A composite cathode of LSCF$(La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_3)\;and\;GDC\; (Gd_2O_3-doped\;CeO_2:Ce_{0.9}Gd_{0.1}O_{1.95_})$ was characterized in terms of an electrode response, using a point contact in an Yttria-Stabilized Zirconia (YSZ) electrolyte incorporated into AC two-point impedance spectroscopy. The point-contacted configuration amplifies the responses occurring near the YSZ/cathode interface through the aligned point contact on the planar LSCF/GDC electrode. The point contact interface increases the bulk resistance allowing the estimation of the point contact geometry and resolving the electrode-related responses. The resultant impedance spectra are analyzed through an equivalent circuit model constructed by resistors and constant phase elements. The bulk responses can be resolved from the electrode-related portions in terms of spreading resistance. The electrode-related polarizations are measured in terms of temperature and oxygen partial pressure. The modified impedance spectroscopy is discussed in terms of methodology and analytical aspects, toward resolving the electrode-polarization issues in solid oxide fuel cells.
Alloys of Fe-(5, 10, 15)Al and Fe-(10, 20, 30, 40)Cr were corroded at 700 and $800^{\circ}C$ for 70 hr in either atmospheric air or 1 atm of Ar+$1%SO_2$ gases. In these atmospheres, Fe-5Al and Fe-10Cr alloys displayed poor corrosion resistance. In atmospheric air, Fe-5Al alloys formed oxide nodules, while Fe-10Cr alloys formed thick scales and internal oxides. In Ar+$1%SO_2$ gases, Fe-5Al and Fe-10Cr alloys formed thick, nonadherent bi-layered scales, which grew primarily by the outward diffusion of Fe ions and inward diffusion of oxygen and sulfur ions. By contrast, in atmospheric air and Ar+$1%SO_2$ gases, Fe-(10, 15)Al and Fe-(20, 30, 40)Cr alloys displayed good corrosion resistance by forming $Al_2O_3$ and $Cr_2O_3$ layers on the surface, respectively.
The passivation of AZ91D Mg alloys through plasma anodization depends on several process parameters, such as power mode and electrolyte composition. In this work, we study the dependence of the thickness, composition, pore formation, surface roughness, and corrosion resistance of formed films on the electrolyte temperature at which anodization is performed. The higher the electrolyte temperature, the lower is the surface roughness, the smaller is the oxide thickness, and the better is the corrosion resistance. More specifically, as the electrolyte temperature increases from 10 to $50^{\circ}C$, the surface roughness (Ra) decreases from 0.7 to $0.15{\mu}m$ and the corrosion resistance increases from 3.5 to 9 in terms of rating number in a salt spray test. The temperature increase from 10 to $50^{\circ}C$ also causes an increase in magnesium content in the film from 25 to 63 wt% and a decrease in oxygen from 66 to 21 wt%, indicating dehydration of the film.
In this study, we investigated the effects of BiAlSiO glass composition on its glass forming range, thermal properties, and plasma resistance. The results showed that increasing the Al2O3 content suppressed the tendency for crystallization and hindered glass formation beyond a certain threshold. Bi2O3 was found to increase the content of non-bridging oxygen, resulting in a decrease in glass transition temperature and an increase in thermal expansion coefficient. Furthermore, the etching rate was found to improve with increasing Al2O3 content but decrease with increasing SiO2 content. It was concluded that the boiling point of fluorinated compounds should be considered to 900℃. Therefore, this study is expected to contribute to the understanding of the properties of BiAlSiO glass and its application to low temperature melting PRG compositions.
Cancer stem cells (CSCs) are a small population of tumor cells characterized by self-renewal and differentiation capacity. CSCs are currently postulated as the driving force that induces intra-tumor heterogeneity leading to tumor initiation, metastasis, and eventually tumor relapse. Notably, CSCs are inherently resistant to environmental stress, chemotherapy, and radiotherapy due to high levels of antioxidant systems and drug efflux transporters. In this context, a therapeutic strategy targeting the CSC-specific pathway holds a promising cure for cancer. NRF2 (nuclear factor erythroid 2-like 2; NFE2L2) is a master transcription factor that regulates an array of genes involved in the detoxification of reactive oxygen species/electrophiles. Accumulating evidence suggests that persistent NRF2 activation, observed in multiple types of cancer, supports tumor growth, aggressive malignancy, and therapy resistance. Herein, we describe the core properties of CSCs, focusing on treatment resistance, and review the evidence that demonstrates the roles of NRF2 signaling in conferring unique properties of CSCs and the associated signaling pathways.
Most fishing nets used in fish cage aquaculture are made of synthetic fibers such as polyamide (PA) and polyethylene (PE). Therefore, it is challenging to maintain the internal volume of the fish cage due to biofouling, which can increase the load on the cage or reduce dissolved oxygen levels by impeding smooth current flow. To address this issue, research has been conducted to replace conventional synthetic fiber cage nets with brass nets, demonstrating certain benefits such as improved productivity and ease of fish cage management. However, given the need for a more thorough examination of brass fishing net weaving technology and performance, this study assessed the optimal weaving method for brass fishing nets to be used in fish cages. Additionally, it provided essential data for the practical application of brass fishing nets by evaluating their weight, tensile strength, elongation, fatigue resistance, and wear resistance. The study concluded that weaving brass fishing nets using the chain link method ensures durability, ease of installation, and compact storage in a scroll-like form. Moreover, due to their superior fatigue and wear resistance properties, brass nets can offer increased utility if appropriate net diameter and length are selected to compensate for their higher weight per unit area and relatively higher cost compared to existing fiber fishing nets.
To identify the pathogenetic role of reactive oxygen free radical-induced oxidation reaction in endotoxin-induced acute lung injury, we infused endotoxin into 8 domestic pigs; endotoxin only (n=3), pretreatment with dimethylthiourea (DMTU) (n=5). We observed the sequential changes in hemodynamic parameters, the concentration of plasma oxidized glutathione (GSSG) in pulmonary arterial and venous blood, and albumin content in bronchoalveolar lavage fluid (BALF). The results were as follows. 1) While cardiac output decreased, mean pulmonary arterial pressure, pulmonary vascular resistance, and alveolar-arterial oxygen difference increased over phase 1 (0-2 hr) and phase 2 (2-4.5 hr) by endotoxin, DMTU attenuated the above changes only during phase 2. 2) While the concentration of plasma GSSG increased significantly by endotoxin during phase 2, there were no significant differences between pulmonary arterial and venous GSSG contents during both phases. The increase in plasma GSSG content was attenuated by DMTU. 3) The content of BALF albumin was significantly lower in DMTU group than that of endotoxin group. These results suggest that reactive oxygen free radical-induced oxidation reaction may have an important pathogenetic role in endotoxin-induced acute lung injury in pigs, which seems to be greater during phase 2 rather than phase 1.
To estimate pollution status of livestock wastewater on four piggeries and one abattoir in Taegu area, physicochemical water analysis such as pH, suspended solid(SS), biochemical oxygen demand(BOD) and chemical oxygen demand(COD), and bacteriological examinations such as number of total viable cells and number of coliform with or without antibiotic resistance were carried out. The results obtained were as follows : The pH values of raw sewage ranged from 9.0 to 7.2 that of the effluent treated was lowed to 5.6~7.7. The SS values of raw sewage ranged from 5,275ppm to 120ppm and those of the efflunet decreased to 162~30ppm. The BOD values of raw sewage ranged 6,200ppm to 120ppm and those of the effluent treated decreased to 111 ~80ppm. The COD values of raw sewage ranged from 5,725ppm to 298ppm and those of the effluent decreased to 137~76ppm. The total viable cells of raw sewage ranged from $8.5{\times}11^{11}$/ml to $9.9{\times}10^7$/ml, those of the effluent decreased to $5.6{\times}10^6{\sim}4.2{\times}10^8/ml.$ The total coliforms of raw sewage ranged from $5.5{\times}10^9$/ml to $1.3{\times}10^5$/ml, those of the effluent decreased to $3.6{\times}10^4ml{\sim}9.0{\times}10^6$/ml. The incidence of streptomycin resistant coliforms was the highest(1.8~66.7%), and followed by tetracycline(1.7~64%), kanamycin(9.3~50.l%), ampicillin(0.06~45.5%) and chloramphenicol(14.3~33.5%) to total coliforms of raw sewage. The incidence of antibiotic resistant coliforms of raw sewage in farms ranged from 3.4~66.7% and that of abattoir's was 0.06% to 14.3%. Antibiotic resistant coliform counts of raw sewage ranged from 1.3$\times$10$^{8}$ /ml to 3.9$\times$10$^3$/ml, those of the effluent decreased to $3.0{\times}10^1{\sim}2.3{\times}10^5/ml$.
The electrical and mechanical properties in indium-tin-oxide films deposited on polymer substrate were examined. The materials of substrates were polyethersulfone (PES) which have gas barrier layer and anti-glare coating for plastic-based devices. The experiments were performed by rf-magnetron sputtering using a special instrument and buffer layers. Therefore, we obtained a very flat polymer substrate deposited ITO film and investigated the effects of buffer layers, and the instrument. Moreover, the influences of an oxygen partial pressure and post-deposition annealing in ITO films deposited on polymer substrates were clarified. X-ray diffraction observation, measurement of electrical property, and optical microscope observation were performed for the investigation of micro-structure and electro-mechanical properties, and they indicated that as-deposited ITO thin films are amorphous and become quasi-crystalline after adjusting oxygen partial pressure and thermal annealing above $180^{\circ}C$. As a result, we obtained 20-25 ${\Omega}/sq$ of ITO films with good transmittance (above 80 %) of oxygen contents with under 0.2 % and vacuum annealing. Furthermore, using organic buffer layer, we obtained ITO films which have a rather high electrical resistance (40-45 ${\Omega}/sq$) but have improved optical (more than 85 %) and mechanical characteristics compared to the counterparts. Consequently, a prototype reflective color plastic film LCD was fabricated using the PES polymer substrates to confirm whether the ITO films could be realized in accordance with our experimental results.
고상반응법을 이용하여 $SrCo_{0.8}Fe_{0.1}Nb_{0.1}O_{3-{\delta}}$ 조성의 산화물을 합성하였으며, 합성된 분말은 압축 성형 후 $1250^{\circ}C$에서 소결하여 치밀한 세라믹 분리막을 제조하였다. XRD 분석을 통해 단일상의 페롭스카이트 구조를 확인하였다. 산소 분압이 0.21 atm, 측정 온도가 $800{\sim}950^{\circ}C$인 조건하에서 산소투과를 분석한 결과 온도가 증가할수록 산소투과량은 증가하였고, $950^{\circ}C$에서 $1.839mL/min{\cdot}cm^2$로 최대값을 나타내었다. 니오븀(Nb)을 포함한 세라믹 분리막의 상안정성 및 이산화탄소 내성을 확인하기 위하여 $900^{\circ}C$에서 이산화탄소가 500 ppm이 포함된 혼합공기를 이용하여 장기투과 실험을 수행하였다. 이산화탄소에 노출된 $SrCo_{0.8}Fe_{0.1}Nb_{0.1}O_{3-{\delta}}$의 상안정성은 XRD와 TG로 분석하였다. 분석 결과, 이산화탄소에 노출된 $SrCo_{0.8}Fe_{0.1}Nb_{0.1}O_{3-{\delta}}$ 조성의 경우 약 8%의 $SrCO_3$가 생성되었으나, 이 수준의 $SrCO_3$ 생성량은 분리막의 산소투과도에 큰 영향을 주지 않는 것을 확인하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.