  • In this studies, structural, dielectrical piezoelectrical properties and temperature stability of 0.05Pb(Pb($Mg_{1/3}Nb_{2/3}$)$O_3$+ 0.95Pb($Zr_{0.53}Tio_{0.47}$)$O_3$+$\alpha$[wt%] $Cr_2O_3$ piezoelectric ceramics fabricated by the Hot-Press method were investigated. And Poisson ratios of the specimens were measured in order to see that they can be used as the substrates for energy-trapped devices. The specimens of which Poisson ratio was more than 3/1 had the $\alpha$ range 0.3~0.75, and piezoelectric properties were degraded in the range $\alpha$$\geq$0.75, and temperature stability was good in the $\alpha$ range 0.5~0.75. Accordingly, the optimal point of $Cr_2O_3$ additive weight is sure to be in the vicinity of 0.5[wt%].

첨가제에 의한 0.05PAN-0.95PZT계 세라믹의 유전 특성에 관한 연구 (A study on the dielectric characteristics of 0.05PAN-0.85PZT ceramics with additive)

  • 김현철;신혜경;김진섭;윤현상;배선기
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1661-1663
    • /
    • 2000
  • This study was to measure the dielectric characteristics of 0.05Pb($Al_{0.5}Nb_{0.5}$)-0.95Pb($Zr_{0.52}Ti_{0.48})O_3$[PAN-PZT] system ceramics according to the variation of $Cr_{2}O_3$, $Fe_{2}O_3$ addition amount. 0.0$\sim$1.2[wt%] and according to sintering temperature after creating the specimens with a general sintering way. The results of this study were summarized as follows : the dielectric constant at 20[$^{\circ}C$] reduced dy increasing additive on the whole. The dielectric loss was minimum value of 12.77[%], sintered at 1200[$^{\circ}C$], dopped with $Cr_{2}O_3$ 0.3[wt%] and minimum value of 10.89[%], sintered at 1200[$^{\circ}C$], dopped with $Fe_{2}O_3$ 0.6[wt%]. The variation rate of dielectric constant according to the change of frequency was decreased slowly by increasing frequency. The temperature coefficient of capacitance turned out increasing the stability of the temperature, decreased $Cr_{2}O_3$ 0.3wt% showed its minimum value 0.59[%/$^{\circ}C$], the maximum value 0.9[%/$^{\circ}C$] with $Cr_{2}O_3$ 3wt%.

  • PDF

첨가제에 의한 0.05PAN-0.95PZT계 세라믹의 압전특성에 관한 연구 (A study on the piezoelectric characteristics of 0.05PAN-0.95PZT ceramics with additive)

  • 김현철;허석현;김진섭;임인호;배선기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.419-422
    • /
    • 2000
  • This paper was to measure the structure, piezoelectric properties of 0.05Pb($A1_{0.5}$$Nb_{0.5}$)-0.95Pb($Zr_{0.52}$$Ti_{0.48}$)$O_3$ ceramics dopped with additive after creating the specimens with a general method. It is shown that X-ray diffraction pattern variation of lines (200) have tendency to move in simple peak by addition of additive. According to the increase of $Cr_2$$O_3$, tetragonality hardly have variation, according to the increase of $Fe_2$$O_3$, tetragonality decreased on the whole. According to dopping with $Cr_2$$O_3$ and $Fe_2$$O_3$, electromechanical factor(kp) largely increased, in case of sintering at $1200^{\circ}C$ kp was maximum value of 40.04[%] at $Cr_2$$O_3$ 0.3wt%, and maximum value of kp 42.9 [%] at $Fe_2$$O_3$, 0.9wt%. In case of sintering at 120$0^{\circ}C$, mechanical duality factor(Qm) was maximum value of Qm 268.8 at $Cr_2$$O_3$, 0.9 wt%.

  • PDF

PAN-PZT계 세라믹스를 이용한 적층형압전변압기의 특성 (Characteristics of A Multilayer Piezoelectric Transformer Using PAN-PZT Ceramics)

  • 박타리;이동균;최지원;신용덕;김현재;고태국;윤석진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.143-146
    • /
    • 2002
  • The characteristics of a multilayer piezoelectric transformer were investigated using 0.05Pb(A $l_{0.5}$N $b_{0.5}$) $O_3$-0.95Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$+0.9wt%N $b_2$ $O_{5}$+0.5wt%Mn $O_2$+0.04wt% $V_2$ $O_{5}$ ceramics. The multilayer piezoelectric trans formers were developed for voltage step-up. The multilayer ceramic technology was applied in piezoelectric transformer. The electrical characteristics of the piezoelectric transformer (33x8.5x1mm) has the efficiency of above 85%, step-up ratio of 70 under the 130 kΩ load, and driving frequency of 93.5kHz, respectively.ctively.y.y.

  • PDF

$Pb(Mn_{1/3}Sb_{2/3})O_3-Pb(Zr_{0.52}Ti_{0.48})O_3$계 세라믹스의 전기적 특성과 미세구조에 미치는 ZnO 첨가영향 (The Effect of ZnO Addition on the Electric Properties and Microstructure of $Pb(Mn_{1/3}Sb_{2/3})O_3-Pb(Zr_{0.52}Ti_{0.48})O_3$Ceramics)

  • 김민재;최성철
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1108-1114
    • /
    • 1999
  • Microstructure and electrical properties of ZnO-doped (0-5 mol%) 0.05 Pb(Mn1/3Sb2/3)O3-0.95 PZT ceramics were investigated. Sintering temperature was decreased to 100$0^{\circ}C$ due to eutetic reaction between PbO and ZnO. Grain-size increased up to adding 1mol% ZnO and then decreased. Compositions of grain and grain-boundary were investigated by WDS. Lattice parameter was decreased with ZnO addition. Density increased with ZnO addition and reached to the maximum of 7.84(g/cm2) at 2 mol% ZnO. The effect of ZnO on electrical properties of PMS-PZT was investigated. At 3mol% ZnO addition electromechanical coupling factor(kp) was about 50% and relative dielectric constant($\varepsilon$33/$\varepsilon$0) was 997 Mechanical quality factor(Qm) decreased with ZnO addition. Lattice parameters and tetragonality(c/a) were measured to investigate relationship between the electric properties and substitution of Zn2+. At 3 mol% ZnO tetragonality was maximiged at c/a=1.0035 Curie temperature (Tc) decreased slightly with ZnO addition.

  • PDF

Cr+Fe 첨가시 PAN-PZT계 세라믹의 전기적 특성에 미치는 영향 (The effect on the electric characteristics of PAN-PZT ceramics dopped with Cr+Fe)

  • 신혜경;김현철;허석현;김진섭;배선기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.251-254
    • /
    • 2000
  • This paper was to measure the structure, electric characteristics of 0.05Pb($(Al_{0.5}Nb_{0.5})$) - 0.95Pb$(Zr_{0.52}Ti_{0.48})O_3$ ceramics dopped with Cr+Fe. The results of this paper were gotten such as follows; The dielectric constants were decreased with Cr+Fe. The dielectric loss was minimum value of 1.008[%], dopped with Cr+Fe O.9[wt%] at 1200[$^{\circ}C$], In case of sintering at 1150[$^{\circ}C$], electromechanical factodkp) was maximum value of kp 42.73[%], at Cr+Fe 0.9[wt%]. The mechanical quality factor(Qm) was maximum value at Cr+Fe 1.2 [wt%], Also, in case of dopped with Cr+Fe, it make a improvement in temperature coefficient of resonant frequency at 0.3[wt%], 1150[$^{\circ}C$].

  • PDF

Tripod Polishing을 이용한 불균질 재료의 TEM 시편준비 방법과 미세조직 관찰 (TEM Sample Preparation of Heterogeneous Materials by Tripod Polishing and Their Microstructures)

  • 김연욱;조명주
    • Applied Microscopy
    • /
    • 제34권2호
    • /
    • pp.95-102
    • /
    • 2004
  • 본 실험에서는 tripod polishing 방법을 이용하여 Pd/GaN/Sapphire 박막, PZT/MgO/Si 박막, 304 stainless steel 분말, $Mo_5Si_3/Mo_2B$ diffusion couple의 매우 다양한 물성이 포함된 불균질 재료의 TEM 시편을 제작하고 분석하였다. Tripod polishing을 사용하여 시편을 준비하면 시편의 종류에 관계없이 시편의 선단부에 매우 광범위한 전자빔 투과 영역을 지닌 TEM 시편을 얻을 수 있었으며, Pd/GaN/Sapphire 박막, PZT/MgO/Si 박막과 같이 기판이 경한 반도체 재료의 경우에는 연마 정도가 균일하며 연마과정 동안 오염이 심하지 않기 때문에 ion milling으로 cleaning 없이 TEM 관찰이 가능하다. 한편 304 stainless steel 분말과 같은 금속재료의 경우 짧은 시간의 ion milling 은 시편의 오염 제거에 도움된다. $Mo_5Si_3/Mo_2B$ diffusion couple에 형성된 실리사이드는 큰 취성 때문에 polishing 동안 시편이 깨지는 현상으로 전자가 투과할 수 있을 정도의 연마가 불가능하여 1시간 정도 ion milling 연마가 필요하다. Tripod polishing으로 TEM 시편을 준비하면 분석하고자 하는 지역을 정확하고도 넓게 연마할 수 있다. 또한 비교적 짧은 시간 내에 ion milling 없이 TEM 시편을 제작할 수 있기 때문에 ion milling에서 유발되는 여러 가지 문제점들을 해결할 수 있는 장점이 있었다. 그러나 tripod polishing은 전부 수작업으로 시편을 준비하기 때문에 시편을 제작하는 과정 동안 매우 세심한 주의가 요구되며 제작자의 숙련도와 경험을 필요로 하는 단점이 있다.

PMWN-PZT계 압전세라믹의 poling에 의한 유전율의 변화 특성 (The Trends of Dielectric Constant Variation by Poling of PMWN-PZT Geramics)

  • 홍종국;이종섭;채홍인;정수현;임기조
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.494-496
    • /
    • 2000
  • The properties of piezoelectric and dielectric for 0.05Pb$(Mn_{0.4}W_{0.2}Nb_{0.4})O_3$ - $0.95PbZr_{x}Ti_{1-x}O_{3}$ compositions have been investigated. In the composition of 0.05Pb$(Mn_{0.4}W_{0.2}Nb_{0.4})O_3$-$0.95PbZr_{0.51}Ti_{0.49}O_{3}$, the values of $k_p$ and ${\varepsilon_{33}}^T/{\varepsilon}_0$ are maximized, but $Q_m$ was minimized ($k_p$=56.5[%], $Q_m$=1130, $d_{33}$=258[pC/N], ${\varepsilon_{33}}^T/{\varepsilon}_0$=1170). The grain size was suppressed and the uniformity of gram was improved at the $1100[^{\circ}C]$. Dielectric constant increase at the Ti rich, but decrease at the Zr rich after poling. Because the dielectric constant after poling is determined by compromising effects between dipole switching and electostriction inducing stress(dielectric constant increasing factor) and dipole rotation to the poling direction (dielectric constant decreasing factor).

  • PDF

PMWN-PZT계 압전세라믹의 압전 및 유전 특성 (Characteristics of Piezoelectric and Dielectric of PMWN-PZT Ceramics)

  • 홍종국;이종섭;채홍인;윤만순;정수현;임기조
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.188-191
    • /
    • 2000
  • The properties of piezoelectric and dielectric for 0.05Pb(Mn$\_$0.4/W$\_$0.2/Nb$\_$0.4/)O$_3$ - 0.95PbZr$\_$x/Ti$\_$1-x/O$_3$ compositions have been investigated. In the composition of 0.05Pb(Mn$\_$0.4/W$\_$0.2/Nb$\_$0.4/)O$_3$ - 0.95PbZr$\_$0.51/Ti$\_$0.49/O$_3$, the values of k$\_$p/ and $\varepsilon$$\_$33/$\^$T// $\varepsilon$$\_$0/ are maximized, but Q$\_$m/ was minimized (k$\_$p/=56.5[%], Q$\_$m/=1130, d$\_$33/=258[pC/N], $\varepsilon$$\_$33/$\^$T// $\varepsilon$$\_$0/=1170). The grain size was suppressed and the uniformity of grain was improved at the 1100[˚C]. Also, we can see the dielectric constants variations between the before poling and after poling. This effect results from the effect(increase element of dielectric constants) between dipole switching and electrostriction inducing stress and dipole direction to the poling orientation(decrease element of dielectric constants). At x=0.51, we can find MPB(morphotropic phase boundary).

  • PDF

$MnO_2$첨가에 따른 PMN-PT계 완화형 강유전체에서의 압전특성 (Piezoelectric Properties of PMN-PT Relaxor Ferroelectrics with $MnO_2$Addition)

  • 박재환;박주영;박재관;김병국;김윤호
    • 한국세라믹학회지
    • /
    • 제37권10호
    • /
    • pp.1021-1024
    • /
    • 2000
  • PMN-PT계 완화형 강유전체에서 MnO$_2$첨가가 압전물성에 미치는 영향을 -40~10$0^{\circ}C$의 온도범위에 걸쳐 조사하였다. 각각의 시편들은 -4$0^{\circ}C$에서 1.0kV/mm의 전계를 10분간 가하여 분극처리를 한 후 승온하면서 공진 반공진법에 의해 압전물성을 측정하였다. 0.9MN-0.1PT계의 경우 MnO$_2$를 첨가하였을 때 $K_{p}$ 는 거의 유지되면서도 Q$_{m}$ 값이 큰 폭으로 상승하였는데, 0.5wt% MnO$_2$첨가의 경우 -4$0^{\circ}C$에서 95로부터 480으로 증가하였다. 일반 강유전체인 PZT계에 대한 MnO$_2$의 첨가효과와 비교할 때 PMN계 완화형 강유전체에서도 동일한 경향성을 보임을 확인하였다.

  • PDF