  • Amorphous $MgNi_{1-x}Ti_x$ alloys with the composition of x=0.02, 0.03, 0.05 and 0.07 were synthesized by mechanical alloying. The synthesized alloys were investigated by electrochemical test, XRD and SEM. As increasing Ti concentration, the initial discharge capacity was raised more than that of nanocrystalline Mg-Ni 289 mAh/g, but the electrodes were degraded faster. Comparing to other synthesized alloys, $MgNi_{0.95}Ti_{0.05}$ alloy showed the highest initial discharged capacity 474 mAh/g and maintained $54\%$ of the initial capacity after 10 cycles.

  • PDF

Zr-V계 Laves상 수소저장합금의 전기화학적 성질 (Electrochemical Properties of Laves Phase Zr-V System Hydrogen Absorbing Alloys)

  • 박찬교;조태환
    • 한국수소및신에너지학회논문집
    • /
    • 제8권2호
    • /
    • pp.51-56
    • /
    • 1997
  • Laves상 $ZrV_2$합금은 다량의 수소를 저장하지만 수소와의 결합력이 강하여 Ni-MH전지의 전극으로는 부적당하다. 전극에 응용하기 위해 $ZrV_2$합금중의 V의 일부를 Ni로 치환하여 수소와의 결합력을 약하게 하였다. 이와 같은 Zr-V-Ni계 합금에 대해 전기화학적 성질, 전극의 평형전위로부터 합금중의 수소의 열역학적성질 및 2차전지전극에의 응용가능성을 조사하였다.

  • PDF

NiTiCu 형상기억합금의 피로특성 (Fatigue Characterization of NiTiCu Shape Memory Alloys)

  • 한지원;박성범
    • 한국안전학회지
    • /
    • 제29권4호
    • /
    • pp.28-33
    • /
    • 2014
  • Recently, the actuator worked by the driving recovery-force of the thermo elastic martensitic transformation of shape memory alloys(SMA) has been studied. This paper presents a study on the fatigue life of shape memory alloy (SMA) actuators undergoing thermally induced martensitic phase transformation under various stress levels. shape memory recoverable stress and strain of Ti-44.5at.%Ni-8at.%Cu alloys were by means of constant temperature tensile tests. Differential scanning calorimetry (DSC) was employed in order to investigate the transformation characteristics of the alloy before the tests. the results were summarized as follows. The martensite inducing stress incerased with the increasing of the Cu-contents. The fatigue life decreased with the increasing of the test load and the Cu-content. The data acquired will be very useful during the design process of an SMA NiTiCu element as a functional part of an actuator.

A Study on the Electrode Characteristics of a New High Capacity Non-Stoichiometry Zr-Based Laves Phase Alloys for Anode Materials of Ni/MH Secondary Battery

  • Lee Sang-Min;Yu Ji-Sang;Lee Ho;Lee Jai-Young
    • 전기화학회지
    • /
    • 제3권2호
    • /
    • pp.72-75
    • /
    • 2000
  • For the purpose of developing the non-stoichiometric Zr-based Laves phase alloy with higher capacity and better performance for electrochemical application, extensive work has been carried out in KAIST. After careful alloy design of $ZrMn_2-based$ hydrogen storage alloys through varing their stoichiometry while susbstituting or adding some alloying elements, the $Zr-Ti-(Lh-V-Ni)_{2.2},\;Zr-Ti-(Mn-V-Cr-Ni)_{1.8\pm0.1}$ with high capacity and better performance was developed. Consequently the $Zr-Ti-(Mn-V-Ni)_{2.2}$ alloy has a high discharge capacity of 394mAh/g and shows a high rate capability equaling to that of commercialized $AB_5$ type alloys. On the other hand, in order to develop the hydrogen storage alloy with higher discharge capacity, the hypo-stoichiometric $Zr(Mn-V-Ni)_{2-\alpha}$ alloys substituted by Ti are under developing. As the result of competitive roles of Ti and $stocihiometry({\alpha})$, the discharge capacity of $Zr-Ti-(Mn-V-Cr-Ni)_{l.8\pm0.1}$ alloys is about 400mAh/g(410 mAh/g, which shows the highest level of performance in the Zr-based alloy developed. Our sequential endeavor is improving the shortcoming of Zr-based Laves phase alloy for commercialization, i.e., poor activation property and low rate capability, etc. It is therefore believed that the commercialization of Zr-based Laves phase hydrogen storage alloy for Ni-MH rechargeable battery is in near future.

도재용착용 Ni-Cr계 합금의 이트륨 첨가물이 도재전단결합강도에 미치는 영향 (Effect of yttrium additives on the shear bond strength of porcelain fused to Ni-Cr alloy for porcelain fused metal crown)

  • 우제승;노세라;노형록;임청하;이정환
    • 대한치과기공학회지
    • /
    • 제41권2호
    • /
    • pp.71-80
    • /
    • 2019
  • Purpose: In this study, to evaluate the effect of oxide changes on the shear bond strength according to the composition of Ni-Cr alloys for porcelain fused matal crown, T-4 alloys, Zeroy alloys and Zeroy-X alloys were selected. Methods: 20 specimens were fabricated using selected Ni-Cr alloys and porcelain powders. A Ni-Cr alloy having a diameter of 5 mm and a height of 25 mm was produced and the metal surface was polished. Porcelain powder was fired on the polished metal surface to a diameter of 5 mm and a height of 3 mm. The experiment group consisted of three groups, T-4(TNA), Zeroy(ZNA) and Zeroy-X(ZXA). The fabricated specimens were mounted on a jig of a universal testing machine(UTM) and fracture strength was measured by applying a shear force at a UTM crosshead speed of 0.5 mm/min. The fracture strength was calculated as the bond strength between the porcelain and the alloy. The surface of the fractured alloy was analyzed by X-ray diffraction(XRD) and scanning electron microscopy(SEM), and the components of the oxide were measured by energy dispersive X-ray spectroscopy(EDX) line profile method. Results: In SEM, XRD and EDX analysis, yttrium tended to increase the mechanical and chemical bonding forces. The shear bond strength of ZXA group containing yttrium showed the highest value at 27.53 MPa. Conclusion: Based on the results of this study, it is considered that the yttrium-added Ni-Cr alloy is clinically acceptable in porcelain shear bond strength.

V22Ti16Zr16Ni39X7(X=Cr, Co, Fe, Mn, Al) 금속수소화물전극에 관한 연구 (A Study on the V22Ti16Zr16Ni39X7(X=Cr, Co, Fe, Mn, Al) Metal Hydride Electrodes)

  • 김정선;조원일;조병원;윤경석;김상주
    • 한국수소및신에너지학회논문집
    • /
    • 제5권1호
    • /
    • pp.1-8
    • /
    • 1994
  • Lattice structure, hydrogen absorption characteristics, discharge capacity and cycle life of $V_{22}Ti_{16}Zr_{16}Ni_{39}X_7$(X= Cr, Co, Fe, Mn, Al) alloys were investigated. The matrix phases of these alloys were the C14 Laves phase. Chromium-containing alloy had a vanadium-rich phase in addition to the Laves phase. The chromium, maganese, or aluminum-containing alloys had lower hydrogen equilibrium pressure and larger hydrogen absorption content than the cobalt or iron-containing alloys. The discharge capacities of these alloys were 270~330mAh/g. The discharge capacity according to the alloying element X decreased in the order of Mn>Cr>Co, Al)Fe. The charge/discharge cycle lives of the chromium, cobalt or iron-containing alloys were longer than those of maganese or aluminum-containing alloys due to the lower vanadium dissolution rate.

  • PDF

CORROSION BEHAVIOR OF NI-BASE ALLOYS IN SUPERCRITICAL WATER

  • Zhang, Qiang;Tang, Rui;Li, Cong;Luo, Xin;Long, Chongsheng;Yin, Kaiju
    • Nuclear Engineering and Technology
    • /
    • 제41권1호
    • /
    • pp.107-112
    • /
    • 2009
  • Corrosion of nickel-base alloys (Hastelloy C-276, Inconel 625, and Inconel X-750) in $500^{\circ}C$, 25MPa supercritical water (with 10 wppb oxygen) was investigated to evaluate the suitability of these alloys for use in supercritical water reactors. Oxide scales formed on the samples were characterized by gravimetry, scanning electron microscopy/energy dispersive spectroscopy, X-ray diffraction, and X-ray photoelectron spectroscopy. The results indicate that, during the 1000h exposure, a dense spinel oxide layer, mainly consisting of a fine Cr-rich inner layer ($NiCr_{2}O_{4}$) underneath a coarse Fe-rich outer layer ($NiFe_{2}O_{4}$), developed on each alloy. Besides general corrosion, nodular corrosion occurred on alloy 625 possibly resulting from local attack of ${\gamma}$" clusters in the matrix. The mass gains for all alloys were small, while alloy X -750 exhibited the highest oxidation rate, probably due to the absence of Mo.

Electrodeposition Characteristics and Magnetic Properties of CoFeNi Thin Film Alloys

  • Song, Jae-Song;Yoon, Do-Young;Han, Choon;Kim, Dae-Heum;Park, Dyuk-Young;Myung, No-Sang
    • 전기화학회지
    • /
    • 제5권1호
    • /
    • pp.17-20
    • /
    • 2002
  • 다양한 조성의 CoFeNi합금이 chloride bath와 sulfate bath에서 전해도금 되어졌고, 합금의 도금 특성과 자기특성이 관찰되어졌다. CoFeNi합금 박막의 전해도금에 있어서 Fe조성의 증가는 chloride bath에서보다 sulfate bath에서 빠르게 증가하였다. 전류효율은 큰 변화가 보이지 않는 chloride bath와 달리 sulfate bath에서는 $750\%$에서 $50\%$로 큰 폭으로 감소하였다. Co, Fe, Ni조성이 $80\%,\;10\%,\;10\%$되는 CoFeNi합금이 이번 실험에서 가장 우수한 연자성 재료로 평가되었으며, 그때의 Coercivity는 3 Oe이고 높은 squareness값을 보였다

급속응고된 Al81-(x+y)Si19NixCey 합금의 나노조직과 기계적 특성 (Nano Structure and Mechanical Properties of Rapidly Solidified Al81-(x+y)Si19NixCey Alloy)

  • 이태행;홍순직
    • 한국분말재료학회지
    • /
    • 제10권6호
    • /
    • pp.406-414
    • /
    • 2003
  • In order to produce good wear resistance powder metallurgy Al-Si alloys with high strength, addition of glass forming elements of Ni and Ce in $Al_{81}$Si$_{19}$ alloy was examined using SEM, TEM, tensile strength and wear testing. The solubility of Si in aluminum increased with increasing Ni and Ce contents for rapidly solidified powders. These bulk alloys consist of a mixed structure in which fine Si particles with a particle size below 500 nm and very fine A1$_3$Ni, A1$_3$Ce compounds with a particle size below 200 nm are homogeneously dispersed in aluminum matrix with a grain size below 600 nm. The tensile strength at room temperature for $Al_{81}$Si$_{19}$, $Al_{78}$Si$_{19}$Ni$_2$Ce$_{0.5}$, and $Al_{76}$Si$_{19}$Ni$_4$Ce$_1$ bulk alloys extruded at 674 K and ratio of 10 : 1 is 281,521, and 668 ㎫ respectively. Especially, $Al_{73}$Si$_{19}$Ni$_{7}$Ce$_1$ bulk alloy had a high tensile strength of 730 ㎫. These bulk alloys are good wear-resistance bel ter than commercial I/M 390-T6. Specially, attactability for counterpart is very little, about 15 times less than that of the I/M 390-T6. The structural refinement by adding glass forming elements such as Ni and Ce to hyper eutectic $Al_{81}$Si$_{19}$ alloy is concluded to be effective as a structural modification method.d.tion method.

과잉 Zr을 첨가한 MmNi4.5Mn0.5Zrx(x=0, 0.025, 0.05, 0.1) 합금의 수소용기 적용에 관한 연구 (Study on the Application for Hydrogen Storage Tank of MmNi4.5Mn0.5Zrx(x=0, 0.025, 0.05, 0.1) Alloys Containing Excess Zr)

  • 강길구;박승갑;강세선;권호영
    • 한국재료학회지
    • /
    • 제12권8호
    • /
    • pp.624-633
    • /
    • 2002
  • In order to improve the hydrogen storage capacity and the activation properties of the hydrogen storage alloys, the rare-earth metal alloy series, MmN $i_{4.5}$M $n_{0.5}$Z $r_{x}$(x=0, 0.025, 0.05, 0.1), are prepared by adding excess Zr in MmN $i_{4.5}$M $n_{0.5}$ alloy. The various parts in hydrogen storage vessel consisted of copper pipes reached the setting temperature within 4~5 minutes after heat addition, which indicated that storage vessel had a good heat conductivity required in application. The performance test on storage vessel filled with rare-earth metal alloys of 1000 gr was also conducted after hydrogen charging for 10 min at $18^{\circ}C$ under 10 atm. It showed that the average capacity of discharged hydrogen volume was found to be for $MmNi_{4.5}$ $Mn_{0.5}$ and $MmNi_{4.5}$ $Mn_{x}$ 0.5/$Zr_{samples}$ indicated that the released amount of hydrogen for this $AB_{5}$ type alloys was more than 92 % of theoretic value, and also it was found that the optimum discharging temperature for obtaining an appropriate pressure of 3 atm was determined to be $V^{\circ}C$ for $MmNi_{4.5}$ $Mn_{0.5}$$Zr_{x}$(x=0, 0.025, 0.05, 0.1) hydrogen storage alloys. The released amount of these hydrogen storage samples was 125 $\ell$ , 122.4 $\ell$ and 108.15 $\ell$/kg for $MmNi_{4.5}$ $Mn_{0.5}$ $Zr_{0.025}$ $MmNi_{4.5}$M $n_{0.5}$Z $r_{0.05}$, and MmN $i_{4.5}$ Mn_0.5$Zr_{0}$, at $70^{\circ}C$ respectively. Amount of the 2nd phases increase with increase on Zr contents in $MmNi_{4.5}$$Mn_{0.5}$ $Zr_{ 0.1}$/ alloy. This phenomenon indicates that$ ZrNi_3$ in $MmNi_{4.5}$ $Mn_{0.5}$ $Zr_{x}$ / phase, which shows the maximum storage capacity and the strong resistance to intrinsic degradation, is considered as a proper alloy for hydrogen storage. As the Zr contents increase, the activation time and the plateau pressure decreases and sloping of the plateau pressure increases.creases.eases.s.