Comparison of Microstructure & Mechanical Properties between Mn-Mo-Ni and Ni-Mo-Cr Low Alloy Steels for Reactor Pressure Vessels (원자로 압력용기용 Mn-Mo-Ni계 및 Ni-Mo-Cr계 저합금강의 미세조직과 기계적 특성 비교)

  • Kim, Min-Chul;Park, Sang Gyu;Lee, Bong-Sang
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.3
    • /
    • pp.194-202
    • /
    • 2010
  • Application of a stronger and more durable material for reactor pressure vessels (RPVs) might be an effective way to insure the integrity and increase the efficiency of nuclear power plants. A series of research projects to apply the SA508 Gr.4 steel in ASME code to RPVs are in progress because of its excellent strength and durability compared to commercial RPV steel (SA508 Gr.3 steel). In this study, the microstructural characteristics and mechanical properties of SA508 Gr.3 Mn-Mo-Ni low alloy steel and SA508 Gr.4N Ni-Mo-Cr low alloy steel were investigated. The differences in the stable phases between these two low alloy steels were evaluated by means of a thermodynamic calculation using ThermoCalc. They were then compared to microstructural features and correlated with mechanical properties. Mn-Mo-Ni low alloy steel shows the upper bainite structure that has coarse cementite in the lath boundaries. However, Ni-Mo-Cr low alloy steel shows the mixture of lower bainite and tempered martensite structure that homogeneously precipitates the small carbides such as $M_{23}C_6$ and $M_7C_3$ due to an increase of hardenability and Cr addition. In the mechanical properties, Ni-Mo-Cr low alloy steel has higher strength and toughness than Mn-Mo-Ni low alloy steel. Ni and Cr additions increase the strength by solid solution hardening. In addition, microstructural changes from upper bainite to tempered martensite improve the strength of the low alloy steel by grain refining effect, and the changes in the precipitation behavior by Cr addition improve the ductile-brittle transition behavior along with a toughening effect of Ni addition.

Observation of Densification Behavior during the Sintering of Ni-added $MoSi_2$ Powder Compacts (Ni을 첨가한 $MoSi_2$분말성형체의 소결시 치밀화거동의 관찰)

  • 이승익
    • Journal of Powder Materials
    • /
    • v.4 no.4
    • /
    • pp.298-303
    • /
    • 1997
  • The activated sintering behavior of $MoSi_2$ powder compacts with addition of 0.5 and 1.0 wt.%Ni during the sintering under As atmosphere was studied. The shrinkage was measured and the microstructures were observed by SEM (scanning electron microscopy) and BEI (backscattered electron image) along with the phase analysis by EDS during heating up to 155$0^{\circ}C$ and holding for various time at 155$0^{\circ}C$. The most of shrinkage occurred upon heating and 92% of theoretical density was attained after sintering for 1 hr at 155$0^{\circ}C$. However, little shrinkage ensued even for prolonged sintering over 1 hr at 155$0^{\circ}C$. A liquid film formed at about 135$0^{\circ}C$ along necks and grain boundaries. The polyhedral grain structure composed of $(Mo,Ni)_5Si_3$and $Ni_2Si$ across the $MoSi_2$ grain boundary developed at 155$0^{\circ}C$. It was concluded that the activated sintering of $MoSi_2$ powder by Ni led to the diffusion of Si into Ni decreasing the liquidus temperature and the enhanced diffusion of Mo and Si through such a liquid phase and/or interboundary of $(Mo,Ni)_5Si_3$.

  • PDF

Effect of Ni and Mo Addition on Fatique Property in 12Cr Steel (12Cr강의 피로특성에 미치는 Ni+Mo 첨가의 영향)

  • Lee, Jin-Kyung;Bae, Dong-Su
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.24 no.4_2
    • /
    • pp.435-441
    • /
    • 2021
  • This research was performed to study the effect of the Ni + Mo addition on the fatigue properties in 12Cr steel. After heat treatment of 12Cr steel and 12Cr-Ni-Mo steel, tensile tests, impact tests, hardness tests, and rotary bending fatigue tests were performed, respectively. The fatigue fracture surface was observed and analyzed using SEM and EDS. The fatigue limit of 12Cr steel was 554 MPa, which was 49 MPa higher than 505 MPa of 12Cr-Ni-Mo steel. Striations, which are the shape of the typical fatigue fracture surface, were observed at the fracture surface near the starting point of fatigue fracture in the 12Cr steel and 12Cr-Ni-Mo steel. However, unlike the case of 12Cr steel, 12Cr-Ni-Mo steel also had a mixed fracture surface with the fatigue and the ductile fracture surface. When brittle non-metallic inclusions exist near the starting point of fatigue failure, the crack propagation was further promoted and the fatigue life was drastically reduced.

Study on Effects of Ni/Al2O3 Catalysts Added with Mo on Durability Improvement in Steam Reforming Reactions (Mo를 첨가한 Ni/Al2O3 촉매의 수증기 개질반응에서의 내구성 증진 특성연구)

  • Won, Jong Min;Park, Gi Woo;Lee, Jin Woo;Hong, Sung Chang
    • Korean Chemical Engineering Research
    • /
    • v.54 no.4
    • /
    • pp.560-567
    • /
    • 2016
  • In this study, we characterized steam reforming reactions and surface of $Ni/Al_2O_3$ catalysts. Ni-Mo based catalysts were prepared by loading Mo as the co-catalyst and reaction activities of the Ni-Mo based catalysts were compared with those of Ni-based catalysts. Through the $H_2$-TPR and XPS analysis it was confirmed that this characteristic efficiency. $O_2$-TPO analysis was performed to examine the deposition characteristics, bonding structures and evaporation characteristics of carbon deposited on the surface of catalysts after long run experiments were performed for steam reforming reactions. As the results, it was found that durability was improved in Ni-Mo based catalysts inhibiting formation of graphitic carbon species which reduced reaction activities of the catalysts by strongly interacting with Ni in the steam reforming reaction.

A Study on the Sulfur-Resistant Catalysts for Water Gas Shift Reaction III. Modification of $Mo/γ-Al_2O_3$ Catalyst with Iron Group Metals

  • Park, Jin Nam;Kim, Jae Hyeon;Lee, Ho In
    • Bulletin of the Korean Chemical Society
    • /
    • v.21 no.12
    • /
    • pp.1233-1238
    • /
    • 2000
  • $Mo/{\gamma}-Al_2O_3catalysts$ modified with Fe, Co, and Ni were prepared by impregnation method and catalytic activity for water gas shift reaction was examined. The optimum amount of Mo loaded for the reaction was 10 wt% $MoO_3$ to ${\gamma}-Al_2O_3.$ The catalytic activity of $MoO_3/{\gamma}-Al_2O_3was$ increased by modifying with Fe, Co, and Ni in the order of Co${\thickapprox}$ Ni > Fe. The optimum amounts of Co and Ni added were 3 wt% based on CoO and NiO to 10 wt% $MoO_3/{\gamma}-Al_2O_3$, restectively. The TPR (temperature-programmed reduction) analysis revealed that the addition of Co and Ni enganced the reducibility of the catalysts. The results of both catalytic activity and TPR experiments strongly suggest that the redox property of the catalyst is an important factor in water gas shift reaction on the sulfided Mo catalysts, which could be an evidence of oxy-sulfide redox mechanism.

Soild-state reaction in Ti/Ni multilayers

  • ;;;;Y.V.Kudryavtsev;B.Szymanski
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1999.07a
    • /
    • pp.140-140
    • /
    • 1999
  • Ti/Ni multilayered films (MLF) are ideal for neutron optics particularly in neutron guides and focusing devices. This system also possesses the tendency of amorphization through a solid-state reaction (SSR). This behaviors are closely related to the electronic structures and both magneto-optical (MO) and optical properties of metals depend strongly on their electron energy structures. Mutual inter-diffusion of the Tin and Ni atoms in the MLF caused by a low temperature annealing should decrease the thickness of pure Ni, as well as change the chemical and atomic order in the reactive zone. The application of the MO spectroscopy to the study of SSR in the MLF allows us to obtain an additional information on the changes in the atomic and chemical orders in the interface region. The optical one has no restriction on the magnetic state of the constituent sublayers. Therefore, the changes in magnetic, MO and optical properties of the Ti/Ni MLF due to SSR can be expected. To the best of our knowledge, the MO and optical spectroscopies were not used for this purpose. SSR has been studied in the series of the Ti/Ni MLFs with bilayer periods of 0.65-22.2nm and constant ratio of the Ti to Ni sublayers thickness by using MO and optical spectroscopies as well as an x-ray diffraction. The experimental MO and optical spectra are compared with the computer-simulated spectra, assuming various interface models. The relative changes in the x-ray diffraction spectra and MO properties of the Ti/Ni MLF caused by annealing are bigger for the multilayers with "thick" sublayers, or the SSR with the formation of amorphous alloy takes place mainly in the Ti/Ni multilayers with "thick" sublayers, while in the nominal threshold thickness of the Ni-sublayer for the observation of the equatorial Kerr effect in the as-deposited and annealed Ti/Ni MLFs of about 3.0 and 4.5nm thick is explained by the formation of amorphous alloy during the deposition or the formation of the nonmagnetic alloyed regions between pure components as a result of the SSR. For the case of Ti/Ni MLF the MO approach is more sensitive for the determination of the thickness of the reacted zone, while x-ray diffraction is more useful for structural analyses.structural analyses.

  • PDF

Influence of Mo Addition on High Temperature Deformation Behavior of L12 Type Ni3Al Intermetallics

  • Han, Chang-Suk;Jang, Tae-Soo
    • Korean Journal of Materials Research
    • /
    • v.26 no.4
    • /
    • pp.167-172
    • /
    • 2016
  • The high temperature deformation behavior of $Ni_3Al$ and $Ni_3(Al,Mo)$ single crystals that were oriented near <112> was investigated at low strain rates in the temperature range above the flow stress peak temperature. Three types of behavior were found under the present experimental conditions. In the relatively high strain rate region, the strain rate dependence of the flow stress is small, and the deformation may be controlled by the dislocation glide mainly on the {001} slip plane in both crystals. At low strain rates, the octahedral glide is still active in $Ni_3Al$ above the peak temperature, but the active slip system in $Ni_3(Al,Mo)$ changes from octahedral glide to cube glide at the peak temperature. These results suggest that the deformation rate controlling mechanism of $Ni_3Al$ is viscous glide of dislocations by the <110>{111} slip, whereas that of $Ni_3(Al,Mo)$ is a recovery process of dislocation climb in the substructures formed by the <110>{001} slip. The results of TEM observation show that the characteristics of dislocation structures are uniform distribution in $Ni_3Al$ and subboundary formation in $Ni_3(Al,Mo)$. Activation energies for deformation in $Ni_3Al$ and $Ni_3(Al,Mo)$ were obtained in the low strain rate region. The values of the activation energy are 360 kJ/mol for $Ni_3Al$ and 300 kJ/mol for $Ni_3(Al,Mo)$.

Transformation of C9 Aromatics on Metal Loaded Mordenite (금속담지 Mordenite 에 의한 C9 Aromatics 전환반응)

  • Lee, Hak-Sung;Kim, Byung-Kyu;Park, Bok-Soo
    • Applied Chemistry for Engineering
    • /
    • v.1 no.2
    • /
    • pp.240-248
    • /
    • 1990
  • The catalytic activity and selectivity of metal loaded H-mordenite for transalkylation of $C_9$ aromatics were studied in a continuous flow fixed bed reactor under high pressure. Nickel loaded H-mordenite(T-Ni) catalyst showed high activity and slow decay of activity. Molybdenum and nickel loaded H-mordenite(T-NiMo) catalyst also showed high activity and suppressed coking of hydrocarbons. The selectivity of xylene for T-Ni and T-NiMo catalysts decreased with temperature, but that for T catalyst(commercial grade) monotonically increased with temperature within the experimental range. The performance of T-Ni and T-NiMo catalysts was better than that of T catalyst in terms of initial activity and its decay. The addition of Mo improved slightly stability of T-Ni catalyst.

  • PDF

Fractured Surface Morphology and Mechanical Properties of Ni-Cr Based Alloys with Mo Content for Dental Applications

  • Kim, Hyun-Soo;Son, Mee-Kyoung;Choe, Han-Cheol
    • Journal of the Korean institute of surface engineering
    • /
    • v.49 no.3
    • /
    • pp.260-264
    • /
    • 2016
  • In this study, fractured surface morphology and mechanical properties of Ni-Cr-Mo alloys with various contents of Mo for dental material use have been evaluated by mechanical test. The alloys used were Ni-13Cr-xMo alloys with Mo contents of 4, 6, 8, and 10 wt.%, prepared by using a vacuum arc-melting furnace. Ni-13Cr-xMo alloys were used for mechanical test without heat treatment. The phase and microstructure of alloys using an X-ray diffraction (XRD) and optical microscopy (OM) were evaluated. To examine the mechanical properties of alloys according to microstructure changes, the tensile test and the hardness test were carried out using tensile tester. To understand the mechanism of Mo addition to Ni-Cr alloy on mechanical property, the morphology and fractured surfaces of alloys were investigated by field-emission scanning electron microscope (FE-SEM). As a result, 79Ni-13Cr-8Mo alloy was verified that the tensile strength and the hardness were better than others. Varying Mo content, the changes of microstructures of alloys were identified by OM and SEM and that of 79Ni-13Cr-8Mo alloy was proved fabricated well. Microstructures of alloys were changed depending on Mo content ratio. It has been observed that 8% alloy had the most suitable mechanical property for dental alloy.

Effect of Ni on the Mechanical Properties and Fracture Characteristics of Austempered Ductile Iron (오스템퍼드 구상흑연주철의 파괴특성에 미치는 Ni의 영향에 관한 연구)

  • Baek, Sang-Ho;Kim, Hong-Beom;Kim, Chang-Kuy;Choi, Chang-Ock
    • Journal of Korea Foundry Society
    • /
    • v.14 no.1
    • /
    • pp.52-61
    • /
    • 1994
  • The effect of Ni addition, on the mechanical properties and fracture characteristics of Mo-Cu and Mo-Ni-Cu alloyed ductile iron austenitized at $900^{\circ}C$ and austempering temperatures of $250^{\circ}C$, $300^{\circ}C$ and $350^{\circ}C$. The tensile strength, yield strength and hardness are decreased and elongation and impact value are increased in both Mo-Cu and Mo-Ni-Cu alloyed austempered ductile iron, with increased austempering temperature. According to the austempering temperature are increased, the amount of retained austenite are increased. Maximum value of fracture toughness is obtained at $350^{\circ}C$ austempering temperature at this condition, the amount of retained austenite came to 40% in Mo-Ni-Cu alloyed ADI and 34% in Mo-Cu alloyed ADI. The fracture surface of ADI which had represented high toughness are showed a quasi-cleavage pattern and a dimple pattern with micro void. Comparing the fracture characteristics of Mo-Cu alloyed ADI with that of Mo-Ni-Cu alloyed ADI, the latter was superior to the former.

  • PDF