• Title/Summary/Keyword: Non-metallic inclusions

Search Result 32, Processing Time 0.022 seconds

The Formation Behavior of Non-metallic Inclusion in the Ba-added Hyper Duplex STS (Hyper Duplex STS 중 Ba 첨가 시 비금속개재물 생성거동)

  • Joo, S.W.;Hong, S.H.;Park, Y.M.;Kim, K.T.;Kim, J.S.;You, B.D.
    • Transactions of Materials Processing
    • /
    • v.20 no.7
    • /
    • pp.504-511
    • /
    • 2011
  • The alkaline earth metal Ba has a relatively low melting point. Because of its significantly high affinity to oxygen, nitrogen and sulfur, it is highly functional as a steel refining agent. But Ba can adversely affect the properties of steel especially the workability, because it can form a variety of inclusions. So, understanding of these inclusions is needed for improvement of the properties of steel. Thus a fundamental study in the formation behavior of non-metallic inclusions in Ba added Hyper Duplex STS melts was investigated. The amount of Ba, holding time and temperature were considered as experimental variables. The number of non-metallic inclusions decreased and the large particle size of non-metallic inclusions increased as the amount of Ba increased. The number of non-metallic inclusions also decreased and the large particle size increased with increased holding times and temperatures of molten steel.

Failure analysis of powder compacting punches made of powder metallurgy high speed steels (분말고속도공구강으로 만든 분말성형펀치의 손상분석)

  • 홍성현
    • Journal of Powder Materials
    • /
    • v.7 no.2
    • /
    • pp.78-84
    • /
    • 2000
  • P/M high speed steels(1.28% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V, bal. Fe) from two different venders were applied to powder compacting punch. The test results show that failure lifes were very different between two punches. These were no difference in volume fraction and mean size of carbides(MC or M6C) but non-metallic inclusions in two punches. Small amount of non-metallic inclusion in the punch did not greatly affect impact energy and transverse rupture strength (TRS). But, fatigue life was drastically decreased by non-metallic inclusions. These results show that fatigue failure was initated around non-metallic inclusion by cyclic load and the fatigue life was greatly affected by the presence of non-metallic inclusions in the punch.

  • PDF

Effect of Non-metallic Inclusions on Heat Affected Zone Delayed Cracking of High Strength Steels by Hydrogen (고장력강 용접열영향부의 지연균열에 미치는 개재물의 영향)

  • 엄동석;정호신;익본공
    • Journal of Welding and Joining
    • /
    • v.7 no.2
    • /
    • pp.49-59
    • /
    • 1989
  • The effect of non-metallic inclusions on the HAZ hydrogen induced cracking was investigated. Quench and temper high tensile strength steels containing various sulphur contents were employed. The sulphur contents range between 0.007% and 0.040%. Non-metallic inclusions were mainly MnS type sylphide and Mn-Al-Si type. The sensitivity of HAZ delayed cracking was evaluated by implant testing. Diffusible hydrogen content was varied by controlling the moisture absorbing condition of manual arc welding electrodes. The one was asreceived condition, the other was dipping the electrodes in the water for ten minutes. The main results obtained were as follows; 1) The results of implant test showed that critical stress increased with increasing S content up to 0.013%. But steel containing 0.040%S showed lower critical stress than that of 0.013% S. These result suggest that there will be optimum S content to prevent HAZ delayed cracking of high strength steels. 2) Under the lower D.H.C. level, critical stress was increased with rolling reduction, but higher D.H.C. level, effect of rolling reduction was not recognized.

  • PDF

Inspection of Non-metallic Inclusions in Thin Steel Sheets Using Magnetic Flux Leakage Method (누설자속법을 이용한 박강판의 결함탐상)

  • 임종수;손대락
    • Journal of the Korean Magnetics Society
    • /
    • v.10 no.6
    • /
    • pp.302-309
    • /
    • 2000
  • An MFL (Magnetic Flux Leakage) testing system has been developed in order to inspect the non-metallic inclusions in the thin steel sheets. We have made a differential type flux-gate magnetometer using the measurement of apparent coercive field strength of soft magnetic core. The specifications of the electromagnet was determined using FEM software, and MFL testing system with 3 axis degree of freedom was constructed. The feasibility testing for non-metallic inclusion was shown using the system. By digitizing MFL signal and using 2-D graphic display, we could identify various surface defects other than the inclusions.

  • PDF

Analysis of the Residual Stress Produced by non-metallic Inclusions during Rail Manufacturing Process (레일의 제조공정에서 비금속 개재물에 의한 레일의 잔류응력 해석)

  • 구병춘;정우현;이희성;서정원
    • Proceedings of the KSR Conference
    • /
    • 1999.05a
    • /
    • pp.352-357
    • /
    • 1999
  • During the cooling process of rail, residual stresses are produced due to the difference of the coefficients of thermal expansion between rail and inhomogeneous non-metallic inclusions such as sulphides and oxides. A micro-mechanical approach is used to obtain the stresses in the inclusions and matrix, After obtaining the stress of an elliptical inhomogeneous inclusion in an infinite domain, average stresses of randomly distributed spherical inclusions are obtained by use of Mori-Tanaka's self consistent method. The magnitude of the calculated residual stress is near to the yield stress of the matrix in case of the spherical inclusions.

  • PDF

Effect of Non-Metallic Inclusions and Hot Rolling Process Parameters on Hydrogen Induced Cracking of Linepipe Steels (라인파이프 강재의 수소유기균열에 미치는 열간압연 공정변수의 영향)

  • Koh, Seong Ung;Jung, Hwan Gyo;Kang, Ki Bong
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.4
    • /
    • pp.257-266
    • /
    • 2008
  • AHydrogen induced cracking (HIC) was phenomenologically studied in terms of the effect of nonmetallic inclusions and hot rolling process parameters. By comparing the level of non-metallic inclusions in two different kinds of commercial grade steels having different HIC resistance, the role of non-metallic inclusions in HIC occurrence was investigated. Change in inclusion morphology and distribution during hot rolling was also studied throughout slab, rolling at austenite recrystallization region (roughing mill; RM) and rolling at austenite non-recrystallization region (finish mill; FM). In addition, the contribution of RM and FM parameters to HIC was investigated from the standpoint of change in inclusion morphology during hot rolling processes. As a result, HIC was closely related to the separation of large complex inclusion during hot rolling process. Large complex inclusions originated from the improper Ca treatment, after which equilibrium composition of slag should have resulted in eutectoid composition. By controlling the equilibrium slag composition equivalent to eutectoid one, HIC resistance could be improved due to the reduced size of inclusions. In addition, change in reduction/pass in RM had an effect on HIC resistance of steels while that in FM did not. Increase in the reduction/pass in the latter stage of RM improved HIC resistance of steels by enhancing the void enclosure around inclusions.

Discrete Element Simulation of the Sintering of Composite Powders

  • Martina, C. L.;Olmos, L.;Schneiderb, L. C. R.;Bouvardc, D.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.262-263
    • /
    • 2006
  • The free sintering of metallic powders blended with non sintering inclusions is investigated by the Discrete Element Method (DEM). Each particle, whatever its nature (metallic or inclusion) is modeled as a sphere that interacts with its neighbors. We investigate the retarding effect of the inclusions on the sintering kinetics. Also, we present a simple coarsening model for the metallic particles, which allows large particles to grow at the expense of the smallest.

  • PDF

A Review of Kinetic Model for Production of Highgrade Steel : Part. 1. Simulation Model Based on Coupled Reaction (고급강 제조 반응 모델의 검토 : Part. 1. Coupled Reaction 기반 시뮬레이션 모델)

  • Kim, Jeong-In;Kim, Sun-Joong
    • Resources Recycling
    • /
    • v.30 no.1
    • /
    • pp.3-13
    • /
    • 2021
  • In the secondary refining process for the production of high-grade steel, the proper composition is maintained by alloying elements, and non-metallic inclusions are controlled for high cleanliness. Complex reactions occur simultaneously between the molten steel, slag, inclusions, refractories, and alloying elements during the secondary refining process. Previous works have reported simulation models based on kinetics to predict the compositional changes in molten steel, slag, and inclusions in actual processes. Analytical reviews are required for the models to predict the process accurately. In this study, we reviewed and analyzed simulation models based on the coupled reaction model for the secondary refining process.

Studies in Iron Manufacture Technology through Analysis of Iron Artifact in Han River Basin during the Proto-Three Kingdoms

  • Kim, Soo-Ki
    • Conservation and Restoration of Cultural Heritage
    • /
    • v.1 no.1
    • /
    • pp.9-22
    • /
    • 2012
  • The most widely excavated iron artifacts used as weapons or farm tools from central southern regions of Korea were subjects of non-metallic inclusion analysis through metallographic examination, microhardness measurement, and scanning electron microscopy with energy dispersive X-ray spectroscopy. Through metallographic interpretation and study of the analyzed results, the steel manufacturing and iron smelting using heat processing in the iron artifacts excavated from the central southern region of the ancient Korean peninsula was studied, and the analysis of the non-metallic inclusions mixed within the metallic structures was interpreted as the ternary phase diagram of the oxide to infer the type of iron ores for the iron products and the temperature of the furnace used to smelt them. Most of the ancient forged iron artifacts showed $Al_2O_3/SiO_2$ with high $SiO_2$ contents and relatively low $Al_2O_3$ contents for iron ore, indicating t hat for $Al_2O_3$ below 5%, it is presumed that magnetic iron ores were reduced to bloom iron (sponge iron) with direct-reduction process for production. The temperature for extraction of wustite for $Al_2O_3$ below 1% was found to be $1,020{\sim}1,050^{\circ}C$. Considering the oxide ternary constitutional diagram of glassy inclusions, the steel-manufacturing temperature was presumed to have been near $1,150{\sim}1,280^{\circ}C$ in most cases, and minimum melting temperature of casting iron part excavated in Daeseong-ri. Gyeonggi was near $1,400^{\circ}C$, and it is thought that hypoeutectic cast iron of about 2.3% carbon was casted and fragility of cast iron was improved by decarburizing in solid state.