A Study on the Desulfurization of Petroleum Cokes by Microwave Heating (마이크로웨이브 가열에 의한 석유 코크스의 탈황에 관한 연구)

  • Park, Min-Gyu;Kang, Tae-Won
    • Clean Technology
    • /
    • v.8 no.1
    • /
    • pp.11-17
    • /
    • 2002
  • Petcokes is the final product obtained from a refinery process. This petcokes includes high percentage of inorganic and sulfur compounds. Currently, the petcokes produced from domestic refinery plants include more than 6% of sulfur. To use petcokes as valuable raw materials, the weight percentage of sulfur must be lower than 2% of sulfur. Solvent extraction, thermal desulfurization, and hydro-desulfurization have been used to remove the sulfur. In this study, we attempted new approach to remove the sulfur introducing microwave energy. Microwave increase the reaction rates by providing the fast heating and disconnecting the bonding structure of the molecules. The experiments of microwave thermal desulfurization and microwave plus hydrogen gas were carried out to remove the sulfur. We obtained 68.3% of sulfur removal rate with the 2 hours of reaction time and 1835 W of microwave powder. In the experiment of microwave with hydrogen gas, we obtained 86.4% of sulfur removal rate with the 1.5 hours of reaction time and 1835 W of microwave power. If we increase reaction time or decrease the particle size of petcokes, we expect more than 90% of sulfur removal.

  • PDF

Effect of V2O3 and CaO Concentrations on the Viscosity of 5-Component Petcoke Slag (V2O3와 CaO의 농도에 따른 5-성분계 석유코크스 슬래그의 점도 변화)

  • Yang, Yoonjung;Oh, Myongsook S.
    • Applied Chemistry for Engineering
    • /
    • v.31 no.6
    • /
    • pp.688-696
    • /
    • 2020
  • Petroleum coke (petcoke) is widely used, next to coal, as a gasification feedstock. In gasification processes, the viscosity of the ash and the formation of crystalline phases must be understood to ensure the continuous removal of slag. This study investigates the effect of CaO and V2O3 on petcoke slag viscosity. The viscosity of the molten slag was measured in the temperature range of 1100~1600 ℃ while varying the concentration of each component. The crystalline phases formed in a cooled slag were examined. The most slag samples tested in this study exhibited crystalline slag behavior. The increased CaO concentration resulted in a lower viscosity and a lower Tcv. The viscosity behavior changed from the glassy to crystalline slag and also showed a higher Tcv as the concentration of V2O3 increases. Most slag samples showed different crystalline phases from top to bottom. Anorthites and Ca-V phases were observed in the top and middle section, while the bottom section mainly showed V2O3 and anorthite. The vanadium in the ash forms Ca-V and V-Fe phases and also remains in molten slag. A low melting Ca-V phase can contribute to lowering the viscosity.