• 제목/요약/키워드: Positive Temperature Coefficient(PTCR)

검색결과 70건 처리시간 0.024초

High $T_c$ Pb-free (1-x)$BaTiO_3-x(Bi_{1/2}Na_{1/2})TiO_3$ 세라믹의 미세구조와 PTCR 특성 (Microstructure and PTCR characteristic of high $T_c$ lead-free ((1-x)$BaTiO_3-x(Bi_{1/2}Na_{1/2})TiO_3$ characteristic)

  • 김철민;조용수;정영훈;이영진;이미재;백종후;이우영;김대준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.32-32
    • /
    • 2008
  • Microstructure and positive temperature coefficient of resistivity (PTCR) characteristics of $0.9BaTiO_3-0.1(Bi_{0.5}Na_{0.5})TiO_3$ [BaBiNT] ceramics doped with $Nb_2O_5$ were investigated in order to develop the Pb-free high Curie temperature ($T_c$)(>$160^{\circ}C$) PTC thermistor. The BaBiNT ceramics showed a tetragonal perovskite structure, irrespective of the added amount of $Nb_2O_5$. They also have a homogeneous microstructure. The resistivity of BaBiNT ceramics was gradually decreased by doping $Nb_2O_5$, which might be due to $Nb^{+5}$ ions substituting for $Ti^{+4}$ sites. The PTCR characteristics of BaBiNT ceramics appeared when the amount of doped $Nb_2O_5$ exceeded 0.0025mol%. Moreover, the abrupt grain growth was observed for the 0.03mol% $Nb_2O_5$added BaBiNT ceramics. It showed an especially high $T_c$ of approximately $172^{\circ}C$ and good PTCR characteristics of a high $\rho_{max}/\rho_{min}$ ratio ($2.96\times10^3$), a high resistivity temperature factor (11.40/$^{\circ}C$) along with a relatively low resistivity ($3.5\times10^4\Omega{\cdot}cm$).

  • PDF

정저항요업체의 제조와 전기적 성질 (Preparation and Electrical Properties of PTCR Ceramic Materials)

  • 정형진;윤상옥
    • 한국세라믹학회지
    • /
    • 제22권2호
    • /
    • pp.11-16
    • /
    • 1985
  • The semiconducting ceramics having positive temperature coefficient of resistivity in he family of 0.25mol% $Sb_2O_3$ doped barium titanates were prepared with AST ($4Al_2O_3$.$9SiO_2$.$3TiO_2$) and $MnO_2$ as additives and these electrical properties were investigated. The PTCR characteristic in these ceramic materials was improved by the addition of AST and $MnO_2$ because the addition of AST decreased the room temperature resistivity and controlled grin size due to the formation of a liquid phase during sintering and the addition of $MnO_2$ improved by forming acceptor level on the intergranular layer. On dependence on the switching time as switching temperature was increased the initial power and switching time increased.

  • PDF

고온가압소결한 $\alpha-SiC-ZrB_2$ 복합체의 전기전도기구 (Electrical Conductive Mechanism of Hot-pressed $\alpha-SiC-ZrB_2$ Composites)

  • 신용덕;주진영;권주성
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제48권2호
    • /
    • pp.104-108
    • /
    • 1999
  • The electrical conductive mechanism and temperature dependence of electrical resistivity of $\alpha-SiC-ZrB_2$ composites with $ZrB_2$ contents were investigated. The electrical resistivity of hot-pressed composites was measured by the Pauw method form $25^{\circ} to 700^{\circ}C$. The electrical resistivity of the composites follow the electrical conduction model for a homogeneous mixture of two kind of particles with different conductivity. Also, the electrical resistivity versus temperature curves indicate the formation of local chains of $ZrB_2$ particles. In case of $\alpha-SiC-ZrB_2$ composites containing above 39vol.% $ZrB_2$ showed positive temperature coefficient resistance(PTCR), whereas the electrical resistivity of $\alpha-SiC-21vol.% ZrB_2$ showed negative temperature coefficient resistance(NTCR).

  • PDF

$Nb_2O_5$가 도핑된 (1-x)$BaTiO_3$ - $x(Bi_{0.5}K_{0.5})TiO_3$ 무연 세라믹스의 PTCR 효과 (The PTCR Effect in Lead-free (1-x)$BaTiO_3$ - $x(Bi_{0.5}K_{0.5})TiO_3$ Ceramics Doped with $Nb_2O_5$)

  • 정영훈;박용준;이영진;백종후;이우영;김대준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.52-52
    • /
    • 2008
  • The positive temperature coefficient of resistivity (PTCR) effect in (1-x)$BaTiO_3$ - $x(Bi_{0.5}K_{0.5})TiO_3$ doped with $Nb_2O_5$ was investigated. $(Bi_{1/2}K_{1/2})TiO_3$ (BKT) is more environment-friendly than $PbTiO_3$ in order to use in PTC thermistors. The incorporation of 1 mol% BKT to $BaTiO_3$ increased the Curie temperature (Tc) to $148^{\circ}C$. Doping of $Nb_2O_5$ to $Ba_{0.99}(Bi_{0.5}K_{0.5})_{0.01}TiO_3$ (BaBKT) ceramic has enhanced its PTCR effects. For the sample containing 0.025 mol% $Nb_2O_5$, it showed good PTCR properties; low resistivity at room temperature (${\rho}_r$) of 30 $\Omega{\cdot}cm$, a high PTCR intensity of approximately $3.3\times10^3$, implying the ratio of maximum resistivity to minimum resistivity (${\rho}_{max}/{\rho}_{min}$) in the measured temperature range, and a large resistivity temperature factor (a) of 13.7%/$^{\circ}C$ along with a high Curie temperature (Tc) of $167^{\circ}C$. In addition, the cooling rate of the samples during the sintering process had an influence on their PTCR behavior. All the samples showed the best ${\rho}_{max}/{\rho}_{min}$ ratio when they have cooled down at a rate of $600^{\circ}C$/min.

  • PDF

Ca 첨가가 PTCR 써미스터의 전기적 특성에 미치는 영향 (The Effects of Ca Addition on Electrical Properties of PTCR Thermistor)

  • 김병수;김종택;김철수;김용혁;이덕출
    • 한국전기전자재료학회논문지
    • /
    • 제11권2호
    • /
    • pp.121-127
    • /
    • 1998
  • In this paper, to develop PTCR(Positive Temperature Coefficient of Resistance) thermistor with high withstanding voltage, Ca were added to. the compositions of $(Ba_{0.9165-X}-Sr_{0.08}-Ca_X-Y_{0.0035})TiO_3+MnO_2$ 0.02wt%+$SiO_2$ 0.5wt%. the effects of Ca additions were researched according the increasing of Ca from 0[mol%] to 20[mol%], and the electrical properties were investigated. As increasing Ca additions from 0[mol%] to 20[mol%], the grain size of the specimens was reduced from 11.1[${\mu}m$] to 6.15[${\mu}m$], and also the sintered density was reduced from 5.43[$g/cm^3$] to 5.05[$g/cm^3$] and their the breakdown voltages were increased from 163[V/mm] to 232[V/mm]. It is shown that the breakdown voltage was increased with amount of Ca additions.

  • PDF

무연 BaTiO3-(Bi0.5K0.5)TiO3 PTCR 세라믹과 PTCR 특성에 미치는 Nb2O5의 효과 (Lead-free BaTiO3-(Bi0.5K0.5)TiO3 PTCR Ceramics and Effects of Nb2O5 on Its PTCR Characteristics)

  • 정영훈;박용준;이미재;이영진;백종후;최진수;이우영
    • 한국재료학회지
    • /
    • 제18권9호
    • /
    • pp.475-481
    • /
    • 2008
  • Positive temperature coefficient of resistivity (PTCR) characteristics of (1-x)$BaTiO_3-x(Bi_{0.5}K_{0.5})TiO_3$ ceramics doped with $Nb_2O_5$ were investigated in order to develop the Pb-free PTC thermistor available at high temperatures of > $120^{\circ}C$. The PTCR characteristics appearing in the ($B_{i0.5}K_{i0.5})TiO_3$ (< 5 mol%) incorporated $BaTiO_3$ ceramics, which might be mainly due to $Bi^{+3}$ ions substituting for $Ba^{+2}$ sites. The 0.99$BaTiO_3-0.01(Bi_{0.5}K_{0.5})TiO_3$ ceramics showed good PTCR characteristics of a low resistivity at room temperature (${\rho}_r$) of $31{\Omega}{\cdot}cm$ a high ${\rho}_{max}/{\rho}_{min}$ ratio of $5.38{\times}10^3$, and a high resistivity temperature factor (${\alpha}$) of $17.8%/^{\circ}C$. The addition of $Nb_2O_5$ to 0.99$BaTiO_3-0.01(Bi_{0.5}K_{0.5})TiO_3$ ceramics further improved the PTCR characteristics. Especially, 0.025 mol% $Nb_2O_5$ doped 0.99$BaTiO_3-0.01(Bi_{0.5}K_{0.5})TiO_3$ ceramics exhibited a significantly increased ${\rho}_{max}/{\rho}_{min}$ ratio of $8.7{\times}10^3$ and a high ${\alpha}$ of $18.6%/^{\circ}C$, along with a high $T_c$ of $148^{\circ}C$ despite a slightly increased ${\rho}_r$ of $31{\Omega}{\cdot}cm$.

The Development of an Electroconductive SiC-ZrB2 Ceramic Heater through Spark Plasma Sintering

  • Ju, Jin-Young;Kim, Cheol-Ho;Kim, Jae-Jin;Lee, Jung-Hoon;Lee, Hee-Seung;Shin, Yong-Deok
    • Journal of Electrical Engineering and Technology
    • /
    • 제4권4호
    • /
    • pp.538-545
    • /
    • 2009
  • The SiC-$ZrB_2$ composites were fabricated by combining 30, 35, 40 and 45vol.% of Zirconium Diboride (hereafter, $ZrB_2$) powders with Silicon Carbide (hereafter, SiC) matrix. The SiC-$ZrB_2$ composites, the sintered compacts, were produced through Spark Plasma Sintering (hereafter, SPS), and its physical, electrical, and mechanical properties were examined. Also, the thermal image analysis of the SiC-$ZrB_2$ composites was examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed via X-Ray Diffractometer (hereafter, XRD) analysis. The relative density of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$, and SiC+45vol.%$ZrB_2$ composites were 88.64%, 76.80%, 79.09% and 88.12%, respectively. The XRD phase analysis of the sintered compacts demonstrated high phase of SiC and $ZrB_2$ but low phase of $ZrO_2$. Among the SiC-$ZrB_2$ composites, the SiC+35vol.%$ZrB_2$ composite had the lowest flexural strength, 148.49MPa, and the SiC+40vol.%$ZrB_2$ composite had the highest flexural strength, 204.85MPa, at room temperature. The electrical resistivities of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$ and SiC+45vol.%$ZrB_2$ composites were $6.74\times10^{-4}$, $4.56\times10^{-3}$, $1.92\times10^{-3}$, and $4.95\times10^{-3}\Omega{\cdot}cm$ at room temperature, respectively. The electrical resistivities of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$ SiC+40vol.%$ZrB_2$ and SiC+45[vol.%]$ZrB_2$ composites had Positive Temperature Coefficient Resistance (hereafter, PTCR) in the temperature range from $25^{\circ}C$ to $500^{\circ}C$. The V-I characteristics of the SiC+40vol.%$ZrB_2$ composite had a linear shape. Therefore, it is considered that the SiC+40vol.%$ZrB_2$ composite containing the most outstanding mechanical properties, high resistance temperature coefficient and PTCR characteristics among the sintered compacts can be used as an energy friendly ceramic heater or electrode material through SPS.

PTCR Characteristics of BaTiO$_3$Thin Films made by rf/dc Magnetron Sputter Technique

  • Song, Min-Jong;So, Byung-Moom;Kim, Tae-Wan
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권2호
    • /
    • pp.28-31
    • /
    • 2000
  • BaTiO$_3$cerameic thin films doped with Mn were manufactured by rf/dc magnetron sputter technique. We have investigated crystal structure, surface morphology and PRCR(positive-temperature coefficient of resistance) characteristics of the specimen depending on second heat-treatment temperature. Second heat treatment of the specimen were performed in the temperature range of 400 to 1350$\^{C}$ X-ray diffraction patterns of BaTiO$_3$ thin films show that the specimen heat treated below 600$\^{C}$ is an amorphous phase and the one heat treated above 1100$\^{C}$ forms a poly-crystallization . In this specimen heat-treated at 1300$\^{C}$, a lattice constant ratio(c/a) was 1.188. Scanning electron microscope(SEM) image of BaTiO$_3$ thin films of the specimen heat treated in between 900 and 1100$\^{C}$ shows a grain growth. At 1100$\^{C}$, the specimen stops grain-growing and becomes a poly-crystallization . A resistivity-temperature characteristics of the specimen depends on the doping concentrations of Mn. A resistivity ratio between the value at room temperature and the one above Curie temperature was 10$^4$ for pure BaTiO$_3$ thin films and 10$\^$5/ fo BaTiO$_3$ : additive 0.127mol% MnO

  • PDF

$\beta-SiC+39vol.%TiB_2$ 복합체의 전기저항률 (Electrical Resistivity of the $\beta-SiC+39vol.%TiB_2$ Composites)

  • 박미림;황철;신용덕;이동윤
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 연구회
    • /
    • pp.15-18
    • /
    • 2001
  • The composites were fabricated 61 vol% $\beta$-SiC and $39vol%TiB_2$ powders with the liquid forming additives of 8, 12, 16wt% $Al_2O_3+Y_2O_3$ by hot pressing at $1730^{\circ}C$ and subsequent pressed annealing and pressureless annealing at $1750^{\circ}C$ for 4 hours to form YAG. The result of phase analysis of composites by XRD revealed $\alpha$-SiC(6H), $TiB_2$, and YAG($Al_5Y_3O_{12}$) crystal phase. The relative density of composites were increased with increasing $Al_2O_3+Y_2O_3$ contents. The fracture toughness showed the highest value of $7.77MPa{\cdot}m^{1/2}$ for composites added with 12wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity and the resistance temperature coefficient showed the lowest of $7.3{\times}10^{-4}{\Omega}{\cdot}cm$ and $3.8{\times}10^{-3}/^{\circ}C$, respectively, for composite added with 12wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) in the temperature range of $25^{\circ}C$ to $700^{\circ}C$.

  • PDF

SPS on/off Pulse Time 조건에 따른 SiC-$ZrB_2$ 복합체 특성 (Properties of a SiC-$ZrB_2$ Composite by condition of SPS on/off Pulse Time)

  • 신용덕;주진영;이희승;박진형;김인용;김철호;이정훈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.314-314
    • /
    • 2010
  • The SiC-$ZrB_2$ composites were fabricated by combining 40vol.% of Zirconium Diboride(hereafter, $ZrB_2$) powders with Silicon Carbide(hereafter, SiC) matrix. TheSiC+40vol.%$ZrB_2$ composites were manufactured through Spark Plasma Sintering(hereafter, SPS) under argon atmosphere, uniaxial pressure of 50MPa, heating rate of $100^{\circ}C$/min, sintering temperature of $1,500^{\circ}C$ and holding time of 5min. But one on/off pulse sequence(one pulse time: 2.78ms) is 10:9(hereafter, SZ10), and the other is 48:8(hereafter, SZ48). The physical and mechanical properties of the SZ12 and SZ48 were examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed via X-Ray Diffraction(hereafter, XRD) analysis. The apparent porosity of the SZ10 and SZ48 composites were 9.7455 and 12.2766%, respectively. The SZ10 composite, 593.87MPa, had higher flexural strength than the SZ48 composite, 324.78MPa, at room temperature. The electrical properties of the SiC-$ZrB_2$ composites had Positive Temperature Coefficient Resistance(hereafter, PTCR).

  • PDF