Gd$_2O_3$:Eu phosphor particles with spherical and filled morphology

  • Roh, Hyun-Sook;Kang, Yun-Chan;Park, Hee-Dong;Park, Seung-Bin
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2002.08a
    • /
    • pp.253-256
    • /
    • 2002
  • $Gd_2O_3$:Eu phosphor particles were prepared by largescale ultrasonic spray pyrolysis process. The morphological control of $Gd_2O_3$:Eu particles in spray pyrolysis was performed by adding polymeric precursors into spray solution containing nitrate salts. The effect of composition and amount of polymeric precursors on the morphology, crystallinity, and photoluminescence characteristics of $Gd_2O_3$:Eu particles was investigated. The influence of chain length of PEG on the morphology and photoluminescence intensity was investigated. $Gd_2O_3$:Eu particles prepared from aqueous solution containing no polymeric precursors had a hollow structure and rough surfaces after annealing process. The phosphor particles prepared from solution containing 0.1M CA and 0.lM PEG with high molecular weight as 1,500 had a spherical and filled morphology and the highest photoluminescence intensity, which was 48% higher than that of the $Y_2O_3$:Eu commercial product.

  • PDF

Synthesis and Photo Luminescent Characteristics of SrAl2O4:Eu2+,Dy3+ Phosphor using Polymer Matrix (폴리머 매트릭스를 전구체로 사용한 SrAl2O4:Eu2+,Dy3+ 축광성 형광체의 합성 및 형광 특성)

  • Kim, Soo-Jong;Kwon, Hyuk-Sil
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.8
    • /
    • pp.671-679
    • /
    • 2007
  • [ $SrAl_2O_4:Eu^{2+},\;Dy^{3+}$ ] phosphor was synthesized using the impregnation method, and its photoluminescence and long-afterglow properties were investigated, A mixture of $Sr(NO_3)_2,\;Al(NO_3)_2\;9H_2O,\;EuCl_3\;6H_2O,\;DyCl_3\;6H_2O,\;NdCl_3\;6H_2O$ salts were dissolved in distilled water and impregnating into the polymer precursor. After drying, the impregnated mixture was heat treated at $900-1400^{\circ}C$ for 2h in a $N_2-H_2$ reduction atmosphere. The microstructure and crystal structure of the $SrAl_2O_4:Eu^{2+},\;Dy^{3+}$ powders were examined by scanning electron microscopy and X-ray diffraction, respectively. The photoluminescence spectra showed an excitation band along over wide wavelength of 250-450nm, and a broaden emission with a maxima peak at 360nm. In addition, the spectra also showed a good long after glow that decayed over a 1000sec period after 10 min excitation illumination.

Luminescent Characteristics and Synthesis of Sm3+-Doped CaWO4 Phosphors (CaWO4:Sm3+ 형광체의 합성과 발광특성)

  • Ryu, Jong-Hang;Yoon, So-Jin;Yu, Il
    • Korean Journal of Materials Research
    • /
    • v.24 no.7
    • /
    • pp.339-343
    • /
    • 2014
  • $CaWO_4:Sm_x$(x = 0, 0.5, 1.0, 1.5, 2.0 mol%) white phosphors with different concentrations of $Sm^{3+}$ ions were synthesized using the hydrothermal method. The crystal structure, surface, and optical properties of the $CaWO_4:Sm_x$ phosphors were investigated using X-ray diffraction(XRD), field-emission scanning electron microscopy(FE-SEM), photoluminescence(PL) and photoluminescence excitation(PLE). From the XRD results, the crystal structure of the $CaWO_4:Sm$ phosphors was found to be tetragonal. The $CaWO_4:Sm$ phosphors became more cohesive with increasing $Sm^{3+}$-ion concentration. The photoluminescence excitation(PLE) peak of the phosphors, at around 250 nm, was ascribed to the transition from the 1A1 ground-state to the high-vibration level of 1T2 in the $WO{_4}^{2-}$ complex. The maximum emission spectra of the phosphors were observed when the $Sm^{3+}$ concentration was 0.5 mol%. The luminescence intensity of the $CaWO_4$ phosphors was decreased for $Sm^{3+}$ concentrations greater than 0.5 mol%.

Effects of Carrier Leakage on Photoluminescence Properties of GaN-based Light-emitting Diodes at Room Temperature

  • Kim, Jongseok;Kim, Seungtaek;Kim, HyungTae;Choi, Won-Jin;Jung, Hyundon
    • Current Optics and Photonics
    • /
    • v.3 no.2
    • /
    • pp.164-171
    • /
    • 2019
  • Photoluminescence (PL) properties of GaN-based light-emitting diodes (LEDs) were analyzed to study the effects of carrier leakage on the luminescence properties at room temperature. The electrical leakage and PL properties were compared for LEDs showing leakages at forward bias and an LED with an intentional leakage path formed by connecting a parallel resistance of various values. The leakages at the forward bias, which could be observed from the current-voltage characteristics, resulted in an increase in the excitation laser power density for the maximum PL efficiency (ratio of PL intensity to excitation power) as well as a reduction in the PL intensity. The effect of carrier leakages on PL properties was similar to the change in PL properties owing to a reduction of the photovoltage by a reverse current since the direction of the carrier movement under photoexcitation is identical to that of the reverse current. Valid relations between PL properties and electrical properties were observed as the PL properties deteriorated with an increase in the carrier leakage. The results imply that the PL properties of LED chips can be an indicator of the electrical properties of LEDs.

Luminescent Characteristics and Synthesis of Eu3+- Doped Y2O3 Red Phosphors (Y2O3 : Eu3+ 적색 형광체의 발광특성)

  • Yu, Il
    • Korean Journal of Materials Research
    • /
    • v.31 no.10
    • /
    • pp.582-585
    • /
    • 2021
  • Y2O3:Eux (x = 0.005, 0.01, 0.02, 0.03, 0.05, 0.1 mol) phosphors are synthesized with different concentrations of Eu3+ ions by solvothermal method. The crystal structure, surface and optical properties of the Eu doped Y2O3 phosphors are investigated using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), and photoluminescence (PL) and photoluminescence excitation (PLE) analyses. From X-ray diffraction (XRD) results, the crystal structure of the Eu doped Y2O3 phosphor is found to be cubic. The maximum emission spectra of the Eu doped Y2O3 phosphors are observed at 0.05 mol Eu3+ concentration. The photoluminescence of 615 nm in the Eu doped Y2O3 phosphors is associated with 5D07F2 transition of Eu3+ ions. The decrease in emission intensity of 0.1 mol Eu doped Y2O3 is interpreted by concentration quenching. The International Commission on Illumination (CIE) coordinates of 0.05 mol Eu doped Y2O3 phosphor are X = 0.6547, Y = 0.3374.

Effect of Fabricating Nanopatterns on GaN-Based Light Emitting Diodes by a New Way of Nanosphere Lithography

  • Johra, Fatima Tuz;Jung, Woo-Gwang
    • Korean Journal of Materials Research
    • /
    • v.23 no.3
    • /
    • pp.177-182
    • /
    • 2013
  • Nanosphere lithography is an inexpensive, simple, high-throughput nanofabrication process. NSL can be done in different ways, such as drop coating, spin coating or by means of tilted evaporation. Nitride-based light-emitting diodes (LEDs) are applied in different places, such as liquid crystal displays and traffic signals. The characteristics of gallium nitride (GaN)-based LEDs can be enhanced by fabricating nanopatterns on the top surface of the LEDs. In this work, we created differently sized (420, 320 and 140 nm) nanopatterns on the upper surfaces of GaN-based LEDs using a modified nanosphere lithography technique. This technique is quite different from conventional NSL. The characterization of the patterned GaN-based LEDs revealed a dependence on the size of the holes in the pattern created on the LED surface. The depths of the patterns were 80 nm as confirmed by AFM. Both the photoluminescence and electroluminescence intensities of the patterned LEDs were found to increase with an increase in the size of holes in the pattern. The light output power of the 420-nm hole-patterned LED was 1.16 times higher than that of a conventional LED. Moreover, the current-voltage characteristics were improved with the fabrication of differently sized patterns over the LED surface using the proposed nanosphere lithography method.

Photoluminescence Characteristics of ZnGa2O4 Nano-phosphors by Combustion Method (연소합성법으로 제작한 ZnGa2O4 나노형광체의 광학적 특성)

  • Kim, Se-Jun;Choi, Hyung-Wook
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.1
    • /
    • pp.14-17
    • /
    • 2010
  • $ZnGa_2O_4$ powder were prepared by combustion method and $Mn^{2+}$ ions, a green luminescence activator, and $Cr^{3+}$ ions, a red luminescence activator were separately doped into $ZnGa_2O_4$. The characteristics of the synthesized nano powder were investigated by means of X-ray diffraction (XRD), Scanning Electron Microscope (SEM), and photoluminescence (PL). The various $ZnGa_2O_4$ peaks, with the (311) main peak, appeared at all sintering temperature XRD patterns. The PL specctrums of $ZnGa_2O_4$ powder showed main peak of 425 nm, and maximum intensity at the sintering temperature of $1200^{\circ}C$. SEM images shown that nano sized particles(about 200 nm) were of spherical shape. The characteristics of $ZnGa_2O_4$ containing 0.004 mol $Mn^{2+}$(505 nm, green) and $ZnGa_2O_4$ containg 0.002 mol $Cr^{3+}$ (696 nm, red) were shown to be the best.

Influences of Spinodal Decomposition of InGaAsP Layer on Photoluminescence Characteristics (InGaAsP 에피막의 Spinodal분해 조직구조가 Photoluminescence 특성에 미치는 영향)

  • Lee, Jong-Won
    • Korean Journal of Materials Research
    • /
    • v.5 no.8
    • /
    • pp.936-944
    • /
    • 1995
  • The effects of Spinodal decomposition induced phase separated microstructure of InGaAsP/InP heterostructure on photoluminescence(PL) intensity and FWHM(full-width at half maximum) were investigated in this study. Lattice mismatches were measured by double crystal x-ray diffractometer, and the microstructures of phase separated InGaAsP were observed by transmission electron microscopy. It was found that the misfit stress calculated from lattice mismatch was related to the periodicity of Spinodal modulation. Strong dependence of PL intensity and FWHM on the modulation periodicity was also found. For systematic understanding of these observations, the interaction elastic strain energy function induced by misfit stress was proposed. The calculation illustrated that the microstructure of the epilayer such as Spinodal decomposition played an important role in determining the optoelectronic properties such as PL intensity and PL FWHM.

  • PDF

Effects of growth interruption on the photoluminescence characteristics of InGaAs/InP quantum wells (성장정지효과에 의한 InGaAs/InP 양자우물구조의 Photoluminescence 특성 변화)

  • 문영부;이태완;김대연;윤의준;유지범
    • Journal of the Korean Vacuum Society
    • /
    • v.7 no.2
    • /
    • pp.104-111
    • /
    • 1998
  • The InGaAs/InP quantum wells(QWs) were grown by low pressure metalorganic chemical vapor deposition and the effects of growth interruption steps on their interfacial structures were investigated by measuring photoluminescence spectra. When InP or InGaAs surface was treated under the same group V ambient, the full width at half maximum (FWHM) of the QW peak increased possibly due to the incorporation of impurities during the growth interruption time. When InP surface was treated under $AsH_3$, howerer, the PL peak showed red-shift due to the As-P exchange reaction and the change of FWHM was not remarkable. The effective thickness of InAs interfacial layer formed during $AsH_3$, treatment on the InP surface was calculated to be 1~2 monolayers. In the case of InGaAs treatment under $PH_3$, the PL peak energy and the FWHM increasied. This results suggest that $PH_3$ treatment on the InGaAs surface suppresses the incorporation of As into the subsequent InP layer and the local replacement of As by P occurs simultaneously.

  • PDF

Luminescence properties of asymmetric double quantum well composed of $Al_xGa_{l-x}As/AlAs/GaAs$ system ($Al_xGa_{l-x}As/AlAs/GaAs$계로 이루어진 비대칭 이중 양자우물 구조에서의 광 luminescsnce 특성 연구)

  • 정태형;강태종;이종태;한선규;유병수;이해권;이정희;이민영;김동호
    • Korean Journal of Optics and Photonics
    • /
    • v.3 no.3
    • /
    • pp.183-190
    • /
    • 1992
  • Luminescence properties of asymmetric double quantum well structure composed of $Al_x/Ga_{1-x}$ /As AIAs/GaAs have been studied by steady state and time-resolved photoluminescence and phtoluminescence excitation spectroscopy at low temperature. Two quantum well samples with different barrier thickness (15$\AA$ and 150$\AA$) were prepared to investigate the dependence of tunneling characteristics on barrier thickness. The abscence of excitonic recombination peak from $Al_x/Ga_{1-x}$As well for the 15$\AA$ barrier sample indicates a very fast electron tunneling to GaAs well. Meanwhile, T-X transition between well and barrier is supposed to be a major route for the fast decay of luminescence from $Al_x/Ga_{1-x}$As well in the 150$\AA$ barrier sample. Time-resolved photduminescence from GaAs well of 15$\AA$ sample shows the exsitence of the rise with 100 ps which is attributed to the hole tunneling.

  • PDF