• 제목/요약/키워드: Number of Void

검색결과 137건 처리시간 0.026초

In vitro Estimation of The Hounsfield Units and The Volume and Void of Canine Struvite Stones as Predictors of Fragility in Extracorporeal Shock Wave Lithotripsy

  • Wang, Ji-hwan;Hwang, Tae-sung;Jung, Dong-in;Yeon, Seong-chan;Lee, Hee-chun
    • 한국임상수의학회지
    • /
    • 제34권3호
    • /
    • pp.178-184
    • /
    • 2017
  • The aim of this study was to determine whether Hounsfield units (HUs), volume, and various void parameters can predict stone fragility in extracorporeal shock wave lithotripsy (ESWL). HU, volume, porosity, number of voids/stone volume, and void distribution of 30 struvite stones were estimated using helical computed tomography (CT) and micro-CT. The number of shock waves necessary for full fragmentation was accepted as a measure of the stone fragility in ESWL. The correlations between the number of shock waves and the HU, volume, porosity, and number of voids/stone volume were examined. The number of shock waves of the two groups according to the void distribution was also compared. Stone volume correlated with the number of shock waves. Shell-patterned struvite stones were significantly less susceptible to fragmentation in ESWL than non-shell-patterned struvite stones. Stone volume and void distribution may be predictors of the outcome of ESWL treatment.

기공닫힘부 폐쇄정도 결정을 위한 평가방법 연구 (Evaluation methods for Void Closing Behavior in Large Ingot)

  • 최익준;최호준;윤덕재;이근안;임성주
    • 소성∙가공
    • /
    • 제20권5호
    • /
    • pp.339-343
    • /
    • 2011
  • This paper presents methods for analyzing the extent of cylindrical-shaped void closure. In addition, a quantitative relationship between change in void fraction and height reduction ratio of a compressed specimen is proposed. The height reduction ratio, number of deformation steps and billet rotation were chosen as key process parameters influencing the void closing behavior, namely, the changes in void shape and size during hot open die forging of a large ingot. The extent of void closure was analyzed from microscopic observations and estimated from tensile test results. The tensile strengths of specimens with closed voids and those without were compared for various reduction ratios in height. The results confirmed that void closure occurs at reduction ratios greater than 30 %. The void closing behavior could be expressed as a hyperbolic tangent function of reduction ratio in height, number of paths, and billet rotation. The knowledge presented in this paper could be helpful for optimizing deformation paths in open die forging processes.

Micro X-ray CT 촬영을 통한 세립 점성토의 간극비 추정 방법 연구 (Study on a methodology for estimation of void ratio of very fine clayey soil by using micro X-ray CT scan)

  • 허성준;김광염;권영철;김홍택;신휴성
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2010년도 추계 학술발표회
    • /
    • pp.392-403
    • /
    • 2010
  • In this study, a new methodology by using the X-ray CT scan is proposed for estimating void ratio of very fine clayey soil. Since the particle size of the clay is too fine to calculate the volume of void inside the clays, CT scanning tests with a number of clay specimens that were artificially set to have various designated void ratios have been carried out. From the tests, a relationship between the CT values and void ratios is given to be used for estimating the invisible void ratio of very fine clay from a representative CT value scanned. The linear relationship was able to be acquired finally. It is expected that micro X-ray CT scanning can be capable of capturing the void ratio of very fine soils without any errors inherent in the conventional specific gravity tests.

  • PDF

대형 잉곳의 기공압착 효과 향상을 위한 폐쇄조건 연구 (Void Closing Conditions of Large Ingot by Path Schedules)

  • 최익준;최호준;김대원;최석우;임성주
    • 소성∙가공
    • /
    • 제19권8호
    • /
    • pp.480-485
    • /
    • 2010
  • In this work, the closing behavior of cylindrical-shaped voids was experimentally investigated according to various parameters such as reduction ratio in height, initial void size and billet rotation during hot open die forging process. The reduction ratio in height, number of path, and billet rotation were chosen as key process parameters which influence the void closing behavior including the change of void shape and size. On the other hand, values of die overlapping and die width ratio were set to be constant. Void closing behavior was estimated by microscopic observation. Based on the observations, it was confirmed that application of billet rotation is more efficient to eliminate the void with less reduction ratio in height. The experimental results obtained from this study could be helpful to establish the optimum path schedule of open die forging process.

인공적 침상보이드의 갭길이 변화에 따른 음향방출 특성 (Characteristics of acoustic emission according to variation gap length on artificial needle shape void)

  • 박재준;김상남
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제8권4호
    • /
    • pp.495-503
    • /
    • 1995
  • As lengthen gap leng of artificial needle shape void 0.24.rarw.1.5[mm]), the amplitude of AE(Acoustic Emission) pulses was enlarged and number of pulses be generated was few. The longer gap length of void, the shorter breakdown time. As a result of this, I found that existen of void in insulation mate was fatal deterioration of insulation. According to phase angle of applied voltage, time being void was scattered largely in region of phase angle of pulses of origination in phase angle of applied voltage. The result will be used to analysis of void diagnosis.

  • PDF

3D micro-CT analysis of void formations and push-out bonding strength of resin cements used for fiber post cementation

  • Uzun, Ismail Hakki;Malkoc, Meral Arslan;Keles, Ali;Ogreten, Ayse Tuba
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권2호
    • /
    • pp.101-109
    • /
    • 2016
  • PURPOSE. To investigate the void parameters within the resin cements used for fiber post cementation by micro-CT (${\mu}CT$) and regional push-out bonding strength. MATERIALS AND METHODS. Twenty-one, single and round shaped roots were enlarged with a low-speed drill following by endodontic treatment. The roots were divided into three groups (n=7) and fiber posts were cemented with Maxcem Elite, Multilink N and Superbond C&B resin cements. Specimens were scanned using ${\mu}CT$ scanner at resolution of $13.7{\mu}m$. The number, area, and volume of voids between dentin and post were evaluated. A method of analysis based on the post segmentation was used, and coronal, middle and apical thirds considered separately. After the ${\mu}CT$ analysis, roots were embedded in epoxy resin and sectioned into 2 mm thick slices (63 sections in total). Push-out testing was performed with universal testing device at 0.5 mm/min cross-head speed. Data were analyzed with Kruskal-Wallis and Mann-Whitney U tests (${\alpha}=.05$). RESULTS. Overall, significant differences between the resin cements and the post level were observed in the void number, area, and volume (P<.05). Super-Bond C&B showed the most void formation ($44.86{\pm}22.71$). Multilink N showed the least void surface ($3.51{\pm}2.24mm^2$) and volume ($0.01{\pm}0.01mm^3$). Regional push-out bond strength of the cements was not different (P>.05). CONCLUSION. ${\mu}CT$ proved to be a powerful non-destructive 3D analysis tool for visualizing the void parameters. Multilink N had the lowest void parameters. When efficiency of all cements was evaluated, direct relationship between the post region and push-out bonding strength was not observed.

The Analysis of Discharge Distribution due to the Inner Void of Extra High Voltage Cable

  • Kim Tag-Yong;Hong Jin-Woong
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • 제5C권4호
    • /
    • pp.155-160
    • /
    • 2005
  • This paper addresses the discharge characteristics of cross-linked polyethylene according to void by the Weibull function. It analyzes discharge number and amount of discharge using Weibull distribution to identify the inter-relationship between partial discharge and defect. We detected a 10 second discharge. The applied voltage increased by 1 [kV] at discharge inception voltage. As a result, in a no-void specimen, the shape parameter was consistent according to the increase of voltage, whereas, in a void specimen, it increased according to the increase of voltage. As the result, the shape parameter expressed a fixed value at no-void specimen. However, in void specimen, according to increasing voltage shape parameter rapidly increases.

수종 인상재의 혼합방법에 따른 기포형성과 표면 재현력에 관한 연구 (A STUDY ON THE VOID FORMATION AND DETAIL REPRODUCTION ACCORDING TO THE VARIOUS IMPRESSION MATERIALS AND MIXING METHODS)

  • 류형선;임헌송;임주환;조인호
    • 대한치과보철학회지
    • /
    • 제40권2호
    • /
    • pp.140-155
    • /
    • 2002
  • Void-free impression taking is important for the fabrication of accurate dental restorations. One of the essential properties of an impression material used for indirect fabrication of precision castings is the reproduction of the fine detail. The objective in this study was to determine the influence of mixing methods on the number of voids and surface detail reproduction. The number of voids and surface detail reproduction were evaluated with the steteomicroscope $SZ-PT^{(R)}$ and photographed. The results were as follows ; 1. In comparison of the void formation according to mixing methods of all impression materials, mechanical mixing was better than hand mixing and there was significant difference(p<0.05) 2. In comparison of the void formation according to hand mixing of alginate impression materials($TOKUSO\;A-1{\alpha}^{(R)},\;CAVEX\;IMPRESSIONAL^{(R)},\;AROMA \;FINE\;DF\;III^{(R)}$), there was no significant difference among alginate groups. But the number of void was increased in the order of $Panasil^{(R)}\;contact,\;TOKUSO\;A-1{\alpha}^{(R)},\;Permlastic^{(R)}$ light bodied and there was significant difference (p<0.05). 3. In comparison of the void formation according to mechanical mixing of alginate impression materials($TOKUSO\;A-1{\alpha}^{(R)},\;CAVEX\;IMPRESSIONAL^{(R)},\;AROMA FINE\;DF\;III^{(R)}$), there was no significant different among alginate groups. But the number of void was decreased in order of $TOKUSO\;A-1{\alpha}^{(R)},\;Permlastic^{(R)}light\;bodied,\;Panasil^{(R)}$ contact and there was significant difference (p<0.05). 4. In comparison of the surface detail reproduction according to mixing methods of 3 types of impression materials($TOKUSO\;A-1{\alpha}^{(R)},\;Permlastic^{(R)}\;light\;bodied,\;Panasil^{(R)}\;contact$), there was no significant difference between hand mixing and mechanical mixing method 5. The surface detail reproduction was only influenced by impression materials, and produced better in order of $TOKUSO\;A-1{\alpha}^{(R)},\;Panasil^{(R)}\;contact,\;Permlastic^{(R)}$ light bodied. There was significat difference among 3 type of impression materials(p<0.05). From the above results, void formation is influenced by mixing methods and surface detail reproduction is influenced by impression materials than mixing methods. Therefore, to fabricate accurate restorations, proper impression material and mechanical mixing method are more effective and available clinically.

수지이동 성형공정에서 기공형성에 미치는 모세관압의 영향에 관한 실험적 연구 (An Experimental Study on the Effect of Capillary Pressure on the Void Formation in Resin Transfer Molding Process)

  • 이종훈;김세훈;김성우;이기준
    • 유변학
    • /
    • 제10권4호
    • /
    • pp.185-194
    • /
    • 1998
  • 수지이동 성형공정에서 섬유직조가 수지에 의해 함침될 때 발생하는 기공 또는 나쁜 젖음성은 최종 성형품의 물성 저하에 심각한 영향을 미치게 된다. 본 연구에서는 함침공정에서의 수지 유동특성을 파악하고 기공 형성기구를 규명하기 위하여, 빔 형태의 금형을 대상으로 실리콘 오일과 평직형태의 유리섬유를 사용하여 미시적인 유동가시화 실험을 수행하였다. 시간과 압력에 따른 수지의 침투길이를 측정함으로써 섬유직조의 기공률에 따른 비정상상태의 투과계수와 모세관압을 측정하였고, 낮은 조업압력과 낮은 기공률에서는 모세관압이 함침공정에서 중요한 가공변수임을 확인할 수 있었다. 비디오 카메라를 이용하여 유동전단면의 이동을 근접 확대 촬영하여 기공이 형성되는 과정을 미시적으로 관찰함으로써, 섬유와 수지의 표면에너지에 의해 발생되는 모세관압이 기공의 형성에 미치는 영향을 조사하였다. 그 결과, 수지충전을 유발하는 전체 구동압력에서 모세관압이 상대적으로 클수록 기공은 더욱 쉽게 생성되는 것으로 나타났다. 또한 수지의 점도와 섬유직조의 기공률이 각각 변화할 때, 모세관수에 따른 기공의 함량을 화상 해석 기법(image analysis technique)을 사용하여 정량적으로 측정하였다. 수지가 섬유직조 내로 함침될 때 임계모세관수(Ca~2.75$\times$$10^{-3})이상에서는 기공이 형성되지 않았으며, 그 이하에서는 모세관수가 감소함에 따라 기공의 함량이 지수적으로 증가하였다. 생성된 기공의 함량은 점도에 관계없이 유사한 변화 경향을 보였으며, 모세관수가 동일한 조건에서는, 기공률이 감소함에 따라 기공의 함량이 감소하였다.

  • PDF

압하율에 따른 기공압착 거동에 관한 실험적 연구 (An Experimental Study on Void Closure Behavior with respect to Reductions in Height)

  • 최익준;최호준;박훈재;최석우;정택우;박동규;최성규;임성주
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.114-117
    • /
    • 2009
  • In this work, closing behavior of the voids generated in a casting process was investigated for various parameters such as reductions in height void size and billet rotation during hot open die forging process. The reduction in height and path schedule including the number of paths and billet rotation were chosen as key process variables to express the change of geometrical void shape and void closing behavior. On the other hand, values of die overlapping and die width ratio were set to be constant. Extend of void closure was observed and evaluated using tensile test and microscope. Based on the experimental result, it is ensured that void closure do not occur at 15% and 30% reduction in height as well as one or two rotations of a billet. The useful datum obtained from this study could be utilized to establish an optimum path schedule in the open die forging process.

  • PDF