The relationship between magnetic parameter and microwave absorbing performance evaluation factor of electomagnetic wave absorber such as matching frequency, matching thickness were investigated for Ni-Zn ferrite composites. It was identified that the maximum value of ${\mu}_{r}$" is shift to low frequency with decrese Ni/Zn ratio and the value of ${\mu}_{r}$" is maximum in the case of Ni/Zn=1. All Ni-Zn ferrite composites in this study have two matching frequencies in 1-12 GHz frequency. It can be suggested that $f_{m1}$ is proportional to resonance frequency and $f_{m2}$ is proportional to the saturation magnetization.
Composition and process conditions for low temperature sintered NiCuZn ferrites were investigated, so as to fabricate multilayered chip inductor. The$Fe_2O_3$ deficiency for low temperature sintering was decreased with NiO contents of NiCuZn ferrites. The permeability of NiCuZn ferrites can be controlled in the range of 12~562 with the variation of NiO and $Co_3O_4$ contents. The $Q_{max} $ frequency of NiCuZn ferrites was decreased from 50 MHz to 3 MHz linearly with permeability increase from 60 to 560. The relation between the $Q_{max}$ frequency(Y) and permeability(X) of NiCuZn ferrites was expressed with the following empirical equation, logY=4.2-1.4logX.
Nanostructured spinel NiZn ferrites were prepared by the sol-gel method from metal nitrate raw materials. Analyses by X-ray diffraction and scanning electron microscopy showed the average particle size of NiZn ferrite was under 50 nm. The single phase of NiZn ferrites was obtained by firing at 250${\circ}C$, resulting in nanoparticles exhibiting normal ferrimagnetic behavior. The nanostructured $Ni_{1-X}Zn_XFe_2O_4$ (x=0.0∼1.0) were found to have the cubic spinel structure of which the lattice constants ${\alpha}_2$ increases linearly from 8.339 to 8.427 ${\AA}$ with increasing Zn content x, following Vegard's law, approximately. The saturation magnetization $M_s$ was 48 emu/g for x=0.4 and decreased to 8.0 emu/g for higher Zn contents suggesting the typical ferrimagnetism in mixed spinel ferrites. Pure NiZn ferrite phase substituted by Cu was observed before using the additive but hematite phase was partially appeared at $Ni_{0.2}Zn_{0.2}Cu_{0.6}Fe_2O_4$. On the other hand, the hematite phase in this NiZn Cu ferrite was disappeared after using the additive of acethyl aceton with small amount. The saturation magnetization Ms of $Ni_{0.2}Zn_{0.8-y}Cu_yFe_2O_4$(y=0.2∼0.6) as measured was about 51 emu/g at 77K and 19 emu/g at room temperature, respectively.
We demonstrate that a partial loading of $Ni_{0.5}Zn_{0.5}Fe_2O_4$ (Ni-Zn ferrite) film remarkably improves impedance matching of electrically small $Ba_3Co_2Fe_{24}O_{41}$ ($Co_2Z$) hexaferrite antenna. A 3 ${\mu}m$ thick Ni-Zn ferrite film was deposited on a silicon wafer by the electrophoresis deposition process and post-annealed at $400^{\circ}C$. The fabricated Ni-Zn ferrite film has saturation magnetization of $268emu/cm^3$ and coercivity of 89 Oe. A partial loading of the Ni-Zn ferrite film on the $Co_2Z$ hexaferrite helical antenna increases antenna return loss to 24.7 dB from 9.0 dB of the $Co_2Z$ antenna. Experimental results show that impedance matching and maximum input power transmission to the antenna without additional matching elements can be realized, while keeping almost the same size as the $Co_2Z$ antenna size.
Proceedings of the International Microelectronics And Packaging Society Conference
/
2002.11a
/
pp.109-113
/
2002
본 연구에서는 공침법에 의한 초미세분말을 이용하여 제조된 (NiCuZn)-ferrite와 건식법을 이용하여 제조된 (NiCuZn)-ferrite의 저온소결 특성 및 전자기적 특성을 상호 비교 분석하였다. 조성은 (N $i_{0.4-x}$C $u_{x}$Z $n_{0.6}$)$_{1+w}$(F $e_2$$O_4$/)$_{1-w}$에서 x의 값을 0.2, w의 값은 0.03으로 고정하였고, 소결은 공침법으로 합성된 분말의 경우 초기열처리과정을 거쳐 최종적으로 90$0^{\circ}C$에서, 건식법의 경우 11$50^{\circ}C$의 온도에서 진행하였다. 그 결과, 공침법으로 제조된 (NiCuZn)-ferrite는 건식법으로 제조된 (NiCuZn)-ferrite보다 20$0^{\circ}C$이상 낮은 소결온도에서 높은 소결밀도 값을 가졌으며, 품질계수 등 칩 인덕터에서 중요한 요소인 전자기적 특성이 우수하게 나타났다. 또한, 공침법으로 합성된 페라이트는 분말의 초기열처리온도에 따라 최종소결 특성이 크게 변하였다. 그밖에 공침법과 건식법으로 합성한 (NiCuZn)-ferrite의 결정성, 미세구조들을 XRD, SEM, TEM을 이용하여 비교 고찰하였다.하였다.다.
Kim, H.G.;Kim, S.R.;Lee, S.H.;Cho, H.C.;SaGong, G.
Proceedings of the KIEE Conference
/
1997.07d
/
pp.1355-1357
/
1997
In this study, the ferrite/rubber composite microwave absorbers mixed Ni-Zn ferrite and $Ni_2Y$ ferroxplana were prepared in order to control matching condion. The variation of the material constants($\dot{\varepsilon}$, $\dot{\mu}$) and microwave absorbing characteristics were investigated with various ferrite mixing ratio. The material constants of ferrite/rubber composite microwave absorber could be controlled by variation ferrite mixing radio. The matching frequency and thickness could be controlled with various ferrite mixing ratio.
In this study, nano-sized NiCuZn-ferrites for the multi-layered chip inductor application were prepared by a coprecipitation method and its electromagnetic properties were analyzed. Also, the property of low temperature sintering were studied with the initial heat treatment of powder.$(Ni_{0.4-x}Cu_xZn_{0.60})_{1+w}(Fe_2O_4)_{1-w}$ (x=0.2, w=0.03) were calcined at $300^{circ}C~750^{circ}C.$ The sintered NiCuZn-ferrites at $900^{\circ}C$ showed good apparent density $4.90g/cm^3,$ and magnetic properties of initial permeability 164 and quality factor 72. As the calcination temperature increase, the grain size of NiCuZn-ferrite increased with irregular grain distribution and its magnetic properties were deteriorated.
Proceedings of the International Microelectronics And Packaging Society Conference
/
2002.05a
/
pp.165-168
/
2002
본 연구에서는 칩인덕터 코어 소재로 사용되는 (NiCuZn)-ferrite를 습식합성법을 이용하여 나노크기의 초미세 분말을 합성하였으며, 합성된 (ZiCuZn)-ferrite 의 제조공정 및 전파기적 특성에 관하여 고찰하였다. 조성은 (N $i_{0.4-x}$C $u_{x}$Z $n_{0.6}$)$_{1+w}$ (F $e_2$$O_4$)$_{1-w}$에서 x의 값을 0.05~0.25 범위로 변화시켰으며, w 값은 0.03으로 고정하였다. 소결은 8$50^{\circ}C$에서 9$50^{\circ}C$의 범위에서 진행하였다. 나노크기의(NiCuZn)-ferrite를 사용함으로서 시약급 원료로 제조된 것보다 소결온도를 낮출 수 있었고, 밀도가 높은 페라이트 소결체를 얻을 수 있었다. 또한 초투자율, 품질계수 등 전자기적 특성이 우수하게 나타났다. 그 밖에 습식합성법으로 합성한 (NiCuZn)-ferrite 의 결정성, 미세구조 등을 XRD, SEM 을 이용하여 고찰하였다.하였다.다.
Ni-Zn ferrite powder was obtained by wet method that was to be coprecipitated the metal nitrates, Fe($NO_3$)$_3$ㆍ$9H_2$O, Ni($NO_3$)$_2$ㆍ$6H_2$O, Zn($NO_3$)$_2$ㆍ$6H_2$O to make a high permeability material. The composition of the ferrite powder was $Fe_2$$O_3$ 52 mol%, NiO 14.4 mol%, ZnO 33.6 mol%. Ni-Zn ferrite powder was compounded by precipitating metal nitrates with NaOH in vessel at the synthetic temperature of $90^{\circ}C$ for 8 hours. Calcination temperature and sintering temperature were $700^{\circ}C$ and $1150^{\circ}C$~$1250^{\circ}C$, respectively, for 2 hours. And the other ferrite powder was also prepared by the wet ball milling that was to be mixed the metal oxides as same as the above chemical composition. We studied the properties of the powder and the electromagnetic characteristics of the sintered cores obtained from there two different processes. Wet direct process produced smaller particle size with narrower distribution of the size and more purified ferrite whose sintered cores had high permeability and high magnetization.
The pick up impurity was studied for preparing the NiCuZn ferrite powder by a ball milling method that usually uses in the industrial ceramic process. The raw materials of NiO, CuO, ZnO, and $Fe_2O_3$ powder were weighted according to various spinel composition and mixed for 18 hrs by a wet ball milling method after that the slurry was followed by spray dried and calcined at $700^{\circ}C$ 3 hrs. The calcined NCZF powder was finally ball milled during 65 hrs as same method. The stainless steel ball and jar are used as mixing and milling equipment and the solid concentration of the slurry was 25 vol%. The impurities, stainless steel pickup, were effected by the composition of raw materials especially iron oxide, nickel oxide in the mixing process and by the rate of calcine of NiCuZn ferrite in final milling process. The empirical equation of stainless steel pickup was driven in the wet ball milling system. Finally, the composition of NiCuZn ferrite could be controlled by the empirical equation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.