청색 $\textrm{Ca}\textrm({Al}_{0.97}\textrm{B}_{0.03})_2\textrm{O}_4$: $\textrm{Eu}^{+2},\;\textrm{Nd}^{+3}$ 형광체의 잔광 특성에 관한 연구 (A Study on the Phosphorescent Characteristics of Blue $\textrm{Ca}\textrm({Al}_{0.97}\textrm{B}_{0.03})_2\textrm{O}_4$: $\textrm{Eu}^{+2},\;\textrm{Nd}^{+3}$ Phosphor)

  • 김대수;이임렬
    • 한국재료학회지
    • /
    • 제9권1호
    • /
    • pp.3-7
    • /
    • 1999
  • The change of phosphorescent property with chemical modification and co-doping of Nd as an auxiliary activator in CaAl$_2$$O_4$: Eu\ulcorner, Nd\ulcorner phosphor, employing Nd\ulcornerion(0.6%) and an co-activator maintained its afterglow for 4.5 hours. And also the initial persistent brightness and phosphorescent property were further improved both by substituting Al by B atoms and incorporation of Nd\ulcorner ion. It was found that the persistent time was 30 hours for&Ca(Al_{0.97}\;B_{0.03}) $_2$$O_4$:EU\ulcorner(0.3%), Nd\ulcorner(0.6%) phosphor.

  • PDF

인광물질 인 Ir(PPy)$_3$를 이용한 유기전기발광소자의 효율 개선에 관한 연구 (A Study on the improvement in efficiencies of Organic-Light Emitting Devices Using the Phosphor, Ir(PPy)$_3$)

  • 김준호;김윤명;구자룡;이한성;하윤경
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.178-181
    • /
    • 2001
  • The organic light-emitting devices (OLEDs) based on fluorescence have low efficiencies due to the requirement of spin-symmetry conservation. By using the phosphorescent material, the internal quantum efficiency can reach 100 %, compared to 25 % in the case of the fluorescent material. Thus, the phosphorescent OLEDs have recently been extensively studied and showed higher internal quantum efficiencies then the conventional OLEDs. In this study, we investigated the characteristics of the phosphorescent OLEDs, with the green emitting phosphor, Ir(ppy)$_3$ (tris(2-phenylpyridine)iridium). The devices with a structure of ITO/TPD/Ir(PPy)$_3$ doped in the host material/BCP/Alq$_3$/Li:Al/Al were fabricated, and its electrical and optical characteristics were studied. By changing the doping concentration of Ir(PPy)$_3$ and the host materials, we fabricated several devices and investigated the device characteristics.

  • PDF

($Eu^{2+}$, $Nd^{3+}$를 도핑시킨 $BaAl_{2}O_{4}$ 형광체의 광학 및 장잔광특성 (Optical and Long After-Glow Characteristics of $Eu^{2+}$, $Nd^{3+}$ doped $BaAl_{2}O_{4}$ Phosphorescent Crystals)

  • 김정환;김병규;이동규
    • 한국응용과학기술학회지
    • /
    • 제19권3호
    • /
    • pp.174-180
    • /
    • 2002
  • In recent days, the study of a new phosphorescent phosphor has been performed in order to overcome the defect of sulfide phosphor and increase the brightness and long after-glow characteristic of phosphorescent phosphor. Particularly, sulfide phosphor usually used is so chemically unstable that the study of oxide phosphors are processing. $Eu^{2+}$, $Nd^{3+}$ doped Ba-Al-O phosphors sintered at $600{\sim}1500^{\circ}C$ for 2hours had the PL emission spectrum and after-glow over $1200^{\circ}C$. In this system, as the mole concentration of alumina increases, emission bands of phosphors moved from 500nm to 380nm. The optimum concentration of flux was 5wt% and after-glow characteristics of phosphors were found at the host material molar ratio ($BaCO_{3}:Al_{2}O_{3}$), 1:1 and 1:3.

차선의 시인성 향상을 위한 SrAl2O4 : Eu2+,Dy3+ 축광 마이크로 캡슐화에 관한 연구 (Microencapsulation of SrAl2O4 : Eu2+,Dy3+ Phosphorescent Phosphor for Enhanced Visibility of Road Lanes)

  • 박재일;정수환;정인우
    • 접착 및 계면
    • /
    • 제17권3호
    • /
    • pp.110-116
    • /
    • 2016
  • 야간 우천시 수막에 의한 차선의 재귀반사 효율 감소로 운전자의 시인성이 저하되고 있으며 이로 인해 많은 사고가 발생한다. 시인성을 높이기 위해 메틸메타크릴레이트의 현탁중합 시 소수성으로 표면이 개질된 $SrAl_2O_4:Eu^{2+}$,$Dy^{3+}$ 축광 물질을 도입하고 이를 캡슐화하였다. 표면 개질에 사용된 물질과 라디칼 개시제의 종류, 사용된 축광 물질의 양, 그리고 캡슐의 입도가 캡슐 내부의 축광 물질 함량($W_{TGA}$)에 미치는 영향을 TGA를 사용하여 분석하였다. 그 결과 축광 물질의 함량은 7~81 wt%까지 넓은 분포를 나타내었으며, 이러한 결과는 현탁중합이 넓은 함량 범위의 축광 물질을 캡슐화하는데 적합한 것을 의미한다. 축광 물질의 함량이 낮은 경우에는 캡슐의 입도가 감소함에 따라 $W_{TGA}$이 증가하였으나, 축광 물질의 함량이 높을 때에는 캡슐의 입도에 별 영향을 받지 않았다. 축광 캡슐 중 지름 $425{\sim}710{\mu}m$의 축광 캡슐을 활용하여 형광 차선 시편을 제작하였으며 LED램프를 20 min 동안 조사한 후 광원을 제거하였을 때, 100 s 동안 약 $300mcd/m^2$ 이상의 휘도를 유지했다. 이러한 결과로 미루어 보아 제조된 축광 캡슐은 차선 위의 유리 비드를 대체하기에 충분한 가능성을 가짐을 알 수 있었다.

Electrical Characteristics of Green Emitting Phosphor $Ir(PPY)_3$ Doped OLEDs

  • Kim, Jun-Ho;Kim, Yun-Myung;Ha, Yun-Kyung;Kim, Young-Kwan;Kim, Jung-Soo
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • 제11C권3호
    • /
    • pp.53-57
    • /
    • 2001
  • The organic light-emitting devices (OLEDs) based on fluorescence have low efficiency due to the requirement of spin-symmetry conservation. By using the phosphorescent material, internal quantum efficiency can reach 100%, compared with 25% in the case of the fluorescent material. Thus, phosphorescent OLEDs have recently been extensively studied and shown higher internal quantum efficiency than the conventional OLEDs. In this study, we investigated the characteristics of the phosphorescent OLEDs with the green emitting phosphor, $Ir(ppy)_3$ (tris(2-phenylpyridine)iridium). The device with a structure of ITO/TPD$Ir(ppy)_3$ doped in BCP/BCP/$Alq_3$/Li:Al/Al was fabricated, and its electrical and optical characteristics were studied. By changing the doping concentration of $Ir(ppy)_3$, we fabricated several devices and investigated their characteristics.

  • PDF

SrAl2O4: Eu2+, Dy3+ 축광안료의 고온안정성에 관한 연구 (Thermal Stability of SrAl2O4: Eu2+, Dy3+ with Long Afterglow Phosphorescence)

  • 김진호;이승용;김태호;한규성;황광택;조우석
    • 한국세라믹학회지
    • /
    • 제51권6호
    • /
    • pp.618-622
    • /
    • 2014
  • Oxide phosphorescent phosphor has an wide application in ceramic art and decoration due to its chemical and mechanical properties. Here, phosphorescent properties of strontium aluminate phosphor ($SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$) emitting yellowish-green light was investigated with thermal treatment at $1250^{\circ}C$ under air and reducing atmosphere. The characterizations of thermally treated samples were analyzed using X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX), fluorescence spectrometer. $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ still showed a good phosphorescent properties after annealing process in reducing atmosphere, while phosphorescence of $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ annealed in air seriously degraded, due to oxidation of $Eu^{2+}$ to $Eu^{3+}$ ions. It was also observed that $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ annealed in reducing atmosphere emitted yellowish-green light during 3 h after being exposed to sunlight.

인광특성이 있는 금속 착물의 합성과 그 물질을 이용한 소자 제작 및 소자 특성 평가 (Study on the Characteristics and Fabrication of Organic Light Emitting Devices Using the Synthesised Phosphorescent Metal Complexes)

  • 김영관;손병청;김준호
    • 한국응용과학기술학회지
    • /
    • 제19권2호
    • /
    • pp.97-102
    • /
    • 2002
  • Recently, the phosphorescent organic light-emitting devices (OLEDs) have been extensively studied for their high internal quantum efficiency. In this study, we synthesised several phosphorescent metal complexes, and certified their composition using NMR. We also investigated the characteristics of the phosphorescent OLEDs with the green emitting phosphor, $Ir(ppy)_{3}$. The devices with a structure of indium-tin-oxide(ITO)/N,N'-diphenyl-N,N'-(3-methylphenyI}-1,1'-biphenyl-4,4'-diamine (TPD)/metal complex doped in host materials/2,9-dimethyl-4,7-diphenyl-l,10-phenanthroline(BCP)/tris (8-hydroxyquinolinato) Aluminum($Alq_{3}$)/Li:Al/Al was fabricated, and its electrical and optical characteristics were studied. By changing the doping concentration of tris(2-phenylpyridine)iridium ($Ir(ppy)_{3}$), we fabricated several devices and investigated their characteristics.

글리신-질산염 연소법으로 합성된 SrAl2O4:Eu2+,Dy3+ 형광체의 발광 및 장잔광 특성 (Photoluminescence and Long-phosphorescent Characteristics of SrAl2O4:Eu2+,Dy3+ Phosphor by Glycine-nitrate Combustion Method)

  • 이영기;김정열;이유기
    • 한국재료학회지
    • /
    • 제20권7호
    • /
    • pp.364-369
    • /
    • 2010
  • A $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor powder with stuffed tridymite structure was synthesized by glycine-nitrate combustion method. The luminescence, formation process and microstructure of the phosphor powder were investigated by means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and photoluminescence spectroscopy (PL). The XRD patterns show that the as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor was an amorphous phase. However, a crystalline $SrAl_2O_4 $ phase was formed by calcining at $1200^{\circ}C$ for 4h. From the SEM analysis, also, it was found that the as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor was in irregular porous particles of about 50 ${\mu}m$, while the calcined phosphor was aggregated in spherical particles with radius of about 0.5 ${\mu}m$. The emission spectrum of as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor did not appear, due to the amorphous phase. However, the emission spectrum of the calcined phosphor was observed at 520 nm (2.384eV); it showed green emission peaking, in the range of 450~650 nm. The excitation spectrum of the $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor exhibits a maximum peak intensity at 360 nm (3.44eV) in the range of 250~480 nm. After the removal of the pulse Xe-lamp excitation (360 nm), also, the decay time for the emission spectrum was very slow, which shows the excellent longphosphorescent property of the phosphor, although the decay time decreased exponentially.

$SrAl_2O_4:Eu^{+2},\;Dy^{+3}$ 장잔광 형광체에 있어서 발광 및 장잔광특성에 미치는$B_2O_3$의 영향 (Effects of $ B_2O_3$ composition for the photoluminescence and after-glow charcteristics of $SrAl_2O_4:Eu^{+2},\;Dy^{+3}$ phosphors)

  • 이영기;엄기석
    • 한국결정성장학회지
    • /
    • 제14권3호
    • /
    • pp.123-128
    • /
    • 2004
  • 융제(flux)로서 $B_2O_3$의 농도를 0-10 wt%까지 변화시킨 $SrAl_2O_4$ : $Eu^{+2}$, $Dy^{+3}$계 장잔광 형광체를 고상반응법으로 합성한 후, $B_2O_3$의 첨가량에 따른 결정특성과 장잔광 축광재료로서 가장 중요한 발광 및 장잔광 특성을 조사하였다. $SrAl_2O_4$ : Eu$^{+2}$, $Dy^{+3}$계 형광체는 $B_2O_3$의 농도에 관계없이 520nm 파장을 최대 발광파장으로 하는 발광스펙트럼을 나타내었고, 3wt%의 $B_2O_3$ 농도에서 최대 발광강도를 나타내었다. 그리고 $SrAl_2O_4$ : Eu$^{+2}$, $Dy^{+3}$ 형광체의 잔광강도 역시 $B_2O_3$의 농도에 무관하게 시간에 따라 모든 시료에서 지수 함수적으로 감소하였으나, $B_2O_3$의 농도가 3wt%인 경우에 발광의 감쇠속도가 작은 뛰어난 장잔광특성을 나타내었다.