재료에 비하여 임계밀도가 높아 MRI등에 널리 이용되고 있다. 한편 $Nb_3Sn$층은 화합물이므로 bending이나 winding등의 코아 제작시 테이프 도체에 응력이 작용하면 화합물층에 취성으로 인한 크랙이 발생하여 부분적으로 파단이 일어나 임계전류 특성이 열화하며 무응력 상태에 비하여 크게 저하된다. 따라서 이와 같은 $Nb_3Sn$복합초전도 테이프의 실질적인 적용을 위해서는 선재의 제조과정 뿐만 아니라 가동 중에 기계적 응력에 대한$Nb_3Sn$복합 초전도 테이프의 미시적 거동 특성을 필히 이해하여야 할 필요가 있다. 본 연구에서는 음향방출기법(Acoustic Emission)을 이용하여 $Nb_3Sn$ 복합초전도 테이프에 대해서 일정변형속도(constant extension rate)제어로 인장하중이 작용할 경우 발생하는 AE 신호특성과 이에 대응하는 각 화합물층의 미시적 변형거동 특성과의 상관관계를 분석하였다.

  • PDF

분말의 함량 및 적층공정이 Tape Casting법으로 제조된 Ni-Zn Ferrite의 물성에 미치는 영향 (Effect of Solid Loading and Lamination Process on the Properties of Ni-Zn Ferrite Made by Tape Casting Method)

  • 이창호;김경용;이창호;김경용
    • 한국세라믹학회지
    • /
    • 제31권6호
    • /
    • pp.595-600
    • /
    • 1994
  • Ni0.3Zn0.7Fe2O4 ferrite specimens were fabricated by dry pressing and tape casting method. The properties of each specimen were measured and compared. In order to design and manufacture the chip devices effectively, one important criterion can be that the sintered density of the laminated body should approach close to that of the dry pressed body which is regarded as standard. This requirement could be satisfied by controlling the solid loading of the ferrite sheet, lamination temperature and pressure. Using the optimum conditions (solid loading 55 wt%, lamination temperature 6$0^{\circ}C$, lamination pressure 400 kg/$\textrm{cm}^2$, sintered at 125$0^{\circ}C$ 2h) a sintered ferrite, with the density of 5.18g/㎤ and permeability of 1390 at 0.5 MHz, were obtained.

  • PDF

분무 열분해에 의한 미세 BSCCO 전구체 분말의 합성 (Synethisis of fine BSCCO precursor powder by spray pyrolysis)

  • 김성환;유재무;고재웅;김영국;박성창
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 추계학술대회 논문집
    • /
    • pp.99-102
    • /
    • 2003
  • Many researches on synthesis process for BSCCO precursor powders have been developed for high J$_{c}$ BSCCO-2223/Ag tape. Spray pyrolysis method for fabrication of precursor powder has many advantages, such as high purity, fine particle size of BSCCO precursor powder. Fine, spherical powders were prepared by ultrasonic spray pyrolysis from the aqueous solution of metal nitrates. BSCCO precursor powders were synthesized with 0.1 M concentration and heat treatment conditions. Average particle size for spray pyrolysis powders was 1.5 ~ 3 ${\mu}{\textrm}{m}$. BSCCO -2223/Ag tape was prepared by PIT method and followed by various sintering conditions. The critical current density of BSCCO-2223/Ag tape sintered in low oxygen partial pressure was ~ 23 kAcm$^{-2}$.

  • PDF

Rheology of Slurries and Effects of Polymer Volume Ratio in Aqueous PZT Tape Casting

  • Yoon, Seok-Jin;Shin, Hyo-Soon;Lee, Dong-Kyun;Kang, Chong-Yun;Park, Ji-Won;Kim, Hyun-Jai
    • The Korean Journal of Ceramics
    • /
    • 제7권1호
    • /
    • pp.16-19
    • /
    • 2001
  • For the fast dry of the aqueous tape, the process which water was reaplaced by organic solvent was proposed. Socalled, it was the solvent washing dry. Three organic solvents (methanol, ethanol and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol and acetone were available organic solvents for this method. The tapes washed in methanol, ethanol and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not found any more, The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated.

  • PDF

Investigation of $I_c$ Degradation Behavior in Bent Bi-2223 Tapes under Pressurized Liquid Nitrogen using a $\rho-shaped$ Sample Holder

  • Shin Hyung-Seop;Dizon John Ryan C.;Choi Ho-Yeon;Ha Dong-Woo;Oh Sang-Soo
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제7권4호
    • /
    • pp.4-9
    • /
    • 2005
  • The degradation behavior of the critical current $(I_c)$ of Bi-2223 superconducting tapes under pressurized liquid nitrogen were investigated using a newly developed p-shaped sample holder which gives a series of bending strains to a sample. Three kinds of commercially available multi-filamentary Bi-2223 superconducting tapes were used. At atmospheric pressure, the Ie degradation behavior depended on the manufacturing process undergone by each tape. The tapes externally reinforced or densified by over pressure showed better bending strain tolerance than the Ag alloy-sheathed Bi-2223 tape. But these tapes showed a significant $I_c$ degradation when pressurized to 1 MPa in liquid nitrogen. For all samples, after depressurization to atmospheric pressure from 1 MPa, the Ie was completely recovered to its initial values at atmospheric pressure. When the samples were subjected to a thermal cycle wherein the tape was warmed up to room temperature after being depressurized from 1 MPa, it was found that the larger degradation of $I_c$ occurred at the regions where significant ballooning occurred, such as $0\%\;and\;0.2\%$. However, an improved ballooning damage tolerance was observed in the highly-densified tape.

Solvent Washing Dry Method for Aqueous Tape Casting

  • Yoon, Seok-Jin;Shin, Hyo-Soon;Park, Ji-Won;Kang, Chong-Yun;Kim, Tae-Song;Kim, Hyun-Jai
    • The Korean Journal of Ceramics
    • /
    • 제7권2호
    • /
    • pp.55-57
    • /
    • 2001
  • For the fast dry of the aqueous tape, the process which water was replaced by organic solvent was proposed. Socalled, it was the solvent washing dry. Three organic solvents (methanol, ethanol and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol and acetone were available organic solvents for this method. The tapes washed in methanol, ethanol and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not found any more. The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated.

  • PDF

BSCCO(2223)/Ag 다심 초전도선재의 접합공정 개발 (Development of joining process of the BSCCO(2223)/Ag multi-filament tapes)

  • 김규태;김정호;안혁;장석헌;주진호
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 학술대회 논문집
    • /
    • pp.120-122
    • /
    • 2003
  • We jointed Bi(Pb)-Sr-Ca-Cu-O multifilament tapes and evaluated their electrical properties. In order to improve connectivity of multifilarnents, single-filament tape was inserted between two multifilament tapes or multifilament was stepped by mechanical remove. The critical current ratio (CCR) and n-value of the jointed tapes were evaluated as a function of uniaxial pressure. It was observed that CCR and n-value were 24.8-29.0% and 2.5-2.8 for lap-jointed tape. On the other hand, the corresponding values were improved to 51.8-61.9% and 2.9-5.1 for three stepped jointed tape, and 63.4-67.9% and 3.4-4.2 for double MSM lap-jointed tape, respectively. These improvements are to be due to better interconnection between filaments of two tapes.