Morphology control of glassy carbon coating layer to additive ethylene glycol and phenolic resin (페놀수지 및 에틸렌 글리콜을 첨가한 유리질 카본 코팅층의 물성 제어)

  • Joo, Sang Hyun;Joo, Young Jun;Lee, Hyuk Jun;Sim, Young Jin;Park, Dong Jin;Cho, Kwang Youn
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.32 no.3
    • /
    • pp.89-95
    • /
    • 2022
  • In this study, glassy carbon coating was performed on the graphite using a phenolic resin and a curing agent was mixed with ethylene glycol as an additive to form the uniform surface. The phenolic resin was dried and cured under the environments of hot air, then converted into a glassy carbon layer by pyrolysis at 500~1,500℃. FTIR, XRD, SEM analysis, and density/porosity/contact angle measurement were performed for characterization of glassy carbon. The pyrolysis temperature for high-quality glassy carbon was optimized to be about 1,000℃. As the content of the additive increased, the effect of reducing surface defects on the coated surface, reduction of porosity, increase of contact angle, and increase of density were investigated in this study. The method of forming a glassy carbon coating layer through an additive is expected to be applicable to graphite coating and other fields.

Studies on the Extending of Plywood Adhesives used Foliage Powder (낙엽분말(落葉粉末)을 이용(利用)한 합판용(合板用) 접착제(接着劑)의 증량(增量)에 관(關)한 연구(硏究))

  • Kim, Jong-Man;Bark, Jong-Yeol;Lee, Phil-Woo
    • Journal of Korean Society of Forest Science
    • /
    • v.42 no.1
    • /
    • pp.83-100
    • /
    • 1979
  • It was planned and performed to study the possibility on the use of inexpensive and easily acquirable foliage powder, which processed by pulverizing after dried, instead of imported expensive wheat flour for the extending of plywood adhesives. Pine leaves of softwood trees, Poplar, Oak and Sycamore leaves of broad leaved species were selected and harvested to pulverize into the minute foliage powder. The harvested foliages from each selected species were pulverized into 40 mesh particles after dried at $100{\sim}105^{\circ}C$ condition during 24 hours in drying oven. To compare the extending effect of plywood adhesives with these foliage powders 100 mesh wheat flour using at current plywood industry was also prepared. Foliage powder and wheat flour were extended into 10, 20, 30, 50 and 100% to the urea and phenol formaldehyde resin. After plywoods were processed by the above extending method shear strength of extended plywoods were analyzed and discussed. The results obtained at this study are as follows: 1) Among 10% extensions of urea formaldehyde resin plywood, dry shear strength of plywood extended by wheat flours was the highest and that of non-extended plywood the next. Plywood extended with foliage powder showed the lowest dry shear strength. The order of dry shear strength of plywoods extended by foliage powder was that of Oak foliage powder extension, the best, that of Sycamore, that of Pine, and that of Poplar. 2) Among 20% extensions of urea formaldehyde resin plywood, plywood extended by wheat flour showed the highest dry shear strength, and the next was plywood by Poplar foliage powder. All these two showed higher dry shear strength than non-extension plywoods. Except Poplar, dry shear strength of foliage powder extension plywoods was bad, but the order of dry shear strength of plywoods extended by foliage powder was Pine, Poplar and Oak. 3) In the case of 30% extensions of urea formaldehyde resin plywood, dry shear strength of wheat flour extension was the highest and non-extension the next. Dry shear strength of foliage powder extension plywoods was poor with a rapid falling-off in strength. 4) Among 50% and 100% extensions of urea formaldehyde resin plywood, only wheat flour showed excellent dry shear strength. In the case of foliage powder extension, low dry shear strength showed at the 50% extension of Pine and Poplar, and plywoods of 50% extension of Oak foliage powder delaminated without measured strength. All plywoods of 100% foliage powder extension delaminated, and then shear strength were not measured. 5) Among wet shear strength of 10% extensions of urea formaldehyde resin plywood, wheat flour extension was the highest as in the case of dry shear strength, and non-extension plywood the next. Except Poplar foliage extension, all foliage powder extension plywoods showed low shear strength. 6) Wet shear strength of plywoods of 20% extension lowered in order of non-extension plywood, plywood of wheat flour extension and plywood of foliage powder extension, but other plywoods of foliage powder extension except plywoods of Poplar and Oak foliage powder extension delaminated. 7) Wet shear strength of 30% or more extension of urea formadehyde resin plywood were weakly measured only at 30% and 50% extension of wheat flour, and wet shear strength of plywoods extended by foliage powder were not measured because of delaminating. 8) Dry shear strength of phenol formaldehyde plywoods extended by 10% wheat flour was the best, and shear strength of plywoods extended by foliage powder were low, but the order was Oak, Poplar, and Pine. Plywood of Sycamore foliage powder extension delaminated. 9) In the case of 20% extensions of phenol formaldehyde resin, dry shear strength of plywood extended by wheat flour was the best, but plywood of Pine foliage powder extension the next, and the next order was Oak and Poplar foliage powder. Plywood of Sycamore foliage powder extension delaminated. 10) Among dry shear strength of 30% extensions of phenol formaldehyde plywood, that of Pine foliage powder extension was on the rise and more excellent than plywood of wheat flour extension, but Poplar and Oak showed the tendency of decreasing than the case of 20% extension. Plywood of Sycamore foliage powder extension delaminated. 11) While dry shear strength of 50% and 100% extension plywoods were excellent in the case of Pine foliage powder and wheat flour extension, that of hardwood such as Poplar, Oak, and Sycamore foliage powder extension were not measured because of delaminating. 12) As a filler the foliage powder extension of urea formaldehyde resin is possible up to 20% with Poplar foliage powder. And also as an extender for phenol formaldehyde resin, Pine foliage powder can be added up to the same amount as that in the case of wheat flour.

  • PDF

Studies on Manufacture of Hanji(Korean Paper) Sludge·Wood Particle Composite - I. Physical Properties of Hanji(Korean Paper)Sludge·Wood Particle Composite (한지(韓紙) 슬러지·목재(木材) 파티클 복합(複合)보드의 제조연구(製造硏究) - I. 한지(韓紙) 슬러지·목재(木材) 파티클 복합(複合)보드의 물리적(物理的) 성질(性質))

  • Lee, Phil-Woo;Lee, Hak-Lae;Son, Jung-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • v.29 no.2
    • /
    • pp.109-117
    • /
    • 2001
  • This research was carried out to develop the Hanji(Korean paper) sludge wood particle composite utilizing the waste sludges occurring from the making process of Hanji(Korean paper). In the research, four mixing ratios of white or black sludge to wood particle(10:90, 20:80, 30:70, and 40:60), three types of the resin adhesives(PMDI, urea and phenol resin) and three levels of the densities(0.60, 0.75 and 0.90) were designed to investigate the physical properties of Hanji(Korean paper) sludge wood particle composite. The linear expansion of Hanji(Korean paper) sludge wood particle composite was not always increased, compared to control boards. For thickness swelling, PMDI-bonded composites had the lowest value, and thickness swelling of composite was generally decreased with the increase of Hanji sludge. The water absorption of white sludge wood particle composite had no tendency, hut that of black sludge wood particle composite was decreased with an increase of mixing ratio of Hanji sludge.

  • PDF

Effects of High Temperature and Radiation on the Properties of Thermal, mechanical and Shielding Ability of Neutron Shielding Materials (고온 및 방사선이 중성자 차폐재의 열적, 역학적 및 차폐능 특성에 미치는 영향)

  • Jo, Su-Haeng;Hong, Sun-Seok;Jeong, Myeong-Su;Do, Jae-Beom;Park, Hyeon-Su
    • Korean Journal of Materials Research
    • /
    • v.9 no.4
    • /
    • pp.404-408
    • /
    • 1999
  • Effects of heating time and radiation under high temperature on the properties of thermal, mechanical and shielding ability of modified (KNS-101), hydrogenated bisphenol-A(KNS-201) type epoxy resin and phenol-novolac(KNS-301) type epoxy resin based neutron shielding materials that are used for shipping casks for radioactive material have been investigated. At early stages, the offset temperatures of KNS-101, KNS-201 and KNS-301 increased with the heating time under high temperature, but it was rarely affected by the heating time in the later stages. In addition, the thermal conductivities of KNS-101 and KNS-201 decreased with heating time, but that of KNS-301 increased with the heating time. On the contrary, the thermal expansion coefficients of neutron shielding materials decreased with heating time. At the high temperature, the tensile strength and flexural strength of the shielding materials decreased with heating time. On the contrary, the thermal expansion coefficients of neutron shielding materials decreased with heating time. At the high temperature, the tensile strength and flexural strength of the shielding materials of KNS-101 and KNS-301 increased with heating time, but those of KNS-201 decreased with heating time. The shielding ability of neutron shielding materials slightly increased with the radiation dose, and shielding abilities of shielding materials of KNS-101 and KNS-201 were affected to a more extent than that of KNS-301 by radiation dose under high temperature.

  • PDF

Organic Compounds in the Nak Dong River and Its Toxicity (낙동강 수질중 유기물질과 독성)

  • 류병호;심종환;최진택;조현철;정종순
    • Journal of Environmental Health Sciences
    • /
    • v.20 no.1
    • /
    • pp.39-53
    • /
    • 1994
  • This study aims to investigate organic compounds and its toxicity by Ames test and chromosomal aberration in the water of the Nak Dong River. Six sampling sites such as Goryung, Hagueun, Maelie, Duksan, Haedong and Myungiang were selected for these pur15oses. 200 l water samples were absorbed on XAD-2 resin columns (2.5X30cm), eluted with organic solvents mixture of acetone: cyclohexane and then dried under vacuum condition. The extracts from the XAD-2 resin was injected into GC/MS and 184 organic compounds were identified such as aldehydes, aromatic compounds, ketones, phenols, hydrocarbons, alcohols, carboxylic acids, alkanes and some unknowns. The US EPA priority pollutants such as naphthlene, bis(2-ethylhexyl)phthalate and other pollutants, 1,2-diethyl benzene, 1,2,3,4-tetrahydronaphthalene and cyclohexanol were detected in these samples. The concentration of chemical pollutants such as 1,2-diethyl benzene, nephthalene, 1,2,3,4-tetrahydronaphthalene, bis(2-ethylhexyl)phthalate and cyclohexanol were ranged into 1.228 $\mu$g/l, 298 $\mu$g/l, 30.191 $\mu$g/l, 1.147 $\mu$g/l and 2.839 $\mu$g/l, respectively. The mutagenic activity of XAD-2 extracts were tested on Salmonella typhimurium TA 98, TA 100, TA 1535 and TA 1537 and then exhibited strong mutagenic activity against S. typhimurium TA 98 and TA 100 in the presence of S$_9$. Amon them, bis(2-ethylhexyl)phtalate and 1,2-diethyl benzene showed the most strongest mutagenic activity against S. typhimurium TA 98 and TA 100 in the presence of S$_9$. On the other hands, chromosomal aberration of XAD-2 extracts in the human blood cells were not occurred by the sampling water at Goryung, Hagueun, Maelie and Duksan, Chromosomal aberration were also not occurred by the each concentration of 0.05, 0.1 amd 0.3 mg/l of each 1,2-diethyl benzol, bis(2-ethylhexyl)phthalate, naphthalene, phenol, cyclohexanol and benzothiazol test solution.

  • PDF

New Application of Clay Filler for Carbon/Carbon Composites and Improvement of Filler Effect by Clay Size Reduction

  • Jeong, Eui-Gyung;Kim, Jin-Hoon;Lee, Young-Seak
    • Carbon letters
    • /
    • v.11 no.4
    • /
    • pp.293-297
    • /
    • 2010
  • To investigate new potential application of a clay material for C/C composites, illite added C/C composites were prepared with various illite contents. The improvement of filler effect by illite size reduction was also investigated using wet ballmilling by evaluating illite/phenolic resin infiltration using bulk density and porosity measurements, chemical structural changes of the composites using XRD, and thermal oxidation stability in air of the composites using TGA. The size reduction of illite resulted in narrower particle size distribution and improved illite infiltration into carbon preform. And the resultant C/C composites prepared with illite had even more improved thermal oxidation stability in air, showing more increased IDTs up to $100^{\circ}C$, compared to those of the C/C composites with pristine illite, due to the SiC formation through carbothermal reduction between illite and carbon materials. The illite induced delay in oxidation of the illite-C/C composites was also observed and the delayed oxidation behavior was attributed to the layered structure of illite, which improved illite/phenol resin infiltration. Therefore, the potential use of illite as filler to improve oxidation stability of C/C composite can be promising. And the size reduction of illite can improve its effect on the desired properties of illite-C/C composites even more.

Effect of Aminosiloxane Modifier on Chemorheological Properties of Ortho-cresol Novolac Epoxy (Ortho-cresol Novolac형 에폭시의 화학레올로지 특성에 미치는 아민 개질제의 영향)

  • 김윤진;안병길;김우년;서광석;김환건;윤초규
    • Polymer(Korea)
    • /
    • v.26 no.1
    • /
    • pp.88-97
    • /
    • 2002
  • The effect of aminosiloxane modifier on the chemorheological properties of ortho-cresol novolac epoxy/phenol novelac/triphnylphosphine resin system was investigated aat different isothermal curing temperatures. By adding the aminosiloxane to the resin system, not only conversion rate and conversion were increased but also glass transition temperature was promoted. Critical conversion and gelation time obtained at the crossover point between storage and loss moduli were reduced and thus the viscosity was increased by the aminosiloxane. $C_1$ and $C_2$ in the WLF equation calculated from the glass transition temperature as a function of conversion and measured viscosity were found to vary with the curing temperature. By applying the change of glass transition temperature with conversion, $C_1$ and $C_2$ to WLF equation, it was possible to predict accurately the viscosity change with isothermal curing reaction.

Studies on Manufacture of Hanji(Korean Paper) Sludge·Wood Particle Composite II. Mechanical Properties of Hanji(Korean Paper) Sludge·Wood Particle Composite (한지(韓紙) 슬러지·목재(木材) 파티클 복합(複合)보드의 제조연구(製造研究) II. 한지(韓紙) 슬러지·목재(木材) 파티클 복합(複合)보드의 기계적(機械的) 성질(性質))

  • Lee, Phil-Woo;Lee, Hak-Lae;Son, Jungil;Kim, Hyun-Joong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.2
    • /
    • pp.121-127
    • /
    • 2002
  • This research was carried out to develop the Hanji(Korean paper) sludge·wood particle composite utilizing the waste sludges occurring from the making process of Hanji(Korean paper). At the research, four mixing ratios of white or black sludge to wood particle(10:90, 20:80, 30:70 and 40:60), three types of the resin adhesives(PMDI, urea and phenol resin) and three levels of the densities(0.60, 0.75 and 0.90) were designed to investigate the mechanical properties of Hanji(Korean paper) sludge·wood particle composite. In the white and black sludge·wood particle composites, bending properties(MOR, MOE) showed the decreasing tendency according to the increase of sludge additive, but it was clearly increased with the increase of specific gravity. Also tensile strength had the same tendency as in these bending properties. The internal bond strength of white sludge·wood particle composite had no tendency, but that of black sludge·wood particle composite was decreased as an increase of Hanji sludge additive.

Properties of Sawdust Board Made from Thinned Logs( I ) - Effect of Pressure and Press Time (간벌재로 제조된 톱밥보드의 물성(I) - 가압압력 및 열압시간의 영향 -)

  • 오승원
    • Journal of Korea Foresty Energy
    • /
    • v.21 no.2
    • /
    • pp.10-16
    • /
    • 2002
  • In this study, sawdust boards with a density 0.6g/$cm^2$, powder phenol resin containing 10% were made from thinned logs of Pinus densiflora, Larix leptolepis and Pinus koraiensis. Four levels of the pressure and press time were designed to investigate the effect on the properties of sawdust boards. Thickness swelling and water absorption were increased as press time was decreased. The condition of 3-stage pressure for lower thickness swelling and water absorption of board was 40$\rightarrow$30$\rightarrow$20kgf/$cm^2$. Bending strength and brinell hardness were decreased as press time was decreased. But there have no change with pressing pressure. These results indicated that properties of sawdust board were affected by press time.

  • PDF

Effect of Surface-Modified Carbon Fiber on the Mechanical Properties of Carbon/Epoxy Composite for Bipolar Plate of PEMFC (표면처리 탄소섬유가 PEMFC용 탄소/에폭시 복합재료 분리판의 기계적 강도에 미치는 영향)

  • LEE, HONGKI;HAN, KYEONGSIK
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.31 no.1
    • /
    • pp.49-56
    • /
    • 2020
  • Epoxy/carbon composite was used to prepare a bipolar plate for polymer electrolyte membrane fuel cell (PEMFC). Phenol novolac-type epoxy and diglycidyl ether of bisphenol A (DGEBA)-type epoxy mixture was used as a matrix and graphite powder, carbon fiber (CF) and graphite fiber (GF) were used as carbon materials. In order to improve the mechanical properties of the bipolar plate, surface-modified CF was incorporated into the epoxy/carbon composite. To determine the cure temperature of the epoxy mixture, differential scanning calorimetry (DSC) analysis was performed and the data were introduced to Kissinger equation in order to get reaction activation energy and pre-exponential factor. Tensile and flexural strength was obtained by using universal testing machine (UTM). The surface morphology of the fractured specimen and the interfacial morphology between epoxy matrix and CF or GF were observed by a scanning electron microscopy (SEM).