• 제목/요약/키워드: Optimum welding condition

검색결과 142건 처리시간 0.032초

철도차량 하부구조의 적정 용접조건에 관한 연구 (Study on Optimal Welding Conditions for Underframe of Railway Vehicles)

  • 정상호;김해지
    • 한국기계가공학회지
    • /
    • 제20권4호
    • /
    • pp.1-7
    • /
    • 2021
  • In this study, MIG welding was performed on extruded 6005A-T6 material, which is used in the base panel of railway vehicles. The material was considered as the experimental base material, and argon shielding gas and ER5356 and ER4043 filler metals were used as the consumable welding materials. Welding coupons were prepared under various welding conditions by using an auto-welding system that various welding conditions applied 2.5Hz and 4.5Hz the pulse frequency of SynchroPuls function of welding machine and 1.0mm and 1.5mm of root face affect the weld penetration of welding joint. The welding current and voltage were also varied for this testing. On the basis of the results obtained, optimum welding conditions are proposed.

6061-T6 합금의 최적 마찰교반 용접 조건 규명 및 전기화학적 특성 평가 (Evaluation of Electrochemical Characteristic and Investigation on Optimum Condition in Friction Stir Welding for 6061-T6 Al Alloy)

  • 김성종;장석기
    • 한국표면공학회지
    • /
    • 제41권6호
    • /
    • pp.341-350
    • /
    • 2008
  • In friction stir welding for 6061-T6 with various traveling speed and rotation speed conditions, the best mechanical characteristics presented in traveling speed of 507 mm/min and rotation speed of 1100RPM. The maximum tensile strength and yield strength increased with the increasing of traveling speed. The result of the electrochemical characteristic evaluation in friction stir welding at optimum conditions for 6061-T6 Al alloy presented a good characteristics compare to base metal.

자동차용 극저탄소 냉연강판의 Mash Sem TB를 이용한 용접시 특성에 관한 연구 (A study on characteristics of Mash Seam TB weld in ultra-low carbon steel applied on automotive body)

  • Han, Chang-Woo;Lee, Chang-Hee
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2001년도 춘계학술발표대회 개요집
    • /
    • pp.189-191
    • /
    • 2001
  • This study introduces the new way for the evaluation criteria of the Mash-Seam Tailored Blank weldability, The materials used are low carbon automotive galvanized and high strength steels and the evaluation of weldability are examined with various thickness. Welding tests were conducted for both similar thickness and dissimilar thickness cases. The criteria developed for optimum welding conditions were based on the relationship among results of die press forming test, weld transverse tensile test, Erichsen test and microhardness measurements. The application of the developed criteria(fracture ratio, strength ratio, etc) in obtaining optimum welding condition revealed that a weld which satisfied ant of the criteria did not fracture during actual die press test.

  • PDF

Development of Optical Device Housing Compacted Using SUS304L Granulated Powders

  • Suzuki, Hironori;Hara, Toshihiro;Ogino, Yukinobu;Sato, Yasushi;Tomota, Yo
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.754-755
    • /
    • 2006
  • In order to develop the SUS304L housing by powder metallurgy for an optical device useful for the FTTH communication system, the optimum compacting pressure and sintering temperature were investigated using granulated powder as the material to satisfy high air-tightness and high laser-weldability. Then the laser-welding test of specimen made under the optimum condition was carried out to observe welding sputters.

  • PDF

극저탄소 냉연강판의 Mash Seam TB를 이용한 용접 시 특성과 평가에 관한 연구 (A study on characteristics and evaluation of Mash Seam TB weld in ultra-low carbon steel applied on automotive body)

  • Han, Chang-Woo;Lee, Chang-Hee
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2001년도 추계학술발표대회 개요집
    • /
    • pp.81-84
    • /
    • 2001
  • This study introduces the new way for the evaluation criteria of the Mash-Seam Tailored Blank weldability, The materials used are low carbon automotive galvanized and high strength steels and the evaluation of weldability are examined with various thickness. Welding tests were conducted for both similar thickness and dissimilar thickness cases. The criteria developed for optimum welding conditions were based on the relationship among results of die press forming test, forming limit diagram, Erichsen test and microhardness measurements. The application of the developed criteria(fracture ratio, strength ratio, etc) in obtaining optimum welding condition revealed that a weld which satisfied ant of the criteria did not fracture during actual die press test and FLD dome test.

  • PDF

Al 6082-T6 MIG 용접에서 기공방지를 위한 용접공정 개발 (The Development of Welding Process to Prevent Porosity in MIG Welding of Al 6082-T6)

  • 백상엽;정연호;김원일;조상명
    • Journal of Welding and Joining
    • /
    • 제28권6호
    • /
    • pp.28-34
    • /
    • 2010
  • This paper was described on investigation to prevent porosity in high speed MIG Welding of Al 6082-T6. Porosity measurement was carried out by using image analysis of micrographs with the help of an analysis software. The main parameter was arc length and torch progressive angle. The porosity ratio was increased as arc length was increased. The arc length was increased depending upon the output voltage. By proper selection of pulse waveform parameter, the stable arc of one pulse one drop was generated. The porosity ratio of optimum condition in one pulse one drop was lower than high voltage condition. When torch progressive angle was an angle of advance $10^{\circ}$, porosity ratio was minium.

잠호용접부 균열방지를 위한 용접 플락스 및 시공기법 개발 (Development of Welding Flux and Process for Prevention of Cold Cracking in SAW Weld Metal)

  • 최기영;김찬;김영필
    • 대한조선학회 특별논문집
    • /
    • 대한조선학회 2007년도 특별논문집
    • /
    • pp.118-127
    • /
    • 2007
  • SAW(Submerged Arc Welding) process is generally applied to a wide range of welding area in the fabrication of steel structure. This process has a good characteristic properties such as the high quality of welds and the high deposition rates, but in case of welding on a thick steel plate, it also has higher cold crack susceptibility than that of a thin steel plate. The purpose of this research is to find the main factor of crack generation and clarify the countermeasure for crack prevention, and then establish the optimum welding condition in a heavy thick steel plate. The results of this study are as follows, 1. The cause of crack generation is found the diffusible hydrogen penetrated into weld metal by decomposition of the remained moisture in SAW flux during welding. 2. For the removal of diffusible hydrogen, the raw materials of SAW flux are to be dehydrated at the high temperature in the initial manufacturing stage. 3. Mechanical properties of weld metal welded with the dehydrated SAW flux were evaluated very excellent, furthermore the weld metal has been proved to have low diffusible hydrogen content with 3.1ml /100g. 4. The weldability and quality welded with thick steel plates were improved by establishing the new optimum welding condition.

  • PDF

T-joint 용접부의 형상에 따른 역학적 메카니즘에 관한 연구 (A Study on the Mechanical Mechanism According to the Groove Shape of T-welded Joint)

  • 방한서;김종명
    • Journal of Welding and Joining
    • /
    • 제17권6호
    • /
    • pp.53-61
    • /
    • 1999
  • The use of thick plate in increasing in recent years due to the rapid expansion of chemical plants, nuclear plants, ships and other industrial plants. Welding is the most popular joining techniques employed in manufacturing industrial machineries and structures. Normally, Groove shapes are prepared according to appropriate rules and regulations such as KS, JIS, AWS, LR, DNV and etc. for various thicknesses of plate. However those groove angles tend to be too large. As a result of large groove angle, residual stress, deformation of material and strength reduction is obtained. Therefore, the reliability and safety of structures and machinery tend to be decreasing. Therefore, in this paper, theoretical as well as experimental study are carried out to find optimum groove shapes for T-welded joint of mild steel. The test specimen are made in same condition with simulation model. Welding residual stresses measurement by sectional cutting method. ⅰ) The mechanical difference for change the thickness of plate and groove angle are not appeared. ⅱ) In a mechanical point of view minimum preparation angle(40°) is more suitable than maximum groove angle(60℃). ⅲ) The measurement value and distribution of welding residual stresses are not effected largely by groove angle. It is mechanical restraint that mainly affect welding residual stresses distribution. In mechanical point of view minimum groove angle is more suitable than maximum groove angle. Therefore, it is appropriate to minimize the size of groove shape in strength and safety.

  • PDF

TWB용 고강도 박판 강재의 $CO_2$ 레이저 용접성 및 성형성 ([ $CO_2$ ] Laser Weldability and Formability of High Strength Steels for Tailored Blanks Applications)

  • 이원범;박성호
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.365-372
    • /
    • 2004
  • 1)고강도강 BOP 시험 결과 강종에 차이 없이 용접속도에 따라 유사한 비드 형상을 가지는 것으로 나타났다. 한편 1.2t 시험편의 적정 용접속도는 $4\~8m/min$으로 나타났다. 2) 용접속도가 빠를수록 비드폭은 작아지며, 경도값은 높게 나타났다. 그리고, 최고 경도값은 강의 성분(Ceq)에 비례하는 것으로 나타났음, 그 결과 TRIP80(Ceq=0.53)의 경우 최고 520Hv이상의 경도값을 가지고 있었다. 3) LDH test 결과 DP강의 모재대비 용접부의 성형성이 약 $90\%$ 정도로 나타났으며, TRIP 및 일반 고강도강은 약 $80\%$의 성형성을 갖는 것으로 확인되었다. 4) He을 보호가스로 사용시 기공의 형성은 크게 억제되었다. 그리고 Ar 사용시에는 기공 형성이 He에 비해 많이 형성되는 것으로 나타나 사용시 주의가 필요한 것으로 보인다. 기공 형성은 TRIP > 60C/45R > DP 순서로 나타나 DP강이 가장 좋은 레이저 용접성을 가지고 있었다.

  • PDF