Journal of the Korean Applied Science and Technology
/
v.19
no.2
/
pp.117-122
/
2002
A silicone softner (SS-5), a permanent press (PP) finish, was prepared by blending silicone oil KF-96 (as a lubricating component) and beef tallow hardened oil (as a softening component) which was synthesized from fatty polyamide salts. The prepared SS-5 and the PP finishing resin were applied to PP finishing cotton cloth and P/C gingham sample by one-bath method. The properties such as crease recovery, tear strength, and bending resistance were tested. The samples treated with SS-5 and PP finishing resin showed improved properties when comparing with the untreated ones, with the ones treated only with PP finishing resin, with ones treated with commercial PP finishing softners and PP finishing resin. The grades of fabric samples treated with 3% SS-5 were fifth grade in the bending resistance test.
Journal of the Korean Applied Science and Technology
/
v.15
no.1
/
pp.1-7
/
1998
Lubricating softner(SOS-2) for permanent press(PP) finish was prepared by blending water, beef tallow hardened oil for improving softness, and the emulsion which was synthesized from N-hexadecanoyl-N,N'-bis(2-hexadecamidoethyl)amine as a softening component and silicone oil KF-96 as a lubricating component. The prepared SOS-2 and the PP finishing resin were applied to PP finishing cotton broad cloth and P/C gingham samples using one bath method. The properties such as tear strength, crease recovery, bending resistance test were tested. The samples treated with SOS-2 and PP finishing resin have improved properties, compared with nontreated samples, those treated only with PP finishing resin, those treated with commercial PP finishing softners and PP finishing resin.
Park, Chang-Hwan;Kim, Seung-Jin;Kim, Young-Geun;Park, Hong-Soo
Journal of the Korean Applied Science and Technology
/
v.12
no.1
/
pp.29-34
/
1995
Silicone softner(SSN-3) for permanent press(PP) finish was prepared by blending beef tallow hardened oil for Improving softness, water, the emulsion, which was synthesized from pentaerythritol monostearate as a softening component and silicone oil KF-96 as a lubricating component. The prepared SSN-3 and the PP finishing resin were applied to PP finishing cotton broad cloth and P/C gingham samples using one bath method. The properties such as crease recovery, tear strength, bending resistance test were tested. The samples treated with SSN-3 and PP finishing resin have improved properties, compared with nontreated samples, those treated only with PP finishing resin, those treated with commercial PP finishing softners and PP finishing resin. Also from the bending resistance test, the two kinds of fabric samples treated with SSN-3 of 3% showed grade 5 and these were good enough in feeling.
Proceedings of the Korean Society of Dyers and Finishers Conference
/
2011.03a
/
pp.91-91
/
2011
폴리프로필렌(PP)은 고결정성 범용수지로서 염색성, 내열성, 촉감 등의 문제로 의류용 소재로는 부적합하여 초기에는 카펫용 섬유로서 가염형 폴리프로필렌 섬유가 상업화 되었지만 성공하지는 못하였다. 그 후, 섬유 산업도 의류용 외의 산업자재, 생활 자재 분야 등이 성장함에 따라, 폴리프로필렌 섬유의 수요가 확대되었다. 최근들어 스포츠 액티브 의류가 일반의류 트렌드로 들어오면서 기능성 섬유가 요구되고 이 분위기에 맞춰 다시 한번 폴리프로필렌 섬유의 의류화가 요구되는 시점이 되었으며 섬유중 에너지 소비량이 가장 적고, 쉽게 재용해할 수 있으며 소각시 유해 가스발생량이 매우 적은 특징등이 있기 때문에 지구 환경보호의 입장에서 폴리프로필렌 섬유가 재검토되고 있다. 이번 실험은 분산염료를 이용하여 농도별, 온도별, 시간별, 후처리시 시간과 온도의 변화로 가염 PP/PET 섬유의 염색특성을 알아보기 위해 실험 진행하였다. 실험에 사용되는 시약은 1급으로, $CH_3COOH$, NaOH, $Na_2S_2O_4$이며, 조제는 분산제, 정련제를 사용하였다. 먼저 온도별 실험에서 $40^{\circ}C$에서 승온하여 각각 $100^{\circ}C$, $110^{\circ}C$, $120^{\circ}C$, $130^{\circ}C$에서 온도에 따라 염색되는 정도를 알아보았다. 가장 높은 흡진을 보이는 온도에서 각각 40min, 50min, 60min, 70min 염색 유지시간 실험을 하여 염색이 안정되는 시간을 측정하였다. 위의 실험 결과 최적의 조건으로 염색농도에 따른 Build up 실험을 진행하였다. 가염 PP/PET 섬유는 일반 Polyester처럼 $120{\sim}130^{\circ}C$에서 가장 높은 염색농도 값(K/S)을 보인다. 또한 $130^{\circ}C$에서의 유지시간에서는 50 min 이상 진행시 더 이상의 흡진이 없거나, 염료의 탈락이 있음을 알수 있다. Build up 실험에서는 8.0%까지 실험하였지만, 결과는 그 이상농도를 사용하여도 염색은 가능함을 알 수 있었다. 후처리에 대한 실험에서 염료에 따라 차이가 있지만 크게 영향을 받지 않는 것으로 보이며, 제품성 평가 결과를 보면 후처리를 했을 경우 견뢰도가 우수한 것을 알 수 있었다.
Polypropylene(PP) is a textile material with various functions such as eco-friendliness, lightness, and elasticity. Although most synthetic fibers can be dyed and finished, but original PP is difficult to dye or finish due to its extremely hydrophobic properties, so its application expansion is limited. In order to solve this problem, dyeable PP was developed, and various researches on textiles for clothing such as mass production technology, fine fiberization and performance improvement are in progress. Plasma treatment is a processing method for modifying the surface of fabrics, and has effects such as hydrophilization, deepening color, improving adhesion, and surface polymerization. In this study, plasma treatment was applied to study changes in hydrophilization properties of dyeable PP, surface changes before and after plasma treatment and performance according to hydrophilization.
Journal of the Korean Applied Science and Technology
/
v.21
no.3
/
pp.191-196
/
2004
An emulsion of octadecamidoethylaminoethyl dodecate (which provides softness) and an emulsion silicone oil KF-96 (which provides lubricity) were separately synthesized. Then PP finishing softeners (SSA-7) was prepared by blending of the synthesized emulsions with beef tallow hardened oil (a softness improving agent). PP finishing treatment was carried out with the prepared SSA-7 and PP finishing resin by a one bath method, and several physical properties were tested. As a result, crease recovery, tear strength, softness, lubricity, and bending resistance were all good, indicating that the prepared SSA-7 is a good PP finishing softener.
An attempt was made to synthesize an ammonia adsorbent by the photo-induced grafting of styrene (St) onto polypropylene (PP) nonwoven using benzoin ethyl ether (BEE) as a photosensitizer with urea and trimethylol propane triacrylate in methanol medium. As styrene concentration was increased, the graft yield was increased. It was also found that the graft yield increased with reaction time. The polypropylene grafted with styrene (PP-g-St) was sulfonated by chlorosulfonic acid in dichloroethane and complexed with several metal ion, such as $cO^{+2}$, $nI^{+2}$, $cU^{+2}$, $Zn^{+2}$. The amount of ammonia gas adsorbed by these sample was dependent on the degree of sulfonation, adsorption time, and ammonia gas pressure. The adsorption capacity of ammonia gas by the sulfonated PP-g-St(SPP-g-St) nonwoven with 4. 25 mmol $H^+$/g was 6.61 mmol/g. Metal ion complexed SPP-g-St nonwovens had higher adsorption capacity than SPP-g-St nonwoven and the $Co^{+2}$ complexed SPP-g-St showed 9.90 mmol $NH_3$/g, which was much higher than that of active carbon or silica gel.
Proceedings of the Korea Concrete Institute Conference
/
2008.04a
/
pp.865-868
/
2008
As a part of a series of study, this study reviewed the fire proof characteristics of high performance concrete RC column members using non-stripping form that accompanied metal lath lateral confinement to prevent spalling of high performance concrete which is increasingly used recently, and the results are as follows. Flow and air amount both satisfied target range, and compressive strength, over 80MPa at age 28 days, showed high strength range. As for spalling characteristics, in the case of plain in which no fiber is mixed, severe spalling occurred, and in the case of 0.05% nylon("NY" hereinafter)+polypropylene("PP" hereinafter) fiber mixture, only surface area experienced partial spalling. Regarding non-stripping form changes, both non-stripping 25-20 and non-stripping 50-20 experienced spalling at finish material area, and non-stripping 50-20 showed better spalling proof performance than non-stripping 25-20. In the case of non-stripping 50-40, spalling was prevented, and while mass reduction rate was less than 10%, its temperature hysteresis showed the most excellent fire proof performance with base metal surface area maximum temperature $376.1^{\circ}C$.
D. K. LEE, J. S. LEE, B. J. LEE, H. S. LEE, Y. J. KIM, S. B. PARK, J. P. JOO. Plantar foot pressure analysis during golf swing motion using plantar foot pressure measurement system. Korean Journal of Sport Biomechanics, Vol. 15, No. 1, pp. 75-89, 2005. In this study, weight carrying pattern analysis and comparison method of four foot region were suggested. We used three types of club(driver, iron7, pitching wedge). This analysis method can compare between top class golfer and beginner. And the comparison data can be used to correct the swing pose of trainee. If motion analysis system, which can measure the swing speed and instantaneous acceleration at the point of hitting a ball, is combined with this plantar foot force analysis method, new design development of golf shoes to increase comfort and ball flight distance will be available. 1. Address acting, forces concentrated in rare foot regions and lateral foot of right foot. Back swing top acting, relatively high force occurred in medial forefoot region of left foot and forefoot region of right foot. Impact acting, high force value observed in the lateral rarefoot region of left foot and medial forefoot region of right foot. Finish acting, force concentration observed on the lateral region and rarefoot region of left foot. 2. Forces were increased in address of right foot with clubs length increased. All clubs, back swing top acting, high force value observed in the lateral forefoot region of right foot. All clubs, in impact, high force value observed in the lateral rarefoot region of left foot and medial forefoot region of right foot. Finish acting, force concentration observed on the rarefoot region in driver and lateral foot region in iron on left foot. 3. Right foot forces distribution were increased in address, back swing top and left foot force distribution were increased in impact, finnish
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.