• Title/Summary/Keyword: Porous Mo

Search Result 71, Processing Time 0.026 seconds

Fabrication of Porous MoSi2 material for Heating Element through Self-propagating High Temperature Synthesis Process (연소합성법에 의한 발열성 다공질 MoSi2계 재료의 제조)

  • Song, In-Hyuck;Yun, Jung-Yeul;Kim, Hai-Doo
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.1
    • /
    • pp.62-68
    • /
    • 2004
  • In this study, SHS process has been employed to fabricate porous $MoSi_2$ material with electric-resistive heating capability through the control of pore size. The preform for SHS reaction was consisted of molybdenum powder with different sizes and silicon powder with different contained quantity. The size of the $MoSi_2$ particles thus formed was determined by the generated heat of combustion, not by the size of molybdenum powder. However, the pore size of $MoSi_2$ composite was proportional to the particle size of molybdenum powder. that is the coarser the molybdenum powder used, the larget the formed pore size. Based on these results, the porous $MoSi_2$ composite could be fabricated with a desired pore size. By orienting the porous molybdenum disilicide-based material in the form of pore size gradient, porous materials used for filters with improved dirt-holding capacity can be manufactured.

Fabrication of High Porous Ceramic with Mullite Whisker from Fly Ash (석탄재를 이용한 뮬라이트 휘스커 고다공성 세라믹 제작)

  • Shin, Cheol;Hwang, Kwang-Taek;Kim, Ung-Soo;Han, Kyu-Sung;Choi, Jung-Hoon;Kim, Jin-Ho
    • Korean Journal of Materials Research
    • /
    • v.32 no.5
    • /
    • pp.258-263
    • /
    • 2022
  • Porous ceramics have the advantages of low density, low thermal conductivity, and excellent mechanical properties. Among porous ceramic manufacturing methods, the replica template method allows the easy manufacturing of porous filters with the highest porosity and pores of the desired size, but it also has the disadvantage that the resulting filters have low mechanical strength. To overcome this shortcoming, mullite (3Al2O3·2SiO2) whiskers, which have excellent thermal stability and high mechanical strength, were introduced in porous ceramic structure. The mullite whiskers were synthesized using a composition of Al2O3, flyash and MoO3. The morphologies and crystal structures of the mullite whiskers with MoO3 contents were investigated in detail. When the porous ceramic with mullite whiskers was fabricated using 20 wt% MoO3 catalyst the most uniform microstructure was obtained, and the mullite whiskers showed the highest aspect ratio of 47.03. The porosity and compressive strength of the fabricated porous ceramic were 82.12 % and 0.83 MPa, respectively.

Fabrication of Porous Mo by Freeze-Drying and Hydrogen Reduction of MoO3/Camphene Slurry (MoO3/camphene 슬러리의 동결건조 및 수소환원에 의한 Mo 다공체 제조)

  • Lee, Wonsuk;Oh, Sung-Tag
    • Journal of Powder Materials
    • /
    • v.19 no.6
    • /
    • pp.446-450
    • /
    • 2012
  • In order to fabricate the porous Mo with controlled pore characteristics, unique processing by using $MoO_3$ powder as the source and camphene as the sublimable material is introduced. Camphene-based 15 vol% $MoO_3$ slurries, prepared by milling at $50^{\circ}C$ with a small amount of dispersant, were frozen at $-25^{\circ}C$. Pores were generated subsequently by sublimation of the camphene during drying in air for 48 h. The green body was hydrogen-reduced at $750^{\circ}C$, and sintered at $1000-1100^{\circ}C$ for 1 h. After heat treatment in hydrogen atmosphere, $MoO_3$ powders were completely converted to metallic W without any reaction phases. The sintered samples showed large pores with the size of about $150{\mu}m$ which were aligned parallel to the camphene growth direction. Also, the internal wall of large pores and near bottom part of specimen had relatively small pores due to the difference in the camphene growth rate during freezing process. The size of small pores was decreased with increase in sintering temperature, while that of large pores was unchanged. The results are strongly suggested that the porous metal with required pore characteristics can be successfully fabricated by freeze-drying process using metal oxide powders.

Fabrication of Porous Mo-Cu by Freeze Drying and Hydrogen Reduction of Metal Oxide Powders (금속산화물 분말의 동결건조 및 수소환원에 의한 Mo-Cu 다공체 제조)

  • Kang, Hyunji;Han, Ju-Yeon;Oh, Sung-Tag
    • Journal of Powder Materials
    • /
    • v.26 no.1
    • /
    • pp.1-5
    • /
    • 2019
  • In this study, porous Mo-5 wt% Cu with unidirectionally aligned pores is prepared by freeze drying of camphene slurry with $MoO_3-CuO$ powders. Unidirectional freezing of camphene slurry with dispersion stability is conducted at $-25^{\circ}C$, and pores in the frozen specimens are generated by sublimation of the camphene crystals. The green bodies are hydrogen-reduced at $750^{\circ}C$ and sintered at $1000^{\circ}C$ for 1 h. X-ray diffraction analysis reveals that $MoO_3-CuO$ composite powders are completely converted to a Mo-and-Cu phase without any reaction phases by hydrogen reduction. The sintered bodies with the Mo-Cu phase show large and aligned parallel pores to the camphene growth direction as well as small pores in the internal walls of large pores. The pore size and porosity decrease with increasing composite powder content from 5 to 10 vol%. The change of pore characteristics is explained by the degree of powder rearrangement in slurry and the accumulation behavior of powders in the interdendritic spaces of solidified camphene.

Effect of Alumina on the Ion-Exchange Capacity of Porous Glasses (다공질유리의 이온교환성에 미치는 알루미나의 영향)

  • 김병호;이덕열;김성길
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.3
    • /
    • pp.251-260
    • /
    • 1988
  • Ion-exchange porous glasses were prepared by heat treatment and subsequently hydro thermalor acid leaching treatment $10Li_2O$.$(90-x)B_2O_3$.$xSiO_2$ base glasses containing various amount of $Al_2O_3$ or $MoO_3$. It was investigated how the phase separation and the cation exchange capacity(CEC) were affected by the addition of $Al_2O_3$ or $MoO_3$. The optimum condition of phase separation in these glasses was about 48$0^{\circ}C$ for 10 hrs. The degree of phase separation was rapidly suppressed by the addition of $Al_2O_3$ up to 10 mol% and thereafter suppression effect was decreased. The maximum value of CEC, about 252meq/100g, was observed with the $1OLi_2O$.$45B_2O_3$.$45SiO_2+7.5Al_2O_3$ porous glass prepared by hydrothermal treatment and its mean pore radius was about 16.3A. The addition of $MoO_3$ accelerated phase separation and leaching rate. Looking at the remakable increment of pore diameter and pore volume of these porous glasses by the addition of $MoO_3$, the effect of $MoO_3$ may be ascribed to the lowering of silica concentration in the borate phase and to the forming of water-soluble complex with silica during the leaching treatment.

  • PDF

Freeze Drying for Porous Mo with Sublimable Vehicles of Eutectic System (공정 계 동결제 슬러리의 동결건조 공정에 의한 Mo 다공체 제조)

  • Lee, Gyu-Tae;Seo, Han Gil;Suk, Myung-Jin;Oh, Sung-Tag
    • Journal of Powder Materials
    • /
    • v.20 no.4
    • /
    • pp.253-257
    • /
    • 2013
  • Freeze drying for porous Mo was accomplished by using $MoO_3$ powder as the source and camphor-naphthalene eutectic system as the sublimable material. Eutectic composition of camphor-naphthalene slurries with the initial $MoO_3$ content of 5 vol%, prepared by milling at $55^{\circ}C$ with a small amount of oligomeric dispersant, was frozen at $-25^{\circ}C$. The addition of dispersant showed improvement of dispersion stability in slurries. Pores were generated subsequently by sublimation of the camphor-naphthalene during drying in air for 48 h. To convert the $MoO_3$ to metallic Mo, the green body was hydrogen-reduced at $750^{\circ}C$, and sintered at $1100^{\circ}C$ for 2 h. The sintered samples, frozen by heated Teflon cylinder, showed large pores with the size of about 40 ${\mu}m$ which were aligned parallel to the sublimable vehicles growth direction. The formation of unidirectionally aligned pores is explained by the rejection and accumulation of solid particles in the serrated solid-liquid interface.

Oxidation Behavior of $SiC/MoSi_2$ Composites Prepared by Reaction Sintering Method (반응소결에 의하여 제조된 $SiC/MoSi_2$ 복합체의 산화 거동)

  • 양준환;한인섭;우상국;서동수
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1588-1598
    • /
    • 1994
  • The SiC/MoSi2 composite materials were fabricated by infiltrating the mixture of molybdenum disilicide and metal silicon(MoSi2+Si=100) to a porous compact of silicon carbide and graphite under the vacuum atmosphere of 10-1 torr. The specimen were oxidized in dry air under 1 atm at 130$0^{\circ}C$~150$0^{\circ}C$ for 240 hours. The oxidation behavior was evaluated by the weight gain and loss per unit area of the oxidized samples. Also, SEM and XRD analysis of the oxidized surface of the samples were carried out. With increasing the MoSi2 content and oxidation temperature, the passive oxidation was found. The trend of weight gain of all samples was followed the parabolic rate law with the formation of a protective layer of cristobalite on the surface.

  • PDF