알루미늄 함량에 따른 알루미늄 주철의 내산화성에 관한 연구 (A Study on the Oxidation Resistance of Aluminum Cast Iron by Aluminum Content)

  • 김동혁
    • 한국주조공학회지
    • /
    • 제40권6호
    • /
    • pp.135-145
    • /
    • 2020
  • Aluminum cast iron has excellent oxidation resistance, sulfurization resistance, and corrosion resistance. However, the ductility at room temperature is insufficient, and at temperatures above 600?, the strength drops sharply and practicality is limited. In the case of heat-resistant cast iron, high-temperature materials containing Cr and Ni account for 30 to 50% or more. However, these high-temperature materials are expensive. Aluminum heat-resistant cast iron is considered as a substitute for expensive heat-resistant materials. Oxidation due to the aging temperature and holding time conditions increases more in 0 wt.% Al-cast iron than in 2 and 4 wt.% Al-cast iron according to oxidized weight and gravimetric oxide layer thickness measurements. As a result of observing the cross-section of the oxide layer, it was found to contain 0 wt.% of Al-cast iron silicon oxide-containing SiO2 or Fe2SiO4 oxide film. In cast iron containing aluminum, the thickness of the internal oxide layer due to aluminum increases as the aging temperature and retention time increase, and the amount of the iron oxide layer generated on the surface decreases.

이온주입 제어에 의한 재료특성 개선에 관한 연구 (A Study on Improvement of Material Characteristics by Control of Ion Implantation)

  • 양영준;이치우;후지타 카즈히사
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권8호
    • /
    • pp.1178-1184
    • /
    • 2008
  • In this study, techniques of ion implantation were used in order to improve the characteristics of metal materials such as the oxidation and wear resistant. In particular it is necessary to develope their oxidation and wear resistant that could be used in severe environmental conditions. There are mainly two elementary technologies including ion implantation and/or thin film coating. Ion implantation method was performed for surface modification. As a result, it was found that some ion implantations methods such as Nb, high-temperature Nb ion implantation and Nb+C combined implantation are somewhat effective for improving the oxidation resistance of TiAl alloy. Furthermore, the fluorine PBII treatment is more effective for improving the oxidation resistance of the TiAl alloy with three-dimensional shapes. The implantation of boron ion into thin film of TiN was also effective for improving the properties of materials like high temperature wear resistance. TiCrN film was applied to the actual seal ring for steam turbines, and it was observed that its sliding property showed a successfully good performance.

Inconel 738LC의 Pt Modified-pack Aluminizing 내산화 코팅의 산화저항성에 미치는 Palladium 완충층의 영향 (Effects of Palladium Buffer Layer on the Oxidation Resistance of Inconel 738LC Oxidation Resistant Coating Layer by Pt Modified-pack Aluminizing)

  • 한원규;최재웅;홍석준;황길호;강성군
    • 한국재료학회지
    • /
    • 제15권4호
    • /
    • pp.233-239
    • /
    • 2005
  • In this study, the effects of Pd buffer layer on the oxidation resistance of Pt modified-pack aluminized Inconel 738LC, used for gas turbine, were investigated. Pd was electroplated on Inconel 738LC, and Pt was electroplated on the electroplated Pd surface. Thus, the thickness of electroplated Pt/Pd was $10\;{\mu}m$ and the atomic ratio of Pt : Pd was about 6 : 4. After Pt/Pd electroplating, Inconel 738LC was pack aluminized to form the oxidation resistant layer. To investigate the oxidation resistance of Pt/Pd modified-pack aluminized Inconel 738LC, iso-thermal oxidation and cyclic oxidation were performed. The iso-thermal oxdation and the cyclic oxidation data indicated that the Pt/Pd modified-pack aluminized Inconel 738LC was more oxidation resistant than the Pt modified-pack aluminized Inconel 738LC. It was thought that the difference of thermal expansion coefficient between Inconel 738LC and Pt was lowered by the Pd buffer layer.

제약회사 폐수처리장 방류수 중 항생제 내성 Enterobacteria에 관한 연구 (Study on Antibiotic Resistant Enterobacteria in Pharmaceutical Effluent)

  • 김재건;김영진
    • 한국환경보건학회지
    • /
    • 제42권1호
    • /
    • pp.34-40
    • /
    • 2016
  • Objectives: This study aims to examine the concentration, diversity, and antibiotic characteristics of penicillin G resistant enterobacteria present in pharmaceutical effluent. Methods: Water sampling was performed from a pharmaceutical company in Gyeonggi-do Province, Korea in March 2015. Water samples were plated in triplicate on tryptic soy agar plates with 32 mg/L of penicillin G. Penicillin G resistant enterobacteria were selected from the effluent and were subjected to 16S rRNA analysis for penicillin G resistant species determination. Identified resistant strains were tested for resistance to various antibiotics. Results: Penicillin G resistant enterobacteria were present at 6.2% as to culturable heterotrophic bacteria. Identified penicillin G resistant enterobacteria exhibited resistance to more than 10 of the antibiotics studied. These resistant bacteria are gram negative and are closely related to pathogenic species. Conclusion: Multi-antibiotic resistant bacteria in the effluent suggest a need for disinfection and advanced oxidation processes for pharmaceutical effluents.

전기방사법에 의해 제조된 폴리우레탄 나노섬유의 수산화알루미늄 내첨에 의한 내염화 특성 향상 (Enhanced Flame Resistant Properties of Aluminum Hydroxide Addition on Electrospun Polyurethane Nanofibers)

  • 김형기
    • 한국화재소방학회논문지
    • /
    • 제30권6호
    • /
    • pp.9-13
    • /
    • 2016
  • 본 논문에서는 내산화성 및 난연성이 향상된 폴리우레탄 나노섬유를 전기방사법 및 수산화알루미늄 내첨을 통해 제조하였다. 전기방사 조건은 인가전압: 20 kV, 폴리머 용액 유량: 1.2 ml/h, 롤러 속도: 120 rpm 및 롤러와 주사기 팁의 거리: 15 cm의 공정변수에서 최적의 조건을 확인하였다. 폴리우레탄 섬유의 내산화성 및 난연성을 향상시키기 위하여, 수산화알루미늄을 전기방사 시 내첨하였다. 제조된 샘플의 열적 특성을 평가하기 위하여 열중량분석기(thermogravimetric analysis, Shimadzu, TGA-50H)를 사용하였다. 또한 관련 분석을 통해 고분자 분해 온도(polymer decomposition temperature), 적분열분해 진행온도(integral procedure decomposition temperature), 최종 분해 온도(final decomposition temperature) 및 열분해 후 잔여량 등을 분석하였다. 그리고 분해 반응의 속도론적 고찰을 위해 Horowitz-Metzger 적분식을 통해 활성화 에너지를 해석하였다. 수산화알루미늄의 내첨에 의해, 분해 활성화 에너지가 50% 이상 증가함을 확인하였다. 이는 수산화알루미늄이 $300{\sim}500^{\circ}C$에서 열분해함에 따라 수화반응에 의해 폴리우레탄 나노섬유의 열분해 저항성이 커지기 때문인 것으로 파악된다.

양극 산화 (Anodic Oxidation)

  • 노해용
    • 기술사
    • /
    • 제33권6호
    • /
    • pp.16-23
    • /
    • 2000
  • Anodizing processes is the conversion of the aluminum surface to aluminum oxide while the part is the anode in an electrolytic cell. The object of the anodizing was increased corrosion resistant, paint adhesion and was provided unique, decorative colors. Many electrolytes, under different conditions, have been used for the anodic oxidation of alumminum and its alloys. This paper deals with the procedures used in the anodic oxidation of aluminum and its alloys, the nature and properties of the oxide films, their uses and anodizing equipment and process control.

  • PDF

제약공단 방류수 유입 하천에서의 항생제 내성 bacteria에 관한 연구 (Study on Antibiotic Resistant Bacteria in Surface Water Receiving Pharmaceutical Complex Effluent)

  • 김영진;김영규
    • 한국환경보건학회지
    • /
    • 제42권6호
    • /
    • pp.409-418
    • /
    • 2016
  • Objectives: The purpose of this study was to characterize penicillin G resistant bacteria in surface water from pharmaceutical complex effluent. Methods: Surface water was sampled from pharmaceutical complex effluent in Gyeonggi-do Province, Korea in March 2015. Water samples were plated in triplicate on tryptic soy agar plates with 32 mg/L of penicillin G. Penicillin G resistant bacteria were selected from the effluent and subjected to 16S rRNA analysis for the penicillin G resistant species determination. Identified resistant strains were tested for resistance to various antibiotics. Results: Penicillin G resistant bacteria were present at 8.0% in terms of culturable heterotrophic bacteria. Identified penicillin G resistant bacteria exhibited resistance to more than nine of the antibiotics studied. These resistant bacteria are gram negative and are closely related to pathogenic species. Conclusion: Multi-antibiotic resistant bacteria in the surface water of pharmaceutical complex effluent suggest the need for disinfection and advanced oxidation processed for pharmaceutical effluent.

Improving Accident Tolerance of Nuclear Fuel with Coated Mo-alloy Cladding

  • Cheng, Bo;Kim, Young-Jin;Chou, Peter
    • Nuclear Engineering and Technology
    • /
    • 제48권1호
    • /
    • pp.16-25
    • /
    • 2016
  • In severe loss of coolant accidents (LOCA), similar to those experienced at Fukushima Daiichi and Three Mile Island Unit 1, the zirconiumalloy fuel claddingmaterials are rapidlyheateddue to nuclear decay heating and rapid exothermic oxidation of zirconium with steam. This heating causes the cladding to rapidly react with steam, lose strength, burst or collapse, and generate large quantities of hydrogen gas. Although maintaining core cooling remains the highest priority in accident management, an accident tolerant fuel (ATF) design may extend coping and recovery time for operators to restore emergency power, and cooling, and achieve safe shutdown. An ATF is required to possess high resistance to steam oxidation to reduce hydrogen generation and sufficient mechanical strength to maintain fuel rod integrity and core coolability. The initiative undertaken by Electric Power Research Institute (EPRI) is to demonstrate the feasibility of developing an ATF cladding with capability to maintain its integrity in $1,200-1,500^{\circ}C$ steam for at least 24 hours. This ATF cladding utilizes thin-walled Mo-alloys coated with oxidation-resistant surface layers. The basic design consists of a thin-walled Mo alloy structural tube with a metallurgically bonded, oxidation-resistant outer layer. Two options are being investigated: a commercially available iron, chromium, and aluminum alloy with excellent high temperature oxidation resistance, and a Zr alloy with demonstratedcorrosionresistance.Asthese composite claddings will incorporate either no Zr, or thin Zr outer layers, hydrogen generation under severe LOCA conditions will be greatly reduced. Key technical challenges and uncertainties specific to Moalloy fuel cladding include: economic core design, industrial scale fabricability, radiation embrittlement, and corrosion and oxidation resistance during normal operation, transients, and severe accidents. Progress in each aspect has been made and key results are discussed in this document. In addition to assisting plants in meeting Light Water Reactor (LWR) challenges, accident-tolerant Mo-based cladding technologies are expected to be applicable for use in high-temperature helium and molten salt reactor designs, as well as nonnuclear high temperature applications.

A Study on Development of Advanced Environmental-Resistant Materials Using Metal Ion Processing

  • Fujita Kazuhisa;Kim Hae-Ji
    • Journal of Mechanical Science and Technology
    • /
    • 제20권10호
    • /
    • pp.1670-1679
    • /
    • 2006
  • The development of the oxidation, wear and corrosion resistant materials that could be used in severe environmental conditions is needed. The elementary technologies for surface modification include ion implantation and/or thin film coating. Furthermore, in order to develop ion implantation technique to the specimens with three-dimensional shapes, plasma-based ion implantation (PBII) techniques were investigated. As a result, it was found that the ion implantation and/or thin film coating used in this study were/was effective for improving the properties of materials, which include implantations of various kinds of ions into TiAl alloy, TiN films formed on surface of base material and coatings in high-temperature steam. The techniques proposed in this study provide useful information for all of the material systems required to use at elevated temperature. For the practical applications, several results will be presented along with laboratory test results.

Mg Alloy의 Burning과 Plasma Electrolyte Oxidation 표면처리에 대한 연구 (The Characteristic in Mg Alloy with Burning and Plasma Electrolyte Oxidation Surface Treatment)

  • 유재인;최순돈;장호경
    • 한국진공학회지
    • /
    • 제19권5호
    • /
    • pp.326-330
    • /
    • 2010
  • Plasma electrolyte oxidation (PEO) 표면처리된 Mg 합금을 scanning electron microscopy (SEM) 방법으로 표면에 형성된 산화 막을 조사 분석하였다. 측정은 상온에서 수행하였다. Burning 및 PEO 방식의 표면처리 방법을 통해 제작 된 시료의 산화막을 SEM, EDS 및 I-V 측정을 통해 분석하였다. 그 결과 burning 방식의 표면처리가 PEO보다 내식성이 떨어지는 단점이 있지만, 전도성이 부여되는 결과를 나타낸다.