• 제목/요약/키워드: Nickel powders

검색결과 115건 처리시간 0.021초

비수용성 매질로부터 Ni(OH)2 반응슬러리의 환원반응에 의한 니켈 분말의 제조 (Preparation of Nickel Powders by the Reduction of Ni(OH)2 Reactant Slurries from Nonaqueous Media)

  • 최은영;이윤복;윤석영;김광호;김진천;임영목;김형국;김양도
    • 한국재료학회지
    • /
    • 제15권5호
    • /
    • pp.334-339
    • /
    • 2005
  • Nickel Powders were synthesized by the reduction of $Ni(OH)_2$ reactant slurries from nonaqueous media, and the morphological characteristics of nickel powders with the addition of NaOH, the composition of mixed solvents, reaction temperature and reaction time were investigated. The NaOH addition changed the structure of agglomeration in the submicron range. As the volume ratio of TEA to DEA increased, the powders slightly suppressed the agglomeration between particles and their size increased. The reaction temperature on size and shape of nickel powders was significant. As reaction time was shortened from 40 min to 0.3 min at $220^{\circ}C$, size distribution of nickel powders was transferred to a narrow size distribution owing to the presence of smaller particles with below $1.0\;{\mu}m$.

가압수소환원법에 의한 알루미나 분말상의 니켈 코팅층 형성에 관한 연구 (Formation of Ni layer onto alumina powders by hydrogen reduction technique)

  • 김동진;정헌생;유케닝
    • 한국결정성장학회지
    • /
    • 제6권3호
    • /
    • pp.415-423
    • /
    • 1996
  • 황산니켈염 수용액에서 가압수소환원법을 이용하여 알루미나 분말상에 니켈 코팅층을 형성하기 위하여 실험조건(수소분압, 반응온도, $PdCl_{2}$ 첨가량, 알루미나의 종류 및 입도)을 변화시키면서 니켈이온의 환원속도 및 석출상태를 조사하였다. 환원온도 $165^{\circ}C$, 수소분압 300 psi, 코팅촉매제 $PdCl_{2}\;2\;mg/\ell$를 첨가한 조건에서 균질한 니켈코팅층을 얻을 수 있었다.

  • PDF

무전해 니켈 도금법으로 제조된 니켈-다이아몬드 복합분체의 특성 (Characteristics of Nickel-Diamond Composite Powders by Electroless Nickel Plating)

  • 안종관;김동진;;이재령;이익규;정헌생
    • 한국분말재료학회지
    • /
    • 제11권3호
    • /
    • pp.224-232
    • /
    • 2004
  • Ni-diamond composite powders with nickel layer of round-top type on the surface of synthetic diamond (140/170 mesh) were prepared by the electroless plating method (EN) with semi-batch reactor. The effects of nickel concentration, feeding rates of reductant, temperature, reaction time and stirring speeds on the weight percentage and morphology of deposited Ni, mean particle size and specific surface area of the composite powders were investigated by Atomic Adsortion Spectrometer, SEM-EDX, PSA and BET. It was found that nucleated Ni-P islands, acted as catalytic sites for further deposition and grown into these relatively thick layers with nodule-type on the surface of diamond by a lateral growth mechanism. The weight percentage of Ni in the composite powder increased with reaction time, feeding rate of reductant and temperature, but decreased with stirring speed. The weight percentage of Ni in Ni-diamond composite powder was 55% at 150 min., 200 rpm and 7$0^{\circ}C$ .

물과 에탄올의 혼합용매로부터 니켈 미분말의 합성 및 산화특성 (Synthesis of nickel fine powder in the mixed solvent of water and ethanol and ie oxidation behaviors)

  • 이상근;최은영;이윤복;김광호;박희찬
    • 한국결정성장학회지
    • /
    • 제13권3호
    • /
    • pp.139-144
    • /
    • 2003
  • 유기용매로서 에탄올을 함유한 염화니켈 수용액으로부터 니켈 미분말을 제조하고 이들의 산화특성을 검토하였다. 에탄올을 함유한 염화니켈 수용액에서 히드라진의 환원반응은 반응온도에 크게 의존하였다. 히드라진에 의한 환원반응시간은 반응온도가 증가함에 따라 감소하였다. 반응온도를 제어함으로써 입경이 0.1 $\mu\textrm{m}$-1.0 $\mu\textrm{m}$ 범위를 갖는 구형 분말을 얻을 수 있었다. 또한, 반응온도가 증가함에 따라 입경은 다소 증가하였고 조대한 입자들의 존재로 인하여 넓은 입도 분포를 나타내었다. $60^{\circ}C$에서 합성된 니켈 분말의 평균 입경과 비표면적은 각각 0.3 $\mu\textrm{m}$와 31.8 $m^2$/g이었다. $300^{\circ}C$에서 니켈 분말의 중량감소는 $Ni(OH)_2$의 분해반응에 기인한 것이다. $200^{\circ}C$ 공기중에서 가열처리한 경우 내산화성은 합성 분말보다 현저하였다

Crystallographic and Magnetic Properties of Nano-sized Nickel Substituted Cobalt Ferrites Synthesized by the Sol-gel Method

  • Choi, Won-Ok;Lee, Jae-Gwang;Kang, Byung-Sub;Chae, Kwang Pyo
    • Journal of Magnetics
    • /
    • 제19권1호
    • /
    • pp.59-63
    • /
    • 2014
  • Nano-sized nickel substituted cobalt ferrite powders, $Ni_xCo_{1-x}Fe_2O_4$ ($0.0{\leq}x{\leq}1.0$), were fabricated by the sol-gel method, and their crystallographic and magnetic properties were studied. All the ferrite powders showed a single spinel structure, and behaved ferrimagnetically. When the nickel substitution was increased, the lattice constants and the sizes of particles of the ferrite powders decreased. The M$\ddot{o}$ssbauer absorption spectra of $Ni_xCo_{1-x}Fe_2O_4$ ferrite powders could be fitted with two six-line subspectra, which were assigned to a tetrahedral A-site and octahedral B-sites of a typical spinel crystal structure. The increase in values of the magnetic hyperfine fields indicated that the superexchange interaction was stronger, with the increased nickel concentration in $Ni_xCo_{1-x}Fe_2O_4$. This could be explained using the cation distribution, which can be written as, $(Co_{0.28-0.28x}Fe_{0.72+0.28x})[Ni_xCo_{0.72-0.72x}Fe_{1.28-0.28x}]O_4$. The two values of the saturation magnetization and the coercivity decreased, as the rate of nickel substitution was increased. These decreases could be explained using the cation distribution, the magnetic moment, and the magneto crystalline anisotropy constant of the substituted ions.

수은 음극 상 전착에 의한 니켈 아말감의 제조와 그 물성 (Nickel Amalgamation by Electro-deposition Process Using Mercury Cathode and Its Properties)

  • 김기호
    • 한국표면공학회지
    • /
    • 제38권5호
    • /
    • pp.198-201
    • /
    • 2005
  • Nickel amalgam was Prepared by the electro-deposition with mercury cathode in a modified Watts bath. Homogeneous nickel amalgam was obtained. The fluidity of the amalgam decreased gradually with increased nickel quantity and become solid finally. Nickel powders of sub-micron size were obtained by a distillation of mercury from the amalgam. The characterization of the nickel amalgam was studied by SEM and x-ray diffractometry.

니켈-흑연복합분말의 흑연코어 기화거동에 관한 연구

  • 윤기병;김동진;정헌생
    • 한국재료학회지
    • /
    • 제3권3호
    • /
    • pp.300-309
    • /
    • 1993
  • 본 연구에서는 다공성 니켈재료의 원료분말로 활용될 수 있는 hollw 니켈금속분말 계조를 위한 니켈-흑연복합분말의 흑연코어 기화과정에 관하여 실험을 행하였다. 수증개-수소 혼합가스에 의한 복합분말중 흑연코어의 기화온도는 $800^{\circ}C$~$900^{\circ}C$였으며, 약 1시간의 기화반응에 의해 내부가 텅 빈 hollw니켈금속분말을 얻을 수 있었다. 흑연코어의 평균입도가 21$\mu\textrm{m}$인 82.2tw,% 니켈-17.87tw.5 흑연 복합분말로부터 제조된 hollw니켈금속분말을 100Kg/c$\textrm m^2$의 압력으로 압축, 성형한 성형체의 겉보기 기공도는 45%이었으며, 이성형체를 진공로에서 $1150^{\circ}C$ 의 온도로 1시간 소결하여 30%의 기공도와 소재내에 균질한 기공분포를 갖즌 소결체를 얻음으로써 다공성재료 제조시 hollow분말을 원료로 사용하여 재료 내의 기공에 관한 제반사항을 쉽게 조절할 수 있다는 가능성을 확인하였다.

  • PDF

Effect of Reaction Conditions on the Preparation of Nano-sized Ni Powders inside a Nonionic Polymer

  • Kim, Tea-Wan;Kim, Dong-Hyun;Park, Hong-Chae;Yoon, Seog-Young
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.462-463
    • /
    • 2006
  • Monodispersed and nano-sized Ni powders were synthesized from aqueous nickel sulfate hexahydrate $(NiSO_4{\cdot}6H_2O)$ inside nonionic polymer network by using wet chemical reduction process. The sucrose was used as a nonionic polymer network source. The effect of reaction conditions such as the amount of sucrose and a various reaction temperature, nickel sulfate hexahydrate molarity. The influence of a nonionic polymer network on the particle size of the prepared Ni powders was characterized by means of X-ray diffraction (XRD), scanning electron microscopy (SEM), and particle size analysis (PSA). The results showed that the obtained Ni powders were strong by dependent of the reaction conditions. In particular, the Ni powders prepared inside a nonionic polymer network had smooth spherical shape and narrow particle size distribution.

  • PDF

엣칭용 염화철폐액의 처리에서 미반응철의 재생방법 (Regeneration Methods for Iron Powers in the Treatment of the Waste FeCl3 Etching Solution)

  • 박찬우;정우원;이만호
    • 공업화학
    • /
    • 제8권4호
    • /
    • pp.595-601
    • /
    • 1997
  • 철 환원법에 의한 엣칭용 염화철 폐액의 처리에서 니켈이 부착된 미반응 철분을 재생하기 위해서 볼밀 및 초음파 처리를 사용하였다. 철분을 2회 재생하였을 때 니켈 제거 효율은 볼밀을 2시간 처리한 경우와 초음파를 4시간 처리한 경우 각각 94.0%와 82.1%이었다. 재생 처리하지 않고 철분을 3회 사용하였을 때 니켈 제거 효율은 40.0%이었다. 처리시간이 증가함에 따라 볼밀처리에서는 철분의 크기가 감소하였으나, 초음파 처리에서는 철분의 크기 변화가 거의 없었다.

  • PDF

수열합성법을 이용한 구형 니켈분말 제조 (Preparation of Spherical Nickel Powder by Hydrothemal Process)

  • 원창환;배장호;이종현;김병범
    • 한국분말재료학회지
    • /
    • 제11권3호
    • /
    • pp.217-223
    • /
    • 2004
  • Submicron nickel powders were prepared from aqueous solution under hydrothermal condition. The experimental conditions including the types of protective agents, concentration of the solution and the pH were studied in detail. Starting concentration of nickel ion is a dominant factor affecting particle size. It was shown that the subsequent addition of Poly Vinyl Pyrrolidone(PVP) and Sodium Dodecyle Sulfate(SDS) can help to disperse the nickel powder. X-ray diffraction and SEM were employed to characterize the products.