We have investigated the effects of hydrogen injection via in-situ gas addition ($O_2$, $H_2$, or $O_2$ + $H_2$ gas) and plasma post-treatment (Ar or Ar + H plasma) on material properties of ZnO that is considered to be as a channel layer in transparent thin film transistors. The variations in the electrical resistivity, optical transmittance and bandgap energy, and crystal quality of ZnO thin films were characterized in terms of the methods and conditions used in hydrogen injection. The resistivity was significantly decreased by injection of hydrogen; approximately $10^6\;{\Omega}cm$ for as-grown, $1.2\;{\times}\;10^2\;{\Omega}cm$ for in-situ with $O_2/H_2\;=\;2/3$ addition, and $0.1\;{\Omega}cm$ after Ar + H plasma treatment of 90 min. The average transmittance of ZnO films measured at a wavelength of 400-700 nm was gradually increased by increasing the post-treatment time in Ar + H plasma. The optical bandgap energy of ZnO films was almost monotonically increased by decreasing the $O_2/H_2$ ratio in in-situ gas addition or by increasing the post-treatment time in Ar + H plasma, while the post-treatment using Ar plasma hardly affected the bandgap energy. The role of hydrogen in ZnO was discussed by considering the creation and annihilation of oxygen vacancies as well as the formation of shallow donors by hydrogen.
광자결정의 밴드갭이 크면서도 모든 편광방향에 대해 동일하게 설계될 수 있다면, 이러한 광밴드갭은 다양한 소자의 응용에 있어 보다 유용해 질 수 있다. 현재까지는 원형의 공기구멍으로 이루어진 삼각격자 구조가 가장 큰 광밴드갭을 갖는 것으로 알려져 왔으나, 본 논문에서는 각종 구조적 변화에 의한 밴드갭의 변화경향을 분석하고 체계화함에 따라, 모든 편광방향에 대해 광밴드갭이 동일하면서 가장 크게 되는 새로운 격자구조를 제안하였다. 이 구조의 광밴드갭 비율$(\Delta\omega/\omega)$은 기존의 삼각격자에 비해 약 $30\%$ 정도 증대된 것임을 확인하였다.
$Dy^{3+}$ and $Eu^{3+}$-co-doped $La_2MoO_6$ phosphor thin films were deposited on sapphire substrates by radio-frequency magnetron sputtering at various growth temperatures. The phosphor thin films were characterized using X-ray diffraction (XRD), scanning electron microscopy, ultraviolet-visible spectroscopy, and fluorescence spectrometry. The optical transmittance, absorbance, bandgap, and photoluminescence intensity of the $La_2MoO_6$ phosphor thin films were found to depend on the growth temperature. The XRD patterns demonstrated that all the phosphor thin films, irrespective of growth temperatures, had a tetragonal structure. The phosphor thin film deposited at a growth temperature of $100^{\circ}C$ indicated an average transmittance of 85.3% in the 400~1,100 nm wavelength range and a bandgap energy of 4.31 eV. As the growth temperature increased, the bandgap energy gradually decreased. The emission spectra under ultraviolet excitation at 268 nm exhibited an intense red emission line at 616 nm and a weak emission line at 699 nm due to the $^5D_0{\rightarrow}^7F_2$ and $^5D_0{\rightarrow}^7F_4$ transitions of the $Eu^{3+}$ ions, respectively, and also featured a yellow emission band at 573 nm, resulting from the $^4F_{9/2}{\rightarrow}^6H_{13/2}$ transition of the $Dy^{3+}$ ions. The results suggest that $La_2MoO_6$ phosphor thin films can be used as light-emitting layers for inorganic thin film electroluminescent devices.
An optical transmitter, which is a key component of the optical transmission system, converts the electrical signal to optical signal and consists of a high-speed current-pulse driver for laser diode and low-speed feedback loops that stabilize optical power against aging, power supply voltage fluctuations, and ambient temperature changes. In this paper, the power-stabilizing part, which forms the bulk of the optical transmitter circuitry was designed in integrted circuits. Operational amplifiers and reference voltage generation circuits, which were identified as key building blocks for the power-stabilizing feedback loops, were designed and were subsequently verified through HSPICE simulations. The designed operational amplifier consists of a two-stage folded cascode amplifier and class AB output stage, whereas the reference voltage is obtained by bandgap reference circuits. Finally the power-stabilizing circuitry was laid out based on 3\mu$m CMOS design rules for fabrication.
Experimental results are reported concerning temperture effects from room temperature to 100\ulcorner on the optical properties of N-and P-type hydrogenated amorphous silicon films prepared by RF glow discharege. Optical absorption coefficient and optical bandgap have been measured and analyzed as a function of temperature. Optical absorption coefficient increase monotonically with temperature, while the optical bandgape of doped amorphous silicons decrease linearly by about 4-7x10**-4 [ev/k].
Two-dimensional materials have been received significant interest after the discovery of graphene due to their fascinating electronic and optical properties for the application of novel devices. However, graphene lack of certain bandgap which is essential requirement to achieve high performance field-effect transistors. Analogous to graphene materials, molybdenum disulfide ($MoS_2$) as one of transition-metal dichalcogenides family presents considerable bandgap and exhibits promising physical, chemical, optical and mechanical properties. Here we studied nonvolatile memory based on $MoS_2$ which is grown by chemical vapor deposition (CVD) method. $MoS_2$ growth was taken on $1.5{\times}1.5cm^2$$SiO_2$/Si-substrate. The samples were analyzed by Raman spectroscopy, atomic force microscopy and X-ray photoelectron spectroscopy. Current-voltage (I-V) characteristic was carried out HP4156A. The CVD-$MoS_2$ was analyzed as few layers and 2H-$MoS_2$ structure. From I-V measurement for two metal contacts on CVD-$MoS_2$ sample, we found typical resistive switching memory effect. The device structures and the origin of nonvolatile memory effect will be discussed.
기존 실리콘 박막 태양 전지는 적외선에 대한 감응도와 흡수도가 낮아서 광흡수율을 증가시킬 경우 효율의 효과적인 개선이 기대되어진다. 이를 개선하기 위해서 밴드갭이 Si에 비해 상대적으로 낮은 Ge을 도입함으로써 Si와 Ge 화합물을 형성할 경우 결정상태와 수소 함유량에 따라 밴드갭 조절이 가능하다. 또한 Ge는 Si에 비해 빛에 대한 감응도가 우수하여 광흡수율을 증가시킬수 있다. 단 SiGe 박막의 Ge 량이 일정량이상 많아질 경우 박막 내 결함 등의 생성으로 광변환 효율이 오히려 감소하므로 Ge 량의 적정화가 필요하다. 본 실험에 사용된 SiGe:H Layer는 SiH4 가스와 GeH4 가스를 혼합하여 증착하였고 증착장비는 PECVD를 이용하였다. GeH4/SiH4+GeH4 가스는 각각 0, 0.03, 0.1, 0.5, 1의 비율로 증착하였으며, 파워는 플라즈마의 방전특성을 알아본 후 최소파워를 이용하여 증착하였다. 이는 증착 시 플라즈마에 의한 박막 손상을 최소화하기 위함이다. Ellipsometry를 이용하여 박막의 두께와 optical bandgap을 측정하였고, FTIR, Raman scattering 등을 측정하였다.
ZnMgBeGaO/Ag/ZnMgBeGaO multilayer structures were sputter grown and characterized in detail. Results indicated that the electrical properties of the ZnMgBeGaO films were significantly improved by inserting an Ag layer with proper thickness (~ 10 nm). Structures with thicker Ag films showed much lower optical transmission, although the electrical conductivity was further improved. It was also observed that the electrical properties of the multilayer structure were sizably improved by annealing in vacuum (~35 % at $300^{\circ}C$). The optimum ZnMgBeGaO(20nm)/Ag(10nm)/ZnMgBeGaO(20nm) structure exhibited an electrical resistivity of ${\sim}2.6{\times}10^{-5}{\Omega}cm$ (after annealing), energy bandgap of ~3.75 eV, and optical transmittance of 65 % ~ 95 % over the visible wavelength range, representing a significant improvement in characteristics versus previously reported transparent conductive materials.
$TeO_x$ thin films were deposited at various $O_2$/Ar gas-flow ratios by a reactive RFmagneton sputtering technique from $TeO_2$ and Te targets. X-ray diffraction (XRD) results revealed that the $TeO_x$ thin films were amorphous. The structure and chemical composition of the $TeO_x$ thin films were investigated by fourier transform infrared spectroscopy (FT-IR) and X-ray photoelectron spectroscopy (XPS). The optical characteristics of the $TeO_x$ thin films were investigated by an Ellipsometer and a UV-VIS-NIR spectrophotometer. According to the $O_2$/Ar gas-flow ratios, the atomic composition ratio of $TeO_x$ thin films was divided into two regions(x=1-2, 2-3). Different optical characteristics were shown in each region. With an increasing $O_2$/Ar gas-flow ratio, the refractive index of the $TeO_x$ thin films decreased and the optical bandgap of the films increased.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.