Electroless Ni-P coating is widely used for chemical, electronic, and semiconductor equipment parts because of its corrosion resistance. The incorporation of chemically-inert PTFE particles into the Ni-P films improves properties such as, non-stick, anti-adhesive and better corrosion resistance. However, soft PTFE particles degrade the hardness, wear and abrasion resistance. In this study, effects of PTFE and W addition to the Ni-P-coatings were compared by the XRD, SEM, sheet resistance, contact angle, and microhardness measurements. The change in sheet resistance was negligible, but contact angle was doubled by the addition of PTFE and W. The microhardness was lower for Ni-P-PTFE, but higher for Ni-P-PTFE-W coatings, compared to that of Ni-P coatings.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2013.05a
/
pp.59-59
/
2013
Ni-P 도금 피막층에 W를 함유시켜 고내식성을 목적으로 하는 Ni-W-P 도금에 대하여 연구 하였다. 도금액 조건의 최적화 및 도금온도와 pH 등이 가 피막특성에 미치는 영향을 조사하여 피막 크랙이 발생하지 않고 내식성 및 내마모성이 우수한 무전해 Ni-W-P 도금 공정을 확립하였다.
Journal of the Microelectronics and Packaging Society
/
v.17
no.1
/
pp.25-31
/
2010
In this study, we investigated the morphology and thermal stability of interfacial phases in joint between lead free solder(Sn-3.0Ag-0.5Cu) and electroless Ni-W-P under bump metallizations(UBM) with different tungsten contents as a function of thermal aging. Content of phosphorus of each deposits was fixed at 8 wt.%, and content of tungsten was variated each 0, 3, 6 and 9 wt.%. Specimens were prepared by reflowing at $255^{\circ}C$, aging range was $200^{\circ}C$ and up to 2 weeks. After reflow process, in the electroless Ni(W)-P/solder joint, the interfacial intermetallic compound(IMC) was showed both $(Cu,Ni)_6Sn_5$ and $(Ni,Cu)_3Sn_4$. UBM and generated IMC at the interface of lead free solder was proportionally increased with aging time. The thickness of IMC was increased because the generation rate of $Ni(W)_3P$ decreased with increasing contents of W.
본 연구는 텅스텐 소결에 저온 활성제로 작용하는 Ni-P 공정합금을 미량첨가하여 제조공정의 간단화를 통한 새로운 W-Cu계 전기접점제조를 목표로 하였다. 이를 위해 1회 용침공정을 통해 제조한 W(Ni-P)-Cu 합금에 대한 전기접점특성을 조사하여 접점의 미세구조 관점에서 논의하였다. Ni-P 합금첨가한 접점은 기존의 순수 W-Cu 합금에 비해 낮은 접촉저항 및 낮은 아크소모를 나타내는 우수한 접점성능을 보여주었다. 이것은 Ni-P합금이 Cu용침이 개시되기전 짧은 승온단계에서 분말간의 강한 결합과 Cu용침에 유리한 기공통로를 갖는 W 분말 골격체의 형성을 유도하기 때문인 것으로 판단된다.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2018.06a
/
pp.81-81
/
2018
Bi-Te계 열전소자는 상온에서의 열전 효율이 우수하기 때문에 항공, 컴퓨터 등의 열전발전 또는 열전냉각 모듈에 널리 사용된다. 이 열전소자를 활용한 열전모듈은 다수의 n형 및 p형 열전소자가 세라믹 위에 형성된 Cu 전극에 전기적으로 직렬이 되도록 서로 솔더링 접합이 되어 있는 구조를 가지고 있다. 이처럼 직렬 연결된 방식에서는 높은 접합강도를 필요로 한다. 열전모듈 제작 시 Bi-Te 계 소자를 바로 Cu 기판에 접합시키면 솔더에 들어있는 Sn과 기판의 Cu가 접합하는 과정에서 소재 내로 확산하여 접합강도를 저하시킨다. 이러한 열전모듈의 접합강도 저하를 막기 위해 무전해 Ni-W-P 도금층을 확산 방지층으로 적용하였다. 본 연구에서는 Ni-W-P 도금이 Bi-Te 계 열전 모듈의 접합강도에 미치는 영향을 조사하였다. 본 연구에서는 Bi-Te계 열전소자에 양호한 밀착성을 가지는 Ni-W-P 도금층을 형성시키기 위해서 알루미나 분말을 이용한 sand-blasting 방법을 사용하여 Bi-Te 소재 표면에 분사하는 방법으로 표면을 거칠게 하였다. 그 후 무전해 Ni-W-P 도금을 $85^{\circ}C$에서 20분간 실시하여 약 4um의 Ni-W-P 도금층을 형성시켰다. 열전 모듈은 Sn-Ag-Cu 솔더를 사용하여 제작하였으며 접합강도는 Bonding tester를 사용하여 측정하였다. 제작한 열전 모듈의 단면 및 파단면 관찰을 통하여 접합강도가 변하는 요인을 조사하였다. 제작한 열전 모듈의 단면을 FE-EPMA로 관찰한 결과 Ni-W-P 도금층이 Bi-Te 소자와 Sn과 Cu사이의 확산을 방지하는 확산방지층 역할을 하는 것을 관찰할 수 있었다. 또한 열처리 전 열전모듈과 200도, 150시간 열처리 후 접합강도를 각각 측정해 본 결과, 열처리 후의 접합강도가 상승하는 것을 확인 할 수 있었다. 따라서 Bi-Te계 열전모듈 제작에 무전해 Ni-W-P 도금층을 형성시키므로 인해 확산방지층의 생성과 접합강도의 상승에 도움을 주었다.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
1988.10a
/
pp.64-66
/
1988
The present investigation has been performed on the manufacturing process of Ni-P doped W-Cu electric contacts by infiltration techniques. The addition of small amount of Ni-P alloy aimed at forming a rigid and homogeneous skeleton structure of W-powders which favours subsequent infiltration process of Cu-melts. The experimental results revealed that the small addition of Ni-P alloy appreciably enhances the sintering process of W at low temperatures (even at 1000$^{\circ}C$), simultaneously causing a considerable change of skeleton Morphology and its related best infiltration behaviour of Cu-melts.
Journal of the Korean institute of surface engineering
/
v.28
no.4
/
pp.207-218
/
1995
Tungsten(W) metal has excellent properties in heat-resistance, corrison-resistance and impact-resistance but W-Metal is hard to sinter because higher than $2,000^{\circ}C$ is required to sinter W-powder. Con-sequently, a deposit technique of Nikel Phosphorus(NiP) on W-powber by the liquid reduction precipitation method was performed. Sintering temperature of the resulting W-NiP composite was lowered around to $1,000^{\circ}C$, and the mechanical properties of the sintered body was studied. The most suitable conditions for NiP thin film deposit on W-Powder by the liquid reduction precipitation method, which are composition, concentration, pH and temperature of the liquid reduction solution, were considered. The activated sintering was carried out in a reducing condition furnace. Components and properties of the sintered body were investigated by the density and the hardness measurements, X- ray diffraction analysis, and microscopic photographs of the surface. Quantity of NiP thin film on W-powder could be varied by the change of the liquid reduction solution composition. The sintering temperature of W-NiP composite powder is lowered to $950^{\circ}C$ from $2,000^{\circ}C$ and the hardness is increased (ca. 720 Hv). Large shrinkage could be observed since density was increased from 5.5 to 11.0 g/$cm^2$ which 86.2% of theoretical density. W metal and $Ni_3P$ crystal were detected through X-ray diffraction on the sintered body. Perfectly activated sintering was observed by microscopic photographs.
Cho, Jin Ki;Park, Sang Wook;Kang, Seung Goon;Son, Seong-Ho
Korean Journal of Metals and Materials
/
v.46
no.11
/
pp.725-729
/
2008
Deposition characteristics of electroless plated Ni-W-P films were investigated for various complexing agents. Used complexing agents are sodium citrate, sodium gluconate and sodium malonate. In this study, the existing mixed potential theory could explain the overall mechanism of Ni-W-P electroless plating for all complexing agents. The deposition rate could be also expected by the theory. The deposited Ni-W-P films were evaluated in term of surface hardness and corrosion resistance. Microhardness of the deposit increased about 1,000 Hv after heat treatment for one hour at $400^{\circ}C$, because it was above the crystallization temperature of $Ni_3P$. The deposited Ni-W-P films can exhibit excellent corrosion resistance in using sodium malonate as a complexing agent, the other hand the using sodium gluconate was the worst corrosion resistance. The worst corrosion resistance was due to a large number of nano-sized pin-holes or small pores. The plating current at the mixed potential increases when the using sodium malonate as a complexing agent, it was explained by the cross section.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2011.05a
/
pp.201-201
/
2011
크롬대체도금으로 개발 추진되고 있는 전기Ni-W합금도금피막은 경질크롬 도금피막보다도 고온에서 경도 및 내 산성이 우수하고, 유리성형용 금형으로 사용되고 있다. 최근 일본에서는 지금까지의 무전해Ni-W-P합금피막에 비해서 텅스텐, 인의 함유율이 높고, 질산 이외의 염산, 황산의 산성 환경과 암모니아, 수산화나트륨 등의 알칼리성 환경에서도 부식이나 변색이 생기지 않는 무전해Ni-W-P합금도금기술을 크롬도금을 대체하는 도금으로서 개발하고 있다.
The present work has attempted to investigate the dependence of Cu infiltration kinetics on in-situ structure modification of W powder skeleton in W-Cu system. In-situ structure modification of W skeleton by addition of 0.3wt%Ni-P eutectic alloy was designed to proceed during heat-up of the W compact for Cu infiltration process. It was found that the Ni-P added W skeleton underwent remarkable stucture change only during heating-up. its structure was composed of large necks of W particles above 0.5 in the ratio of neck to particle size and smooth pore channels. The infiltration experiment showed that the infiltration kinetics for the W-Ni-P followed well the linear relationship of h vs. $t^{1/2}$ the rate constant K of which was in good agreement with the theoretical value. On the other hand, in case of the pure W skeleton a lower K value by 20% than the theoretical one was obatined. Such discrepancy is discussed in terms of skeleton structure induced infiltration mechanics.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.