Pore Structure Modification and Characterization of Porous Cordierite with Chemical Vapor Infiltration (CVI) SiC Whisker (화학증착 탄화규소 휘스커에 의한 다공성 코디어라이트의 기공구조 개질 및 특성평가)

  • Kim, Ik-Whan;Kim, Jun-Gyu;Lee, Hwan-Sup;Choi, Doo-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.2
    • /
    • pp.132-137
    • /
    • 2008
  • The main purpose of this study is enhancing the filtering efficiency, performance and durability of filter by growing SiC whiskers on cordierite honeycomb substrate. The experiment was performed by Chemical Vapor Infiltration (CVI) in order to control pore morphology of substrate. Increasing the mechanical strength of porous substrate is one of important issues. The formation of "networking structure" in the pore of porous substrate increased mechanical strength. The high pressure gas injection to the specimen showed that a little of whiskers were separated from substrate but additional film coating enhanced the stability of whisker at high pressure gas injection. Particle trap test was performed. More nano-particle was trapped by whisker growth at the pore of substrate. Therefore it is expected that the porous cordierite which deposited the SiC whisker will be the promising material for the application as filter trapping the nano-particles.

Effect of Water and Aluminum Sulfate Mole Ratio on Pore Characteristics in Synthesis of AlO(OH) Nano Gel by Homogeneous Precipitation (균일침전에 의한 AlO(OH) 나노 겔 합성에서 물/황산알루미늄의 몰 비가 세공특성에 미치는 영향)

  • Choe, Dong-Uk;Park, Byung-Ki;Lee, Jung-Min
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.9 s.292
    • /
    • pp.564-568
    • /
    • 2006
  • AlO(OH) nano gel is used in precursor of ceramic material, coating material and catalyst. For use of these, not only physiochemical control for particle morphology, pore characteristic and peptization but also studies of synthetic method for preparation of advanced application products were required. In this study, AlO(OH) nano gel was prepared through the aging and drying process of aluminum hydroxides gel precipitated by the hydrolysis reaction of dilute NaOH solution and aluminum sulfate solution. In this process, optimum synthetic condition of AlO(OH) nano gel having excellent pore volume as studying the effect of water and aluminum sulfate mole ratio on gel precipitates has been studied. Water and aluminum sulfate mole ratio brought about numerous changes on crystal morphology, surface area, pore volume and pore size. Physiochemical properties were investigated as using XRD, TEM, TG/DTA, FT-IR, and $N_2$ BET method.

Characterization of nano-fiber web structures using a morphological image processing

  • Kim, Jooyong;Lee, Jung-Hae
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2003.10a
    • /
    • pp.100-100
    • /
    • 2003
  • An image processing algorithm has been developed in order to analyze the nanofiber web images obtained from a high magnification microscope. It has been known that precise pore detection on thick webs is extremely difficult mainly due to lack of light uniformity, difficulty of fine focusing and translucency of nanofiber web. The pore detection algorithm developed has been found to show excellent performance in characterizing the porous structure, thus being a promising tool for on-line quality control system under mass production. Since the images obtained from an optical microscope represent only web surface, a scale factor has been introduced to estimate the web structure as a whole. Resulting web structures have been compared to those by mercury porosimetry, especially in pore size distribution. It has been shown that those two structures have a strong correlation, indicating that scaling of a single layer web structure can be an effective way of estimating the structure of thick fiber webs.

  • PDF

Gas Permeation Characteristics of Porous Alumina Membrane Prepared by Anodic Oxidation (양극산화에 의한 다공성 알루미나 막의 기체투과 특성)

  • 함영민
    • Journal of environmental and Sanitary engineering
    • /
    • v.13 no.3
    • /
    • pp.72-78
    • /
    • 1998
  • For investigation into gas permeation characteristics, the porous alumina membrane with asymmetrical structure, having upper layer with 10 nanometer under of pore diameter and lower layer with 36 nanometer of pore diameter, was prepared by anodic oxidation using DC power supply of constant current mode in an aqueous solution of sulfuric acid. The aluminium plate was pre-treated with thermal oxidation, chemical polishing and electrochemical polishing before anodic oxidation. Because the pore size depended upon the electrolyte, electrolyte concentration, temperature, current density, and so on, the the membranes were prepared by controling the current density, as a very low current density for upper layer of membrane and a high current density for lower layer of membrane. By control of current quantity, the thicknesses of upper layer of membranes were about $6{\;}{\mu}m$ and the total thicknesses of membranes were about $80-90{\;}{\mu}m$. We found that the mechanism of gas permeation depended on model of the Knudsen flow for the membrane prepared at each condition.

  • PDF

Preparation and Characterization of Demineralized Bone Particle Impregnated Poly(L-lactide) Scaffolds

  • Gilson Khang;Park, Chong-Soo;John M. Rhee;Lee, Sang-Jin;Lee, Young-Moo;Park, Myoung-Kyu;Lee, Hai-Bang;Lee, Ilwoo
    • Macromolecular Research
    • /
    • v.9 no.5
    • /
    • pp.267-276
    • /
    • 2001
  • In order to endow with new bioactive functionality from demineralized bone particle (DBP) as natural source to poly(L-lactide) (PLA) synthetic biodegradable polymer, porous DBP/PLA as natural/synthetic composite scaffolds were prepared and compared by means of the emulsion freeze drying and solvent casting/salt leaching methods for the possibility of the application of tissue engineered bone and cartilage. For the emulsion freeze drying method, it was observed that the pore size decreased in the order of 79$\mu\textrm{m}$ (PLA control) > 47$\mu\textrm{m}$ (20% of DBP) > 23 $\mu\textrm{m}$ (40% of DBP) > 15$\mu\textrm{m}$ (80% of DBP). Porosities as well as specific pore areas decreased with increasing the amount of DBR. It can be explained that DBP acts like emulsifier resulting in stabilizing water droplet in emulsion. For the solvent casting/salt leaching method, a uniform distribution of well interconnected pores from the surface to core region were observed the pore size of 80 ∼70 $\mu\textrm{m}$ independent with DBP amount. Porosities as well as specific pore areas also were almost same. For pore size distribution by the mercury intrusion porosimeter analysis between the two methods, the pore size distribution of the emulsion freeze drying method was broader than that of the solvent casting/salt leaching method due to the mechanism of emulsion formation. Scaffolds of PLA alone, DBP/PLA of 40 and 80%, and DBP powder were implanted on the back of athymic nude mouse to observe the effect of DBP on the induction of cells proliferation by hematoxylin and eosin staining for 8 weeks. It was observed that the effect of DBP/PLA scaffolds on bone induction are stronger than PLA scaffolds, even though the bone induction effect of DBP/PLA scaffold might be lowered than only DBP powder, that is to say, in the order of DBP only > DBP/PLA scaffolds of 40 and 80% DBP > PLA scaffolds only for osteoinduction activity. In conclusion, it seems that DBP plays an important role for bone induction in DBP/PLA scaffolds for the application of tissue engineering area.

  • PDF

Preparation and Characterization of Plasmid DNA Encapsulated in Liposomes (플라스미드 유전자를 함유한 리포좀의 제조 및 특성)

  • Park, Hyo-Min;Chung, Soo-Yeon;Go, Eun-Jung;Lee, Hwa-Jeong
    • Journal of Pharmaceutical Investigation
    • /
    • v.33 no.3
    • /
    • pp.209-213
    • /
    • 2003
  • The objective of this study was to construct the pegylated liposomes containing plasmid DNA with optimal encapsulation efficiency. Plasmid DNA $(pGL2\;clone\;753,\;{\sim}6\;kb)$ was encapsulated by the freeze/thawing method into liposomes composed of 1-palmitoyl-2-oleyl-sn-glycerol-3-phosphocholine (POPC), didodecyl dimethyl ammonium bromide (DDAB), distearoylphosphatidyl ethanolamine polyethylene glycol 2000 (DSPE-PEG 2000) and DSPE-PEG 2000-male-imide. The liposomes containing plasmid DNA were then extruded through two stacked polycarbonate filters with series of different pore sizes to control the liposome size. The plasmid DNA entrapped in the liposomes was separated from free plasmid DNA by Sephadex CL-4B column chromatography. The decreased pore size of polycarbonate filters resulted in the decreased size of liposomes. The encapsulation efficiency was markedly affected by the cationic lipid (DDAB) concentration, but to a low degree by the size of liposomes and by the amount of plasmid DNA.

Structure Variation of Polypropylene Hollow Fiber Membrane with Operation Parameters in Stretching Process (연신 공정 조업변수에 따른 폴리프로필렌 중공사막의 구조 변화)

  • Lee Gyu-Ho;Kim Jin-Ho;Song Ki-Gook;Kim Sung-Soo
    • Polymer(Korea)
    • /
    • v.30 no.2
    • /
    • pp.175-181
    • /
    • 2006
  • Hybrid process of thermally-induced phase separation and stretching was developed for the preparation of microporous polypropylene hollow fiber membranes. Precursor for stretching was prepared by using soybean oil as a diluent and benzoic acid as a nucleating agent far the sphenlite control and it was stretched far the micrporous hollow fiber membrane. The effects of stretching ratio and deformation rate for stretching process were investigated. Increase of stretching ratio resulted in the greater pore size with nonuniform size distribution. Higher deformation rate also increaser the pore size with uniform size distribution. Stretching ratio was closely related with the orientation of polymer chain and increased the mechanical strength of the fiber. Increase of deformation rate had little effects on the orientation of crystalline phase, and decreased the orientation of amorphous phase which caused the decrease of tensile strength of the fiber and broke the micro-fibrils connecting spherulites to form a circular pore shape.

Selective Separation of $CO_2/CH_4$ by Pore Structure Modification of Activated Carbon Fiber (활성탄소섬유의 기공구조 변형을 이용한 $CO_2/CH_4$의 선택적 분리 기술)

  • Moon, S.H.;Park, S.Y.
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.29 no.9
    • /
    • pp.1027-1034
    • /
    • 2007
  • This research was focused on the selective separation of $CO_2$ or $CH_4$ from mixture of these gases, by controlling the size of pore or pore gate. Pitch based activated carbon fibers(ACF) were used as adsorbents. The size of pore gate was controlled by the molecule having similar size to that of pore opening. After the adsorption of adsorbate on pore surface, planar molecules such as benzene and naphthalene covered the pore gate. The slow release of adsorbate from the pores covered by planar molecules makes apertures between planar molecules covering pore gate and this structure can be fixed by rapid pyrolysis. The control of pore gate using benzene as covering molecules could not accomplished due to the simultaneous volatilization of benzene and adsorbate$(CO_2)$ caused by similar temperatures of benzene volatilization and adsorbate desorption. Therefore we replaced benzene with naphthalene looking for the stability at a $CO_2$ desorption temperature. The naphthalene molecule was adsorbed on the ACF up to 15% of ACF weight and showed no desorption until $100^{\circ}C$, indicating that the molecule could be used as a good cover molecule. Naphthalene could cover almost all the pore gate, reducing BET surface area from 753 $m^2/g$ to 0.7 $m^2/g$. A mixed gas$(CO_2:CH_4=50:50)$ was adsorbed on the naphthalene treated OG-7A ACF. The amount of $CO_2$ adsorption increased with total pressure, whileas thai of $CH_4$ was not so much influenced on the pressure, indicating that $CO_2$ made more compounds on the ACF surface along with total pressure increase. The most $CO_2$ and the least $CH_4$ were adsorbed in the condition of 0.4 atm, resulting in the highly pure $CH_4$ left in ACF.