• Title/Summary/Keyword: Pitch residue

Search Result 22, Processing Time 0.026 seconds

The Electrochemical Migration Phenomenon of the Ni-Cr Seed Layer of Sputtered FCCL

  • Ahn, Woo-Young;Jang, Joong Soon
    • Journal of the Korean institute of surface engineering
    • /
    • v.47 no.2
    • /
    • pp.63-67
    • /
    • 2014
  • As the demand for fine-pitch FPCB (Flexible Printed Circuit Board) increases, so do the number of applications of sputtered FCCL (Flexible Copper Clad Laminate). Furthermore, as the width between the circuit patterns decreases, greater defects are observed in the migration phenomenon. In this study we observed changes in ion migration in real circuit-pattern width using sputtered FCCL. We found that as the applied voltage and residue thickness of the NiCr seeds increase, ion migration occurs faster. If the NiCr seed layer thickens due to a high cathode power and long deposition time while being sputtered, the NiCr will form a residue that quickly becomes a factor for incurring ion migration.

Enhanced Removal Efficiency of Low-Concentration Cesium Ion in Water Phase by Using Petroleum Residue Pitch (석유계 잔사유 피치를 이용한 수중에서 저농도 세슘 이온의 제거효율 향상)

  • Choi, Tae Ryeong;Ha, Jeong Hyub;Choi, Suk Soon
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.29 no.4
    • /
    • pp.25-31
    • /
    • 2021
  • In this research, in order to effectively utilize the petroleum residue pitch, it was used as an adsorbent for removal of cesium ion. In this experiment, acid modification (hydrochloric acid, sulfuric acid) treatment was performed on the adsorbent to improve the ability to remove low-concentration cesium ions dissolved in water. As a result, when the reaction was performed with 9 M sulfuric acid at 25 ℃ and for 240 min, the removal efficiencies of 1.0 and 2.5 mg/L cesium ions were 66 and 51%, respectively. In addition, as the adsorption time increased in the batch experiment, the removal capacity of 1.0 and 2.5 mg/L cesium ions was improved, and when the adsorption reached for 32 hr, the removal efficiencies were 72 and 68%, respectively. Also, in order to increase the ability to remove the remaining cesium ions, an experiment was performed by temperature change (25, 37, 49 ℃), and 1.0 and 2.5 mg/L cesium ions contained in water under the operating conditions of 49 ℃ and 32 hr showed removal efficiencies of 90 and 81%, respectively. Consequently, these experimental results were intended to be used as an adsorption technology that can economically treat low-concentration cesium ions contained in water.

Mesophase formation behavior in petroleum residues

  • Kumar, Subhash;Srivastava, Manoj
    • Carbon letters
    • /
    • v.16 no.3
    • /
    • pp.171-182
    • /
    • 2015
  • Mesophase pitch is an important starting material for making a wide spectrum of industrial and advanced carbon products. It is produced by pyrolysis of petroleum residues. In this work, mesophase formation behavior in petroleum residues was studied to prepare environmentally-benign mesophase pitches, and the composition of petroleum residues and its influence on the mesophase formation was investigated. Two petroleum residues, i.e., clarified oil s (CLO-1, CLO-2) obtained from fluid catalytic cracking units of different Indian petroleum refineries, were taken as feed stocks. A third petroleum residue, aromatic extract (AE), was produced by extraction of one of the CLO-1 by using N-methyl pyrrolidone solvent. These petroleum residues were thermally treated at 380℃ to examine their mesophase formation behavior. Mesophase pitches produced as a result of thermal treatment were characterized physico-chemically, as well as by instrumental techniques such as Fourier-transform infrared spectroscopy, nuclear magnetic resonance, X-ray diffraction and thermogravimetry/derivative thermogravimetry. Thermal treatment of these petroleum residues led to formation of a liquid-crystalline phase (mesophase). The mesophase formation behavior in the petroleum residues was analyzed by optical microscopy. Mesophase pitch prepared from CLO-2 exhibited the highest mesophase content (53 vol%) as compared to other mesophase pitches prepared from CLO-1 and AE.

New Products for High Reliable Connections in Packaging Technology

  • Mueller, Tobias
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2006.10a
    • /
    • pp.179-212
    • /
    • 2006
  • 1. $Welco^{(R)}$ Ultra fine solder powders are suitable for wafer bumping applications; mass production of ultra fine powders with high quality and high yield. - UFP based pastes for wafer bumping by stencil printing ($60-80{\mu}m$ pitch) are now available - Residue free solder flux was developed; meets voids specification of 20%. - F645 type 5 paste is suitable for components 01005

  • PDF

Effects of Pitch Softening Point-based on Soft Carbon Anode for Initial Efficiency and Rate Performance (피치계 소프트 카본 음극재 제조 시 피치의 연화점이 음극재 초기 효율 및 율속 특성에 미치는 영향)

  • Kim, Kyung Soo;Im, Ji Sun;Lee, Jong Dae;Kim, Ji Hong;Hwang, Jin Ung
    • Applied Chemistry for Engineering
    • /
    • v.30 no.3
    • /
    • pp.331-336
    • /
    • 2019
  • In this study, required properties and optimized procedure conditions for the pitch based soft carbon anode of lithium ion battery was investigated for improving the initial efficiency and rate performance. Each petroleum residue was thermally treated at 360, 370, and $410^{\circ}C$ for 3 hours to synthesis a pitch and the corresponding pitch shows the softening point of 86, 98, and $152^{\circ}C$, respectively. The elemental analysis and thermal characteristics of the pitch were investigated by EA analysis and TGA. It was noted that the low H/C and improved thermal stability were obtained with the high softening point. The obtained pitch was carbonized at $1,200^{\circ}C$ for 1 hour to produce a soft carbon based anode. As a result of investigating the crystal structure by XRD analysis, it was found that the crystallinity of soft carbon increased with increasing the softening point. It was considered that relatively higher boiling components and decreases in the evaporation component resulted the components participation for cyclization during the heat treatment process. The soft carbon based anode with an improved crystallinity shows the enhanced initial efficiency and rate performance. The mechanism of both improvements was also discusssed based on the developed crystal structure of soft carbon based anode materials.

Speaker Verification Performance Improvement Using Weighted Residual Cepstrum (가중된 예측 오차 파라미터를 사용한 화자 확인 성능 개선)

  • 위진우;강철호
    • The Journal of the Acoustical Society of Korea
    • /
    • v.20 no.5
    • /
    • pp.48-53
    • /
    • 2001
  • In speaker verification based on LPC analysis the prediction residues are ignored and LPCC(LPC cepstrum) are only used to compose feature vectors. In this study, LPCC and RCEP (residual cepstrum) extracted from residues are used as feature parameters in the various environmental speaker verification. We propose the weighting function which can enlarge inter-speaker variation by weighting pitch, speaker inherent vector, included in residual cepstrum. Simulation results show that the average speaker verification rate is improved in the rate of 6% with RCEP and LPCC at the same time and is improved in the rate of 2.45% with the proposed weighted RCEP and LPCC at the same time compared with no weighting.

  • PDF

Flux residue effect on the electrochemical migration of Sn-3.0Ag-0.5Cu (Sn-3.0Ag-0.5Cu 솔더링에서 플럭스 잔사가 전기화학적 마이그레이션에 미치는 영향)

  • Bang, Jung-Hwan;Lee, Chang-Woo
    • Journal of Welding and Joining
    • /
    • v.29 no.5
    • /
    • pp.95-98
    • /
    • 2011
  • Recently, there is a growing tendency that fine-pitch electronic devices are increased due to higher density and very large scale integration. Finer pitch printed circuit board(PCB) is to be decrease insulation resistance between circuit patterns and electrical components, which will induce to electrical short in electronic circuit by electrochemical migration when it exposes to long term in high temperature and high humidity. In this research, the effect of soldering flux acting as an electrical carrier between conductors on electrochemical migration was investigated. The PCB pad was coated with OSP finish. Sn3.0Ag0.5Cu solder paste was printed on the PCB circuit and then the coupon was treated by reflow process. Thereby, specimen for ion migration test was fabricated. Electrochemical migration test was conducted under the condition of DC 48 V, $85^{\circ}C$, and 85 % relative humidity. Their life time could be increased about 22% by means of removal of flux. The fundamentals and mechanism of electrochemical migration was discussed depending on the existence of flux residues after reflow process.

Pitch-based carbon fibers from coal tar or petroleum residue under the same processing condition

  • Kim, Jiyoung;Im, Ui-Su;Lee, Byungrok;Peck, Dong-Hyun;Yoon, Seong-Ho;Jung, Doo-Hwan
    • Carbon letters
    • /
    • v.19
    • /
    • pp.72-78
    • /
    • 2016
  • Spinnable pitches and carbon fibers were successfully prepared from petroleum or coal pyrolysis residues. After pyrolysis fuel oil (PFO), slurry oil, and coal tar were simply filtered to eliminate the solid impurities, the characteristics of the raw materials were evaluated by elemental analysis, 13C nuclear magnetic resonance spectrometer, matrix-assisted laser desorption/ionization time-of-flight mass spectrometer (MALDI-TOF-MS), and so on. Spinnable pitches were prepared for melt-spinning carbon fiber through a simple distillation under strong nitrogen flow, and further vacuum distillation to obtain a high softening point. Carbon fibers were produced from the above pitches by single-hole melt spinning and additional heat treatment, for oxidization and carbonization. Even though spinnable pitches and carbon fibers were processed under the same conditions, the melt-spinning and properties of the carbon fiber were different depending on the raw materials. A fine carbon fiber could not be prepared from slurry oil, and the different diameter carbon fibers were produced from the PFO and coal tar pitch. These results seem to be closely correlated with the initial characteristics of the raw materials, under this simple processing condition.

Oxidation Resistance and Graphitization of Boron Oxide Implanted Carbon/Carbon Composites

  • Joo, Hyeok-Jong;Oh, In-Hwan;Ahn, Il-Hwan
    • Carbon letters
    • /
    • v.5 no.3
    • /
    • pp.127-132
    • /
    • 2004
  • Chop molding composites and 2D carbon/carbon composites were manufactured by hot press molding method. Phenol resin of novolac type was used for matrix precursor and PAN-based carbon, PAN-based graphite and pitch-based carbon fiber were used for reinforcement and boron oxide was used for oxidation retardant. All of the composites were treated by $2000^{\circ}C$ and $2400^{\circ}C$ graphitization process, respectively. After graphitization process, amount of a boron residue in carbon/carbon composites is much according to irregularity of used raw materials. Under the presence of boron in carbon/carbon composites, catalytic effect of boron was a little at $2000^{\circ}C$ graphitization temperature. However, it was quite at $2400^{\circ}C$ graphitization.

  • PDF

리튬 2차전지 anode용 탄소재료 구조의 방전용량에 대한 영향

  • 양철민;양갑승
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 1996.10a
    • /
    • pp.124-130
    • /
    • 1996
  • The hydrocarbons containing more than 10 carbons(0.1% of total volume, C10+), residue of aromatization from aliphatic hydrocarbons, were condensated in the presence of catalyst aluminumchloride and cocatalyst nitrobenzene(NB) to be pitchs with desirable properties. The properties of pitch were affected by the concentration of cocatalyst chosen 20 and 30wt.%. The pitch with 30wt.% NB showed higher carbon yield and lower crystallinity than that with 20wt.% NB. The two pitches were heat treated at 1000C and measured of charge/discharge capacity of the carbon as an anode. The carbon prepared at 20wt.% NB exhibited excellent cyclic stability with a capacity of 218mAh/.g and that at 30wt.% exhibited rather low cyclic stability with higher capacity of 235mAh/g.

  • PDF