• 제목/요약/키워드: Open cell foam

검색결과 38건 처리시간 0.024초

Sound Damping of a Polyurethane Foam Nanocomposite

  • Sung, Chang-Hyun;Lee, Kyung-Sick;Lee, Kyu-Se;Oh, Seung-Min;Kim, Jae-Hoon;Kim, Min-Seok;Jeong, Han-Mo
    • Macromolecular Research
    • /
    • 제15권5호
    • /
    • pp.443-448
    • /
    • 2007
  • To improve the sound damping effect of flexible polyurethane foam, with an open-cell structure, various plate-like fillers, such as bentonite, organophilic clay and sodium montmorillonite intercalated with poly(ethylene glycol), were incorporated for the creation of nanocomposites. The plate-like fillers effectively improved the sound damping within the high frequency range. The structures of the nanocomposites and foam were examined using X-ray diffraction and scanning electron microscopy. The mechanical properties and flammability of the foams were also examined.

초저주파 대역 수중 자체소음 저감에 관한 실험 연구 (An Experiment on Reduction of Infrasonic Underwater Self-Noise)

  • 이성욱;이용국;김성렬
    • 한국음향학회지
    • /
    • 제30권1호
    • /
    • pp.17-21
    • /
    • 2011
  • 수중에서 음향신호를 측정할 때에 청음기 주위에서의 유동에 의해 발생하는 초저주파 대역 자체소음을 저감시키기 위해 청음기 주위에 다공성 발포재를 씌우는 기법의 효과를 해상 실험을 통해 고찰하였다. 두께가 다른 10 ppi 폴리우레탄 발포재를 이용하여 실험한 결과, 2-10 Hz 대역에서 발포재의 두께가 1 cm일 때에는 최대 20 dB 그리고 발포재의 두께가 3 cm인 경우에는 최대 28 dB의 자체소음 저감 효과가 있음을 확인하였다.

Effect of Rubber on Microcellular Structures from High Internal Phase Emulsion Polymerization

  • Park, Ji-Sun;Chun, Byoung-Chul;Lee, Seong-Jae
    • Macromolecular Research
    • /
    • 제11권2호
    • /
    • pp.104-109
    • /
    • 2003
  • A microcellular, which combines a rubber with the conventional formulation of styrene/divinylbenzene/sorbitan monooleate/water system, was prepared using high internal phase emulsion (HIPE) polymerization. Although the open microcellular foam with low density from the conventional HIPE polymerization shows highly porous characteristics with fine, regular and isotropic structure, the one having much smaller cell size is desirable for various applications. In this study, a polybutadiene was introduced to reduce the cell size with comparable properties. Major interests were focused on the effects of rubber concentration and agitation speed on the cell sizes and compression properties. Scanning electron microscopy was used to observe the microcellular morphology and compression tests were conducted to evaluate the stress-strain behaviors. It was found that the cell size decreased as rubber concentration increased, reflecting a competition between the higher viscosity of continuous phase and the lower viscosity ratio of dispersed to continuous phases due to the addition of high molecular weight rubber into the oil phase of emulsion. A correlation for the average cell size depending on agitation speed was attempted and the result was quite satisfactory.

나노점토가 연질 폴리우레탄/점토 다공성 나노복합체의 기계적 특성에 미치는 영향 (Effect of Nanoclay on Mechanical Properties of Porous Flexible Polyurethane/Clay Nanocomposites)

  • 옥경민;김규헌;김경록;김동현;김춘환;박홍채;윤석영
    • 한국재료학회지
    • /
    • 제23권7호
    • /
    • pp.366-372
    • /
    • 2013
  • Flexible polyurethane/clay porous nanocomposite foams were synthesized using natural and organically modified montmorillonite clays such as bentonite, closite 10A and closite 30B. The content of nanoclays was varied from 1 to 5 wt% of polyol. Dispersion of clay in Polyurethane(PU) matrix was investigated by X-ray diffraction(Cu-$K{\alpha}$ rays of wavelength $1.54{\AA}$) using an X-ray diffractometer. Also, we determined that the thermal resistance of PU foam increased with added clay, compared to that of pure PU foam. The cell size and the fraction of open cells of the precursor foam were controlled by the addition of clay to the polyurethane foam. Modified clays were found to be more efficient cell openers than the unmodified clay. In addition, the tensile strength and elongation of the polyurethane/clay porous nanocomposites were examined. Increasing clay content increased the mechanical properties of the composites, such as tensile strength, and elongation at break. However, increasing the content over 5 wt% deteriorated the properties of the composites. We found that the nanofillers(bentonite, closite 10A and closite 30B) improved the thermal stability of the nanocomposite foam. The nanocomposite foam containing 3 wt% of closite 30B exhibited the best tensile strength and thermal stability.

Processing and Mechanical Properties of Ni-Cr and Ni-Cr-Al Foams by Pack-Cementation

  • ;최희만
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 추계학술발표대회
    • /
    • pp.19.1-19.1
    • /
    • 2009
  • Open-cell Ni-Cr and Ni-Cr-Al(with gamma/gamma prime microstructure typical of Bi-base super alloys) foams are manufactured by pack-cementation at $1000{\boxplus}$degrees C, followed by homogenization at $1200{\boxplus}C$. The resulting alloyed foams retain the low relative densities (less than 3.5 wt.%). The oxidation behavior of Ni-Cr foams turns out to be identical to that of bulk Ni-Cr alloys, after taking into account the foam's higher surface area. The room-temperature compressive behavior of the Ni-Cr and Ni-Cr-Al is compared to model predictions. Additionally, the foam creep behavior, measured between 680 and $825{\boxplus}C$ in the stress range of 0.1-0.3 MPa, compared to two analytical models, namely strut compression and strut bending as high-temperature deformation modes.

  • PDF

Processing and Properties of Steel Foam Sandwiches

  • Lefebvre, Louis-Philippe;Gauthier, Maxime;Baril, Eric;Voizelle, Benoit
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.91-92
    • /
    • 2006
  • Metallic foams have a combination of attractive properties such as high specific mechanical properties and good energy absorption characteristics. This paper presents the properties of steel foam sandwiches produced using powder metallurgy approach. Metallic powder, solid polymeric binder and a foaming agent are dry-mixed and molded into the desired shape. The molded powder mix is then heat-treated to foam, debind and sinter the material. The resulting material has an open cell structure with high porosity. The structure and properties of sandwiches specimens produced with the process are presented and discussed.

  • PDF

슬러리 코팅 공정으로 제조된 Fe 폼의 기공 특성에 미치는 바인더 함량의 영향 (The Effect of Binder Content for the Pore Properties of Fe Foam Fabricated by Slurry Coating Process)

  • 최진호;양상선;김양도;윤중열
    • 한국분말재료학회지
    • /
    • 제20권6호
    • /
    • pp.439-444
    • /
    • 2013
  • Fe foam with above 90% porosity and 2 millimeter pore size was successfully fabricated by a slurry coating process. In this study, the binder contents were controlled to produce the Fe foam with different pore size, strut thickness and porosity. Firstly, the slurry was prepared by uniform mixing with Fe powders, distilled water and polyvinyl alcohol(PVA) as initial materials. After slurry coating on the polyurethane(PU) foam the sample was dried at $80^{\circ}C$. The PVA and PU foams were then removed by heating at $700^{\circ}C$ for 3 hours. The debinded samples were subsequently sintered at $1250^{\circ}C$ with holding time of 3 hours under hydrogen atmosphere. The three dimensional geometries of the obtained Fe foams with open cell structure were investigated using X-ray micro CT(computed tomography) as well as the pore morphology, size and phase.

슬러리 코팅 공정으로 제조된 Fe 폼의 기공 특성에 미치는 Fe 및 Fe2O3 분말의 혼합 비율의 영향 (The Effect of Fe and Fe2O3 Powder Mixing Ratios on the Pore Properties of Fe Foam Fabricated by a Slurry Coating Process)

  • 최진호;정은미;박다희;양상선;한유동;윤중열
    • 한국분말재료학회지
    • /
    • 제21권4호
    • /
    • pp.266-270
    • /
    • 2014
  • Metal foams have a cellular structure consisting of a solid metal containing a large volume fraction of pores. In particular, open, penetrating pores are necessary for industrial applications such as in high temperature filters and as a support for catalysts. In this study, Fe foam with above 90% porosity and 2 millimeter pore size was successfully fabricated by a slurry coating process and the pore properties were characterized. The Fe and $Fe_2O_3$ powder mixing ratios were controlled to produce Fe foams with different pore size and porosity. First, the slurry was prepared by uniform mixing with powders, distilled water and polyvinyl alcohol(PVA). After slurry coating on the polyurethane(PU) foam, the sample was dried at $80^{\circ}C$. The PVA and PU foams were then removed by heating at $700^{\circ}C$ for 3 hours. The debinded samples were subsequently sintered at $1250^{\circ}C$ with a holding time of 3 hours under hydrogen atmosphere. The three dimensional geometries of the obtained Fe foams with an open cell structure were investigated using X-ray micro CT(computed tomography) as well as the pore morphology, size and phase. The coated amount of slurry on the PU foam were increased with $Fe_2O_3$ mixing powder ratio but the shrinkage and porosity of Fe foams were decreased with $Fe_2O_3$ mixing powder ratio.

HIPE 중합에 의한 미세기공 발포체의 모폴로지 및 물성: 유화계 조성의 영향 (Morphology and Properties of Microcellular foams by High Infernal Phase Emulsion Polymerization: Effect of Emulsion Compositions)

  • 정한균;지수진;이성재
    • 폴리머
    • /
    • 제26권6호
    • /
    • pp.759-766
    • /
    • 2002
  • 스티렌과 물이 주된 원료로 구성된 혼합물을 high internal Phase emulsion (HIP보) 중합을 통하여 균일한 구형의 등방성 구조로 이루어진 저밀도의 열린 구조 미세기공 발포체를 제조하였고, 물, 가교결합제인 divinylbenzene, 사슬이동제인 dodecane의 함량 변화 등의 중합조건이 미세기공발포체의 기공 크기 및 물성에 미치는 영향을 조사하였다. 제조한 HIPE 발포체의 미세구조 모폴로지를 확인하기 위하여 SEM 사진으로 관찰하였고 기계적 물성을 평가하기 위하여 압축시험으로 압축 탄성률을 측정하였다. 연구 결과 오일 상에 수용액 상을 주입할 때 한 방울씩 연속적으로 주입하는 연속투여 방식의 경우가 한번에 주입하는 일괄투여 방식의 경우보다 균일하고 안정한 발포체를 제조하는데 효과적이었다. 교반속도와 계면활성제는 기공 크기와 계면의 window 크기에 상당한 영향을 끼쳤다. 사슬이동제의 첨가는 기공 크기를 증가시켰지만 window 크기는 오히려 감소시켰다. 발포체의 압축 탄성률은 가교결합제의 함량이 증가할수록, 사슬이동제의 함량이 감소할수록 증가하였다.

소스공개 라이브러리를 활용한 선박 저항계산 CFD 코드 개발 (CFD CODE DEVELOPMENT FOR THE PREDICTION OF THE SHIP RESISTANCE USING OPEN SOURCE LIBRARIES)

  • 박선호;박세완;이신형;이상봉;최정은;강선형
    • 한국전산유체공학회지
    • /
    • 제17권2호
    • /
    • pp.21-27
    • /
    • 2012
  • Reynolds-averaged Navier-Stokes equations solver based on a pressure-based cell-centered finite volume method was developed using OpenFOAM libraries, which was an open source and providing computational continuum mechanics libraries. For the reasonable development of the turbulent boundary layer on the bow of the ship, specified library was developed. Grid sensitivities, such as skewness and aspect ratio of a cell, were tested for the solution convergence. Pressure, turbulent kinetic energy, turbulent dissipation rate contours on the ship surface computed by the developed CFD code were compared with those computed by the commercial CFD code, Fluent.