An Investigation on Estimation of the Compressive strength by P Type Schmidt Hammer (P형 슈미트햄머에 의한 압축강도 추정에 관한 검토)

  • 김기정;이용성;이백수;윤기원;최영화;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.11-15
    • /
    • 2002
  • This study is intended to analyze the relationship between the rebound value of P type schmidt hammer and the compressive strength for a quality control of concrete. According to the results, the compressive strength of standard curing specimen increases in proportion to age, but that of air curing specimen hardly increases after 28 days. The rebound value of P type schmidt hammer, however, increases due to carbonation of concrete in air curing specimen. The correlativity between the rebound value and the compressive strength is very favorable in the case of standard curing specimen, but drops remarkably in the case of air curing specimen. Thus, as application of age coefficient is required for exact estimation of the compressive strength, the age coefficient is derived from this study. The age coefficient of P type schmidt hammer is higher at the age of 3 and 7days, and drops significantly, compared with the age of 28days. And it is lower before 28days than that of N type schmidt hammer suggested in Japan, and shows the similar tendency after 28days.

  • PDF

Influence of Aggregate on the Rebound Value of P Type Schmidt Hammer (P형 슈미트햄머의 반발도에 미치는 골재종류의 영향)

  • 김태현;김기정;이용성;이백수;윤기원;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.239-242
    • /
    • 2002
  • This study is intended to investigate the relationship between rebound value of P type schmidt hammer and the compressive strength with various aggregates, and a series of experiments about early strength quality control by P type schmidt hammer was performed. According to the results, the compressive strength of concrete using basalt and limestone aggregate is higher by 3% and lower by 4% than that of concrete using granite aggregate respectively. Concrete using basalt and lime stone aggregate show high rebound value in vertical strike. Estimation of the compressive strength does not show differences in horizontal strike, but the compressive strength is estimated high in order of granite, basalt and limestone aggregate in vertical strike. A good correlation between the rebound value of schmidt hammer and the compressive strength is confirmed regardless of aggregate types, so it could be possible to control the quality of concrete by P type schmidt hammer test when basalt and limestone aggregates are used at the same time.

  • PDF

Investigation on the Validities of Removal Time of the Forms Considering Rebound Number of P Type Shumidt Hammer (P형 슈미트 햄머의 반발도를 이용한 거푸집 탈형시기의 결정에 관한 타당성 검토)

  • 전충근;김상우;신병호;황인성;신병철;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.909-912
    • /
    • 2001
  • This paper presents the validities of the removal time of side forms considering the relationship between rebound number of P type schmidt hammer and compressive strength. According to test results, compressive strength of 40% of W/C at 12 hours shows 16kgf/$cm^{2}$ and 50% of W/C at 15 hours, 13kgf/$cm^{2}$. Rebound number at 9 hours after casting shows 13 and 9 (W/C 40% and W/C 50%). According to the regression analysis, rebound number of P type schmidt hammer to gain 50kgf/$cm^{2}$ of is estimated 20.1. It is thought that desirable rebound number of P type schmidt hammer to gain 50kgf/$cm^{2}$ is determined 25 considering safety factor.

  • PDF

A Study on the Non Destructive Test by P Type Schmidt Hammer for Early Quality Control of Concrete (콘크리트의 초기강도품질관리를 위한 P형 슈미트햄머법 비파괴시험에 관한 연구)

  • 김기정;신병호;이용성;윤기원;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.157-162
    • /
    • 2002
  • This study is intended to present a reference data for effective quality control of concrete through comparing the rebound value of P type schmidt hammer with the compressive strength with variation of mix proportion and curing condition. According to the results, the air-curing specimen shows the higher rebound value than standard specimen except high strength in the whole. Also the vertical stroke shows higher rebound value than horizontal stroke in standard specimen, however, the rebound value of the two does not show prominent difference in air-curing specimen. The estimation equation of compressive strength derived from this experiment estimates the compressive strength more largely than the estimation equation in P type schmidt hammer manual. Therefore it is thought that the new estimation equation that fits our condition will have to be presented.

  • PDF

Determination of Removal Time of the Forms with the Strength Development of High Strength Concrete at Early Age (고강도 콘크리트의 초기강도 발현에 따른 거푸집 탈형시기의 결정)

  • 김은호;김영진;한민철;신병철;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.05a
    • /
    • pp.99-102
    • /
    • 2003
  • This study discusses the determination of removal time of forms with early strength development in high strength concrete. According to the results, as W/B increases by 10%, the setting time is shortened by about 2 hours. The time when compressive strength of 8 MPa is gained is about 20 hours. Bond strength between form and concrete is highest around final setting time, but decreases drastically after that. Amount of concrete sticking on the form is large before setting, but after that, it is little. The rebound value of P type schmidt hammer is measured faster by 2-3 hours than compressive strength. It is also confirmed that the removal of forms is possible when the rebound value of P type schmidt hammer is more than 34

  • PDF

Influence of Material Factors on Estimation of Compressive Strength of Concrete by P Type Schmidt Rammer (P형 슈미트해머에 의한 콘크리트의 압축강도 추정에 미치는 재료요인의 영향)

  • Han Cheon-Goo;Lee Yong-Sung;Han Mn-Cheol
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.4 s.82
    • /
    • pp.459-465
    • /
    • 2004
  • The present paper is intended to investigate the influence of materials such as cement, mineral admixture and aggregate, on the estimation of compressive strength by P type schmidt hammer. According to the results, the materials of concrete, such as the types of cement, the replacing ratio of mineral admixture, the kinds and maximum size of aggregate, hardly influence on non-destructive test by P type schmidt hammer except for alumina cement, hence, P type schmidt can be applicable to most of the concrete with a wide range. Since the correlativity between the rebound value of P type schmidt hammer and compressive strength is very favorable(above coefficient of correlation 0.96) regardless of materials, it is considered that compressive strength can be estimated comparatively exactly by P type schmidt hammer. The estimating formula of compressive strength by rebound value are derived from this experiment as following. $\cdot$Horizontal strike : Fc = 0.765RH - 5.74 (R=0.965) $\cdot$ Vertical strike Fc = 0.793RV - 8.66 (R=0.959)

An Experimental Application of Concrete Using TEA in Construction Field (트리에탄올아민을 사용한 콘크리트의 현장 적용 실험)

  • Hwang, Yin-Seong;Lim, Choon-Goun;Kim, Seong-Soo;Han, Cheon -Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.11a
    • /
    • pp.23-26
    • /
    • 2003
  • This study is intended to investigate the properties of early strength development by application of TEA to the field. According to the results, when TEA is added, fluidity is almost same to base concrete, and increases upto aimed slump after field flowing. Setting time does not differ in the case of base and TEA, but retarded after flowing. The time when compressive strength gains 5 MPa, which side form can be removed, is 23 hours, and so the removal time is shortened by I hours in comparison with plain concrete. But compressive strength is almost same to that of plain concrete at 28 days. The rebound value of P type schmidt hammer show similar tendency to compressive strength, and the rebound value of structure is higher than that of standard curing specimen due to heat capacity effect and drying by the air outside. Therefore, it is thought that if the rebound value of P type schmidt hammer is controled. by about 26 in consideration of open air environment, it is very effective to determine the removal time of side forms.

  • PDF

An Experimental Application of Concrete Using TEA in Construction Field (트리에탄올아민을 사용한 콘크리트의 현장 적용 실험)

  • 황인성;임춘근;김성수;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.05a
    • /
    • pp.23.1-26
    • /
    • 2003
  • This study is intended to investigate the properties of early strength development by application of TEA to the field. According to the results, when TEA is added, fluidity is almost same to base concrete, and increases upto aimed slump after field flowing. Setting time does not differ in the case of base and TEA, but is retarded after flowing. The time when compressive strength gains 5 MPa, which side form can be removed, is 23 hours, and so the removal time is shortened by 1hours in comparison with plain concrete. But compressive strength is almost same to that of plain concrete at 28 days. The rebound value of P type schmidt hammer show similar tendency to compressive strength, and the rebound value of structure is higher than that of standard curing specimen due to heat capacity effect and drying by the air outside. Therefore, it is thought that if the rebound value of P type schmidt hammer is controled. by about 26 in consideration of open air environment, it is very effective to determine the removal time of side forms.

  • PDF

Determination of Removal Time of the Side Form in High Strength Concrete (고강도콘크리트 시공시 측면 거푸집 탈형시기의 결정)

  • Han Cheon-Goo;Han Min-Cheol
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.3 s.81
    • /
    • pp.327-334
    • /
    • 2004
  • In this paper, method for the determination of removal time of the side forms in high strength concrete are discussed using the estimation model of compressive strength development, the development of bond strength and rebound number of P type Schmidt hammer in order to review the validity of existing regulation as to side form removal and offer effective quality control method. According to the results, as W/B increases by $10\%$, the setting time is shortened by about 2 hours. In the scope of the paper, required time to gain 8MPa of compressive strength is determined about 17 ${\~}$20 hours of age and $21{\~}25^{\circ}D{\cdot}D$ of maturity. Bond strength between form and concrete shows the highest value around final setting time, but decreases drastically after that. Amount of concrete sticking on the form is large before setting completed, but after that, its amount shows decline tendency. The rebound value test with P type schmidt hammer can be started faster by 2${\~}$3 hours than compressive strength test. It is also confirmed that the removal of forms is possible when the rebound value of P type schmidt hammer is more than 32. It is found from the results that existing regulation regarding removal time of the side form of high strength concrete provided in KCI needs no revision because required time to gain the strength provided in KCI has no adverse effect on strength development at early age and surface condition during stripping the side form. Effective procedure to decide the removal time of side form can be performed by applying P type Schmidt hammer.

Strength Estimation of the High Strength Concrete by using Rock Test Hammer (암반용 테스트해머 사용에 의한 고강도콘크리트의 강도추정)

  • Seo, Yun-A;Nam, Kyung-Yong;Park, Soo-Hwa;Kim, Seong-Deok;Lim, Nam-Gi;Jung, Sang-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2012.11a
    • /
    • pp.77-79
    • /
    • 2012
  • This paper intends to review possible application in the high strength area through compressive strength estimation of the simulated high strength concrete member using Rock Test Hammer and suggest it as a reference data for the strength estimation technique of the ultra high strength concrete in the future. From the results of our test, in the low strength area less than 15MPa and normal strength area in 15~60MPa, as shown on the existing studies, it is indicated that P Type Schmidt Hammer in the low strength area and N Type Schmidt Hammer in the normal strength area have high correlation of rebound-compressive strength. As the Rock Test Hammer indicated more or less reduced accuracy in the low strength area and the normal strength area but high correlation on the high strength area (50~100MPa) defined on this test, it is determined that it would be possible to make the fastest and simplest compressive strength estimation on the site where the high strength concrete is applied.