Deformation and Fracture Behavior of Structural Bulk Amorphous Metal under Quasi-Static Compressive Loading (준정적 압축하에서 구조용 벌크 아몰퍼스 금속의 변형 및 파괴거동)

  • Shin, Hyung-Seop;Ko, Dong-Kyun;Oh, Sang-Yeob
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.27 no.10
    • /
    • pp.1630-1635
    • /
    • 2003
  • The deformation and fracture behaviors of a bulk amorphous metal, Zr-based one (Zr$\_$41.2/Ti$\_$13.8/Cu$\_$12.5/Ni$\_$10/Be$\_$22.5/: Vitreloy), were investigated over a strain rate range (7x10$\^$-4/~4 s$\^$-1/). The uniaxial compression test and the indentation test using 3mm-diameter WC balls were carried out under quasi-static loading conditions. As a result, at the uniaxial compressive state, the fracture stress of the material was very high (~1,700MPa) and the elastic strain limit was about 2%. The fracture strength showed a strain rate independent behavior up to 4 s$\^$-1/. Using indentation tests, the plastic deformation behavior of the Zr-based BAM up to a large strain value of 15% could be achieved, even though it was the deformation under locally constrained condition. The Meyer hardness of the Zr-based BAM measured by static indentation tests was about 5 GPa and it revealed negligible strain hardening behavior. At indented sites, the plastic indentation occurred forming a crater and well-developed multiple shear bands were generated around it along the direction of 45 degree when the indentation load exceeded 7kN. With increasing indentation load, shear bands became dense. The fracture surface of the specimen after uniaxial compressive tests showed vein-like pattern, typical morphology of many BAMs.

Formation of Nano-oxides on Porous Metallic Glass Compacts using Hydrothermal Synthesis (수열합성 공정을 이용한 금속 다공체의 나노 산화물 형성)

  • Park, H.J.;Kim, Y.S.;Hong, S.H.;Kim, J.T.;Cho, J.Y.;Lee, W.H.;Kim, Ki Buem
    • Journal of Powder Materials
    • /
    • v.22 no.4
    • /
    • pp.229-233
    • /
    • 2015
  • Porous metallic glass compact (PMGC) are developed by electro-discharge sintering (EDS) process of gas atomized $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ metallic glass powder under of 0.2 kJ generated by a $450{\mu}F$ capacitor being charged to 0.94 kV. Functional iron-oxides are formed and growth on the surface of PMGCs via hydrothermal synthesis. It is carried out at $150^{\circ}C$ for 48hr with distilled water of 100 mL containing Fe ions of 0.18 g/L. Consequently, two types of iron oxides with different morphology which are disc-shaped $Fe_2O_3$ and needle-shaped $Fe_3O_4$ are successfully formed on the surface of the PMGCs. This finding suggests that PMGC witih hydrothermal technique can be attractive for the practical technology as a new area of structural and functional materials. And they provide a promising road map for using the metallic glasses as a potential functional application.

Study on the soil contamination characteristics according to the functions of the returned U.S. military base (반환미군기지 기능별 토양오염특성에 관한 연구)

  • Oh, Chang-Gyu
    • Journal of Environmental Impact Assessment
    • /
    • v.22 no.5
    • /
    • pp.481-489
    • /
    • 2013
  • There are U.S. troops with a force about 290,000 strong stationed all around the world, approximately 150 countries. Among the troops, USFK has performed principal part with its stationing for 50 years against the military threat of North Korea. However, as a result of an investigation made into environmental contamination of several bases which were restituted from US to ROK by the Land Partnership Plan in the process of relocation of USFK, it was found that the area was contaminated by not only TPH and BTEX caused by diesel fuel and JP-8 but also various heavy metal over the standard level according to the operations of corps. Among these bases, 4 corps, each of which has different duties and function, were chosen to be analyzed for the characteristics and degrees of soil contamination. Fisrt of all, in armored camp the soil was contaminated by TPH and heavy metal (Zn, Ni, Pb) due to the repairing activities of tracked vehicles and shooting exercises. In army aviation camp, the soil was contaminated by TPH, BTEX and heavy metal (Zn, Cd) due to repairing activities of aircrafts. Also, in engineer camp there was contaminated area polluted by TPH and heavy metal (Zn, Pb) caused by open-air storage of various construction materials and TPH, BTEX and heavy metal (Zn, Pb, Cu) contamination of aircraft shooting area in shooting range camp were detected. Managing environment will be more effective when we identify the contaminative characteristics and take necessary measures in advance.

Evaluation on the sensitization degree for Inconel 600 by double-loop electrochemical potentiokinetic reactivation method (Double-loop electrochemical potentiokinetic reactivation 방법에 의한 Inconel 600의 예민화도 평가)

  • Jeong, Gwang-Hu;Lee, Jeong-Hyeong;Kim, Seong-Jong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.110-110
    • /
    • 2018
  • 여러 니켈합금 중 인코넬 600은 원전 가압경수로(PWR)의 튜브 재료로 널리 사용되는 재료이다. 스테인리스강과 비교하여 우수한 내식성과 기계적 특성으로 인해 화학설비, 발전설비, 그리고 해양설비 등과 같은 여러 산업분야에서도 널리 사용되고 있다. 그러나 가압경수로용 증기 발생기의 튜브 재료와 같은 특수 환경에서 예민화에 따른 입계부식 및 입계응력부식 등의 문제가 흔히 보고되고 있다. 이러한 내구성 문제는 설비 및 장비의 수명, 내구성 그리고 안정성 등의 치명적인 영향을 미친다. 따라서 용접, 열처리, 그리고 가공과정에서 발생하는 Inconel 600의 예민화 및 입계부식에 관한 연구가 활발히 진행되고 있다. 그러나 100시간 이상 장시간 열화된 시편에 대한 예민화 연구는 전무한 실정이다. 본 연구에서는 장시간 열화된 Inconel 600의 예민화를 평가하기 위해 최대 1,000시간까지 열화를 실시하였으며, 이에 대한 평가방법으로 Double-Loop Electrochemical Potentiokinetic Reactivation(DL-EPR) 시험법을 적용하였다. 본 실험에서 사용된 인코넬 600의 화학성분(wt, %)은 0.01 C, 0.05 Si, 0.14 Mn, 15.3 Cr, 0.5 Cu, 0.015 S, 그리고 나머지는 Ni 이다. 예민화 평가를 위한 등온 열화는 전기열처리로를 이용하여, $550^{\circ}C$$650^{\circ}C$에서 최대 1000시간까지 실시하였다. 열화에 따른 미세조직 변화는 scanning electron microscope와 energy dispersive x-ray spectroscopy를 이용하여 실시하였다. DL-EPR 실험은 $25^{\circ}C$의 0.1M $H_2SO_4$ + 0.001M KSCN(potasium thiocyanate) 수용액 하에서 실시하였으며, 분극은 OCP로부터 600 mV(SSE vs.)까지 1.67mV/s 주사속도로 forward scan을 실시 후, 동일한 속도로 OCP까지 reverse scan을 실시하였다. Degree Of Sensitization(DOS)값은 anodic scan peak($I_a$) 값과 reverse scan peak($I_r$) 값의 비로 산출하였다. $$i.e.\;DOS=I_r/I_a{\times}100$$. 그 결과, 온도 변수에 따른 Inconel 600강의 예민화 거동은 서로 상이한 경향을 나타내었다. $550^{\circ}C$의 경우, 열화가 진행됨에 따라 DOS값은 급격하게 증가하는 경향을 나타냈다. 반면, $650^{\circ}C$에서는 일정시간 이후부터 Cr 확산 현상에 의한 탈 예민화 현상이 관찰되었다.

  • PDF

Detailed Abundance Analysis for Plant Host Stars

  • Kang, Won-Seok;Lee, Sang-Gak;Kim, Kang-Min
    • The Bulletin of The Korean Astronomical Society
    • /
    • v.36 no.1
    • /
    • pp.27.1-27.1
    • /
    • 2011
  • We obtained the spectra of 93 Planet host stars and 73 normal field stars in F, G, K type using BOES at BOAO. We measured the equivalent width of Fe and 25 elements lines using the automatic EW measurement program, TAME(Tools for Automatic Measurement of Equivalent-widths) and estimated the elemental abundances by synth and abfind driver of MOOG code. Since the absence of planets in the normal field stars cannot be "completely" proved, this work focused on the chemical abundances and planet properties of planet host stars, which have the massive planets close to the parent star relatively. We carried out an investigation for the difference of abundances between stars with "Hot Jupiter" and normal field stars with no known planets. We examined the chemical composition of 25 elements, such as C, N, O, S, Na, Mg, Al, Si, K, Ca, Sc, Ti, V, Cr, Mn, Co, Ni, Cu, Zn, Sr, Y, Zr, Ba, Ce, Nd, and Eu by EW measurements, and the S abundances were estimated using synthetic spectrum. We have found that [Mg/Fe] and [Al/Fe] for planet host stars have lower limit comparing with those of comparison stars, and [Ca/Fe] of host star with Neptunian planets is relatively lower than the other host stars with massive planets. We have performed the Kolmogorov-Smirnov test, and examined the ratio of planet host stars to all stars for each bin of [X/H]. As a result, we noted that the O, Si, and Ca abfor undances are strongly related with the presence of planets.

  • PDF

An Analysis on Fatigue Fracture of Nuclear Pump Impeller Alloys by Ultrasonic Vibratory Cavitation Erosion (원전 해수 펌프 임펠러 합금의 케비테이션 피로 손상 해석)

  • Hong Sung-Mo;Lee Min-Ku;Kim Gwang-Ho;Rhee Chang-Kyu
    • Journal of Surface Science and Engineering
    • /
    • v.39 no.1
    • /
    • pp.35-42
    • /
    • 2006
  • In this study, the fatigue properties on the cavitation damage of the flame quenched 8.8Al-bronze (8.8Al-4.5Ni-4.5Fe-Cu) as well as the current nuclear pump impeller materials (8.8Al-bronze, STS316 and SR50A) has been investigated using an ultrasonic vibratory cavitation test. For this the impact loads of cavitation bubbles generated by ultrasonic vibratory device quantitatively evaluated and simultaneously the cavitation erosion experiments have been carried out. The fatigue analysis on the cavitation damage of the materials has been made from the determined impact load distribution (e.g. impact load, bubble count) and erosion parameters (e.g. incubation period, MDPR). According to Miner's law, the determined exponents b of the F-N relation ($F^b$ N = Constant) at the incubation stage (N: the number of fracture cycle) were 5.62, 4.16, 6.25 and 8.1 for the 8.8Al-bronze, flame quenched one, STS316 and SR50A alloys. respectively. At the steady state period, the exponents b of the F-N' curve (N': the number of cycle required for $1{\mu}m$ increment of MDP) were determined as 6.32, 5, 7.14 and 7.76 for the 8.8Al-bronze, flame quenched one, STS316, and SR50A alloys, respectively.

Study of the Optimization and the Depth Profile Using a Flat Type Ion Source in Glow Discharge Mass Spectrometry

  • Woo Jin Chun;Kim, Hyo Jin;Lim Heoung Bin;Moon Dae Won;Lee Kwang Woo
    • Bulletin of the Korean Chemical Society
    • /
    • v.13 no.6
    • /
    • pp.620-624
    • /
    • 1992
  • The analytical performance of glow discharge mass spectrometer (GD-MS), using a flat type ion source is discussed. The efficiency of ion extraction was maximized at the distance between anode and cathode of 6 mm. At the operation condition of 4 mA, -1000 volt, and 1 mbar for the source, the optimum voltages for sampler and skimmer were40 volt and -280 volt, respectively. The intensities of Cu, Zn, and Mn were increased as a function of square root of current approximately. Korea standard reference materials (KSRM) were tested for an application study. The detection limits of most elements were obtained in the range of several ppm at the optimized operating condition. The peaks of aluminum and chromium were interfered by those of residual gases. The depth profile of nickel coated copper specimens (3, 5, 10 ${\mu}m$ thickness) were obtained by plotting time versus intensities of Ni and Cr after checking the thickness of nickel coated using a scanning electron microscope (SEM). At this moment, the sputtering rate of 0.2 ${\mu}m/min$ at the optimum operating condition was determined from the slope of the plot of time to the coating thickness. The roughness spectra of specimen's crater after 16 min, discharge were obtained using a Talysuf5m-120 roughness tester as well.

Synthesis, Spectroscopic, and Biological Studies of Chromium(III), Manganese(II), Iron(III), Cobalt(II), Nickel(II), Copper(II), Ruthenium(III), and Zirconyl(II) Complexes of N1,N2-Bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide (N1,N2-bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide의 크롬(III), 망간(II), 철(III), 코발트(II), 니켈(II), 구리(II), 루테늄(III) 및 산화 지르코늄(II) 착물에 대한 합성과 분광학 및 생물학적 연구)

  • Al-Hakimi, Ahmed N.;Shakdofa, Mohamad M.E.;El-Seidy, Ahemd M.A.;El-Tabl, Abdou S.
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.3
    • /
    • pp.418-429
    • /
    • 2011
  • Novel chromium(III), manganese(II), iron(III), cobalt(II), nickel(II), copper(II), ruthenium(III), and zirconyl(II) complexes of $N^1,N^2$-bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide ($H_4L$, 1) have been synthesized and characterized by elemental, physical, and spectral analyses. The spectral data showed that the ligand behaves as either neutral tridentate ligand as in complexes 2-5 with the general formula $[H_4LMX_2(H_2O)]{\cdot}nH_2O$ (M=Cu(II), Ni(II), Co(II), X = Cl or $NO_3$), neutral hexadentate ligand as in complexes 10-12 with the general formula $[H_4LM_2Cl_6]{\cdot}nH_2O$ (M=Fe(III), Cr(III) or Ru(III)), or dibasic hexadentate ligand as in complexes 6-9 with the general formula $[H_2LM_2Cl_2(H_2O)_4]{\cdot}nH_2O$ (M = Cu(II), Ni(II), Co(II) or Mn(II), and 13 with general formula $[H_4L(ZrO)_2Cl_2]{\cdot}8H_2O$. Molar conductance in DMF solution indicated the non-ionic nature of the complexes. The ESR spectra of solid copper(II) complexes 2, 5, and 6 showed $g_{\parallel}$ >g> $g_e$, indicating distorted octahedral structure and the presence of the unpaired electron in the $N^1,N^2$ orbital with significant covalent bond character. For the dimeric copper(II) complex $[H_2LCu_2Cl_2(H_2O)_4]{\cdot}3H_2O$ (6), the distance between the two copper centers was calculated using field zero splitting parameter for the parallel component that was estimated from the ESR spectrum. The antibacterial and antifungal activities of the compounds showed that, some of metal complexes exhibited a greater inhibitory effect than standard drug as tetracycline (bacteria) and Amphotricene B (fungi).

Physicochemical properties of deposited particles on surface of pine leaves as biomarker for air pollution (솔잎가지 표면에 침착된 입자상 물질의 물리화학적 특성 및 대기오염 지표로서의 가능성 고찰)

  • Chung, David;Choi, Jeong-Heui;Lee, Jang-Ho;Lee, Soo-Yong;Lee, Ha-Eun;Park, Ki-Wan;Shim, Kyu-Young;Lee, Jong-Chun
    • Analytical Science and Technology
    • /
    • v.31 no.6
    • /
    • pp.247-258
    • /
    • 2018
  • The purpose of the present study was to investigate whether the degree of air pollution can be evaluated via examination of local plants. Selected sites included two parks in an industrial area, as well as two parks in an urban area. Selected plant samples comprised one-year-old pine shoot leaves. Leaves growing over 2 m from the ground were collected from over 10 pine trees. Leaf surface was analyzed for deposition of 14 trace elements and 16 polycyclic aromatic hydrocarbons (PAHs), including particle size and mass, surface imaging, precipitation-mediated particle removal rate, and concentration. Particle size ranged from 0.4 to $200{\mu}m$, and the volume percentage of particles ${\leq}10$ was 20 %. Deposited particle mass ranged from 0.450-0.825 mg, and precipitation-mediated removal rate ranged from 10.0-27.6 %. Trace element concentration, as measured by ICP/MS after microwave acid digestion, was 18.8-26.3 mg/kg As, 0.08-0.13 mg/kg Be, 0.06-0.08 mg/kg Cd, 4.91-17.8 mg/kg Cr, 5.26-405 mg/kg Cu, 1,930-2,670 mg/kg Fe, 3.03-28.1 mg/kg Pb, 26.9-42.8 mg/kg Mn, 2.66-10.4 mg/kg Ni, 4,560-8,730 mg/kg Al, 2,500-6,120 mg/kg Ba, 5.27-17.8 mg/kg Rb, 40.9-95.3 mg/kg Sr, and 4,030-8,260 mg/kg Zn. Concentration of PAHs, as analyzed by GC/MS/MS after liquid-liquid extraction and purification of deposited particles, ranged from 1.17 to 12.378 mg/kg for ${\Sigma}PAH_{16}$ and from 1.17 to 12.378 mg/kg for ${\Sigma}PAH_7$.

Source Apportionment Study and Chemical Composition of PM10 and PM2.5 in the Industrial Complex of Busan City, Korea (SEM-EDX 분석법에 의한 부산 S공업단지의 PM10과 PM2.5의 화학적 조성 및 발생원 추정)

  • Kim, Yong-Seog;Choi, Kum-Chan;Suh, Jeong-Min
    • Journal of Environmental Science International
    • /
    • v.26 no.11
    • /
    • pp.1297-1306
    • /
    • 2017
  • This study identified physical characteristics and aerosol particle sources of $PM_{10}$ and $PM_{2.5}$ in the industrial complex of Busan Metropolitan City, Korea. Samples of $PM_{10}$, $PM_{2.5}$ and also soil, were collected in several areas during the year of 2012 to investigate elemental composition. A URG cyclone sampler was used for collection. The samples were collected according to each experimental condition, and the analysis method of SEM-EDX was used to determine the concentration of each metallic element. The comparative analysis indicated that their mass concentration ranged from 1% to 3%. The elements in the industrial region that were above 10% were Si, Al, Fe, and Ca. Those below 5% were Na, Mg, and S. The remaining elements (1% of total mass) consisted of elements such as Ni, Co, Br and Pb. Finally, a statistical tool was applied to the elemental results to identify each source for the industrial region. From a principal components analysis (SPSS, Ver 20.0) performed to analyze the possible sources of $PM_{10}$ in the industrial region, five main factors were determined. Factor 1 (Si, Al), which accounted for 15.8% of the total variance, was mostly affected by soil and dust from manufacturing facilities nearby, Factors 2 (Cu, Ni), 3 (Zn, Pb), and 4 (Mn, Fe), which also accounted for some of variance, were mainly related to iron, non-ferrous metals, and other industrial manufacturing sources. Also, five factors determined to access possible sources of $PM_{2.5}$, Factor 1 (Na, S), accounted for 13.5% of the total variance and was affected by sea-salt particles and fuel incineration sources, and Factors 2 (Ti, Mn), 3 (Pb, Cl), 4 (K, Al) also explained significant proportions of the variance. Theses factors mean that the $PM_{2.5}$ emission sources may be considered as sources of incineration, and metals, and non-ferrous manufacturing industries.